Kiln drying of poles as a means of solving the problems of pre-treatment decay in poles
1985 - IRG/WP 1263
The concept that pre-treatment decay can cause wide variation in the treatability of wood and especially wood poles has caused much discussion and debate in wood preservation circles. Yet it seem only logical that if decay has effected the strength characteristics of the wood and caused a differential moisture content in the wood the treatment of the end product will be highly variable and the lon...
J A Taylor


Biological resistance of steam-compressed wood pretreated with boric compounds
1999 - IRG/WP 99-30190
Wood compression under heating is aimed to enhance dimensional stability and surface hardness. Preservative treatment with an appropriate chemical is additionally required for the protection of wood against biological agents under hazardous service conditions. Boron pretreatment of compressed wood was targeted to a mutual benefit of increasing biological resistance of compressed wood as boron was ...
M K Yalinkilic, W Dwianto, Y Imamura, K Tsunoda, M Takahashi


Effects of steaming heat treatment of wood on the stimulation of termite feeding
1997 - IRG/WP 97-10212
At the 26th IRG conference, we reported that steamed Japanese larch heartwood samples were suffered a serious attack by subterranean termite, Coptotermes formosanus both in choice and no-choice feeding tests. This is possibly caused by the yield of termites stimulants in the wood samples resulting from the steaming process. Since the steaming heat treatment has often been applied to other several ...
S Doi, Y Kurimoto, M Takahashi, T Yoshimura


The effect of treatments in boron steaming medium on boron leaching and strength properties of wood
2008 - IRG/WP 08-40409
The combined effect of boric acid impregnation together with boron steaming and steaming heat treatments were evaluated in this study. Boric acid pre-treated wood samples and untreated ones subjected to steaming heat and direct steaming treatment in a close reactor at 13 bar pressure and 180 ºC for 30 minutes. Compression strength parallel to grain of wood samples, leaching test and pH measuremen...
E D Tomak, Ü C Yildiz, S Yildiz, E Pesman


Proposal for further work on accelerated ageing
1988 - IRG/WP 2314
M-L Edlund


Strength loss associated with steam conditioning and boron treatment of radiata pine framing
1987 - IRG/WP 3438
The combined effect of included defects and wood moisture content on the strength loss of second rotation radiata pine framing following conventional steam conditioning is investigated. The green Modulus of Elasticity (MOE) is reduced by approximately 13% after steaming. When dried after steaming, however, neither the MOE nor MOR is significantly different from unsteamed dried controls....
M J Collins, P Vinden


Thermal treatment of wood: European Processes and their background
2002 - IRG/WP 02-40241
Recent efforts on thermal treatment of wood lead to the development of several processes introduced to the European market during the last few years. The total production capacity of heat treated wood in 2001 is estimated as approx. 165.000 m3. In the paper the different heat processes are presented. The general technology as well as scientific data on the chemical transformation of the cell wall ...
H Militz


Durability of pine modified by 9 different methods
2004 - IRG/WP 04-40288
The decay resistance was studied for pine modified by nine methods of wood modification: 1) Acetylation, 2) Treatment with methylated melamine resin (MMF), 3) Acetylation followed by post-treatment with MMF-resin, 4) Thermal modification, 5) Furfurylation, 6) Maleoylation (using water solution of MG or ethanol solution of maleic anhydride), 7) Succinylation, 8) NMA-modification and 9) modification...
M Westin, A O Rapp, T Nilsson


An investigation of the effects of pre-steaming on the treatment of sawn spruce timber with Celcure A, a copper-chrome-arsenic preservative
1981 - IRG/WP 3150
Difficulties in the treatment of spruce using standard vacuum/pressure techniques with both water-borne and organic solvent preservatives are well known. We have evaluated the influence of steaming on treatability with a waterborne CCA preservative....
C R Coggins


Options for accelerated boron treatment: A practical review of alternatives
1985 - IRG/WP 3329
Boron wood preservatives are almost exclusively applied by momentary immersion and block diffusion storage. Alternative techniques are described which can be used to accelerate boron treatment. Diffusion coefficients have been derived to define the acceleration of diffusion with increasing temperature. Schedules are described for pressure impregnation of green timber, involving steam conditioning,...
P Vinden, T Fenton, K Nasheri


Corrosion of fasteners in heat-treated wood – progress report after two years’ exposure outdoors
2005 - IRG/WP 05-40296
The corrosion of common fastener materials now in use - mild steel, zinc-coated steel, aluminium and Sanbond Z-coated steel – has been evaluated after two years’ exposure outdoors in untreated and heat-treated spruce (Picea abies) respectively. Spruce from South-western Sweden was used. The heat-treatment was carried out in Finland according to the ThermoWood process at a maximum temperature ...
J Jermer, B-L Andersson


Improved resistance of Scots pine and Spruce by application of an oil-heat treatment
2000 - IRG/WP 00-40162
Spruce (Picea abies L. Karst.) and Scots pine (Pinus sylvestris L.) were subject to a heat treatment which was carried out in an oil-bath. The aim was to improve the dimensional stability of the treated wood and its resistance against fungi. The bath of vegetable oil provides a uniform heat transfer at temperatures of 180°C, 200°C and 220°C and protects the submersed wood from oxygen. Heat trea...
M Sailer, A O Rapp, H Leithoff


Heat treatment of bamboo
2001 - IRG/WP 01-40216
Bamboo is a fast growing material with remarkable mechanical properties. In many tropical and subtropical countries bamboo is available in suitable dimensions for a reasonable price. Therefore it is used for many purposes which range from the basket production up to the industrial production of parquet or paper. However, bamboo is known as susceptible to fungal or insect attack and it is difficult...
H Leithoff, R-D Peek


The effects of heat treament on the specific gravity of beech and spruce wood
2003 - IRG/WP 03-40254
The effects of heat treatment on specific gravity of beech (Fagus orientalis) and spruce wood (Picea orientalis) naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 2 x 2 x 3 cm. Heat treatment was than applied to the wood samples at four different temperatures (130 °C, 150 °C, 180 °C and 200 °C) and three different durations...
S Yildiz, Ü C Yildiz, G Colakoglu, E D Gezer, A Temiz


Durability of different heat treated materials from industrial processes in ground contact
2005 - IRG/WP 05-40312
In this study the durability of heat treated wood originating from four different European industrial heat treatment processes in ground contact was examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood/Finland, New Option Wood/France and Menz Holz/Germany where Oil-Heat treated Wood (OHT) is produced. All heat treated materials showed significantly i...
C R Welzbacher, A O Rapp


The effects of heat treatment on the toughness of beech wood
2004 - IRG/WP 04-40283
The effects of heat treatment on toughness of beech (Fagus orientalis) wood naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 5 x 5 x 5 cm. Heat treatment was than applied to the wood samples at three different temperatures (130 °C, 150 °C and 180 °C) and three different durations (2 h, 6 h and 10 h) under air atmospheres. ...
S Yildiz, Ü C Yildiz, E D Gezer, Ali Temiz, E Dizman


Preservative treatment of Pinus elliottii
1987 - IRG/WP 3435
The treatment of Pinus elliottii with copper-chrome-arsenic preservative by four alternative seasoning and treatment methods is investigated. Steam conditioning followed by either alternating pressure method (APM) or 'Q' treatment resulted in inadequate preservative penetration. Air drying or high temperature drying followed by the Bethell process resulted in a high standard of t...
P Vinden, L Carter


Developments in wood preservation processing techniques in New Zealand
1980 - IRG/WP 3143
P Vinden, A J McQuire


Copper naphthenate-treated Southern Pine pole stubs in field exposure. -Part 2: Chemical characterization of full size pole stubs 12 years after treatment
2000 - IRG/WP 00-30246
This study examines the influence of pre-treatment and post-treatment steaming on the character and physio-chemical nature of copper naphthenate in hydrocarbon solvent treated pine in larger, pole diameter, pole stub-length samples. This work is the continuation of two projects that began almost a decade ago. Previous reports indicated that certain morphological changes might occur in small labora...
H M Barnes, D P Kamdem, M H Freeman


The Effect of Heat on the Retention of Ammoniacal Copper Quat (ACQ-AB) onto Scots Pine (Pinus Sylvestris L.) Wood
2008 - IRG/WP 08-40390
In this study, the sapwood of Scots pine (Pinus sylvestris L.) were treated with ammonical copper quat type (ACQ-AB), which is one of the environmentally friendly wood preservatives, by using soaking method as a functions of various temperatures and time. The results indicated that the retention behaviour of ACQ onto the wood was considerably affected by temperature of ACQ solution and treatment t...
M Hakki Alma, A Mukremin Kara


The effects of heat treatment on anatomical changes of beech wood
2004 - IRG/WP 04-40284
The effects of heat treatment on anatomical changes of beech wood (Fagus orientalis) naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 2x2x3 cm and than conditioned at 25 °C and 65 % relative humidity for 3 weeks. Heat treatment was than applied to the wood samples at four different temperatures (130 °C, 150 °C, 180 °C and ...
Ü C Yildiz, Z Gerçek, B Serdar, S Yildiz, E D Gezer, E Dizman, A Temiz


Radio frequency heating times for sterilization radiata pine solid piles
2017 - IRG/WP 17-40815
In this work was sterilized wood packaging material of radiata pine, stacked as solid piles without stickers, for determining the heating times using radiofrequency treatment. The experiments were performed in a radio frequency semi-industrial equipment. The results showed that the radio frequency heating times increases with wood volume and that radio frequency treatments were faster than convent...
H Esquivel, V Sepúlveda, J Torres, L Salvo, R A Ananías


Heat treated timber in Finland
2000 - IRG/WP 00-40158
Heat treatment permanently changes the physical and chemical properties of wood by means of high temperatures (150 - 240°C). Heat treatment darkens the colour of the wood. Heat treatment improves the equilibrium moisture content of the wood and the shrinkage and swelling of the wood is reduced. Very high temperatures improve the resistance to rot and also reduce the susceptibility to fungal decay...
T Syrjänen, E Kangas


Heat treatment of wood strands for OSB production: Effect on the mechanical properties, water absorption and dimensional stability
2002 - IRG/WP 02-40238
The effect of heat treatment on the mechanical and physical properties of commercial OSB strands was evaluated. Heat treatment was applied under inert atmospheric conditions to wood strands. The aim of this study was to examine the heat treatment parameters to achieve significant reduction of thickness swelling (upon exposure to moisture in service) without causing excessive reductions in stren...
G J Goroyias, M D C Hale


Investigation of some technical properties of heat-treated wood
2003 - IRG/WP 03-40266
The objective of this study was to investigate some technical properties of heat-treated wood. Wood heat-treated according to a process intended for wood in above-ground end-uses (European hazard class 3) was subject to the following: · A delamination test according to EN 391 with glulam beams made of heat-treated pine (Pinus sylvestris) and spruce (Picea abies) laminations, assembled with PR...
C Bengtsson, J Jermer, A Clang, B Ek-Olausson