Your search resulted in 1847 documents. Displaying 25 entries per page.
Laboratory Evaluation of the Formosan Subterranean Termite Resistance of Borate-treated Rubberwood Chipboard
2004 - IRG/WP 04-30359
Both no-choice and two-choice 4-week AWPA laboratory tests were performed to evaluate the resistance of borate-treated rubberwood (Hevea brasiliensis) chipboard prepared from a commercial mill run, against the Formosan subterranean termite Coptotermes formosanus. Boric acid (technical granular) was incorporated into the boards during manufacture to achieve loadings of 1.0% or 1.1% boric acid equiv...
A H H Wong, J K Grace
A comparison between high and conventional incision densities for improving preservative treatment of Douglas-fir heartwood lumber
1993 - IRG/WP 93-40009
Incising is required for the preservative treatment of most wood species from the western United States; however, there is considerable debate about the density of incisions required to achieve adequate treatment. Previous studies have shown that the incision effect on treatment is relatively narrow, suggesting that incision densities should be significantly increased over current practices and st...
S T Lebow, J J Morrell
IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 14: Report of sixth inspection (60 months) in Australia
1983 - IRG/WP 499
The IRG/COIPM International Marine Test was installed at Goat Island, Sydney Harbour, in December, 1977. The results of inspections made at 6, 12, 24, 36 and 48 months have previously been reported. This document records the data obtained on the 16.12.82, i.e. after 60 months exposure, at which time only 4 of the test frames remained in test. The surface water temperature at the time of inspection...
L J Cookson, J E Barnacle
A comparative study of some anti-splitting devices, using Eucalyptus saligna and hybrids of Eucalyptus saligna X Eucalyptus spp poles
1983 - IRG/WP 3251
It is commom for some Brazilian wood pole users to require devices such as banding steel, to avoid or reduce splits at the end of Eucalyptus treated poles. On other hand users and manufacturers do not have data to confirm the effectiveness of the banding steel types normally used such as galvanized "Steel-Belt" and galvanized "Wire-Belt". For this reason a comparative study was carried out includi...
F C Geraldo, J A C Sodré
Results on field stake tests against termite – Maximum for 8 years examination at Kumamoto in Japan
2003 - IRG/WP 03-10463
Various preservative treated or modified wood and charcoal painting stakes were tested in field, maximum for eight years in Kumamoto, distributed two main termite species, Coptotermes formosanus and Reticulitermes speratus. After two years in field, untreated sapwood of sugi (Cryptomeria japonica) were observed severe attacks by termites, but the preservative treated stakes were observed no signif...
K Suzuki
Thermal modification of non-durable wood species 2. Improved wood properties of thermal treated wood
1998 - IRG/WP 98-40124
Properties of wood treated in a new heat-treatment process called the PLATO-process have been studied. Several wood species have been treated using this new thermal modification process using a range of process conditions (mainly time and temperature). In this study the characteristics of the treated wood were determined using samples from whole planks treated on pilot plant scale. The modified ch...
B F Tjeerdsma, M J Boonstra, H Militz
Effect of humidity fluctuations on mould growth on pine wood
1989 - IRG/WP 1412
Most studies on mould development on wood material have been made at constant moisture conditions during the experimental period. As a consequence of such studies, a maximum permittable humidity level to avoid mould problems in wood constructions has been recommended. In the practical situation, the constructions are seldom subject to constant humidity or temperature. In the present paper, we repo...
J Bjurman
Window test. Direct testing of wood resistance to decay: A study of its fitness, its reliability and its accelerating factor
1984 - IRG/WP 2219
This is the results of an experiment using the window-test specimens, exposing the specimens to three different types of testing procedure: 1. Natural infestation in the open air; 2. Artificial infestation and exposure in the open air; 3. Artificial infestation in a green-house. The results show good similiraties of the three parallel tests in term of decay, and assess the reliability of the windo...
G R Y Déon, L N Trong
Formation of polychlorinated dibenzo-p-dioxins (PCDD) and polychlorinated dibenzofurans (PCDF) during the combustion of impregnated wood
1995 - IRG/WP 95-50040-19
Wood waste and industrial wood residues often contain various preservatives. The waste management for these residuals can be recycling, deposition or combustion. Among the three possibilities, combustion seems to be the most efficient way of disposal. To obtain detailed information about emissions of organic compounds with environmental impact, especially polychlorinated dibenzo-p-dioxins (PCDD) a...
T Salthammer, H Klipp, R-D Peek
Colonisation and detection of New Zealand sapstain fungi
2000 - IRG/WP 00-10329
Sapstain is the bluish black discolouration in logs and timber caused in New Zealand by Sphaeropsis sapinea (Diploida pinea) and more than twenty different species of the Ophiostomataceae Family. Laboratory and field trials were conducted by inoculating radiata pine to establish staining colour and extent of colonisation with various New Zealand sapstaining fungal species. Colonisation patterns, c...
J M Thwaites, R L Farrell
Controlled envelope treatments of Pinus sapwood, achieved by modifications to impregnation process and carrier solvents
2003 - IRG/WP 03-40258
Specimens of slash pine or radiata pine were treated to a target retention of 0.02% m/m permethrin with conventional light organic solvent fluids or with oil-modified fluids (Tanalith® T). Best achievable envelopes from LOSP fluids were poorly controlled, penetrating not only the target outer 0-5 mm zone (mean 0.019%, RSD 28%), but also breaking through into the 5-10 mm zone (mean 0.013%, RSD 37%...
M J Kennedy, P R S Cobham
A field test with anti-stain chemicals on sawn pine timber in Brazil
1989 - IRG/WP 3513
Field tests were carried out in São Paulo State - Brazil, to evaluate pre-treatment formulations of O-Phenyl-Phenol (OPP) based products. The Sodium Pentachlorophenate solution was used as a reference formulation. The treated test blocks were stacked in a covered shed, and in an uncovered place for air drying. The evaluation was done by measuring the percentage of stained surface on each test blo...
M B B Monteiro, S Brazolin
Effect of point of preservative addition on the mechanical and physical properties of strandboard treated with Tanalith 3485
2000 - IRG/WP 00-40152
Preservative has been added to a PF bonded strandboard at various different stages in the manufacturing cycle and the physical and mechanical properties of the boards have been evaluated (modulus of elasticity, modulus of rupture, thickness swelling, water absorption, internal bond strength, and shear strength). Preservative addition has been examined at five different stages namely green strand d...
G J Goroyias, M D C Hale
Wood decay of Pinus sylvestris L. and Fagus sylvatica L. by marine fungi. Part 2
1991 - IRG/WP 1471
The water-logged wood conservation requires a good knowledge of the wood decay organims which produce the degradation. Previous conducted studies (ESCORIAL, TROYA, GARCIA DE LOS RIOS, 1990) have shown that the incubation times normally used for in vitro laboratory tests are not sufficients for a significant wood degradation. This has been the reason why the aim of this work was the study of such d...
M T De Troya, A M Navarrete, M C Escorial
Organic nitrogen in wood: Growth substrates for a sapstain fungus
1993 - IRG/WP 93-10019
The nitrogen content of mature wood from lodgepole pine was 0.046% as determined by micro-Kjeldahl. Low molecular weight proteins between 14 and 21 kDa were identified in mature wood, branch wood and sap pressed from wood chips. Amino acids were quantified in acid-hydrolyzed wood samples and accounted for between 19 and 35% of the nitrogen in wood. The sapstaining ascomycete Ophiostoma piceae stra...
L D Abraham, C Breuil
Laboratory Evaluation and Field Trial of Chlorothalonil and Copper-based Preservatives and Leaching Performance of Copper in Copper Treated Wood
2002 - IRG/WP 02-30279
Soil block test and field trial of some Chinese plantation wood species pine and poplar treated with chlorothalonil formulations and copper-based preservatives such as ACQ-B and copper citrate (CC) were conducted. The results of soil block test indicated that chlorothalonil formulations and ACQ-B as well as CC are very effective for controlling the 2 fungi species Corious versicolor and Poria plac...
Mingliang Jiang, Ping Wang, Chungen Piao, Zhaobang Li, Quan Lu, Lei Liu
Reduction of kiln brown stain in radiata pine lumber after log fumigation with methyl bromide
1997 - IRG/WP 97-30129
Methyl bromide fumigation of freshly felled radiata pine log sections effectively killed living cells in parenchyma to at least 75mm into sapwood. Lumber cut from logs (fumigated and control) stored 1 month outdoors (dry) showed slightly reduced brown stain when kiln dried at conventional temperatures. A more dramatic reduction and elimination of brown stain was noted in lumber cut from fumigated ...
E Schmidt, M E Hedley, D R Page, D Cross
Diffusion modeling of inorganic wood preservative leaching in service
2005 - IRG/WP 05-50224-5
To evaluate the potential environmental and health implications of leaching of inorganic wood preservatives in service under different conditions, there is a need for a predictive model that provides estimates of the rate and extent of leaching over a wide range of product dimensions and exposure conditions. In this paper, we show that the leaching behavior of inorganic preservative components fr...
L Waldron, P A Cooper, Y T Ung
Accelerated termicidal performance data for new water-based copper linoleate formulations
1996 - IRG/WP 96-30104
An organic solvent based copper linoleate (Culin) has proved itself as an effective wood preservative in long term field trials in South Africa over a period of 30 years. Whilst the organic solvent based product offers good wood preservative performance, primary industrial interest has been in an emulsified version of the product. The objective of this study was to evaluate the influence of two di...
D Conradie, P Turner
Variable tolerance of Ophiostoma spp. and Diplodia pinea to commercial antisapstain products
1998 - IRG/WP 98-10266
A recent survey of the occurrence of sapstain fungi in New Zealand, conducted at The University of Waikato, provided the opportunity to examine fungicidal tolerance amongst new isolates. It also enabled a comparison of tolerance amongst new isolates with those used in routine antisapstain screening trials at Forest Research.
A rapid antisapstain laboratory disc trial was used to determine the ext...
D R Eden, C M Chittenden, B Kreber, J G Van der Waals, R N Wakeling, R L Farrell, T Harrington
Investigation of extracellular mucilaginous material in some wood decay fungi
1996 - IRG/WP 96-10188
The external morphology of the extracellular mucilagenous material (ECM) produced by Coriolus versicolor and Coniophora puteana during colonization of Scots pine and beech was studies using SEM. Specimens were examined in the frozen hydrated, freeze-dried and critical point dried state. All technics produced artefacts but the ECM was best preserved when examined the frozen hydated state. Critical ...
A R Abu, D J Dickinson, R J Murphy
Remedial treatment of creosoted railway sleepers of redwood by selective application of boric acid
1980 - IRG/WP 3134
An ideal preservative for remedial treatment must primarily be characterized by two requirements. First, it must have an ability to diffuse and distribut evenly into the wood and secondly, it must be fixed properly so that it does not leach out too fast. However, these two characteristics conflict with each other, and the choice of preservative must of necessity be a compromise. Wood preservatives...
C Bechgaard, L Borup, B Henningsson, J Jermer
Cyclic delamination analysis of preservative-treated wood/FRP interfaces
2002 - IRG/WP 02-40244
Wood preservative chemicals can interfere with adhesive properties when bonding wood laminates or wood/FRP (Fiber Reinforced Polymer) laminate composites. In this work we studied the effects of various wood preservative treatments, and pre- and post-treatment on wood/wood and wood/FRP bond durability using a severe cyclic delamination test (ASTM D-2559). Pre-treatment of individual laminates with ...
C Tascioglu, B Goodell, R Lopez-Anido
Remediation of a site contaminated with creosote and CCA - a case study
1998 - IRG/WP 98-50101-12
Over sixty years of wood preservation activity conducted by ImpregNor at Ilseng, Norway, has caused serious contamination of the soil. High concentrations of creosote have been found at two separate sites, one in connection to the creosote wood preservation plant, and one further downstream were residues from the creosote preservation have been deposited. High levels of chromium, copper and arseni...
T Rødsand, K Hellum, H Lillemaehlum
Estimation of mycelial biomass by determination of the ergosterol content of wood decayed by Coniophora puteana and Fomes fomentarius
1989 - IRG/WP 1415
The mycelial biomass of fungi decomposing wood materials may be estimated by the use of an ergosterol assay technique.ln decay tests, essentially according to EN 113, estimates made by HPLC analyses on wood decayed by Coniophora puteana and Fomes fomentarius show the increase in biomass in the wood blocks. The ergosterol contents were correlated with dry weight loss determinations. Degradation of ...
K Nilsson, J Bjurman