Performance of groundline bandage remedial treatments in western US species transmission poles
1993 - IRG/WP 93-30019
Groundline bandages are an important element in remedial treatment strategies for utility poles in the United States. Several bandages containing new or reformulated components have recently been developed but have not been adequately tested. This paper reports on the degree of diffusion of copper naphthenate, boron, and sodium fluoride from groundline bandages into pressuretreated Douglas-fir, po...
P G Forsyth, J J Morrell


Comparison of the anti-fungal efficacy of Cobra with drill perforation on oscillating pressure treated spruce transmission poles -Laboratory test
1988 - IRG/WP 3469
A laboratory method for measuring the depth of penetration of the fungicidal concentrations effective against basidiomycetes (brown rot) was developed. The tests on CCB oscillating pressure treated spruce transmission poles have shown that the depth of salt penetration can be increased by about 10 mm by a drill perforation before the impregnation. An even better penetration is reached, however, if...
E Graf, B Zgraggen


Studies and experiences of occurrence and development of soft rot in salt-treated poles of pine (Pinus sylvestris) installed in Swedish transmission lines in the years 1940-1945
1977 - IRG/WP 277
The present work describes the result of microscopic examinations of some 2,000 borings extracted from 20 to 23-year-old salt-treated poles (Scots pine) from the southern and central parts of Sweden. The purpose was to map out the occurrence of soft rot in Sweden and its influence on the mechanical strength of the poles as well as to contribute to the development of new and more satisfactory metho...
H Friis-Hansen


Distribution of boron from fused borate rods in Douglas-fir transmission poles
1996 - IRG/WP 96-30112
The diffusion of boron from fused borate rods (disodium octaborate tetrachydrate) was monitored over 42 months in CCA-treated Douglas-fir transmission poles. The boric acid equivalent was estimated by the curcumin/salicylic acid color test on increment cores removed from the poles. Moisture content of the poles was quite variable but was always above 20 percent. The percent of increment core lengt...
T L Highley, F Green III, W F Finney


Supply of wooden transmission and telephone poles in Tanzania: Problems and possible solutions
1987 - IRG/WP 3424
The eucalypts which have been used widely for utility poles for more than 30 years have dwindled remarkably from traditional supply areas. Consequently, pole-using authorities are considering importing poles from abroad. This alternative is considered unrealistic and costly. The aims of this paper are: - to dispel fears of pole scarcity and to show that an abundant resource of a variety of tree sp...
K K Murira, S A Diwani


Borate diffusion from fused borate rods in douglas-fir transmission poles
1994 - IRG/WP 94-30042
Pressure-treated utility poles have given many years of excellent service, but their lifetime is often shortened by internal decay of the untreated heartwood center, particularly in refractory species, such as Douglas-fir. This paper reports the distribution of boron from fused borate rods installed in CCA-treated Douglas-fir transmission poles. The boric acid equivalent was roughly monitored by t...
T L Highley, W Finney, F Green III


CT scanning of decay in creosoted poles for overhead lines
2013 - IRG/WP 13-30634
Creosote-treated poles have been examined by means of CT scanning in order to investigate the nature of soft spots that have been found more frequently during the last five years in Sweden. CT scanning provides a very good picture of the interior of the poles and decay can easily be detected. It was concluded that the soft spots in most cases were caused by decay which in turn had to do with extre...
C-J Johansson, A Clang, I Johansson, G Berggren


Degradation of Eucalyptus transmission poles varies across regions in Zambia
2018 - IRG/WP 18-30727
Evidence from literature shows that Eucalyptus poles treated with creosote last over 30 years before replacement. However, in Zambia, the life span of such poles has reduced to 5-10 years. The aim of this study was to investigate factors associated with degradation of treated Eucalyptus poles and how these varied across regions in the country. A total of 1200 poles were assessed in three differen...
P Ng’andwe, D Chungu, E Ncube


Field trial with poles of Scots pine treated with six different creosotes
1996 - IRG/WP 96-30115
In the middle of the 50's field trials with creosote-treated poles were started in France, Germany and Sweden. The trials were initiated by WEI (Western-European Institute for Wood Preservation). Six different creosotes were used and 40 poles per creosote were installed at each test field. Results after 39 years of exposure in Simlangsdalen, Sweden are reported. Poles treated with a heavy...
Ö Bergman


Soft rot in CCA-treated utility poles in Sweden
1989 - IRG/WP 1398
Soft rot investigations of CCA-treated utility poles (Pinus sylvestris L.) have been conducted throughout large parts of Sweden during 1974-1985. The investigation included 179 utility poles of the State Power Board which had been used for 10-18 years in the different administrative regions from northern to southern Sweden. In addition, 193 telephone poles from the Östersund area and 218 from the...
H Friis-Hansen, H Lundström


Soft rot penetration - Effect of groundline maintenance treatment on poles in sevice
1983 - IRG/WP 3263
R S Johnstone


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 13: Report of fourth inspection (36 months) in Australia
1981 - IRG/WP 481
This report presents the results of the fourth inspection of the IRG/COIPM International Marine Test specimens installed in Sydney Harbour in December, 1977. The inspection took place on 9th December, 1980, after 36 months exposure. Full details of the treatment and installation of the specimens, as well as results of the first three inspections (after 6, 12, and 24 months exposure), have been pre...
J Beesley


Progress towards controlling soft rot of treated hardwood poles in Australia
1977 - IRG/WP 289
H Greaves


Essais biologiques sur poteaux traités à la Wolmanit C.B. suivant le procédé Boucherie modifé
1974 - IRG/WP 336
D Lapetite, C Jacquiot, J Campredon


A case study on quality control on telephone poles as a cost saving tool in Tanzania
1987 - IRG/WP 3418
A sample of 28 CCA treated Eucalyptus poles from a lot of 2,000 poles awaiting delivery to the field, was studied to reveal the quality of treatment. Results showed a product of very poor quality. Average figures for penetration and retention were 8.4 mm and 2.2 kg/m³; these results are 66% and 91% below the required standards, respectively. Consequences of such results are estimated to amount to...
K K Murira


Effectiveness of "Gang-Nail" plates in preventing splitting of Eucalyptus poles and Brazilian hardwood sleepers
1984 - IRG/WP 3262
This paper presents the results of some tests carried out with an anti-splitting device, placed on the end surfaces of Eucalyptus spp utility poles and Brazilian hardwood sleepers at the beginning of an air-drying period. The type of device used, a "Gang-Nail" plate, reduces significantly the splits at the end-surface of poles, but reduces only a little the splits occurring in sleepers....
A M F Oliveira, J A C Sodré, O B Neto


Field trials of groundline remedial treatments on soft rot attacked CCA treated Eucalyptus poles
1983 - IRG/WP 3222
A total of 17 CCA treated Eucalyptus poles, which were found to contain 2-5 mm of soft rot in October, 1980, were reinspected in October, 1982. In 1980, 11 of the poles were given a supplemental groundline bandage treatment of either Osmoplastic or Patox, while 6 of the poles were designated as untreated controls. Two years after remedial treatment, samples were removed from the poles for microsco...
W S McNamara, R J Ziobro, J F Triana


Inspection results of preservative treated stakes, maximum 33 years in field
1992 - IRG/WP 92-3690
Since in 1958, we have undertaken field experiments in Japan. For these field experiments, we used sapwoods of Japanese cedar called Sugi (Cryptomeria japonica) because of majority of plantation forest soft wood species in Japan. For some preservatives, we added sapwood of Japanese beech called Buna (Fagus crenata), a main Japanese hard wood species. Dimensions of these specimens were 30 x 30 x 60...
K Suzuki, K Yamamoto, M Inoue, S Matsuoka


Cu, Cr and As distribution in soils adjacent to CCA treated utility poles in Eastern Black Sea Region of Turkey
2004 - IRG/WP 04-50214
In this study, the main objective was to asses the distribution of Cu, Cr, and As in soils adjacent to CCA treated utility poles in Eastern Blacksea Region of Turkey (Trabzon, Rize and Artvin ) and determine the influence of soil composition. Surface (0-5cm), subsurface soil samples (30-40cm) were collected near CCA-treated utility poles and control soil samples away from CCA-treated utility pole...
E D Gezer, Ü C Yildiz, A Temiz, S Yildiz, E Dizman


Japanese wood preserving industry
1990 - IRG/WP 3596
Although a great amount of wood is in use in Japan, a little attention has been paid to the significance and importance of wood preservation. The fact reflects that only less than 0.5% of the total wood consumption is treated with wood preservatives today in the country. Over the 20 years before 1970, the annual volume of preservative treated (pressure treatment) wood was relatively at a stable le...
K Tsunoda


Introduction to a field demonstration of various instruments and methods for the detection of defects in poles
1984 - IRG/WP 2228
H Friis-Hansen


Essais mycologiques sur poteaux traités à la Wolmanit C B
1974 - IRG/WP 339
D Ollier, C Jacquiot


The leaching of copper, chrome and arsenate from CCA-impregnated poles stored for ten years in running water
1978 - IRG/WP 3122
There is no evidence to indicate that the chromium and copper components are leached from the outermost 5 mm of sapwood in poles impregnated with Boliden K33 and Tanalith C and stored in running water for ten years. The arsenic component, however, seems to be leached out during the first few months to an extent of about 20% of the initial amount. The leaching time is dependent on the preservative ...
F G Evans


Decay resistance of wood removed from poles treated with Trichoderma
1989 - IRG/WP 1386
Wood blocks removed from a distribution pole previously treated with a biological control product (Binab FYT pellets) were exposed in soil block tests to selected basidiomycetes. The blocks were removed from regions of poles where Trichoderma colonization had been confirmed by extensive sampling and computer mapping of microbial inhabitants. The results indicate that material from pole interiors c...
A Bruce, B King, T L Highley


Untersuchungen über die Imprägnierbarkeit verschiedener türkischer Holzarten mit wirtschaftlicher Bedeutung
1976 - IRG/WP 370
Holzarten mit einer geringen natürlichen Dauerhaftigkeit können nur dann wirtschaftlich verwendet werden, wenn ihre Gebrauchsdauer durch einen zusätzlichen chemischen Schutz verlängert wird. Holzschutzmaßnahmen können nur regelmäßig geplant werden, wenn die Tränkbarkeit der verwendeten Holzarten bekannt ist. Aufgabe dieser Versuche war es daher, festzustellen, wieweit die Holzarten hinrei...