Loss of preservatives from treated wood during service
1992 - IRG/WP 92-3734
During the 23rd IRG conference in Harrogate the matter of preservative losses from treated wood during service was raised. We were asked to collect information in this field and ask now for help from you. Many tests have been carried out at a laboratory scale to study fixation and leaching from wood treated with different preservatives. Very little, however, is reported on losses of preservatives ...
M-L Edlund, D Rudolph


Assessment of losses of wood preservatives from treated wood by leaching into the environment
1993 - IRG/WP 93-50001-13
Wood preservative chemicals may be lost from treated timber by leaching into water or soil. The degree to which this might occur and its effect on the environment is difficult to assess quantitatively due to the absence of appropriate test methods. This paper describes work to assess test methodology capable of allowing the rates of loss of wood preservative from treated timber to be quantified. T...
R J Orsler, G E Holland


Utility, deterioration and preservation of marine timbers in India
2005 - IRG/WP 05-40314
Timber is extensively used in India in the marine environment for various purposes due to its several advantages over modern materials. Infact, its use is increasing in recent years, finding wider and wider applications and this scenario is not going to change in the near future. Though, the bio-deterioration problem is found very severe in tropical waters, still indigenous methods are widely empl...
B Tarakanadha, M V Rao, M Balaji, P K Aggarwal, K S Rao


The rate of redistribution and loss of leachable preservatives under service conditions
1993 - IRG/WP 93-30026
This paper describes experiments carried out to determine patterns of preservative redistribution and any associated losses which occur when wood containing unfixed water-soluble wood preservatives is exposed to service conditions where leaching is possible. Scots pine sapwood treated with disodium octaborate was used as a model system. Results are recorded and discussed for trials representing pa...
R J Orsler, G E Holland


The shower test method. A leaching test for assessing preservative losses from treated timber under simulated open storage conditions
1993 - IRG/WP 93-50001-04
In the late 1980's against the background of increasing environmental concern a laboratory based accelerated leaching test method for assessing preservative losses-from stored, treated timber was developed by the Dutch organisation for applied Scientific Research (TNO). This test method quantifies the amount of specific preservative components which leach from treated timber under simulat...
J B G A Havermans, W J Homan, M J Boonstra


Volatile losses of wood preservatives
1973 - IRG/WP 236
The purpose of the work we have undertaken so far has been to try to quantify the volatile losses which occur in treated timber, and to examine some of the factors which influence these losses. The preservative compound chosen for the initial part of the programme was the contact insecticide g-BHC. This was attractive for several reasons, not the least of which was that specific and sensitive anal...
J W W Morgan, D F Purslow


Losses of preservatives from treated wood during service. Results from a questionnaire
1994 - IRG/WP 94-50031
From environmental as well as from performance point of view it is of interest to know how much of the preservatives in treated wood that is leached out or evaporated from the wood during service. Many laboratory studies are carried out on leaching from small samples in distilled water or water with different pH. These studies give a good picture of the relative leaching from wood treated with dif...
M-L Edlund


A technique for measuring preservative loss or redistribution during leaching
1983 - IRG/WP 2199
Radiata pine sapwood stakes were treated with benzalkonium chloride (AAC) or copper-chrome-arsenate (CCA). After fixation and drying the outer 2 mm and 2-4 mm layers were removed from one radial longitudinal face. The planed face was coated with a waterproof coating and AAC-treated stakes were leached for 6, 12 or 18 weeks; 12 weeks for the CCA-treated stakes. After airdrying three 2 mm layers (0-...
J A Drysdale


Correlation between modulus of elasticity, mass losses and FTIR spectra of copper treated decayed wood
2006 - IRG/WP 06-10580
The composition of copper-based preservatives will change from copper-chromium to copper-ethanolamine, due to environmental demands. The most important drawback of copper-impregnated wood is the presence of tolerant fungal organisms that have developed an ability to degrade such preserved wood. In order to elucidate these processes, specimens (0.5×1.0×15 cm) made of Norway spruce (Picea abies) w...
M Humar, B Bucar, F Pohleven


Danish wood preservatives approval system with special focus on assessment of the environmental risks associated with industrial wood preservatives
2001 - IRG/WP 01-50166-01
The following is a description of the procedure used by the Danish Environmental Protection Agency to assess the environmental risks associated with preservatives used in the pressure impregnation of wood. The risk assessment covers issues considered to be of significance for the environment and which are adequately documented so as to allow an assessment. Such issues are persistence and mobility ...
J Larsen


Finishes for outdoor timbers
1975 - IRG/WP 378
Anonymous


Management of the wood and additives wastes in the wood processing industries: Problematics and technical answers review
1996 - IRG/WP 96-50073
Management pathways for pure wood subproducts are well known and used; but as soon as additives like preservatives, glues, varnishes or coatings are present within the wood wastes, their disposal or valorization becomes more tricky. The different kinds of mixed wood wastes of the wood processing industries, from the sawmill to the furniture manufacture, are identified herewith and their diversity ...
S Mouras, G Labat, G Deroubaix


Proposed method for out-of-ground contact trials of exterior joinery protection systems
1981 - IRG/WP 2157
Methods for testing the efficacy of preservative treatments for exterior joinery are described using the format of a European Standard. Commercially used treatments applied to jointed test units (L-joints) which are then protected by conventional finishes are exposed to normal outdoor hazards out of ground contact. Assessment is made a) by determining eventual failure through decay and b) by destr...
J K Carey, D F Purslow, J G Savory


JWPA method for testing effectiveness of surface coatings with preservatives against decay fungi
1981 - IRG/WP 2164
In 1979 JWPA established a new method for testing effectiveness of surface coatings in accordance with practical use of preservative-treated lumber. Comparing the new testing method with JIS A 9302, a few new trials - size of wood specimen, weathering procedure, and decay-test procedure - are incorporated....
K Tsunoda


Wood preservation in Poland
2004 - IRG/WP 04-30362
Dynamic growth of market demand for wooden elements and articles, generated in Poland increase of interest in industrial preservation. Today, Poland is a substantial producer and exporter of wood made products. Majority of exported wood - approximately 70% - is scotch pine (Pinus silvestris L.), which, due to its natural durability, requires preservation....
A Kundzewicz


Wood preservatives: Field tests out of ground contact. Brief survey of principles and methodology
1976 - IRG/WP 269
This paper contains the following spots: 1.: The general need for field tests. 2.: Interests and limits of field tests in ground contact. 3.: Various methods in use for out-of-ground contact field tests. 4.: Fungal cellar tests are they an alternative to above-ground decay exposure tests? 5.: Conclusions....
M Fougerousse


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 2: Report of treatment and installation in Australia
1978 - IRG/WP 440
The purpose of this test and the procedures to be followed have been fully set out in documents distributed by the International Research Group on Wood Preservation and numbered IRG/WP/414 and IRG/WP/420. The prescriptions set out in these two documents have been closely followed....
J Beesley


Field test evaluation of preservatives and treatment methods for fence posts
1985 - IRG/WP 3347
This work presents the field test results after fifteen years exposure of Eucalyptus saligna fence posts treated with six different preservatives and five treatment methods. All the combinations with oil-borne preservatives presented the best results and among the waterborne preservatives, the fence posts treated by immersion method were with the lowest performance in the field test....
G A C Lopez, E S Lepage


Screening potential preservatives against stain and mould fungi on pine timber in Zimbabwe
1995 - IRG/WP 95-30063
The search for environmentally and toxicologically safer chemicals for use in the timber preservative industry against stain and mould fungi has been intensified during the past few years. Results of field tests with two chemicals previously evaluated in the laboratory are presented. The conventional sodium pentachlorophenate was the more efficacious chemical against stain and mould fungi, providi...
A J Masuka


A suggested method to test the toxicity of wood preservatives towards the house longhorn beetle
1977 - IRG/WP 275
This method was developed in the Institute for Wood Technology in Sarajevo, Yugoslavia and is used to get quick information on the toxicity of wood preservatives against house longhorn beetle (Hylotrupes bajulus). The method can be used for superficially treated or deeply impregnated wood blocks, and by using small or normal size test material it can be used as a laboratory or field test, and also...
N Vidovic


Marine testing of selected waterborne preservatives
1987 - IRG/WP 4137
In 1978 a marine test was established at West Vancouver, B C. to determine the performance of selected waterborne preservatives. The preservatives in test were chromated-copper-arsenate (CCA-C), ammoniacal copper arsenate (ACA), a modified formulation of ACA which contained a higher copper content (modified ACA), ammoniacal copper zinc arsenate (ACZA) and ammoniacal zinc arsenate (AZA). The wood s...
J N R Ruddick


Registration and approval of wood preservatives in Australia and New Zealand
2001 - IRG/WP 01-50166-06
Wood preservatives are treated as agricultural chemicals in Australia and, at the time of writing, as pesticides in New Zealand. Antisapstain products are currently considered to be agricultural chemicals in New Zealand while wood preservatives in the future will be considered as hazardous substances under the Hazardous Substances and New Organisms Act when this Act is fully implemented. They are ...
H Greaves


Environmental status of wood preservation in the UK
1994 - IRG/WP 94-50018
The environmental status of wood preservatives and treated wood in the UK is summarised. The current legislatory position with respect to approvals, supply, use and waste disposal is considered. The bibliography at the end of this paper contains details of all publications referred to together with other relevant information although this cannot be exhaustive....
M Connell


Testing of wood preservatives against marine borers (Part 1). Method of testing wood preservatives against marine borers (Part 2)
1971 - IRG/WP 37
P C Trussell, C C Walden


Report on the activities of the European Standardization Committee CEN/TC 38 'Methods of Testing wood preservatives'
1980 - IRG/WP 279 E
G Castan