A technical note on the limitations of atomic absorption spectrophotometric analysis of copper/chrome/arsenic solutions according to BS 4072 (1974) and BS 5666: Part 3 (1979)
1988 - IRG/WP 2320
British Standards BS 4072 (1974) and BS 5666: Part 3 (1979) detail an atomic absorption spectrophotometric method for the quantitative determination of copper, chrome and arsenic in both preservative solutions and treated timber. Use of this technique during a research programme at Aberdeen has highlighted some potential inaccuracies with this method if these standard specifications are adhered to...
A J Pendlebury, J A Petty


Harmonisation of technical requirements of treated wood in Europe. What can we learn from the experience in the Nordic countries?
1995 - IRG/WP 95-50040-20
In the Nordic countries the Nordic Wood Preservation Council (NWPC) has since 1972 harmonised the technical requirements for pressure treated timber in a Nordic standard. These requirements were used by the control schemes that exist in every country. In 1976 the first Nordic standard for pressure treated wood was accepted and in 1978 NWPC changed from recommendations to approvals for the preserva...
F G Evans


Screening of the technical performance and aquatic toxicity of N-methylolacrylamide treated wood
2000 - IRG/WP 00-40166
In the course of the last decades chemical modification of wood species, with a limited natural durability, has been subjected to intensive research. As a possible alternative and supplementary treatment of non-durable wood in a range of applications it remains one of the major topics in the wood preservation world. Different modification systems have been scaled-up and are now in an industrialisi...
V Rijckaert, S De Geyter, J Van Acker, M Stevens


Soft-rot testing. Memo to CEN
1983 - IRG/WP 2206 A
1. Development of a single test procedure to assess performance of preservatives against soft rot fungi is an ideal that cannot be realised at present, if results are to be both reproducible between laboratories and pertinent to the practical requirements of individual countries. 2. Consensus opinion amongst members of Sub Group I - Soft rot tests, of Working Group II - Fundamentals of Testing, of the IRG, is that the immediate needs of CEN would be best answered by: (a) a code of recommended practice, (b) a multiplicity of test procedures, and (c) a degree of flexibility in test procedures. 3. The code of recommended practice should recognise the need for: (a) a pure culture, synthetic medium (sand or vermiculite + nutrients), single wood species test to be adopted by all laboratories as a common reference point of testing, (b) mixed inoculum and/or unsterile soil laboratory or fungus cellar tests which account for local variations in the fungal flora, (c) incorporation of a range of wood species where applicable (i.e. where mixed hardwoods comprise the main resource), (d) provision of local internal standards of known performance under field conditions, (e) incorporation of leaching procedures other than standard methods with deionized water (e.g. mild acid, milk alkali, ionic solutions of various salts) where applicable to local exposure conditions, (f) precise definition of the criteria used for establishing toxic thresholds (mass loss, strength loss, microscopic examination). 4. Initial screening tests should remain the province of the individual research worker. 5. The code of recommended practice should have the sole purpose of establishing provisional retention levels for subsequent confirmation by field trial. 6. IRG should list and approve test procedures considered adequate to establish toxic thresholds for preservatives against soft rot fungi. 7. It should be clearly understood that when using a series of test techniques, it is inevitable that a range of toxic thresholds will be obtained for the same preservative. 8. Guidelines should be drawn up for interpretation of test data for subsequent transformation to provisional retention levels. 9. Adoption of the broad principles outlines above is recognition of the dynamic nature of toxic thresholds. The additional information obtained by a more flexible, and complex, approach to testing may make interpretation more difficult but should provide data from which response of preservatives to varying biological and environmental hazards can be more realistically assessed. 10. It is recommended that CEN adopt, in principle, the basic philosophy of testing outlined above and move towards formulation of a Working Document in collaboration with IRG
J A Butcher, D J Dickinson


Less pollution due to technical approaches on accelerated steam fixation of chromated wood preservatives
1988 - IRG/WP 3487
Steaming of freshly treated wood at 100°C to 120°C initiates a spontaneous fixation of copper-chromate-containing wood preservatives. For the performance, a suitable anticorrosive equipment is necessary. Good results can be achieved using a separate steaming equipment which allows a rapid heating of the wood. While warming-up, in the wood some preservative solution extends and can be partly extr...
H Willeitner, R-D Peek


Wood preservation in Canada - Regulation and Registration
2001 - IRG/WP 01-50166-02
The Canadian wood preservation industry is at a critical juncture now as a number of initiatives converge on the industry over the next few years. Issues facing the industry include: Re-evaluation of the conventional wood preservative chemicals - inorganic arsenicals, creosote and pentachlorophenol targeted for July 2001. Delayed registration of new actives as a result of re-evaluation activity an...
P A Cooper


Fixation of chromated wood preservatives through technical drying
1990 - IRG/WP 3623
Twin samples of sawn timber of Pinus sylvestris and Picea sp. were treated with copper-chromate-containing wood preservatives and subsequently kiln resp. air dried. After drying, the distribution of preservative and rate of fixation were determined. Drying of freshly treated wood in a condenser type kiln at temperatures of 60°C and 80°C and in a vacuum type kiln at 55°C with a pressure of about...
R-D Peek, H Klipp


The Technical Criteria on Biological Evaluation of Wood Preservatives for Use Category C4.1 in Southern China
2012 - IRG/WP 12-20481
According to the Regulations on Pesticide management of the People's Republic of China, wood preservatives belong to agrochemicals. The establishment of registration system on wood preservatives would be benefit to management of preservatives, including the market entrance and safety insurance to the human beings, livestock and the environment associated by the application of these preservati...
Xingxia Ma, Mingliang Jiang


Recommendations for handling of mold infestation of wooden artifacts
2012 - IRG/WP 12-10790
The presentation gives an overview of the handling of wooden artifacts with mold infestation. The causes of mold deterioration are demonstrated by investigations in a church, a historic library and a monastery in Germany. Investigated infested wooden artifacts were altars, sculptures, picture frames and sarcophagi. Important investigation methods including indoor climate measurement, material an...
K Plaschkies, B Weiss, W Scheiding


The Impact of Cryopreservation Techniques and of Water Quality on the Wood Degrading Ability of Fungal Strains: Recommendations for Maintenance and Culturing Procedures
2018 - IRG/WP 18-20636
In order to establish an optimal cryopreservation method, strains of Basidiomycete and Ascomycete fungi, which are among the most frequently used for wood durability testing, were evaluated using three cryopreservation procedures at -80°C. The main objective was to prevent decrease of the fungal virulence that may occur due to repeated routine sub-culturing procedures and to optimize the reactiva...
A Stum, M Montibus, I le Bayon, M Kutnik


Bio-preservative properties of technical lignins from South African pulp mills: An investigation towards a conceptualized development of natural compound-based wood preservatives
2018 - IRG/WP 18-30724
The depletion of naturally durable timber and the risk posed by some of the conventional wood preservatives to human health and the environment continue to drive research efforts towards developing new formulations that are benign. Furthermore, the global concept of environmental sustainability aims at optimal use of resources and to comprehensively include conversion of waste to value added produ...
A Alade, L Tyhoda, M Meincken


Assessment of the condition of wooden mill in the area of Kovačevići in Bosnia and Herzegovina
2023 - IRG/WP 23-11030
An excellent example of cultural and technical heritage is almost 100 year old wooden mills near Cazin in Bosnia and Herzegovina. These mills played an important role, especially in times of Bosnian war (1992-95), when this region was cut off from electricity. The laboratory analysis revealed that the respective mill was made of chestnut (Castanea sativa) and oak (Quercus sp.) wood. The sufficient...
B Lesar, R Hasanagic, M Humar