Your search resulted in 1181 documents. Displaying 25 entries per page.
Influence of variable lignin content on brown rot decay of wood
1987 - IRG/WP 1320
Compilation of published data and new experiments with brown-rotting fungi on different timber species suggest that their decay activity, in contrast to soft rot and white rot fungi, is not greatly influenced by the type or amount of lignin present....
T Nilsson, G F Daniel
How to keep coated wood structures sufficiently dry to avoid damage caused by rot
1991 - IRG/WP 2376
During the last ten years, a new type of problems with wood rot has emerged in Scandinavia. Thousands of houses have been damaged by wood rot attaching to the exterior wood panel. This paper provides an overview of finished and ongoing work in order to identify the cause of these problems. In field tests, the moisture conditions were measured in panels coated with different paint systems. The infl...
S Hjort
Biological resistance of phenol-resin treated wood
1990 - IRG/WP 3602
Biological resistance of PF (phenol formaldehyde resin) - treated wood has been tested in relation to the resin properties, wood species and biological factors. When tested using water-soluble PF (mol. wt. 170), ca. 10% RI (resin impregnation) was enough to suppress the decay of Japanese cedar (Cryptomeria japonica) and western hemlock (Tsuga heterophylla) blocks exposed to Tyromyces palustris (br...
M Takahashi, Y Imamura
Conditions and possibility of nanobiocides formulation for wood protection
2008 - IRG/WP 08-30467
During development of nanobiocides for wood protection the need to identify mineral composition of wood in respect of trace elements and nourishing conditions of wood destroying fungi in relation to these elements was discussed....
J Wazny, A Kundzewicz
The resistance of wood coated with different solvent-borne paints against colonisation by decay fungi
2009 - IRG/WP 09-40468
This paper examines different solvent-borne paints characteristics and their decay resistance when applied on pine wood surface. It was determined by the standard ENV 839 procedure. The part of samples were subjected to accelerated ageing according to the EN 84 standard. The discussed commercial paint systems were typical stains or penetrating oil-based products, with or without biocides....
B Mazela, P Hochmańska
Suppression of aerial hypha formation by spent culture filtrate of a non-degradative strain of Postia placenta
1991 - IRG/WP 1498
ME20, a wild-type monokaryotic strain of the brown-rot fungus Postia placenta, does not cause significant weight losses in standard soil-wood block decay tests and fails to form aerial hyphae in liquid and agar culture. This abnormal morphological feature may be caused by the same aberrant physiology that prevents the strain from degrading wood efficiently. ME20 releases elevated levels of the aut...
J A Micales
Aspergillus fumigatus Fresenius resistance to chemical preservatives in piles of pine and birch wood chips
1981 - IRG/WP 1146
Investigation has been carried out on the communities of fungi developing in birch and Scots Pine chip piles in the Ostroleka Pulp and Paper Mill in the North-East of Poland The species composition or fungal communities and their development in a dozen of chip piles during storage was investigated. Untreated and chemically treated birch and pine wood chips were investigated. In all samples the gre...
M H Zielinski
Wood degradation mechanisms by the brown rot fungus Gloeophyllum trabeum
1997 - IRG/WP 97-10229
A mechanism for the degradation of wood by the brown rot fungus Gloeophyllum trabeum is outlined. The mechanism includes the function of redox-cycling, low molecular weight phenolic derivatives which sequester and reduce iron in acidic environments. The role of oxalate for the sequestration of iron (hydr)oxides and the pH dependent transfer of iron to the G. trabeum phenolic chelators, as well as ...
B Goodell, J Jellison
Copper-resistant fungi on pressure impregnated wood in Denmark
1994 - IRG/WP 94-10078
The occurence of Amorphotheca resinae Parbery and its asexual stage Cladosporium resinae (Lindau) de Vries on CCA and CCB treated wood has previously been shown. In the autumn 1993 some other blue stain fungi were found on CCP and CCB treated pine timber, such as Ophiostoma minus (Hedgc.) H. and P. Sydow, Ophiostoma pilifera (Fr.) H. and P. Sydow and Ophiostona piceae (Munch) H. and P. Sydow. The ...
J Bech-Andersen, S A Elborne
Sapwood staining fungi
1974 - IRG/WP 125
The compilation is based on the available literature and on research results from the Royal College of Forestry, Stockholm but I am aware that there are great gaps in it and so it must be looked upon as a basis for collecting more information about these fungi. The review in the presented form needs an explanation. Preparing this review, the presented schedule was set up to facilitate summarisatio...
A Käärik
The yeast Pichia sp. As a short-term biological control agent to fungal spoilage of sawn softwood timber
2000 - IRG/WP 00-10362
Previous work has found isolates of the yeast Pichia to be a successful biological control agent toward moulding of fruits. An isolate was tested for the ability to protect sapwood of Pinus sylvestris timber against visual degrade by surface growth of moulds and staining fungi. Successful protection of autoclaved wood sprayed with a mixture of common wood moulding fungi was achieved when the yeast...
C Payne, H J Staines, A Bruce
Evaluation of New Zealand staining fungi for degradation of radiata pine
1999 - IRG/WP 99-10310
This investigation sought to determine the potential of selected NZ staining fungi to induce weight loss and changes in toughness (impact bending strength) and composition in unseasoned radiata pine sapwood. Furthermore, assays were performed to eveluate enzyme production by staining fungi. Sets of side-matched specimens were inoculated with Ophiostoma floccosum, Sphaeropsis sapinea and O. plurian...
A Schirp, R L Farrell, B Kreber
The effect of creosote and Basilit on the boards of 4 wood species against destructive fungi in Northern Iran
1989 - IRG/WP 3555
The results of the experiments conducted on the boards of maple, hornbeam, alder and beech, show that under the humid and moderate climate condition of Northern Iran, after 30 months, the witness samples were about 10% destructed by fungi, especially by Schyzophyllum commune and Coriolus versicolor. The impregnated samples by Creosote Basilite using Rueping and Bethell methods, were quite intact. ...
D Parsapajouh
Alternative technologies for wood wastes recycling - Part B: Biotreatment of PCP- and creosote-treated wood
1998 - IRG/WP 98-50101-18 b
Alternative technologies have been investigated to detoxify treated wood. Two classes of organic compounds are studied. Creosote-treated wood are classified in France as dangerous wood wastes. A conventional incineration could be provided for these wood wastes but the cost of this elimination could be very high (> 2000 FFR/ton). For these reasons, we have tested two kinds of new processes as al...
S Legay, P Marchal, G Labat
Iron in stone wool - one reason for the increased growth and decay capacity of Serpula lacrymans
1992 - IRG/WP 92-1537
The chemical compositions of stone wool and glass wool were analysed. There was more iron in the stone wool than in the glass wool. It was found that iron present in stone wool was easily dissolved by oxalic acid that Serpula lacrymans is able to produce. The stone wool promoted the decay of pine wood by Serpula lacrymans. The glass wool had no effect on the decay capacity of Serpula Iacrymans. Th...
L Paajanen, A-C Ritschkoff
Physiologic response of Phanerochaete chrysosporium to exposure to triazole fungicides
1994 - IRG/WP 94-10066
Triazoles are increasingly important fungicides which are employed for a variety of applications included wood protection. Several recent studies suggest that white rot fungi are more tolerant of triazole compounds than other wood degrading fungi. Cultural studies using a white rot fungus, Phanerochaete chrysosporium, and 0.2 or 0.8 ppm of tebuconazole or propiconazole suggested that mycelial dry ...
J J Morrell, R K Velicheti
Laboratory determination of the natural decay resistance of some lesser-utilized timbers from Tanzania against wood decay fungi
2004 - IRG/WP 04-10517
Four lesser known/utilized timber species (sap and heartwoods) from Tanzania, namely Albizia lebbeck, Zanthoxylum gilletii, Faurea saligna and Parinari curatellifolia were exposed to the brown rot fungi (Gloeophyllum trabeum and Coniophora puteana) and the white rot fungus (Coriolus versicolor) to determine their natural decay resistance according to the EN 113 standard procedure. The timbers were...
P R Gillah, R C Ishengoma, E Julias, S A Amartey, D H Kitojo
Remedial treatment of wood attacked by insects
1981 - IRG/WP 3175
A review is presented of remedial treatments against wood-boring insects in wood in service. Preconditions and fundamental principles of insect control are compared with the control of fungal attack and reasons are given for the fact that remedial treatments against insects are more commonly applied than against fungi. With regard to insect control measures with a simultaneous preventive effective...
H Kühne
An evaluation on durability of untreated mining timber support
1997 - IRG/WP 97-20121
Wedge blocks in dimension of 5 x 7 to 8 x 155 cm3 were cut from indigeneous scots pine pitprops. Each of wedge block pairs were numbered and half of them were placed as the test blocks between the steel arches and the strata in a hard coal pit. Controls in laboratory and test wedge blocks in the mine were then sawn into 20 by 20 by 300 mm standard test sticks. Impact bending, static bending and MO...
A Bobat
A potential anti-sapstain chemical for sawmills
1984 - IRG/WP 3300
Several biocidal formulations were tested under laboratory conditions in order to discover an alternative antisapstain chemical to chlorophenoxides. The formulations tested were experimental water solutions containing a quaternary ammonium chloride, a commercial fungicide and/or a sodium salt of some carboxylic acids. The effect of sodium carbonate and borax decahydrate in mixture with a quaternar...
I A Linderborg
Effect of light and ventilation condition on the rate of wood decay by the brown rot basidiomycete, Tyromyces palustris
1991 - IRG/WP 1517
Effect of light and the ventilation conditions of incubation jars on the wood decay by Tyromyces palustris (Berk. et Curt.) Murr. FFPRI 0507 was investigated. Under no irradiation of light, the ventilation conditions gave extensive effect on mass loss of the test pieces when the culturing was performed with culture medium designated in Japanese Industrial Standard (JIS) A 9302 (Medium A; glucose 4...
T Suzuki, M Higaki
Investigation of microwave as a means of eradicating dry rot attack in buildings
1992 - IRG/WP 92-1545
A microwave-apparatus developed for treatment of building-structures infested by dry rot was tested in the laboratory. The test-conditions simulated treatment of either infested timber or infested brickwork. Sawdust samples, both wet and dry, infested by viable mycelium of Serpula lacrymans were packed in glass-tubes. The tubes were then placed in the middle of either 20 cm thick wooden beams or 3...
C Kjerulf-Jensen, A P Koch
The chemical analysis and biological evaluation of wood extractives as potential timber preservatives
1995 - IRG/WP 95-30090
Work involved the biological performance of water and organic solvent soluble extractives of four naturally durable wood species, namely; Matumi, Tamboti, Sneezewood and the Turpentine tree. These timber species are known to be naturally durable against termites and fungi (±25 to 35 years). The extractives were evaluated against termites and fungi using impregnated pine pencil stakes in field tes...
P Turner, D Conradie
Kinetic of the wood degradation produced by wood decay fung
1993 - IRG/WP 93-20016
The degradation degree of a wooden structure has a direct influence on its loss of mechanical strength. It's necessary to deepen in non destructive techniques which permit to extrapolate the results obtained in laboratory to structural timber used in the building's construction. This work studies the relationship existing between the pulse velocity of ultrasonic waves and the wei...
M T De Troya, A M Navarrete, A Sanchez, V Bucur
List of wood-destroying fungi in Iran
1976 - IRG/WP 138
This list gives information on the wood-destroying fungi collected in the Iranian forests and from felled logs and boards in sawmills until now. They are mainly from the region of the Caspian Forests and from the climatically dry region between Teheran and Azarbaidjan, North Iran. It is understood, that this document may help to give more knowledge outside the country about the specific problems o...
P Soleimani