Possible targets of wood modification in brown rot degradation
2014 - IRG/WP 14-40676
Wood modification protects wood from fungal degradation in a non-toxic manner. However, the mechanisms behind the decay resistance in modified wood are currently unknown. The aim of this study was to discuss the i) colonisation, ii) nutrient recognition, iii) transcription, iv) depolymerisation and v)…
R Ringman, A Pilgård, G Alfredsen, B Goodell, K Richter


Preliminary evaluation of degradation patterns in wood samples from the Yenikapı shipwrecks
2013 - IRG/WP 13-10798
The uncovering of several shipwrecks during the excavation of the Marmaray Rail Tube Tunnel Project in Istanbul provides an important opportunity to evaluate waterlogged woods buried for centuries. Identification of these woods showed that a variety of species was used in…
C Köse, A M Taylor


The chemistry of wood degradation by Basidiomycetes studied in a van Krevelen diagram
2013 - IRG/WP 13-10805
The atomic composition ratios of decayed wood by Basidiomycetes are mapped in a van Krevelen diagram. It is shown that the wood residue after decay is chemically reduced, rather than oxidized. A previously developed and verified theoretical model for thermal wood modification, relating…
W Willems, H Militz


What molecular biology can tell us about the biodegradation of lignocellulose: the utilization of molecular techniques for the detection, identification and enhanced understanding of wood degrading organisms
2013 - IRG/WP 13-20528
…used in the identification, detection and analysis of wood degrading organisms. An overview of some of the early work on nucleic acid isolation and characterization will be followed by a discussion of the power of sequencing and other procedures for better understanding: the mechanisms involved in the…
J Jellison, B Goodell, G Alfredsen, D Eastwood, G Daniel, S M Cragg, J K Grace


Application of a model for the prediction of fungal degradation of thermally modified beech timber by Trametes versicolor
2013 - IRG/WP 13-40622
…technology is found to be feasible for characterization of the property changes of thermally modified timber (TMT). In opposite to time-consuming and expensive laboratory tests a non-destructive test represents an improvement for the manufacturer of TMT. Therefore the aim of this study was to develop a method…
Clauder, L., Richter S., Unger, W., Pfriem, A


Utilization of TG-DSC to study thermal degradation of beech and silver fir
2013 - IRG/WP 13-40628
Thermal treatment of wood is, besides other wood modification system, used to improve the decay resistance and dimensional stability. However, the chemical changes that are caused by treatment process are still difficult to quantify, characterize and control. Previous studies…
K Candelier, A Treu, J Dibdiakova, E Larnøy, A Petrissans, S Dumarçay, M Pétrissans, P Gérardin


Use of Variable Pressure Scanning Electron Microscopy for in situ Observation of Degradation of Wood Surfaces during Artificial Weathering
2012 - IRG/WP 12-20489
…pressure scanning electron microscopy (VPSEM) is capable of observing electrically non-conductive materials like wood without the need to render the surface conductive by applying a coating of gold, platinum or carbon. Hence, there is the possibility that VPSEM could be used to non-destructively follow the…
F Hatae, Y Kataoka, M Kiguchi, H Matsunaga, J Matsumura


Utilization of thermodesorption coupled to GC-MS to characterize volatiles formation kinetics during wood thermodegradation
2012 - IRG/WP 12-40587
Identification of volatile degradation products produced during wood mild pyrolysis is important to have better insight on thermodegradation mechanisms. Previous studies have shown that thermodesorption coupled to GC-MS is an attractive tool to characterize and quantify…
K Candelier, S Dumarçay, A Pétrissans, M Pétrissans, P Kamdem, P Gérardin


Utilization of thermodesorption coupled to GC-MS to study kinetics of thermodegradation of different wood species
2011 - IRG/WP 11-40559
…(TD-GC-MS) has been investigated to identify volatile degradation products generated during wood heat treatment by mild pyrolysis. For this purpose, wood samples of different softwood and hardwood species have been heat treated under nitrogen for different temperatures comprised between 180 and 230°C during 15…
K Candelier, M Chaouch, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Fungal Attack on Lignin and Cellulose: Elucidation of Brown- and White-Rot Mechanisms Comparing Biomimetic and In-Vivo Degradation Patterns
2010 - IRG/WP 10-10714
…that have been developed over several years on wood degradation mechanisms. This information is combined with new data and analyses to explain why wood decay patterns caused by brown-rot fungi and specific types of white-rot fungi are different. New data, including work with both biomimetic studies on low…
V Arantes, B Goodell, A M F Milagres, Yuhui Qian, T Filley, J Jellison, S Kelley


Glutathione transferases as functional biomarkers of wood degradation?
2010 - IRG/WP 10-10735
The recent release of several fungal genome sequences allows the report of an overview of fungal glutathione transferases (GSTs) focused on their function in the wood-degrading basidiomycete Phanerochaete chrysosporium. A genomic and phylogenetic analysis of GST classes in…
E Gelhaye, M Morel


Simulation and Investigation of Wood Degradation by Erosion Bacteria in Laboratory Experiments
2010 - IRG/WP 10-20431
…set up to establish, monitor and manipulate bacterial wood degradation under low oxygen conditions. Sound pine sticks were placed in waterlogged sediment from a heavily decayed pine pile foundation site in Amsterdam. The system was subject to different gassing treatment regimes in order to investigate the role of
J Gelbrich, E I Kretschmar, N Lamersdorf, H Militz


The Use of Micro-Tensile Testing to Assess Weathering Decay and Oxidative Degradation of Wooden Items
2010 - IRG/WP 10-20433
…presents a method to study the weathering performance of wooden items and to assess the oxidative degradation of wood via the Fenton reaction. Weathering resistance and photo-stability of wood was tested using pine wood (Pinus sylvestris) veneer strips measuring approximately 60 µm in thickness. The veneer…
C Mai, Yanjun Xie, Zefang Xiao, P D Evans, H Militz


Degradation of Carbon-Based Preservatives by Black-stain Fungi
2010 - IRG/WP 10-30533
…to carbon-based preservatives. However, the cause of this resistance is unclear. The fungi may have mechanisms to tolerate these chemicals, or they may be able to degrade and detoxify them. Fungi capable of degrading carbon-based preservatives are of interest for possible bioremediation of carbon-based…
R Stirling, P I Morris


Biological degradation of acetylated wood after 18 years in ground contact and 10 years in marine water
2010 - IRG/WP 10-40522
This paper addresses the resistance to biological degradation of acetylated wood. Firstly, it presents results from an EN 252 test after 18 years’ exposure. The test is still running in Nordic NWPC test fields, Simlångsdalen in Sweden and Viikki in Finland. Results from this test were presented after 5…
P Larsson Brelid, M Westin


Degradation of wood veneers by Fenton’s reagents: effects of low molecular weight phenolic compounds on hydrogen peroxide decay and tensile strength loss
2009 - IRG/WP 09-20400
…containing hydrogen peroxide and iron to mimic mechanisms of brown rot decay and assess the degradation of cellulose through analysis of the tensile properties of the decayed wood. The tensile properties of thin wood strips treated with Fenton system reagents or precursors were determined and correlated to weight…
Yanjun Xie, R Well, Zefang Xiao, B Goodell, J Jellison, H Militz, C Mai


Effect of wood polymers degradation during heat treatment on extracellular enzymatic activities involved in beech degradation by Trametes versicolor
2008 - IRG/WP 08-40392
Effect of heat treatment on extracellular enzymes involved in wood degradation by Trametes versicolor was investigated. Heat-treated and untreated beech blocks were exposed to T. versicolor on malt agar medium and extracellular enzymatic activities investigated. A…
S Lekounougou, G Nguila Inari, M Pétrissans, S Dumarçay, J P Jacquot, E Gelhaye, P Gérardin


Heat treatment, thermal treatment, thermal degradation of wood, carbon nanotubes and Damascus steel swords. What do they all have in common?
2008 - IRG/WP 08-40399
Thermal degradation of wood is a well known phenomenon. Yet heat-treatment of wood can also provide protection for wood against certain environmental hazards. This paper explores some of the aspects of thermal degradation of wood fiber at relatively low temperatures…
Xinfeng Xie, B Goodell, Yuhui Qian, G Daniel


Degradation of polychlorinated organic biocides by the wood decaying fungi
2008 - IRG/WP 08-50253
…Consequently, there is an increased need for development of new strategies for their detoxification. In this work, the bioremediation potential of selected white rot fungi (basidimycetes Pleurotus ostreatus and Trametes versicolor, and ascomycete Hypohylon fragiforme) and one brown rot basidiomycete Gleophyllum…
I Vidic, L Zupancic-Kralj, K Sepcic, F Pohleven


Phenol oxidase activity and one-electron oxidation activity in wood degradation by soft-rot deuteromycetes
2007 - IRG/WP 07-10615
Wood degradation, one-electron oxidation activity as assayed by ethylene generation from 2-keto-4-thiomethylbutyric acid (KTBA), and phenol oxidase activity were measured in cultures of six deuteromyce fungi, with glucose or wood as the carbon source. The four…
H Tanaka, M Yamakawa, S Itakura, A Enoki


Gypsum effects on ‘dry rot’ wood degradation as a function of environment
2007 - IRG/WP 07-10624
‘Dry rot’ fungi are a unique group of brown rot fungi that can degrade wood away from ground contact where other fungi fail to colonize. Successfully occupying this niche is partially due to efficient water and nutrient transport, but mobilizing elements, notably calcium (Ca) and iron (Fe),…
J Schilling, J Jellison


Photo-degradation of modified and non-modified wood, coated with water borne acrylic coatings during artificial light exposure
2007 - IRG/WP 07-30416
A series of experiments were carried out to investigate photo-degradation of thermally modified (at 210oC and – 0.9 bars for two hours) and non-modified spruce wood (Picea abies L (Karst)), coated with transparent and semitransparent (with 3% pigment content)…
M Deka, M Tomažic, M Petric


The Current Situation Of Wood Poles Installed In Ilha Do Mel: A Wood Pole Biodegradation Diagnostic
2007 - IRG/WP 07-40373
Wood CCA and CCB poles installed in Ilha do Mel, an island of Parana State, Brazil, are failed earlier than expected: just five years after being installed many poles need to be replaced with financial implications for the State Energy Company – COPEL. In an effort to answer what causes this failure, this work…
C C Borges, J C Moreschi


Micromorphological Characteristics of Degradation in Bamboo Attacked by White Rot Fungus Lentinus edodes
2006 - IRG/WP 06-10575
…for wood decay, little known is about the decay pattern of bamboos by wood decay fungi. The present work was undertaken to understand the general degradation pattern of bamboo and the influence of polylaminate layers in bamboo fiber walls on the restriction of fungal decay. The weight loss of bamboo species…
Chang Hyun Cho, Kwang Ho Lee, Yoon Soo Kim


Effect of felling time related to lunar calendar on the durability of wood and bamboo -Fungal degradation during above ground exposure test for 2 years- (Preliminary report)
2005 - IRG/WP 05-20311
…study was carried out to know whether the felling time of trees and bamboos based on lunar calendar affects natural durability of felled wood-bamboo or not. Each of one sugi (Cryptomeria japonica) tree of 28 years old and one Moso bamboo (Phyllostachys heterocycla) of around 3 years old was cut 12 times between…
K Yamamoto, S Uesugi, K Kawakami