Your search resulted in 10 documents.


Introduction to a field demonstration of various instruments and methods for the detection of defects in poles
1984 - IRG/WP 2228
H Friis-Hansen


Quantitative assessment of the condition of field specimens
1981 - IRG/WP 2154
Suggestions for a discussion on the desirability of an extension to the existing procedure of assessment of the condition of field specimens by adding more objective, reproducible methods in order to obtain earlier and more specific information than at present on the effect of biological attack on strength and other properties of the specimens as well as the time aspect....
H Friis-Hansen


Report on a field demonstration of methods for detecting defects in wood poles
1984 - IRG/WP 2232
P I Morris, H Friis-Hansen


Summarized comparison of four techniques for detecting defects in poles
1979 - IRG/WP 2126
Since our discussions in open session of Working Group II at Peebles, a number of workers in Australia have collaborated in comparing the efficacy of X-ray, sonic testing, or resistivity measurements for detecting internal defects in poles. The purpose of this circular is to draw to your attention some of the results, in summary form. No attempt has been made to compare techniques. More detailed a...
H Greaves


The secondary treatment of creosoted electricity poles with fused boron rods
1988 - IRG/WP 3485
After preliminary trials selected poles were treated at the groundline with fused boron rods. Early samplings showed that movement was slow in the dry heartwood but after six years the distributions obtained indicate that the system has merit for the treatment of the heartwood of poles in service....
D J Dickinson, P I Morris, B Calver


Decay, decayed wood and the Shigometer
1980 - IRG/WP 281
A L Shigo


The use of the Shigometer® and Pilodyn® as non-destructive test methods for detecting decay in CCA treated eucalypt poles
1981 - IRG/WP 2153
The groundline condition of sixty C.C.A. treated eucalypt poles comprising six different species was examined using the Pilodyn® and Shigometer®. Although sensitive to the presence of soft-rot decay, the Shigometer® would seem to offer little practical advantage in the eucalypt soft-rot decay situation, since a comparable visual examination could reveal the presence and extent of decay. Initial...
L E Leightley


Evaluation of the pulsed-current resistance meter (Shigometer®) for determination of the internal condition of utility poles
1979 - IRG/WP 2128
A number of Telecom poles, which had been removed from service to be replaced by a radio link, were inspected using an electrical resistance meter (Shigometer®). These poles were creosoted, non-durable Victorian species in service in New South Wales. Six of these poles, chosen to represent various internal conditions typical of the range of the population tested, are discussed here. Data, from tr...
J D Thornton, W G Seaman, M McKiterick


The effect of moisture content on the electrical resistance of timber as detected by a pulsed current reistance meter (Shigometer)
1984 - IRG/WP 2212
The literature concerning the use of the Shigometer® for detecting decay in standing trees and wood poles is reviewed and the differences of opinion over the effect of timber moisture content on electrical resistance are highlighted. A simple experiment designed to test this effect is described and the implications of the results for testing poles in service are discussed. There was a large diffe...
P I Morris, D J Dickinson


Soft rot in heartwood of preservative-treated pole stubs of Eucalyptus cypellocarpa L. Johnson
1983 - IRG/WP 1204
Pole stubs of Eucalyptus cypellocarpa L. Johnson, treated in the sapwood with certain waterborne preservatives and exposed for 21 to 23 years in a dry tropical region were severely soft-rotted in the heartwood, as well as the sapwood. They broke with a brash fracture when stress tested (loaded as a cantilever) in the field. The severe soft rot in the heartwood was not detected by the knife test or...
J E Barnacle, G C Johnson, M A Tighe