Changes in pore structure and cell wall volume in wood decayed by brown- and white-rot fungi
1991 - IRG/WP 1501
Sweetgum (Liquidambar styraciflua L.) wood blocks were decayed by Postia (=Poria) placenta or Phanerochaete chrysosporium in soil-block cultures. Decay was terminated at various weight losses, and the pore volumes available to probes of various molecular weight and diameter were determined by the solute exclusion technique (Stone, J.E. and A.M. Scallan. 1968. Cellulose Chem. Technol. 2, 343-358.)....
D S Flournoy


Investigation of temperature effect on fixation of Celcure preservative (ACC) in beech (Fagus orientalis)
2001 - IRG/WP 01-40200
In this research, the fixation speed of Celcure 2% (ACC) preservative salt, under temperature of 17°C, 27°C and 50°C, on intact and stained wood specimens of beech was investigated. For this purpose, blocks of wood with 5x5x7 cm dimensions were prepared and saturated with 2% ACC concentration by full-cell process. The specimens were put in three incubators at the above-mentioned temperatures. F...
A Karimi, M Ghorbani


Accelerated decay tests to investigate postulated effects of tannins on CCA efficacy in wood
1988 - IRG/WP 3497
Five groups of blocks (10 x 10 x 5 mm³) viz., Pinus patula, Pinus patula impregnated to 4% (w/w) tannin; Eucalyptus grandis, Eucalyptus grandis with natural tannins extracted; and extracted Eucalyptus grandis with tannins returned as above; were prepared. Blocks from each group were then treated to 0, 5, 10 and 15 kg/m³ CCA and challenged in four 15-week decay tests, viz., soil burial, and expos...
U L Scherer, A A W Baecker


Soft rot decay of Belian (Eusideroxylon zwageri) wood
1995 - IRG/WP 95-10119
The heartwood of Belian (Eusideroxylon zwageri), an East Malaysian timber species, is naturally durable due to its certain unique anatomical features and high content of extractives. The timber can tolerate years of exposure to hazardous conditions in ground contact and other situations without any significant loss in its strength. A few Belian transmission poles sampled from one locality in Saraw...
A H H Wong, A P Singh


Comparison of the effects of borate, germanate and tellurate on fungal growth and wood decay
1992 - IRG/WP 92-1533
The tetra-hydroxy borate ion is known to undergo complexation with polyols and has been shown to inhibit dehydrogenase enzymes in this way. It has been previously suggested that this complexation is responsible for the inhibition of fungal growth and the protection of boron treated timber. Other ions that have the ability to complex with polyols have also been shown to inhibit dehydrogenase activi...
J D Lloyd, D J Dickinson


An investigation of the effects of pre-steaming on the treatment of sawn spruce timber with Celcure A, a copper/chrome/arsenic preservative
1981 - IRG/WP 3180
Difficulties in the treatment of spruce using standard vacuum/pressure techniques with both water-borne and organic solvent preservatives are well known. The growth characteristics of spruces (Picea spp) make them attractive candidates for forestry schemes. In 1975 the UK Forestry Commission had about 400 000 hectares, about 20% of total UK forest area, planted with Sitka spruce (Picea sitchensis)...
C R Coggins


Effects of fixation conditions and seawater on leaching of wood treated with marine retention CCA
1997 - IRG/WP 97-50088
The effect of post-treatment conditioning temperature and humidity on leaching of chromated copper arsenate (CCA) was compared in seawater and deionized water. Southern pine cubes treated to 40 kg/m3 CCA were stored at 2° C and 82% relative humidity (RH), 24° C and 65% RH, or 32° C and 30% RH for 3, 10, or 17 days. Cubes were then leached in deionized water or artificial seawater. The rate of l...
S T Lebow


Effects of seed origin and site on both wood density and longitudinal fluid uptake of Sitka spruce (Picea sitchensis (Bong.) Carr.) with height in the tree grown in the United Kingdom
2002 - IRG/WP 02-40226
The variation in density and longitudinal fluid uptake was investigated in short specimens of wood taken from eight seed origins of Sitka spruce trees grown at two sites in the UK. Five trees of each seed origin at each site were sampled at three heights (1, 2 and 3 m above ground level). The density of the samples decreased with increasing height within the stem. This corresponded with increasin...
I Usta, M D C Hale


Preliminary studies to assess the effects of aeration and lowered humidity on the decay capacity, growth and survival of the dry rot fungus Serpula lacrymans (Wulf ex. Fr.)
1997 - IRG/WP 97-10208
Novel microcosms were used to test separately the effects of aeration and humidity on the decay capacity, linear spread and survival of Serpula lacrymans. The application of a pumped air supply resulted in an effective cessation of fungal activity when all but the lowest of the air flow rates was used. Furthermore, the lowest air flow rate caused marked growth tropisms away from the stress. In sep...
G A Low, J W Palfreyman, N A White, H J Staines, A Bruce


Microbial decay of an archaeological wood
1994 - IRG/WP 94-10053
A light and transmission electron microscopic investigation of an archaeological wood was undertaken to determine the cause of its deterioration. The wood came from a bulwark constructed in early 1100 in the lake Tingstäde Träsk on the island Gotland in Sweden. The samples of the wood, which was identified as Pinus sylvestris, were taken from a depth of 0.85 m below the bottom level. The wood wa...
A P Singh, T Nilsson, G F Daniel


The residual effects of remedial timber treatments on bats
1986 - IRG/WP 1281
By means of controlled laboratory experiments it was established that timber treatment fluids containing g-HCH and pentachlorophenol (PCP) and used according to manufacturers recommendations rapidly cause the death of pipistrelle bats roosting in contact with timber treated between six weeks and 14 months previously. The chemicals responsible are presumably ingested when the bats groom their fur a...
P A Racey, S M Swift


Effects of alkali treatment on some mechanical and chemical properties of creosote treated oaks
1991 - IRG/WP 2366
To date, there is a lack of information on the effects of chemical treatment on the performance of creosote preservative treated oak sleepers. This factorial experiment was designed to analyze three main effects: species (Quercus alba and Quercus rubra) creosote treatment (treated and untreated), and alkali (NaOH) soaking (0, 1, and 10 percent). The modulus of elasticity (MOE) and fiber stress at ...
P Chow, A J Reinschmidt, E J Barenberg, L C Chang


How predictive are laboratory experiments for assessing the effects of chitin synthesis inhibitors (CSI) on field colonies of terrnites? - A comparison of laboratory and field data from Australian mound-building species of termit
1996 - IRG/WP 96-10143
A singular advantage of using mound building species of termite is their directly accessible nest. This allows evaluation of control methods by accurate assessment of the effects at the colony level. The mound building species Coptotermes acinaciformis (Froggatt) and Nasutitermes exitiosus (Hill) were used to test the CSI, hexaflumuron, in laboratory and field trials. Laboratory results showed tha...
M Lenz, P V Gleeson, L R Miller, H M Abbey


Effect of treating process on efficacy of CCA in a laboratory decay test
1990 - IRG/WP 3628
Test samples of Pinus radiata sapwood measuring 40x40x500 mm³ were treated with a range of concentrations of the copper-chrome-arsenate (CCA) formulation "Tanalith C" using Rueping (empty cell), Lowry (empty cell) and Bethell (full cell) treatment processes. Samples were then reduced to 40x40x7 mm³ test blocks and exposed to the decay fungus Coniophora puteana using an agar/block technique. Repl...
M E Hedley, K Nasheri, J G Van der Waals


Effects of drying processes on termite feeding behaviour against Japanese larch wood
2001 - IRG/WP 01-10390
We investigated the effects of current drying schedules for larch lumbers on the termite feedings. Thermal analyses were also conducted to investigate degradation of wood components. Choice feeding tests showed specimens dried under high-temperature schedules were evidently susceptible against termite attacks. These schedules produced the feeding-attractants, which were suggested by the TGA result...
S Doi, Y Kurimoto, H Takiuchi, M Aoyama


Effect of microfibril orientation of bamboo cell wall on soft rot penetration hyphae
1994 - IRG/WP 94-10087
The effect of microfibrillar orientation of bamboo (Phyllostachys virideglaucescence) cell wall on the development of soft rot (Chaetomium globosum) penetration hyphae was investigated. It was found that the soft rot penetration hyphae normally followed the microfibril angle of the cell wall. Bamboo cell walls have alternating broad and narrow lamellae with different microfibrillar angles. The mic...
O Sulaiman, R J Murphy


Effects of two wood preservatives and one water repellant on the settlement of fouling communities in a tropical marine environment
2002 - IRG/WP 02-30293
Observations made on recruitment of fouling organisms on treated panels exposed at an Indian harbour, Krishnapatnam on the east coast (Lat: 13028’ to 13059’ N; Long: 80010’ to 80016’ E) during November, 1997 to October, 1999 are reported and compared with fouling communities on control panels. Wooden panels of Erythrina variegata, Paraserianthus falcataria, Tetrameles nudiflora an...
B Tarakanadha, K S Rao


Estimation of oral toxicity of boron as a bait toxicant and the trophallactic effects between individual members of termite colonies.
2003 - IRG/WP 03-10495
In recent years, because of the favourable environmental characteristics of boron, researchers in the wood preservation industries have refocussed on the use of boron as a major wood preservative against wood-destroying insects. Currently the greatest use of boron compounds is in remedial treatments. Boron has been found to have slow-acting toxicity against subterranean termites. Because of thi...
B M Ahmed


Comparative studies on the species effects of wood preservatives
1989 - IRG/WP 3521
For the examination of the resistance against fungal attack, wood blocks of 3 softwood species were treated with CCA (type 3), CFK, AAC and IF-1000 independently. The wood blocks were exposed to the fungal decay with Tyromyces palustris. The degradation of the wood blocks treated with these preservatives was quite widely different among wood species examined in this study. Hem-fir treated with CCA...
K Yamamoto, S Matsuoka


Multiple-Phase Pressure (MPP) Process: Pilot plant trials for disposal of kickback using reverse osmosis membrane filtration
2001 - IRG/WP 01-40202
The MPP Process (a one-stage CCA treatment and accelerated fixation process) generates ~ 250 litres of kickback per cubic metre of timber treated. Composition of kickback is mainly wood sugars and traces of copper, chromium and arsenic. In pilot plant scale trials, MPP process kickback was filtered through a Reverse Osmosis (RO) membrane of a type found from earlier small-scale trials to be the mo...
H Pearson, G Durbin, M E Hedley


Degradation features of waterlogged archaeological compression wood
1998 - IRG/WP 98-10258
The degradation characteristics of waterlogged archaeological compression wood excavated in South Korea were examined by transmission electron microscopy (TEM) and confocal laser scanning microscopy (CLSM). Degradation of Pinus compression wood occurred mainly in the inner part of S2 layer. In contrast, the outer part of S2 layer remained relatively intact. CLSM and TEM showed the erosion type of ...
Yoon Soo Kim, A P Singh


A study on the pressure impregnation of Eucalyptus globulus fence-posts with CCA preservatives. Part 2
1989 - IRG/WP 3514
This paper describes the second part of a study on pressure impregnation of Eucalyptus globulus fence-posts with CCA preservatives presented at the IRG 19th Meeting. Fence-posts of three diameter classes, were treated, considering only one treatment schedule. The results show possibility of vacuum-pressure impregnation of blue gum fence-posts, with diameter less than 9 cm, though mainly by longitu...
L Nunes, D De Sousa Castro Reimão


Quantification of wood decay effects by HPLC analysis
1992 - IRG/WP 92-1576
The present work quantified the effects of the white rot basidiomycetes Coriolus versicolor and Phanaerochaete chrysosporium, and also those of the brown rot fungi Coniophora puteana and Lentinus lepideus, on Pinus patula and Eucalyptus grandis. Wood colonisation was quantified by Kjeldahl nitrogen determinations converted to biomass assays, and degradation was quantified by weight losses produced...
V Singh, M Tarin, G D Shelver, A A W Baecker


Soft rot
1978 - IRG/WP 179
Soft rot decay of treated wood is examined with special reference to hardwoods treated with CCA. Factors which adversely affect the chances of protection of hardwoods against soft rot are discussed. The ratio of the volume of the fibre cell wall to the volume of the fibre lumen is presented as a major factor influencing final preservative concentration in the fibre cell wall, the major strength co...
C R Levy


Diffuse cavity formation in soft rot of pine
1992 - IRG/WP 92-1541
A new type of soft rot of southern pine longitudinal tracheids is described. In this type, soft rot cavities form by diffuse degradation of the S2 cell wall layer by hyphae growing within the cell wall. Erosion is diffuse and irregular as opposed to the restricted, periodic erosion typical of type 1 soft rot cavity formation. Proboscis hyphae remain small (diameter 0.6 to 0.8 µm) and rapidly auto...