Durability of Sugi (Cryptomeria japonica D.DoN ) wood treated in high temperature liquid paraffin
2002 - IRG/WP 02-40221
Sugi(Cryptomeria japonica D.DoN )wood was subject to a heat treatment in high-temperature liquid paraffin for the purpose of improving the resistance against fungi and termites without chemicals. The bath of paraffin liquid, which can provide a uniform heat transfer (±2?), was used at temperatures of 90?,120?and 150?.?ecay resistance according to JIS K 15711) was evaluated using a brown rot fungu...
Y Matsuoka, W Ohmura, S Fujiwara, Y Kanagawa


Changed susceptibility of the chemically and thermally degraded spruce wood to its attack by the dry rot fungus Serpula lacrymans
1999 - IRG/WP 99-10322
In buildings, some intentional or unintended situations can occur at which some wood products are exposed to aggressive chemicals and also to higher temperatures. Occasional activity of fungi on such pre-attacked wood products can be either higher or lower. This paper deals with changes in the susceptibility of spruce wood (Picea abies L. Karst.) to attack by the dry rot fungus Serpula lacrymans, ...
L Reinprecht


Preservative treatment of Pinus elliottii
1987 - IRG/WP 3435
The treatment of Pinus elliottii with copper-chrome-arsenic preservative by four alternative seasoning and treatment methods is investigated. Steam conditioning followed by either alternating pressure method (APM) or 'Q' treatment resulted in inadequate preservative penetration. Air drying or high temperature drying followed by the Bethell process resulted in a high standard of t...
P Vinden, L Carter


Resin bleed after light organic solvent preservative treatment - the effect of drying method and process type
1986 - IRG/WP 3378
The effects of drying method and treatment process type on resin bleed were investigated. High-temperature drying of resinous radiata pine (Pinus radiata D. Don) heartwood resulted in improved wood permeability, higher preservative uptake, and greater resin bleed when treated by the Rueping process. Resin bleed was reduced substantially when timber was treated by the Lowry process, and totally eli...
P Vinden


Observations on the uptake and penetration of various liquids in clear heartwood and sapwood of Pinus radiata D.Don
1983 - IRG/WP 3224
Volumetric uptake of water (aqueous copper-chrome-arsenic (CCA)) or methanol, applied by bulk hydrostatic pressure to air dried clear heartwood specimens of Pinus radiata D. Don, far exceeds that of a wide variety of polar and non-polar solvents. In air dried sapwood, the volumetric uptake of CCA tends to be less than that achieved for most solvents including methanol. No comprehensive explanation...
J E Barnacle


The effect of high temperature and long pressing time on the dimensional stability and decay resistance of OSB
2002 - IRG/WP 02-40237
The exterior use of OSB is restricted because when it is exposed to wet conditions swelling, loss of internal bond strength (IB) and decay occur. In this study an alternative process of pressing which results in the production of dimensionally stable and a more decay resistant strandboard was investigated. Boards were pressed at elevated temperatures for prolonged pressing cycles and their physi...
G J Goroyias, M D C Hale


Experiences from a Danish large scale test by means of a new method of treatment by attack of true dry rot fungus (Serpula lacrymans) in buildings
1994 - IRG/WP 94-10064
Experiences from a new and epoch-making method of treatment in connection with the repair of attack of the true dry rot fungus, Serpula lacrymans (Fr.) S.F. Gray, are described. The paper presents the background of a large scale test comprising repair of more than 150 Danish buildings over a period of approximate 5 years. The method being both gentle to the building and presenting savings of at le...
O Munck, H Sundberg


Quality of timber impregnated with preservatives of class AB after three years in service
2002 - IRG/WP 02-20241
Quality of impregnated timber is most often expressed by penetration and retention of the preservative used. Relatively less information is available about the performance of the final product, e.g. decks, panels etc. regarding product’s surface checks, deformations and overall appearance. Together with the timber durability, the above mention features are of esthetical importance in the above g...
N Terziev


Effects of drying processes on termite feeding behaviour against Japanese larch wood
2001 - IRG/WP 01-10390
We investigated the effects of current drying schedules for larch lumbers on the termite feedings. Thermal analyses were also conducted to investigate degradation of wood components. Choice feeding tests showed specimens dried under high-temperature schedules were evidently susceptible against termite attacks. These schedules produced the feeding-attractants, which were suggested by the TGA result...
S Doi, Y Kurimoto, H Takiuchi, M Aoyama


Wood kiln drying. Simple process of material treament or soft method of preservation? (Le séchage arificiel du bois. Simple opération de traitement du metériau ou méthode douce de préservation?)
1993 - IRG/WP 93-50001-14
Among the processes enabling to extend wood durability, kiln drying can be considered as a treatment and soft preservation method. Dry woods are naturally durable provided they are not subject to important retaking of the moisture. Drying thanks to the application of temperatures from 50 to120°C enable to execute a thermic treatment which kills grubs and mushrooms to ensure a sterilization that c...
F More-Chevalier


Clean creosote - its development, and comparison with conventional high temperature creosote
1983 - IRG/WP 3235
Pigment emulsified creosote (PEC) is presently being tested and shows considerable stability in terms of water content, pigment level, pH, viscosity, rheological behaviour and microscopy. Timber samples from several eucalypt species have been treated with PEC and side matched samples treated with conventional high temperature creosote (HTC). The PEC treated specimens showed higher weight retention...
C W Chin, J B Watkins, H Greaves


Comparison of the in-ground performance of pigment emulsified creosote (PEC) and high temperature creosote (HTC)
2000 - IRG/WP 00-30217
A long-term field trial was conducted in Australia to compare the in-ground performance of two oil-borne preservative formulations, conventional high temperature creosote (HTC) and a modified creosote formulation, pigment emulsified creosote (PEC). Three retentions (50, 100 and 200 kg/m³) were targeted for each formulation. An additional retention of PEC formulation (308 kg/m³), which contained ...
J W Creffield, H Greaves, N Chew, N K Nguyen


The loss of insecticidal action from synthetic pyrethroid-treated wood samples: The effect of high temperatures and relative humidities
1992 - IRG/WP 92-1569
This paper describes the results from bioassays using Hylotrupes bajulus, and chemical analyses, of pyrethroid-treated wood samples following storage for up to 3 years. A range of four storage environments was used consisting of combinations of two temperatures (20°C and 40°C) and two relative humidities (60% and 90%). It is concluded from the chemical analyses that, although losses at room temp...
R W Berry, S J Read


Termite durability of sugi (Cryptomeria japonica) heartwood kiln-dried under high-temperature process in relation to wood extractives
2005 - IRG/WP 05-10547
Termite durability of sugi heartwood samples kiln-dried under a high-temperature process were evaluated by using Reticulitermes speratus (Kolbe) as a test termite sp. The n-hexane extractives of these samples were analysed by a GC technique. The less termite durability was shown on the wood samples dried under the high-temperature process, in comparison with that of the air-dried samples. No GC-p...
S Shibutani, E Obataya, K Hanata, S Doi


Gaseous preservative treatment of wood
1990 - IRG/WP 3631
A recent development in processing wood with a gaseous preservative means that dry, treated wood can be produced in under 30 hours with the benefits of product diversification, faster stock turnover and the ability to respond to short term demand. About 400,000 m³ of wood are treated each year in New Zealand with boron salts to protect from borer infestation. Traditionally this treatment is effec...
R Burton, A J Bergervoet, K Nasheri, P Vinden, D R Page


High Temperature Treated Wood
2008 - IRG/WP 08-40429
High temperature can modify internal structure and physic-chemical properties of wood by a controlled pyrolysis process. Such treatment, among other changes in properties, modifies the wood color in a way that resembles exotic species, increasing its market value. The main objective of this work is to determine the changes in wood properties caused by the effect of temperature and time, in order t...
C C Borges, A L Barbosa, R Faber de Campos, S T Targas


Profiling fungal community in wood decay ecosystem by Denaturing High-Performance Liquid Chromatography
2010 - IRG/WP 10-20443
A DNA-based fingerprinting technique, Denaturing High Performance Liquid Chromatography (DHPLC) was developed to profile fungal communities colonizing indoor timber. Molecular fungal diversity was assessed using amplification based on the Internal Transcribed Spacer (ITS1) rDNA of 74 wood samples collected from infected buildings in France. Due to its high sensitivity, the PCR-DHPLC technique was ...
S Maurice, G Le Floch, M Le Bras-Quéré, J P Rioult, G Barbier


Evaluation of the effectiveness of soaking of high-temperature plywood in low-temperature oil-based wood
2023 - IRG/WP 23-40991
We conducted a preliminary investigation to determine if soaking high-temperature plywood in a low-temperature preservative solution could achieve deeper penetration of the preservative, even in plywood made with refractory wood species such as Japanese larch. Specimens cut from commercial plywood (Japanese larch) were stored at various temperatures before being soaked in the preservative solution...
T Miyauchi, S Isaji, H Shibui, N Furuta, J Miyazaki, H Matusnaga


Proposal for further work on accelerated ageing
1988 - IRG/WP 2314
M-L Edlund


Blue stain in service on wood surface coatings. Part 3: The nutritional capability of Aureobasidium pullulans compared to other fungi commonly isolated from wood surface coatings
1993 - IRG/WP 93-10035
The nutritional capability of Aureobasidium pullulans was previously examined, using agar plate tests, with regard to nutrient sources that are potentially available in fresh and weathered wood (Sharpe and Dickinson, 1992). This study compared these findings with the nutritional capability of four other fungi (Alternaria sp., Cladosporium cladosporoides, Stemphylium sp. and Trichoderma sp.) common...
P R Sharpe, D J Dickinson


Low temperature drying conditions of Pinus radiata wood for avoiding internal stain
1989 - IRG/WP 3507
It has been observed that, if in little sawmills, timber is dried with a low temperature schedule, it arrives at destination with internal sapstain besides of superficial mould. In this study, the lowest drying temperature at which wood should be exposed for sterilization, which results to be 52°C, is searched. It is not possible to avoid entrainment of pentachlorophenol, even though a waiting pe...
M C Rose


Problems caused by termites in buildings in the State of Sao Paulo
1976 - IRG/WP 150
Termites are the main insects attacking buildings in the State of Sao Paulo - Brazil. Their attack occurs in wood and wooden materials as well as paper, textile, leather and so on....
M S Cavalcante


Comparison of cubic and plug samples for preparation and data assembly in permeability study
2000 - IRG/WP 00-20197
In order to determine if plug experimental samples (PES: 30 x 15 mm2 diameter) could be used for inspection of wood permeability characteristics, radial and longitudinal flow directions were prepared according to either PES or cubic experimental samples (CES: 100 x 20 x 20 mm3) from the sapwood zone of Sitka spruce and treated by tanalith-C according to full-cell process. Results from the two prep...
I Usta


Physical properties of ß-1,4-Xylanase produced by Postia (=Poria) placenta: Implications for the control of brown rot
1987 - IRG/WP 1318
The degradation of hemicelluloses is an early event in wood decay by brown-rot fungi. An understanding of the physical properties of hemicellulases may suggest target mechanisms for the development of new control agents. Endo-b-1,4-xylanase was partially purified by column chromatography from wood decayed by Postia (= Poria) placenta. The enzyme was extremely resistant to denaturing conditions; no...
J A Micales, F Green III, C A Clausen, T L Highley


Improved equipment and technique for high pressure sap displacement impregnation of natural round wood
1972 - IRG/WP 309
Hitherto the main problem in the practical application of high pressure sap displacement impregnation (HPSD) has been in devising a satisfactory cap. Such a cap must be easily fitted to different size log ends to give a leak proof seal. The present contribution describes a new type of cap and sealing system designed to meet these requirements....
C G W Mason, F B Shorland