IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 789 documents. Displaying 25 entries per page.


Eastern redcedar included sapwood: Resistance to mold and termites under laboratory conditions
2012 - IRG/WP 12-10765
The heartwood of eastern redcedar (Juniperus virginiana) frequently contains areas of light-colored wood. This “included sapwood” is considered to be a defect by some manufacturers. In this study, sapwood, included sapwood and heartwood samples from five eastern redcedar trees were exposed to mold fungi or to subterranean termites in a no-choice feeding test. Extractives content was also measu...
C Köse, A M Taylor


Using an accelerated laboratory method to evaluate Aureobasidium pullulans colonization on painted surfaces and underlying wood substrate
2012 - IRG/WP 12-20480
Mold growth on painted surfaces can lead to premature paint film failure and is unsightly. Aureobasidium pullulans has been identified as a major cause of black stain on surfaces painted with acrylic or latex paints. In this study, an accelerated laboratory method developed by Zabel and Horner (1981) was used with modifications to the type of agar used and sample evaluation methods. A study was ...
C Schauwecker, L Burns, A Preston


Supercritical impregnation of wood with siloxane
2012 - IRG/WP 12-30595
This paper describes the effect of supercritical impregnation with siloxane on the water repellency of Scots pine (Pinus sylvestris) sapwood samples. Samples were impregnated with a low amount of siloxane dissolved in supercritical carbon dioxide using isopropanol as a co-solvent. Siloxane retention (i.e. weight percent gain (WPG)) of the treated samples was 1.3 % (w/w) as found by mass balance. T...
A Kjellow, F Imsgard, J Fernandes, O Henriksen, E Klaassen, R Wagner, J Delis


Tar-oil uptake vs time in immersion treatment of short pine posts: A simple technique applicable to rural communities of Papua New Guinea
2012 - IRG/WP 12-40608
Pinus caribaea and Araucaria cunninghamii logs ca. 100 mm in diameter were shortened to lengths 25-30 cm, conditioned to at/below fibre saturation point (FSP) for immersion/dip treatment using a hot- and- cold bath open- tank process. Before oven-drying and subsequent treatment, individual test specimens were numbered, their green weights and volumes, and dry weights recorded for basic density, vo...
B K Gusamo, R Tulo


Succession after Fire of Fungal Fruiting Bodies in Mediterranean Pinus pinaster Stands in Spain
2012 - IRG/WP 12-10789
In this study we present the results of a 4-year survey aimed at describing the succession of fungal communities following fire in a Mediterranean ecosystem in Northwest Spain, dominated by Pinus pinaster Ait. After a large wildfire in 2002, six 2 x 50 m study plots were established in burned and unburned areas corresponding to early and late succession stages. During the autumn seasons from 2003 ...
P Vásquez Gassibe, M Hernández-Rodriguez, R Fraile Fabero, J A Oria-De-Rueda, P Martín-Pinto


Effectiveness of CCA-C and CCB preservatives after a 30 years stake test
2012 - IRG/WP 12-30606
The objective of this experiment was to assess the durability of four pine species treated with waterborne preservatives. In order to determinate this, a stake field test, following the IUFRO (International Union of Forestry Research Organizations) recommendations, was installed at Experimental Station of Luiz Antonio (21º 32’ S and 47º 42’ W), State of São Paulo, Brazil. Species under t...
I PJankowsky, E S Lepage, C Salvela, J M Vidal, S Takeshita


Effect of preservative treatment on mechanical performance of round and square poles made of small diameter Scots pine
2012 - IRG/WP 12-40612
A growing proportion of harvested Scots pine (Pinus sylvestris L.) timber originates from the first or second commercial thinning stands. There is a need to find economically viable and high quality wood products that can be manufactured from this raw material. Small log volume means not only demands of increased efficiency for material handling in logistics and manufacturing processes, but also c...
V Möttönen, R Stöd, K Heikkilä, H Heräjärvi


Water absorption and desorption of non treated, pressure impregnated, and pine oil treated glulam made of small diameter Scots pine and Norway spruce
2012 - IRG/WP 12-40616
A growing proportion of harvested timber originates from the first or second commercial thinning stands in Finland, which means smaller average log volumes in comparison to final felling stands. Smaller log volume means challenging wood properties such as higher proportion of juvenile wood and sapwood. Due to these facts, products made of small diameter logs are prone to twist and check, and have ...
H Heräjärvi, V Möttönen, R Stöd


The assessment by visual grading, change of color and ergosterol content ratings, the resistance to mould fungi of treated with wood preservative Scots pine sapwood
2013 - IRG/WP 13-20514
The filamentous (mould) fungi belonging to Ascomycetes, Deuteromycetes group are an cosmopolitan organisms which attacks wooden elements disfiguring them, dropping their value and causing environmental and health hazard. The fungi in a short time cause mainly disfigurement of wood does not effect on strength properties of wood, but with strong prolongation of duration of conditions favourable for ...
A Fojutowski, A Koziróg, A Kropacz


System treatments of Pinus sylvestris - influence on moisture, decay and discoloration
2013 - IRG/WP 13-30612
Biological activity can cause challenges for the use of wood in outdoor exposure. Decay and discolouring fungi influence the service life of wooden constructions, and the moisture content of the wood is often an important factor. The aim of this study was to evaluate the performance of different combinations of preservative/modified wood protection treatments and surface treatments for wooden deck...
A Schabacker, G Alfredsen, L Ross Gobakken, H Militz, P O Flæte


Copper leaching from copper-ethanolamine treated wood during exposure to terrestrial microorganisms
2013 - IRG/WP 13-30621
Copper-ethanolamine based wood preservatives are still the most important solutions for protection of wood in ground applications in Europe. Wood in ground is exposed to variety of organisms, which can act synergistically. In order to simulate these conditions in laboratory, Scots pine (Pinus sylvestris) specimens impregnated with copper-ethanolamine preservative of three different concentrations ...
M Humar, N Thaler, B Lesar


Decay resistance of thermally modified Scots pine after 6 years’ exposure above ground
2013 - IRG/WP 13-40624
In the present study the performance of boards treated by ThermoWood process were studied above ground and the results given are based on a “modified” horizontal double- layer test. The base layer of boards was in direct contact with ground and the conditions were much harder than in the standard method. After six years’ exposure clear differences were found between untreated Scots pine and ...
H Viitanen, S Metsä-Kortelainen, A Nurmi, S Jämsä


Protective effectiveness of antifouling coatings for wooden boats in the Northern Adriatic Sea
2013 - IRG/WP 13-40634
There are various conventional biocide containing antifouling coatings and some more environmentally friendly paints for boats on the market. However, the question of their performance in accordance with the manufacturers’ statements or guaranties arises. The aim of our preliminary investigation was to state which type of antifouling coating exhibits better effectiveness against fouling organism...
M Petrič, M Humar, J Adamek, B Kričej


Unexpected natural decay resistance strategies of durable tropical woods Bocoa prouacencis, Vouacapoua americana, Inga alba and relationship with specific gravity and wood extractives
2014 - IRG/WP 14-10832
The study of decay resistance in wood is of interest for wood end-users but also for the global carbon balance since wood biodegradation is a key driver of forest ecosystem functioning through its impacts on carbon and nutrient cycling. We studied the specific gravity and wood extractive contents in order to understand decay resistance against soil microflora after 90 days exposure of sapwood and ...
N Amusant, M Migg, B Thibaut, J Beauchene


Assessment of Scots pine sapwood susceptibility to moulds by determination of fungi growth and ergosterol content in infested wood
2014 - IRG/WP 14-20540
The susceptibility of wood to filamentous fungi (mould) attack is determine mainly by laboratory methods with descriptive grading of fungal growth on the surface of the wood specimens. It is a lot of different grading scale of fungi growth, but determination of the size of fungi growth is many times not easy, not clear and often difficult. Although the filamentous fungi are not included to microor...
A Fojutowski, A Koziróg, A Kropacz


Copper and chromium leaching from wood impregnated with chromium-copper containing preservatives: Results of different studies
2014 - IRG/WP 14-50300
Copper and chromium based wood preservatives remained one of the most important ingredients for wood protection solutions for protection of wood in demanding applications all-over the world. Leaching of heavy metals from treated wood is important from two different aspects; firstly from performance point of view, and secondly from environmental issues. However, the importance of these studies is i...
M Humar, N Thaler, E Melcher


Functional silicones used as a potential tool for the development of non-biocidal wood treatments
2015 - IRG/WP 15-30665
The increase of wood resistance against biological agents for outdoor use is conventionally performed by deep impregnation with preservatives. However, some of the traditional wood preservatives, used for decades for wood protection and regarded as the most effective, are currently subjected to severe restrictions because of their toxicity. In fact, new preservation technologies are constantly ent...
F Lhumeau, C Delaite, F Marchal, F Pochon, M Kutnik


Performance of kiln-dried and air-dried anti-sapstain treated pallet timber under use scenarios against wood discolouring fungi
2015 - IRG/WP 30669
During their lifespan there is a high probability that wooden pallets and packaging material will be exposed to rainfall or rewetting conditions, increasing the risk of growth of discolouring fungi. Kiln-drying of wooden pallets and packaging material without anti-sapstain treatment does not give efficient protection against wood discolouring fungi during rewetting periods. However additional temp...
A Steitz, E Stoyanova, N Pfabigan, R Gründlinger


Remedial treatment of difficult to access timber in buildings
2015 - IRG/WP 15-40691
The quest to understand remedial treatment for timber framing begun following the ‘leaky building crisis’ in New Zealand which came to prominence in 2000. Several in-situ remedial treatment products are used in New Zealand. However, effectiveness of these treatments is still unclear particularly in situations where not all faces of the timber can be assessed. This research was conducted to det...
T Singh, I Simpson, D Page


Termite and insect resistance of acetylated wood
2015 - IRG/WP 15-40703
The benefits from acetylation of wood to enhance resistance against fungal decay and dimensional stability have been known for many years. Since 2007 Accsys Technologies has been commercially producing Accoya® wood that is based on acetylation of radiata pine. A number of studies on the resistance of acetylated wood to attack by wood destroying termites have been conducted, but there is no common...
F Bongers, M Kutnik, I Paulmier, J Alexander, H Militz


GC-MS Characterizations of Termiticidal Heartwood Extractives from Wood Species Utilized in Pakistan
2016 - IRG/WP 16-10857
Wood species that exhibit innate tolerance to wood destroying organisms such as termites are considered to be naturally durable. This durability can, in part, be due to the complex chemical compounds in the heartwood of naturally durable wood species. We examined the effects of varying concentrations of heartwood extractives on the subterranean termite, Reticulitermes flavipes from four wood spec...
M E Mankowski, B Boyd, B Hassan, G T Kirker


Durability to decay organisms of Pinus nigra subsp. laricio var. corsicana. Influence of the moon phase
2016 - IRG/WP 16-10869
Actually the use of wood has an added value since it is a renewable, biodegradable and recyclable material. For this reason, the evaluation of it natural durability is essential when establishing the level of protection required, being depending on the designated end use of timber. On the other hand, there is a popular belief based on the influence of the moon phase in felling timber, recommending...
M T Troya, M Conde, M J Barriola, F Llinares, V Dorronsoro


CCA Treated Wood, Will It Last 100 Years?
2016 - IRG/WP 16-20575
Copper, chrome and arsenate (CCA) treated wood has a very successful history of use in New Zealand, for at least 60 years. In many parts of the world, CCA has been used for timber treatment since the mid-1930s. In this report, data are presented on the performance of CCA treated pine stakes and poles. Results from ground contact durability tests at Scion and other overseas test performance data su...
T Singh, D Page


Measurement of Cell Wall Moisture in Acetylated Radiata Pine Using Low-Field Nuclear Magnetic Resonance
2016 - IRG/WP 16-20583
Understanding the interaction of water with acetylated wood is necessary to explain how the protective mechanism of acetylation functions. Low-field nuclear magnetic resonance is one technique for assessing water in wood. Pinus radiata earlywood sapwood samples were acetylated to various weight percentage gains and then analysed with this method. Increased levels of acetylation showed significantl...
H G Beck, C A S Hill


Distribution and penetration of the tung oil in wood studied by high-resolution magnetic resonance imaging
2016 - IRG/WP 16-20593
Water repellents as environment-friendly treatments are gaining their popularity as non-biocidal solutions for wood protection. One of the most important water repellents for wood besides waxes and organosilicon compounds are drying oils. Tung oil is one of the best performing oil. However, tung oil, similarly as other oils, does not penetrate deeply into wood, due to its high viscosity. In order...
M Žlahtič, U Mikac, I Serša, M Merela, M Humar


Previous Page | Next Page