Your search resulted in 740 documents. Displaying 25 entries per page.
Progress report on co-operative research project on L-joint testing
1983 - IRG/WP 2192
A F Bravery, D J Dickinson, M Fougerousse
Natural durability of European wood species for exterior use above ground
2003 - IRG/WP 03-10499
The main interest in using more timber for exterior constructions is to protect the environment, where wood is considered an environmentally friendly material. However, chemicals for wood protection are getting more and more restricted, consequently, the focus on the natural durability of wood is increased. Good, well-documented data on the durability of wood species in ground contact exist, which...
B Lindegaard, N Morsing
Co-operative research project on L-joint testing. Progress report to March 1984
1984 - IRG/WP 2211
Each participant was intended to expose L-joints in the main trial on 1 April 1983 and the first sampling, after 8 months exposure, was to be undertaken on 1 December 1983. Some participants have had to vary this schedule. Results are presented from CTFT (France) and PRL (United Kingdom). These show a greater effectiveness by the double vacuum treatments compared with the 1 minute dip treatments. ...
J K Carey, A F Bravery
Aboveground Microbial Decay Test of Biocide Treated and Untreated Wood Exposed to Danish and Humid Tropical Climates
2004 - IRG/WP 04-20306
A co-operative study was initiated to compare the aboveground field decay test of untreated and preservative-treated timbers under Nordic (Danish) and a representative humid tropical (Malaysian) environment according to CEN standard method. Matched specimens of untreated and both preservative-impregnated and surface-treated wood were simultaneously exposed at The Danish Technological Institute (DT...
A H H Wong, N Morsing, K H Henriksen, S Ujang
Interim balance after 20 months of lap-joint exposure
1999 - IRG/WP 99-20164
The application of natural resins and integrated resin systems to improve the performance of Pinus sylvestris was assessed in a lap-joint test according to DIN V ENV 12037 (1996). Lap-joints of Pinus sapwood were exposed at the test field in Hamburg (Germany) in May 1997. The treated lap-joints were assessed with regard to the performance of the resin treatments out of ground. The exposure of lap-...
M Sailer, A O Rapp, R-D Peek, A J Nurmi, E P J Beckers
Co-operative research project on L-joint testing. Progress report to March 1986
1986 - IRG/WP 2272
Further sets of data received from CTFT (France) after 18 months exposure, BAM (Germany) after 18 months exposure, STU (Sweden) after 9.5 months exposure and TI (Denmark) after 12 and 17.5 months exposure are presented and discussed in conjunction with data previously reported. The new data are generally in agreement with those presented previously and indicate the major difference between the co-...
J K Carey, A F Bravery
Co-operative research project on L-joint testing. Progress report to March 1985
1985 - IRG/WP 2236
It was originally intended that each participant would expose L-joints in the main trial on 1 April 1983 with the first sampling at 8 months (1 December 1983) and the second sampling at 18 months (1 October 1984). In the event, some participants have had to vary this schedule. Results after the first sampling have been received from CTFT (8 months), BAM (12 months) and Sipad-IRC (8 months) and aft...
J K Carey, A F Bravery
The accelerated L-joint test method for determination of the out of ground natural durability
1998 - IRG/WP 98-20146
The accelerated L-joint test incorporates a moistening device and uses a close end water trap in an open joint connection with a laminated tenon member consisting of the perishable reference wood species scots pine sapwood and beech.
After one year of exposure it is possible to show a distinct identification of natural durability classes 4 and 5 against the more durable wood species. Both weight ...
J Van Acker, C Brauwers, M Stevens
A field study on the suitability of the European lap-joint test
2001 - IRG/WP 01-20239
Within the framework of the European SM&T Research Project "Co-normative research on field tests for wood preservatives out of ground contact in conjunction with methods for preconditioning test specimens prior to test" (FACT) one aim was to establish the suitability of the European lap-joint test (as it is described in ENV 12037:1996) to assess wood preservatives in the field in EHC 3. Scots ...
M Grinda, Ö Bergman, H-V Borck, D Dickinson, P Esser, R Gründlinger, H Leithoff, S Molnar, L Paajanen, N Pfabigan, E D Suttie, F Thomassin, T Nilsson, J Van Acker, M Van Der Zee, A Voss
Validity of above ground testing according to ENV 12037
2008 - IRG/WP 08-20379
The standard ENV 12037 for testing of treated and untreated wood (lap-joint) exposed above ground
was issued in 1996 by The European Committee for Standardization. A draft for the development of the standard was presented by CEN-TC 38/WG 25/DOC N 076 in 2002. For a test to become valid the median rating of decay for untreated control replicates (Scots pine sapwood) must be equal or greater than ...
Ö Bergman, U Råberg, N Terziev
Above Ground Field Testing – Influence of test method and location on the relative performance of various preservative systems
2008 - IRG/WP 08-20393
Standardized above ground tests such as the lap-joint or test deck methods can be very slow in producing useful information on the relative performance of wood preservative systems. It often requires many years for decay to develop in wood treated to sub-optimal concentrations of standardized preservatives, making relative comparisons of performance between new systems and established preservativ...
A Zahora
The Relative Performance of an Organic Preservative System under UC3A and UC3B Conditions using Two Test Methods
2010 - IRG/WP 10-20429
Coated L-joints have been used for decades to evaluate the performance of wood preservatives in protected environments. This study was conducted using matched coated and uncoated L-joints to simulate above ground protected and unprotect exposures. When exposed to constant moisture in a greenhouse environment, coated and uncoated L-joints give very similar performance results. In contrast, exposi...
C F Schauwecker, A Zahora, A F Preston
Above ground testing at tropical test sites, what have we learned?
2011 - IRG/WP 11-20473
Three different above ground test methods have been utilized at a selection of five tropical and sub-tropical test sites with a variety of treated and untreated material. The results show that a multi-site approach to above ground field tests presents the opportunity for exposure to un-predicted biodeterioration hazards, which may be important for developmental products of poorly characterized fu...
A Preston, A Zahora, Y Cabrera, L Jin, C Schauwecker, P Walcheski
Comparison of rates of wood decay from four different field test protocols following 4-5 years exposure at a site in New Zealand
2011 - IRG/WP 11-30565
The rate of decay of Pinus radiata was evaluated using four different field test protocols at a site near New Plymouth, New Zealand. The average Scheffer index was 86 over the five year period of testing. The field tests were an in-ground stake test (AWPA Std E7-01) and three above ground tests – lap-joint (AWPA Std E16-98), decking (AWPC protocol) and ground proximity tests (AWPA Std E18-06) T...
P Lobb, K Day, A Siraa
Use of the durable species Coast Redwood as a reference system for field testing of Wood Protection systems
2012 - IRG/WP 12-20486
Data is provided and discussed for a number of field exposure tests where the naturally durable wood species Coast redwood, Sequoia sempervirens, was included along with untreated pine and standard preservative treatments. In general, there is potential for higher variability of results with this naturally durable species, but it does suggest that redwood can be a useful reference material for te...
A Zahora, A Preston, L Jin
Moisture performance based wood durability testing
2012 - IRG/WP 12-20495
In the frame of a scientific cooperation within the Swedish research program ‘WoodBuild’ comparative field and laboratory durability studies have been carried out by the Technical Research Institute of Sweden SP and Leibniz University Hannover. One objective was to improve test methods as well as evaluation systems in order to facilitate the use of (field) testing for service life prediction. ...
L Meyer, C Brischke, A Pilgård
Update on "Sandwich" Type Above Ground Field Test Methods
2013 - IRG/WP 13-20506
Our research group has been investigating a number of new designs for above ground field testing to try to provide rapid methods to compare the relative performance of systems in above ground, unprotected exposures. This paper provides an update on what we have found with three variations on a "sandwich" type above ground test arrangement, with comparison to the more traditional lap-joint method ...
A Zahora, L Jin, A Preston
A critical view on early indicators for above ground field performance of wood
2013 - IRG/WP 13-20509
Above ground field tests are quite often a balancing act between the provision of realistic test conditions, reliable statistics, and acceptable long test durations. Within this study we therefore reviewed 543 data sets from above ground field tests performed at 36 different test sites in 8 countries in Australia and Europe. The main objective was to investigate possible correlations between early...
C Brischke, L Meyer, G Alfredsen, P-O Flæte, L Francis, M Hansson, P Larsson Brelid, J Jermer
Field test method for wood in above ground situation - The full CEN/TC 38 guideline for the Sandwich method. Part 1 - Determining the relative protective effectiveness of a wood preservative
2024 - IRG/WP 24-41013
The attached draft CEN Technical Specification (i.e. pre-EN standard) has been drafted in order to become an alternative to the Lap-Joint test method (EN 12037:23) for testing of wood in above ground situation and the draft CEN/TS Part 1 is specifically intended for determining the relative protective effectiveness of a wood preservative. The new draft CEN/TS is based on a test method developed by...
M Westin, R Ringman, A Christof, F Friese
Programme section 2, Test methodology and assessment
1997 - IRG/WP 97-20126
IRG Secretariat
A comparison of soft rot, white rot and brown rot in CCA, CCP, CCF, CCB, TCMTB and benzalkonium chloride treated Pinus radiata IUFRO stakes, after 9-15 years exposure at five test sites in New Zealand
1991 - IRG/WP 1485
The aim of this study was to determine if decay type varies significantly between five field trial test sites of different soil type, aspect and climate in 9-15 year old, replicate CCA, CCF, CCP. CCB, TCMTB and AAC treated IUFRO stakes. A visual on-site assessment of decay type on every test stake was made and observations confirmed by microscopical examination. Regression analyses were used to de...
R N Wakeling
Wood preservatives: Field tests out of ground contact. Brief survey of principles and methodology
1976 - IRG/WP 269
This paper contains the following spots:
1.: The general need for field tests. 2.: Interests and limits of field tests in ground contact. 3.: Various methods in use for out-of-ground contact field tests. 4.: Fungal cellar tests are they an alternative to above-ground decay exposure tests? 5.: Conclusions....
M Fougerousse
Collaborative soft rot tests. Names and addresses of collaborators
1973 - IRG/WP 231
IRG Secretariat
A suggested method to test the toxicity of wood preservatives towards the house longhorn beetle
1977 - IRG/WP 275
This method was developed in the Institute for Wood Technology in Sarajevo, Yugoslavia and is used to get quick information on the toxicity of wood preservatives against house longhorn beetle (Hylotrupes bajulus). The method can be used for superficially treated or deeply impregnated wood blocks, and by using small or normal size test material it can be used as a laboratory or field test, and also...
N Vidovic
IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 2: Report of treatment and installation in Australia
1978 - IRG/WP 440
The purpose of this test and the procedures to be followed have been fully set out in documents distributed by the International Research Group on Wood Preservation and numbered IRG/WP/414 and IRG/WP/420. The prescriptions set out in these two documents have been closely followed....
J Beesley