Degradation features of waterlogged archaeological compression wood
1998 - IRG/WP 98-10258
The degradation characteristics of waterlogged archaeological compression wood excavated in South Korea were examined by transmission electron microscopy (TEM) and confocal laser scanning microscopy (CLSM). Degradation of Pinus compression wood occurred mainly in the inner part of S2 layer. In contrast, the outer part of S2 layer remained relatively intact. CLSM and TEM showed the erosion type of ...
Yoon Soo Kim, A P Singh


Ponding of radiata pine (Pinus radiata) - 1. The effect of bacteria on wood
1998 - IRG/WP 98-10265
Radiata pine (Pinus radiata) wood panels which had been ponded for periods ranging from 2 to 12 weeks were examined by light microscopy, confocal laser scanning microscopy (CLSM), scanning electron microscopy (SEM) and transmission electron microscopy (TEM) for bacterial colonisation of wood and degradation of pit membranes. After 2 weeks of ponding bacteria colonised the outer few cells of wood, ...
A P Singh, Y S Kim, U Schmitt, B S Dawson


Mold and stain fungi associated with Radiata pine logs imported from New Zealand
2000 - IRG/WP 00-10346
The Korean sawmills have recently realized the importance of prevention of fungal discoloration due to increased losses in revenue. Before establishing integrated control strategies of fungal discoloration, more complete knowledge about causal organisms is needed. As a first step, we initiated a through survey of mold and stain fungi colonized commercially important softwood species (Pinus densifl...
Jae-Jin Kim, Gyu-Hyeok Kim


Immuno-electron microscopic localization of extracellular metabolites in spruce wood decayed by brown-rot fungus Postia placenta
1990 - IRG/WP 1441
Degradation by Postia placenta in spruce and birch wood was shown to occur not only in the wood cell wall but also in the middle lamellae region. Middle lamellae was often found to be degraded along the centerline so that cells could separate along this line. Extracellular membrane structures were found surrounding the hyphae and this matrix labelled positively with antisera produced to Postia pla...
Y S Kim, B Goodell, J Jellison


Ponding of radiata pine (Pinus radiata) - 2. The effect of ponding on coating penetration into wood
1998 - IRG/WP 98-10249
Radiata pine (Pinus radiata) wood panels which had been ponded for periods ranging from 2 to 12 weeks, dried and subsequently coated with a primer and examined by light microscopy after staining sections with Sudan IV to enhance the contrast of the primer material. A correlation between the extent of ponding and the extent of coating penetration into wood was observed. The coating penetration var...
A P Singh, S S Gallagher, U Schmitt, B S Dawson, Yoon Soo Kim


Solid state NMR study on pine wood degraded by brown rot fungus Gloeophyllum trabeum
1994 - IRG/WP 94-10067
Blocks of Pinus koraiensis wood were degraded by Gloeophyllum trabeum and examined by solid-state 13C NMR spectroscopy. Chemical compositions were estimated from relative signal aras. There was no evidence for preferential degradation of the noncrystalline cellulose which accounted for about 4% by weight of the wood. Loss of partly ordered cellulose on crystal surfaces exceeded the loss of crystal...
Yoon Soo Kim, R Newman


Database of sapstain fungi affecting lumber, logs and trees
2004 - IRG/WP 04-10534
Sapstain fungi discolour lumber, logs and tree sapwood and are often mistaken for moulds, which cause a superficial discoloration. Stained wood has a lower market value. Further, because stained wood products can potentially carry pathogenic fungi, such products may be refused by importing countries. Addressing these issues involves developing ways for accurately identifying staining fungi, docume...
S Lee, F de Giuli Vallverdu, S Alamouti, Jae-Jin Kim, A Uzunovic, C Breuil


Micromorphological and chemical changes of archaeological woods from wrecked ship's timbers
1987 - IRG/WP 4136
Micromorphological and chemical alterations of sea-waterlogged woods obtained from the ship-wrecked materials which had been submerged in Yellow Sea for over 700 years were investigated. The woods were deteriorated in varying degrees by marine organisms depending on species and parts of the woods. Under the light and scanning electron microscope the morphological characteristics of deteriorated wo...
Y S Kim


Measurement of electrokinetic potential to evaluate adsorption of quaternary ammonium salt
1991 - IRG/WP 3672
Measurement of z-potential in the wood treated with preservatives is suggested as a method for determination of the adsorption of preservative to wood. It has been found that measurement of z-potential of wood treated with quaternary ammonium salt type preservatives can be a useful method to determine the adsorptives phenomena of preservatives and by which there is a remarkable differences in the ...
Yeong Suk Kim


Fixation and leaching characteristics of Douglas-fir treated with CCA-C
2004 - IRG/WP 04-50213
Fixation and leaching characteristics of CCA-treated Douglas-fir was evaluated using the expressate method and the AWPA E11-97 leaching procedure. CCA fixation, as monitored by the chromium reduction, was much faster in heartwood than in sapwood; however, copper and arsenic fixation in heartwood appeared to be incomplete regardless of the extension of fixation time. This poor fixation of copper a...
Gyu-Hyeok Kim, Yun-Sang Song, Dong-heub Lee


Thermal decomposition behavior of CCA-treated wood for safe disposal and the safe recovery of heavy metals through pyrolysis
2006 - IRG/WP 06-50238
If we could estimate the chemical changes in heavy metals by temperature in chromated copper arsenate (CCA)-treated wood during pyrolysis, it is expected that we could solve the environmental problems of heavy metals, which may occur during pyrolysis, and therefore, the thermal decomposition behavior of effective elements of CCA-treated wood was examined to find a safe disposal method. First, CCA-...
Dong Won Son, Dong-heub Lee, Sun-hae Cheon, Myung Jae Lee


Development of preservative treatment method using sub and super critical carbon dioxide
2007 - IRG/WP 07-40385
Significant efforts have been devoted for developing biocide impregnation method into wood materials using supercritical fluid. Developing better understandings of fluid phase and its effect on treatment results would facilitate a more rational development of supercritical fluid (SCF) impregnation. In this project, the preservative treatabilities under super- and sub-critical fluid conditions we...
Myeung-Won Cho, Sung-Mo Kang, Gyu-Hyeok Kim


Effect of steam on fixation of Cu-amine preservative treated wood
2008 - IRG/WP 08-50251
The rates of copper fixation in copper amine preservative treated wood were investigated with different fixation conditions (20° with drying and 50° without drying) and post-steaming. We also measured the degree of leaching for other biocide components (azoles, quatz, and Cu-HDO). Treatments conditioned at 20° with drying required 50 days or more to fix in woods. While copper was stabilized i...
Sung-Mo Kang, In-Yong Hwang, Suk-Kuwon Kim


Improved analysis of field test data related to service life prediction of tropical wood species
2010 - IRG/WP 10-20458
Long field trials of wood in ground contact give valuable data on the natural durability of the material. The European Standard EN 350 gives guidance on how to perform these durability classification, but is limited to the use of averages of in-service life of a set of specimens compared to a reference set. Starting from a database of visual assessment of field stake testing, it is possible to obt...
J Van den Bulcke, A Wong, Ling Wang Choon, Yoon Soo Kim, J Van Acker


Preventing decay in termite monitoring stations
2010 - IRG/WP 10-30546
In-ground monitoring stations and termite baits are widely used in the southern United States with the intent of detecting and eradicating subterranean termite activity near buildings. These stations comprise a wood (or other cellulose material) substrate (monitor) and perhaps a termiticidal toxicant (bait) held in a plastic cage that allows for both easy examination and access by termites. The us...
A M Taylor, Jae-Woo Kim, S Duarte, L Nunes, J D Lloyd


Optimization of oxalic acid production for bioleaching of metal components from CCA-treated wood by an unknown Polyporales sp. KUC8959
2010 - IRG/WP 10-50266
A brown-rot fungus, an unknown Polyporales sp. KUC8959, has recently been identified and proven as a prominent fungal species for bioremediation of CCA-treated wood wastes in our Lab. The fungus produced a larger amount of oxalic acid than other fungi tested, and removed 90 % or more of chromium, copper and arsenic from CCA-treated wood sawdust through bioleaching process. The bioleaching process ...
Yong-Seok Choi, Min-Ji Kim, Jae-Jin Kim, Gyu-Hyeok Kim


Fungal biodegradation of CCA-treated wood wastes
2011 - IRG/WP 10-50276
Fungal biodegradation could be employed as a pretreatment method to alleviate problems caused by landfill disposal of CCA-treated wood wastes (e.g. a shortage of landfill space and a release of leacheate). It could be used to decrease the volume of waste and to remove metals from waste simultaneously. We have screened hundreds of decay fungi, including fungi isolated from CCA-treated wood in servi...
Gyu-Hyeok Kim, Yong-Seok Choi, Jae-Jin Kim


Ambient-temperature borate dip-diffusion treatment of green railroad crossties
2011 - IRG/WP 11-40556
In the USA, borates are increasingly being applied prior to air seasoning and creosote treatment of railroad ties (railway sleepers). Borates are typically applied to green ties by vacuum pressure application at 1 to 10% disodium octaborate tetrahydrate (DOT) concentration or by traditional dip-diffusion treatments at elevated temperatures. Higher temperatures are used to maintain the 30 to 50% so...
Jae-Woo Kim, A M Taylor, C Köse


Decay factors in termite in-ground monitoring stations
2012 - IRG/WP 12-10775
Subterranean termites are serious pests of wood in service in much of the world. One of the most common techniques for monitoring and controlling termites is the use of in-ground monitoring stations which comprise a wood or other cellulosic material monitor (cellulosic matrix) and/or a termiticide bait held in a open plastic holder so facilitates examination and the termite access. Wood and other ...
S Duarte, A M Taylor, Jae-Woo Kim, J D Lloyd, M Duarte, L Nunes


Micromorphological and chemical characteristics of waterlogged archaeological bamboos excavated from the Yellow Sea
2012 - IRG/WP 12-10785
Bamboos have widely used as documentation material in Far Eastern countries such China, Korea and Japan. In particular, bamboo slips as documentation material were extensively used even after the wide spread of paper in those countries. A large number of bamboo slips have been excavated from the shipwreck since 2009 in Korea. Understanding the cause of deterioration of ancient bamboos is crucial f...
Mi Young Cha, Yoon Soo Kim


Fire performance of the wood treated with retardant
2012 - IRG/WP 12-40591
To prepare the eco-friendly fire retardant wood, Japanese red pine (Pinus Densiflora), hemlock (Tsuga Heterophylla), and radiate pine (Pinus Radiata) were treated with inorganic chemicals, such as sodium silicate, ammonium phosphate, and ammonium boric acid. Different combination and concentration of those chemicals were injected by pressure treatment methods. The electron-beam treatment was used ...
Jong In Kim, Mi-ran kang, Sang bum Park, Dong won Son


Fixation and leaching characteristics of Malaysian tropical hardwoods treated with CCA-C
2012 - IRG/WP 12-50289
The fixation and leaching characteristics of 8 Malaysian tropical hardwood (MTH) species treated with chromated copper arsenate (CCA-C) wood preservative were examined. The species evaluated were Acacia (Acacia mangium), Bintangor (Calophyllum sp.), Geronggang (Cratoxylon arborescens), Medang (Litsea sp.), Meranti rambai daun (Shorea acuminata), Putat (Planchonia sp.), Ramin (Gonystylus sp.) and S...
S Salim, S Shahomlail, Z Ashaari, Yong-Seok Choi, Gyu-Hyeok Kim


Developing Analytical Methods for Determination of Quaternary Ammonium Compounds (DDAC) using HPLC and HPLC-MS (Application to treating solution and preservatives treated wood)
2013 - IRG/WP 13-20516
Korea preservative treating industry has mainly used alkaline copper quaternary (ACQ) expected over 80% of market share in Korea. ACQ employs dodecyl dimethyl ammonium chloride (DDAC) and benzyl dimethyl dodecyl ammonium chloride (DBAC) for active ingredient along with copper. The strongly increasing domestic applications for wood preservatives require developing accurate and reproducible analytic...
Sung-Mo Kang, Kwon-Min Kim, Won-Mo Koo, Myeong-Won Cho


Cost effective extension of service life of bridge tie (sleepers) - Effectively applying borate during Boulton conditioning and treatment with copper naphthenate
2014 - IRG/WP 14-30637
Current longevity of creosote treated wooden bridge ties in the South Eastern US is about 15 to 25 years, which is well below of the average service life of 33-50 years of railroad ties. Such short service life increases costs associated with maintenance of railroads including bridge down time for tie replacement as well as the cost for the new ties themselves. Because of this, many railroads are...
J D Lloyd, T Chambers, J-W Kim


Study on Biological Distribution to Conserve the Tripitaka Koreana woodblocks in Haeinsa Temple
2015 - IRG/WP 15-10844
Tripitaka Koreana is the Wood-carved Buddhist scriptures which were made in 13th century. And Janggyeong Panjeon that is depository for the Tripitaka Koreana was built in 15th century. In recent days, biological damage becomes a serious problem to wooden cultural heritage including historical wooden buildings with global warming. In this study, termite monitoring on whole Haein-sa temple area and ...
Si Hyun Kim, Hyun Ju Lee, Yong Jae Chung