Your search resulted in 895 documents. Displaying 25 entries per page.
Durability of thermally modified western hemlock lumber against wood decay fungi
2022 - IRG/WP 22-40954
The chemical modification of wood is gaining popularity as a treatment to increase wood durability in the United States. Further standardization and testing of thermally modified North American species is needed to optimize the production of thermally modified products from regionally available resources. This work measures the impact of thermal modification of western hemlock lumber durability ag...
G Presley, J Cappellazzi, I Eastin
Less environmental impact of wood preservatives by considering the risk of attack in addition to the hazard class system
1995 - IRG/WP 95-50040-10
Hazard classes, which are standardized in Europe in EN 335, are most useful to direct chemical wood preservation towards the organisms which may attack wood in the various fields of utilisation. However, hazard only signifies the fact that an attack may occur without considering the actual risk to attack. To minimize the application of chemicals with respect of less environmental impact it is nece...
H Willeitner
Validating a short-term laboratory method to assess the resistance of timber to biodegradation by marine wood-borers
2021 - IRG/WP 21-10975
Novel approaches to protecting wood in coastal and marine environments are needed as the use of traditional broad-spectrum biocides are now restricted. Wood is widely utilised in marine environments where it can be rapidly degraded by wood-boring organisms, causing billions of dollars of damage per annum. Biocidal compounds such as CCA and creosote have been popular treatments for timber products ...
L S Martin, J R Shipway, G P Malyon, S M Cragg
Surface morphology and short-term water uptake of charred and coated wood
2021 - IRG/WP 21-40916
Charring of the wood surface represents a traditional alternative surface treatment technique with the purpose of aesthetics and protection. By the treatment with flame the surface of wood becomes carbonized and a few millimetres thick charred layer is formed on the top of the wooden element. Further, the charred layer can be removed by brushing, which accentuates the structure of the surface. Add...
J Zigon
Genetic relationships of local infestations by Anobium punctatum, Xestobium rufovillosum and their associated predator Korynetes caeruleus from buildings in North-Eastern Germany
2021 - IRG/WP 21-10982
Wood-destroying pests such as Anobium punctatum and Xestobium rufovillosum cause damage to art and cultural objects as well as to buildings. Monitoring population dynamics of pest species as well as of their naturally occurring counterparts are an essential part in the development of biological control measures as alternatives to conventional wood protection. Therefore, both the dispersal and homo...
C von Laar, C Baar, R Plarre, D P McMahon
Studies on the material resistance and moisture dynamics of Douglas fir and Sitka spruce from Slovenia
2021 - IRG/WP 21-20677
Wood in outdoor applications is subject to various decomposition factors. Wood degradation can be prevented by construction details, biocide protection of wood, wood modification, or selection of naturally durable wood species. Unfortunately, the majority of timber species in Europe do not have naturally durable wood. Imported tree species represent a new pool from which we can draw wood species w...
M Humar, B Lesar, D Krzisnik, E Kerzic, R Brus
Effect of a Water Repellent Treatment on Moisture Behavior of Three Australian Hardwoods: A Preliminary Report
2021 - IRG/WP 21-40921
Wood is inherently hygroscopic and will sorb moisture either directly from the atmosphere or via capillary action. Moisture can have marked effects on wood properties and repeated wetting and drying creates dimensional changes that lead to physical damage. Exposure to elevated moisture levels also increases the risk of fungal attack.
Wood preservatives have long been used to minimize the risk of ...
B Hassan, J J Morrell, K Wood
Carbon footprint of a cross laminated timber building – Torvbraten school case study
2021 - IRG/WP 21-50366
Torvbråten school is a public school in Asker, Norway, that has reached many sustainability goals. The school was the second in Norway to have Nordic Swan Ecolabel and has a 60 % reduction in carbon footprint compared to the reference benchmark. The building is made of cross laminated timber (CLT) and extensive wood use in general. From a wood protection viewpoint, will this sustainability sustai...
L G F Tellnes, J K Naess, M R Hanssen, P-O Flate
Categories in wood preservation hazard, risk, and use
1994 - IRG/WP 94-20048
In various countries hazard-, risk-, or use-categories have been established. The different terms seem to be only a sophisticated language problem, but they are rather a basic principle of the philosophy of wood preservation which is going to obtain importance with respect to the low reputation of chemical wood preservatives in an increasing number of countries. Whilst hazard signifies the fact th...
H Willeitner
Pigment production by the spalting fungus Scytalidium ganodermophthorum and its industry potential
2020 - IRG/WP 20-10957
Scytalidium ganodermophthorum is best known as a pathogen of cultivated mushrooms, with infected cultures turning yellow in color. The fungus is also used in the art form known as ‘spalting’ to produce yellow, green, and purple colors in wood for decorative purposes. Wood colored by fungus in this manner has been traditionally used in the creation of fine art and woodworking since the 16th cen...
R C Van Court, P Vega Gutierrez, S C Robinson
Different levels of acetylation lead to groupwise upregulation of non-enzymatic wood degradation genes of Rhodonia placenta during initial brown-rot decay
2020 - IRG/WP 20-10958
Rhodonia placenta, often used as a model fungus to represent brown rot fungi, uses a two-stepped degradation mechanism to degrade wood. Regarding the overcoming of wood protection systems the initial degradation phase seems to be the crucial point. A new laboratory test enables the separation of the non-enzymatic oxidative and the enzymatic degradation phases, which has previously been proven chal...
M Kölle, R Ringman, A Pilgård
Durability of tropical species from Peru according to European Standards
2020 - IRG/WP 20-10964
Natural durability is defined as the intrinsic resistance of wood against the attack of destructive organisms. There are standardized methods to estimate a durability value. In Europe, the standard EN-350 is responsible for establishing the basic guidelines, as well as the necessary tests to determine this value, which is essential to know the degree of protection needed for the tested wood to ext...
J Valdivia, P Gómez, M T Troya, L Robertson, J A Martín, A Loayza
Durability of Eucalyptus globulus floating structures mussels trough in marine environment against marine borers in the Atlantic coast of Spain
2020 - IRG/WP 20-10965
In Spain, since forever damages caused by marine borers are frequent in wood elements and wood structures located in sea water conditions. Galicia is a region located in the North West of Spanish, above Portugal, characterized by their typical estuaries, where since ancient times, the natural production of mussels from floating structures mussels trough. Since ever, wood species selected to build ...
D Lorenzo, M Touza, J Fernández-Golfin, A Lozano, J Benito
Moisture and temperature conditions in an old, highly moisture-loaded timber building in the Røros municipality, Norway
2020 - IRG/WP 20-10966
A 150 years old log building near Røros, Norway, has been in active use as a cowshed since its erection. The animals are kept inside the cowshed all winter and this causes a situation of a high moisture load on the wooden floor, wooden walls and ceiling. Logging of temperature and humidity over one year shows that there are favourable levels of moisture in the wood and air for development of moul...
M Sand Austigard, J Mattsson
Resistance against marine borers: About the revision of EN 275 and the attempt for a new laboratory standard for Limnoria
2020 - IRG/WP 20-20669
Wood protection technology in the marine environment has changed over the last decades and will continue to do so. New active ingredients, newer formulations, and novel wood-based materials including physically- and chemically-modified wood, together with increasing concerns over environmental impacts of wood preservatives, urgently demand a major revision of EN 275 “Wood preservatives – Deter...
S Palanti, S Cragg, R Plarre
Monitoring of wood preservatives exposed to weathering: Extraction and analysis methods of organic biocides from treated wood and collected rain runoff
2020 - IRG/WP 20-30753
Weathering is the cause of numerous damages for outdoor joineries. Protection of wood using a preservative treatment covered with a coating is a process widely used to limit these damages. However, biocides from preservative treated wood are prone to degradation and leaching, having a direct influence on the joinery service life. This document deals with extraction and analytical methods for bioci...
O Ouali, K Le Ménach, E Raphalen, L Podgorski, S Legay, H Budzinski
Long-term field exposure of wood-plastic composites processed on a commercial-size extruder
2020 - IRG/WP 20-40894
Wood-plastic composites (WPC) contain wood fiber (or flour), thermoplastics and additives and are exposed to UV light, moisture, and biological deterioration in outdoor installations. Accelerated laboratory tests can help to predict the durability of WPCs, but long term evaluations are needed to validate these results. Field exposed above-ground WPC deck boards (30.5 x 139.7 x 609.6 mm) and in-gro...
R E Ibach, C M Clemmons, N M Stark
Performance of a water-borne stain on beech, spruce, MDF and OSB improved by plasma pre-treatment
2020 - IRG/WP 20-40897
Coatings are an important part of wood protection, especially for outdoor applications. In order to provide a good protection, protective coatings need to exhibit good adhesion, mechanical resistance, and weathering resistance. Plasma pre-treatments are an established method to increase the performance of existing coatings including those on wood and wood-based substrates. Moreover, plasma deposit...
S Dahle, J Žigon, I Uranjek, M Petrič
Potenzy of Azadirachta indica heart wood extracts as wood bio-preservative against termite attack
2020 - IRG/WP 20-10972
Extractives in wood are one of the main reasons for wood resistance against bio-degradation. The chemical compositions of extractives from matured Azadirachta indica that are known to be very resistant against bio-degradation were studied to assess their role as wood preservative. Ethanol and toluene were used in the extraction of these compounds from the heartwood of Azadirahcta indica. Chemical ...
L O Aguda, O B Olajide, O Y Aguda
Extraction, identification and antifungal activity of polar extractives originated from various wood species
2020 - IRG/WP 20-20673
Extractives are non-cell wall small molecules present in wood and other lignocellulosic materials that can be removed by solvents. Although they represent a minor fraction in comparison with the structural cell wall components, they are an important source of functional groups or molecules with bioactivity or antioxidant properties, that could be used in medicine, cosmetic or wood preservation. T...
R Herrera, F Poohphajai, J Labidi, S Willför, A Sandak
Biofinish: A Functional Wood Surface Treatment based on Aureobasidium
2020 - IRG/WP 20-40903
Xyhlo Biofinish is a natural and environmentally friendly wood protection concept based on linseed oil impregnation and a fungal-based coating. It emerged in the late 1990s and has been developed over the past 15 years into an industrially applicable process in the Netherlands. The combination of linseed oil impregnation and a surface treatment with the living fungus Aureobasidium extends the serv...
S Rensink, M Sailer, S Roukens, J Gerber, H van der Mel, K Potgieter, J Spit, R Bulthuis, C Struck, M Bennink
PlasmaSolution – Curing of coating formulations using non-thermal plasmas
2020 - IRG/WP 20-40904
Coatings are an important part of wood protection, especially for outdoor applications. In order to provide a good protection, protective coatings need to exhibit good adhesion, mechanical resistance, and weathering resistance. Plasma pre-treatments are an established method to increase the performance of existing coatings including those on wood and wood-based substrates. Moreover, plasma deposit...
S Dahle, J Žigon, M Petrič
Thermal spray coatings to protect wood from termites
2020 - IRG/WP 20-40905
Protecting buildings and construction materials against subterranean termites in Europe relies on combined physical and chemical approaches. Buildings can be protected by physical or physico-chemical barriers such as gravel aggregates, steel mesh or plastic films impregnated with insecticides. Wood and wood-based materials are traditionally protected by insecticides applied on the surface or deepl...
L Podgorski, H Myalska, A Dinoirjean, M Kutnik
Silicate coatings for wood substrates
2020 - IRG/WP 20-40906
Silicate coatings are surface finishing products containing alkali metal silicates or ethyl silicates as main binders. They are traditionally designed and well established for mineral substrates or corrosion protection of steel. The interest for these coatings in wood field is growing because of the benefits they could provide such as high durability, weathering resistance and fireproofing and sus...
A M Cheumani Yona, M Pavlič, M Petrič
Hydrophilization of wood using a FE-DBD air plasma
2020 - IRG/WP 20-40907
One of the goals of surface protection of wood with coatings is to prevent the evolution of moisture in wood, which accelerates its degradation by abiotic and biotic factors. Good wettability of wood is a necessary pre-condition for sufficient protection with water-based coatings. Treatment of wood surface with atmospheric dielectric barrier discharge in configuration with a floating electrode was...
J Žigon, M Petrič, S Dahle