Natural durability and basic physical and mechanical properties of secondary commercially less accepted wood species from Brazil
2002 - IRG/WP 02-10451
The natural durability towards basidiomycete fungi and termites of several secondary timber from Brazil (Vatairea sp., Hymenolobium sp., Inga sp., Manilkara sp., Caryocar sp., Terminalia sp., Apuleia sp.) has been evaluated according to the EN 350-1. Some basic physical and mechanical properties (density, shrinkage, hardness, colour, static strength in flexion and compression) were also measured a...
M-F Thévenon, A Thibaut


Field performance of wood preservative systems in secondary timber species
1997 - IRG/WP 97-30152
The objective of this ongoing study is to evaluate the performance of new, potential, and standard wood preservative systems in secondary North American timber species. Eleven preservative systems were evaluated in this study - ACQ Type B, Copper Citrate 2: l, CDDC, chlorothalonil/chlorpyrifos, copper-8-quinolinolate, tebuconazole/chlorpyrifos, RH287, propiconazole/chlorpyrifos, copper naphthenate...
P E Laks, K W Gutting, R C De Groot


The susceptibility of 35 Amazon wood species to Cryptotermes brevis (Walker)
1982 - IRG/WP 1160
Laboratory tests were carried to evaluate the susceptibility of 35 Amazon hardwoods to Cryptotermes brevis (Walker). The results were analysed statistically and showed that five wood species were non resistant, nine were resistant and the other twenty-one in between those classes of resistance....
M D Canedo


Biological Durability of Laminated Veneer Lumber from Durable and Non-Durable Wood Species
2005 - IRG/WP 05-10567
Laminated Veneer Lumber (LVL) was laboratory manufactured using veneers from decay and non decay resistant species in order to evaluate changes in the durability as a result of the LVL manufacturing process, and to test if the mixing of decay resistant species and non decay resistant species can improve durability. Laboratory soil block test and field test were conducted. The durability of solid w...
P Nzokou, J Zyskowski, S Boury, D P Kamdem


Possibility of use of wood species per class of biological risks. Attempt to determine criteria based on Pr EN 350-1/2/3
1992 - IRG/WP 92-2409
M Rayzal


Utility, deterioration and preservation of marine timbers in India
2005 - IRG/WP 05-40314
Timber is extensively used in India in the marine environment for various purposes due to its several advantages over modern materials. Infact, its use is increasing in recent years, finding wider and wider applications and this scenario is not going to change in the near future. Though, the bio-deterioration problem is found very severe in tropical waters, still indigenous methods are widely empl...
B Tarakanadha, M V Rao, M Balaji, P K Aggarwal, K S Rao


The resistance of fifteen Indonesian tropical wood species to the powder post beetle Heterobostrychus aequalis
1990 - IRG/WP 1429
A preliminary laboratory test on the resistance of 15 tropical wood species to Heterobostrychus aequalis has been carried out using small samples of 7.5 x 5 x 1.5 cm³. The results reveal that Pinus merkusii and Agathis borneensis are very susceptible to Heterobostrychus aequalis. Other 13 species vary between susceptible to resistance There is no signifisant relation between starch content and th...
Jasni, Nana Supriana


Natural resistance of twenty-six Guianese wood species against marine borers
1988 - IRG/WP 4144
This note is a contribution on the study of the natural resistance of some wood species from French Guiana, some of which could be found too in the neighbourhood. Here are presented the results after one year exposure in the marine environment....
L N Trong


Estimation of service life of durable timber species by accelerated decay test and fungal cellar test
2002 - IRG/WP 02-20249
Many kinds of durable wood species for outdoor uses has been imported from all over the world to Japan. However information on the natural durability of these species is not sufficient to estimate the service life of them in the climate of Japan. Highly durable species such as Jarrh, Teak, Ipe, Ekki, Selangan batu, Red wood, Western red cedar showed no significant percent mass losses by accelerate...
K Yamamoto, I Momohara


Some statistics on the Brazilian Wood Preservation Industry: 1980-81
1982 - IRG/WP 3214
Statistical data on the production of pressure treated wood and on the consumption of wood preservatives are given for the years of 1980 and 1981 in Brazil....
M S Cavalcante, F C Geraldo, A R De Freitas


Detection of trace organics by ion mobility spectrometry
1990 - IRG/WP 3635
Ion Mobility Spectrometry (IMS) is a time of flight analytical technique that is suited to detect chemicals in the low parts per billion range. Some of the advantages of IMS are: operation at atmospheric pressure, fast response time (0.1-10 sec), and the ability to characterize individual chemical species in complex matrices without any prior sample preparation. In this paper, the utility of IMS i...
A H Lawrence


Criteria for basidiomycetes testing and ways of defining natural durability classes
1998 - IRG/WP 98-20144
Within the framework of a European research project several laboratories have tested a series of 17 wood species covering the total range of natural durability. Basidiomycete tests are part of the total set up. Although generally based upon standard methods some minor differences in execution of the tests were evaluated for their impact on the results. This variation was superimposed with the fac...
J Van Acker, M Stevens, J K Carey, R Sierra-Alvarez, H Militz, I Le Bayon, G Kleist, R-D Peek


Wood degradation mechanisms by the brown rot fungus Gloeophyllum trabeum
1997 - IRG/WP 97-10229
A mechanism for the degradation of wood by the brown rot fungus Gloeophyllum trabeum is outlined. The mechanism includes the function of redox-cycling, low molecular weight phenolic derivatives which sequester and reduce iron in acidic environments. The role of oxalate for the sequestration of iron (hydr)oxides and the pH dependent transfer of iron to the G. trabeum phenolic chelators, as well as ...
B Goodell, J Jellison


The effect of creosote and Basilit on the boards of 4 wood species against destructive fungi in Northern Iran
1989 - IRG/WP 3555
The results of the experiments conducted on the boards of maple, hornbeam, alder and beech, show that under the humid and moderate climate condition of Northern Iran, after 30 months, the witness samples were about 10% destructed by fungi, especially by Schyzophyllum commune and Coriolus versicolor. The impregnated samples by Creosote Basilite using Rueping and Bethell methods, were quite intact. ...
D Parsapajouh


Natural durability of European wood species for exterior use above ground
2003 - IRG/WP 03-10499
The main interest in using more timber for exterior constructions is to protect the environment, where wood is considered an environmentally friendly material. However, chemicals for wood protection are getting more and more restricted, consequently, the focus on the natural durability of wood is increased. Good, well-documented data on the durability of wood species in ground contact exist, which...
B Lindegaard, N Morsing


Fixation of chromated copper arsenate (CCA) wood preservative in Australian hardwoods: A comparison of three Eucalyptus species
1996 - IRG/WP 96-30107
New environmental guidelines for the management of CCA treatment plants were released in Australia in 1995. This has stimulated interest in techniques for controlling or accelerating the fixation of CCA in freshly treated timber products. The ability to understand, then effectively control and/or accelerate fixation of CCA in treated timber products can be an economic, technical and environmental ...
J Holmes


Resistance of Teak, Balau, keruing and Chengal Wood species against marine borers attack
2004 - IRG/WP 04-10513
Wood samples of Teak (Tectona grandis) , Keruing (Dipterocarpus alatus),Yellow Balau (Shorea laevis) and Chengal (Balanocarpus heimii) were treated by Creosote, using Ruping method. The dimension of samples were 200 x 75 x 20 mm and the retention were 188, 186, 331, 40 kg /m3 respectively. Both treated and untreated samples were installed in sea water (Mahshar in Persian gulf and Bandar Torkman an...
A Rezanejad


The natural durability assessment of secondary hardwood species - laboratory tests
1998 - IRG/WP 98-10295
Laboratory tests have been undertaken to assess the natural durability of 16 species of lesser known hardwoods, or hardwoods from non-traditional sources, including teak from three different plantations. Resistance to decay by both basidiomycetes and soil-inhabiting micro-fungi has been established. ´The data indicated that published information on the durability of these timbers should be treat...
J K Carey, S J Hendry


Standardisation of sapstain tests - A challenge
1992 - IRG/WP 92-2403
In the last decade many new anti-sapstain products have been tested world-wide under laboratory and field conditions. Several extensive test programmes have been executed with different non-standardized test methods and procedures, with the result that the biological findings cannot be compared with each other. In this paper, gathered recommendations will be given in order to standardize test meth...
G Rustenburg, C J Klaver


A technique for determinging the efficacy of wood preservatives for partially treated timber
1988 - IRG/WP 2322
A technique is described for determining the efficacy of wood preservatives either for certain wood species where a full penetration cannot be achieved by normal vacuum-pressure methods or for more permeable species to look at efficacy of treated zone in preventing decay of an untreated core. Both sapwood and heartwood planks of spruce (Picea abies) and pine (Pinus sylvestris) were treated by CCA ...
A J Nurmi


Evaluating the natural durability of native and tropical wood species against Reticulitermes flavip
2004 - IRG/WP 04-10539
Environmental pressures to eliminate arsenate from wood preservatives has resulted in voluntary removal of CCA for residential applications in the United States. A new generation of copper organic preservatives has been formulated to replace CCA for decking and in-ground applications but there is no guarantee that these preservatives represent a permanent solution to all related problems. There...
R A Arango, F Green III, K Hintz, R B Miller


The possible role of mobile CCA components in preventing spore germination in checked surfaces, in treated wood exposed above ground
2001 - IRG/WP 01-30263
Untreated check surfaces are often exposed in CCA-treated lumber of refractory species used above ground since, during weathering, some checks develop beyond the preservative penetrated zone. However, decay is seldom observed in these checks even after many years of exposure. It is hypothesized that minor amounts of mobile CCA preservative components redistribute during weathering into checks, and...
S Choi, J N R Ruddick, P I Morris


Natural Durability of Tropical Species – Variations and Prospects
2005 - IRG/WP 05-10568
The tropical timber resources of the world play an unequivocal role in economic development of both the tropical timber producing and importing regions. This paper describes natural durability as an important and preferred wood quality of tropical species of the world with emphasis on Malaysian hardwoods, the link between various aspects of tropical hardwood durability, hardwood utilization and bi...
A H H Wong, Yoon Soo Kim, A P Singh, Wang Choon Ling


Thermal modification of non-durable wood species 1. The PLATO technology: thermal modification of wood
1998 - IRG/WP 98-40123
The PLATO technology is an innovative upgrading technology with low environmental impact, which can be applied to fast grown and non-durable wood species. This technology is based on a thermal modification of solid wood without the addition of chemicals (e.g. preservatives), consisting of a hydrothermal treatment, followed by drying and curing. The PLATO technology results in a substantial improve...
M J Boonstra, B F Tjeerdsma, H A C Groeneveld


Fumigant movement in Canadian wood species
1984 - IRG/WP 3296
Pole sections prepared from seven Canadian wood species (Thuja plicata, Thuja occidentalis, Pinus contorta, Pinus resinosa, Pinus banksiana, Pseudotsuga menziesii, southern yellow pine) were fumigated with chloropicrin, methylisothiocyanate and Vapam and the rates of fumigant penetration determined. All three fumigants were applied directly into holes bored radially into the pole sections. Analysi...
J N R Ruddick