Your search resulted in 915 documents. Displaying 25 entries per page.
The biological natural durability of timber in ground contact
1994 - IRG/WP 94-20051
The BRE ground contact field trials for the determination of the biological natural durability of different timber species have recently been reviewed. The data obtained from these trials have been used to appraise the different ways in which natural durability may be expressed. It is concluded that the use of the mean as a method of assigning the timber to one of five durability classes may be ac...
G A Smith, R J Orsler
Creosote movement from treated wood immersed in fresh water: Initial PAH migration
2003 - IRG/WP 03-50201
Creosote has a long history of successful use as a wood preservative, but polycyclic aromatic hydrocarbons (PAHs) in this preservative have raised environmental concerns, particularly when creosote-treated wood is used in aquatic environments. A number of models have been developed to predict the risk of creosote use in aquatic environments, but one limitation of these models is a lack of data o...
Sung-Mo Kang, J J Morrell, J Simonsen, S T Lebow
Copper based water-borne preservatives: The biological performance of wood treated with various formulations
1987 - IRG/WP 3451
Wood samples treated with the various components of CCA preservative singly and in combination were tested against a soft rot organism, a copper tolerant brown rot organism and in soil burial both unleached and after leaching. The results suggest that, of the elements tested, fixed copper is essential for preventing soft rot attack and fixed arsenic is essential for preventing attack by a copper t...
S M Gray, D J Dickinson
Examination of timbers from the Mary Rose in storage
1988 - IRG/WP 4149
Timbers from the Tudor ship, Mary Rose, have been examined for the presence of fungal fruiting structures. Wood specimens were also examined for the presence of microbial decay patterns using light and scanning electron microscopy. Structural timbers were surveyed using the Pilodyn for an overall picture of the extent of decay. Mary Rose timbers were predominantly inhabited by marine fungi. Fourte...
R Mouzouras
Collaborative soft rot tests: Proposed amendments to Document No: IRG/WP/208
1973 - IRG/WP 224
J K Carey, J G Savory
300 years water-logged wood: Treatability with CCA-C
1998 - IRG/WP 98-40103
The treatability of 300 years water-logged and recent wood (Abies bornmülleriana M.) was assessed by dip treatment and vacuum and pressure cycling with CCA-C. Treatment runs were evaluated on the basis of weight gain retention and radial and tangential penetration measurements. The preservative penetration and retention levels in the 300 years water-logged wood were higher than in the recent wood...
S N Kartal, N Yilgör
Leaching tests - A paper for discussion
1973 - IRG/WP 221
J W W Morgan
Evaluation of the leach resistance and preservative efficacy of novel biocides as surface treatments applied by brush to spruce (Picea abies)
1998 - IRG/WP 98-30170
The comparative leach resistance and preservative efficacy of a number of alternative organic preservatives (available from Zeneca Specialties) and selected commercially available biocides as surface coatings to wood in Hazard Class 3 have been assessed. Two concentrations of test preservatives were applied by brush to Spruce (Picea abies), including formulation and untreated controls. A leaching ...
I M Tierney, A Bruce, D C R Sinclair, T Yeates
In ground contact field trial results of preservative treated incised and unincised spruce
1996 - IRG/WP 96-40076
Field trials of treated spruce stakes have been demonstrated that incising the stake before treatment improves the preservative uptake both for CCA and creosote. This results in a substantially extended service life for the incised stakes over the unincised stakes for preservative concentrations at commercial levels. After 24 years in ground contact the majority of incised spruce samples are sound...
E D Suttie
A comparison between methods for evaluating the water repellency of wood
1989 - IRG/WP 2328
Wood specimens treated with a number of water repellent formulations have been tested for their water repellency according to four laboratory test methods, based on weight increase, swelling and contact angle measurements, in order to assess the degree of agreement between the different methods. Treatments representing formulations with a wide range of water repellent efficiency were tested both i...
R Nussbaum
Thirty-four year test of on-site preservative treatments to control decay in wood above ground
1993 - IRG/WP 93-30015
This research was initiated in 1958 to investigate efficacy of various preservatives and treating methods for new lumber going into exterior structures of buildings. Post-rail units (2x4 inches) constructed of Southern Pine sapwood, Douglas-fir heartwood, and mill run western hemlock were dip- or brush-treated before or after assembly. Units were trested with pentachlorophenol in various petroleum...
T L Highley, T C Scheffer
Soft rot decay of 23 CCA-treated hardwoods from Sabah, Malaysia, in ground contact in Australia
1986 - IRG/WP 1280
The performance against soft rot decay of 23 CCA-treated hardwoods from Sabah, Malaysia, was examined after 20 months in ground contact at Pennant Hills, Australia. The results indicate that between these species soft rot decay is excluded by different levels of CCA salt suggesting that the threshold level for exclusion of soft rot in these hardwoods is a function of anatomical structure/ultrastru...
R S Johnstone
LCA applied for wooden products
1995 - IRG/WP 95-50059
This paper presents some of the international developments within ISO and SETAC to standardize and harmonize LCA methodologies. In this framework it is also important to be aware of the problems that companies have to generate and validate data for the complete product chain from cradle to grave. This concerns problems in nomenclature of substances and processes, system boundaries, allocation prob...
A Kloppenburg, A Van Dam
Biological effectiveness of ground-contact wood preservatives as determined by field exposure stake tests
1984 - IRG/WP 3297
Field exposure tests conducted on stakes treated with different creosotes, mixtures of creosote and waxy oil as well as different CCA wood preservatives over a period of 25 years, gave the following results: The CCA preservatives provided excellent biological protection to treated stakes, especially against fungal attack. The CCA Type I, currently approved for use under South African conditions is...
W E Conradie, A Pizzi
Practical testing of wood preservatives to prevent weathering damage and infection by micro-organisms on spruce and pine
1989 - IRG/WP 3530
Brush application, is generally used to prevent wooden window frames from decay caused by influence of weathering and fungi. Accordingly 10 boards of pine (Pinus sylvestris) and spruce (Picea abies) were treated with 10 commercially used wood preservatives. The efficiency of fungicides by using chiptest and blue stain test (EN 152), the effectiveness against weathering as well as the course of col...
R Gründlinger, O Janotta, H Melzer, K Messner
Climate indices at work: Above ground decay L-joint tests (EN 330 and AWPA E9) at two sites 12000 km apart and with Scheffer climate indices of 60-65 and 300-330
1996 - IRG/WP 96-20095
Matched sets of Scots pine sapwood (Pinus sylvestris) L-joints were exposed above ground at two field sites for approximately five years. One site, at Garston, Watford, UK has a climate index between 60 and 65 while the other, close to Hilo, HI, USA has an index between 300 and 330. The joints were treated with a range of organic solvent treatments applied either by three minute dip immersion or b...
A F Preston, K J Archer, D M Roberts, J K Carey, A F Bravery
Field trials on preserved timber out of ground contact
1978 - IRG/WP 3154
This report describes two different field trials studying the performance of preservative treatments on timber exposed to the weather, but above the ground. Results are presented on the protection afforded against decay, and on the efficiency of water-repellent preservative treatments in controlling the uptake of moisture by the timber. Proposals for a standard field test system are briefly discus...
D F Purslow, N A Williams
Waterborne silicones as wood preservatives
1995 - IRG/WP 95-30062
For more than thirty years silicones are used as water repellents for masonry. Their excellent properties make them also attractive for non-mineral substrates like wood. Although it was always thought that silicones are not able to perform on wood, a new type of aqueous silicone materials proofed the opposite: Excellent water repellency and astonishing durability were achieved. This paper describe...
R Hager
An interim report on trials with 'Boliden K33' and 'Celcure A' in water of different salinities in the Baltic Sea and in the UK
1974 - IRG/WP 406
It was felt necessary to undertake field trials using large test samples exposed in natural water of different salinity in order to determine preservative leaching and to assess the degree of biological attack....
R A Eaton, D J Dickinson
Assessment of contamination of soil and water at a CCA treatment plant: A demonstration project
1996 - IRG/WP 96-50067
Soil, sludge, dust and water samples were collected at a copper/chromium/arsenic wood preservation plant. Contamination of soil, sludge, dust and surface water with copper, chromium and arsenic was detected. Levels of contamination were sufficiently high to require remediation. Contamination originated from preservative solution dripping from recently treated wood. Migration of contaminants was vi...
P N Durrant, D C R Sinclair, G M Smith
Factors affecting the sorption of preservative during diffusion treatment of wood
1988 - IRG/WP 3500
The sorption of preservative into wood during soaking in aqueous solution was found to comprise absorption as well as diffusion of solute. Absorption was increased by partially seasoning the wood prior to soaking and was characterised by (a) a very rapid initial rate of uptake and (b) an extended period of slow uptake, the rate of which varied with prior conditioning. It was concluded that some pa...
P Vinden
Differential behaviour of wood rotters at water repellent Rubberwood
2000 - IRG/WP 00-10386
Rubberwood samples treated with different concentration of aqueous solution of chromic acid has induced significant increase in water repellency and attains dimensional stability. Though water repellency and dimensional stability was achieved by treatment, the fungal invasion could not be completely controlled. Differential level of decay of brown and white rot in wood treated with water repellent...
H C Nagaveni, S S Chauhan, K S Rao
Performance of treated spruce in Canadian field test sites
1989 - IRG/WP 3506
Spruce material under test in Canadian field test sites is performing better than anticipated. From the comparison of the performance of spruce treated with various preservatives, it appears that penetration may be far more important on durability performance than the preservative itself or the retention of preservatives in the wood. However, there is still insufficient data on the influence of pe...
J P Hösli, E E Doyle
Ground contact performance of wood treated by the MSU process
1990 - IRG/WP 3609
Environmental concerns have prompted a renewed interest in accelerated fixation schemes for CCA-treated wood. Results from stake tests of southern pine (Pinus sp.) treated using a conventional Bethell cycle are compared with matched stakes treated using the MSU Process. The effects of adding boric acid to the preservative formulation are also discussed. Differences among test plots are discussed....
H M Barnes, T L Amburgey, R W Landers
Copper based water-borne preservatives: The use of a thin section technique to compare the protection of wood by copper based preservatives against soft-rot and bacterial decay
1987 - IRG/WP 2286
This paper describes the techniques developed and gives examples of results obtained for the performance of copper based wood preservatives against both the bacterial and fungal hazards....
A M Wyles, D J Dickinson