Your search resulted in 915 documents. Displaying 25 entries per page.
Moisture content and other tested values in. Double layer tests of different size in Lithuania and Germany
2004 - IRG/WP 04-20299
The paper presents measurement results of moisture content and the analysis of durability trial of double layer wood in variants of varying size, conducted in Girionys, Kaunas distr., Lithuania and in Hamburg, Germany. In this trial 3 sample sets of varying size, containing 25, 50 and 100 specimens, are used. The aim of this trial is to ascertain an optimal number of test specimens. The dynamics o...
J Saladis, A O Rapp
A substantively bonded water repellent treatment based on chromium carboxylates
1985 - IRG/WP 3344
Chromium carboxylates soluble in toluene have been synthesised and applied to Scots pine (Pinus sylvestris) sapwood. Without any further treatment, the compounds may be readily leached from wood surfaces with toluene. After a period of heating however, they become fixed to the cell wall, substantial amounts being resistant to leaching even under reflux conditions for several hours. Treatment of wo...
J K Wright, W B Banks, W J Eilbeck
Supply of wooden transmission and telephone poles in Tanzania: Problems and possible solutions
1987 - IRG/WP 3424
The eucalypts which have been used widely for utility poles for more than 30 years have dwindled remarkably from traditional supply areas. Consequently, pole-using authorities are considering importing poles from abroad. This alternative is considered unrealistic and costly. The aims of this paper are: - to dispel fears of pole scarcity and to show that an abundant resource of a variety of tree sp...
K K Murira, S A Diwani
A field trial to assess the potential of antisapstain chemicals for long-term protection of sawn radiata pine
1986 - IRG/WP 3375
Seven chemical formulations were tested as antisapstain treatments for freshly sawn radiata pine sapwood (90x50 mm²). Each formulation was used with and without a water-repellent additive and was sprayed on to 1 m long boards. The boards were then stacked into "mini" packets and stored unprotected from the weather for 6 months. Haipen 50w (at 0.2 or 0.4% active) and NaPCP (1% active) plus 1.5% bo...
J A Drysdale
Borer fauna of Iran biodeterioration of wooden boats in Persian Gulf and Sea of Oman
1997 - IRG/WP 97-10230
In Persian Gulf and Sea of Oman (Indian Ocean) there are thousands of wooden boats from the time of Acheamenian and Sassand dynasti when India was a part of the Persian Empire. Now after 2500 years again, the Indian timbers specially Tectona Grandis and other Indian timbers and also tropical woods of Zanzibar (Tanzania) are brought to the Persian Gulf and Sea of Oman (Indian Ocean). Unfortunately ...
P Niloufari
The use of organic wood preservatives in ground contact and the suitability of laboratory test procedures to determine their efficacy
1999 - IRG/WP 99-20175
Organic fungicides, such as propiconazole, have proven to be highly effective when used as a co-biocide in recently developed wood preservative formulations. They have however been ineffective when used as a stand alone preservative, particularly when used in ground contact (European Hazard class 4). Previous research, using the test methods of ENV 807 (1993), provided conflicting evidence regardi...
I J Herring, D J Dickinson
Prevention of sapstain in logs using water barriers
1997 - IRG/WP 97-30147
Placing logs in ponds or under water sprinklers to keep moisture levels high enough to prevent oxygen tensions rising above inhibitory levels, is a proven method of preventing sapstain. The objective of this experiment was to determine if water barriers significantly reduce the rate of sapstain penetration into logs by maintaining moisture contents, and consequently oxygen tensions, at inhibitory ...
R N Wakeling, D R Eden, C M Chittenden, B Carpenter, I Dorset, J Wakeman, R Kuluz
Water transfer in wood in relation to fungal attack in building - Effect of condensation and diffusion
1992 - IRG/WP 92-1543
Wood is continuously exchanging moisture with the surrounding atmosphere, the temperature and relative humidity are important factors. Wood moisture in this case is not enough to provoque decay by fungi. However, when, during the night, condensation appears cyclically, wood absorbs water and moisture content may be sufficiently high to allow development if drying does not take place. The water tra...
D Dirol, J-M Vergnaud
Bethoguard; A new wood protecting fungicide for use in metal free ground contact wood preservatives
2002 - IRG/WP 02-30301
Research has identified the limitations in both the spectrum of activity and permanence of organic biocides placed in wood in high hazard environments, particularly in the absence of heavy metals such as copper. More specifically, the control of soft rot decay in wood in soil contact has proven to be most problematic.
The new organic biocide, Bethoguard; an oxathiazine, has demonstrated excellen...
S C Forster, G R Williams, M Van Der Flaas, M Bacon, J Gors
A study of methanogenesis and sulphate-reduction: A possible source of explosive gas mixtures in a gold mine
1989 - IRG/WP 1399
Previous work isolated anaerobic bacteria from timbers and drainage water in a gold mine. The present work identifies the predominant methanogen in the mine ecosystem as Methanobacterium bryantii and sulphate-reducing isolates as Desulphovibrio desulphuricans and Desulphotomaculum antarcticum. Laboratory studies using model systems evaluate the activity of methanogenic and sulphate-reducing bacter...
L D Abraham, J F Putterill, A A W Baecker
Wood cement composites using spent CCA treated wood
1999 - IRG/WP 99-50126
The feasibility of using spent or out-of-service CCA treated wood as a component of wood/cement composites was evaluated. Cold pressed wood particle cement boards were made using CCA treated particles from a red pine (Pinus resinosa Ait.) pole removed from service and from untreated red pine wood from a new pole. Boards were manufactured using a range of wood to cement ratios and water to cement r...
Chen Huang, P A Cooper
A novel method for evaluating the performance of water repellents
1987 - IRG/WP 2279
Application of water repellent formulations to timber surfaces offers protection from the weather, reducing degrade and movement. A novel test method has been developed to evaluate the comparative efficacy of such formulations when samples are exposed to weather. The method uses sapstain free sapwood of defect free, untreated, seasoned Radiata pine, (Pinus radiata D. Don.) Water Repellency was det...
A R Moffat
The potential of high pressure pulsation processes to treat white spruce lumber with water-borne preservatives
1988 - IRG/WP 3471
Laboratory work using end sealed 4x8x46 cm³ white spruce samples has been done to explore the suitability of three variants of a 2.1 MPa pulsation process for the impregnation of white spruce with CCA. The results showed that the process improved significantly the penetration of the preservatives and reduced significantly cell collapse, when compared with the results of treatment using a 2.1 MPa ...
J P Hösli, J N R Ruddick
IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 17: Report of fifth inspection (4 years) in Italy
1983 - IRG/WP 4103
The wood samples of Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were submerged in the sea at Follonica, Italy, in April 1977. Follonica, latitude 42°55' North and longitude 10°45' East, is situated on the Tyrrhenian coast. The recorded temperature varies from 13°C to 25°C, salinity 37-38% and pH about 8. The inspections were carried out after 6 months (10/1977), 12 ...
A Gambetta, E Orlandi
Soft rot in heartwood of preservative-treated pole stubs of Eucalyptus cypellocarpa L. Johnson
1983 - IRG/WP 1204
Pole stubs of Eucalyptus cypellocarpa L. Johnson, treated in the sapwood with certain waterborne preservatives and exposed for 21 to 23 years in a dry tropical region were severely soft-rotted in the heartwood, as well as the sapwood. They broke with a brash fracture when stress tested (loaded as a cantilever) in the field. The severe soft rot in the heartwood was not detected by the knife test or...
J E Barnacle, G C Johnson, M A Tighe
Factors affecting the resistance of fibre building boards to fungal attack
1975 - IRG/WP 252
Fungal decay is initiated at lower moisture contents in standard and tempered hardboards (18%) than in pine sapwood (26%). In contrast, in a saturated atmosphere, the equilibrium moisture contents of standard hardboard (14%) and of tempered hardboard (12.5%) are much lower than the moisture content permitting decay initiation whilst the equilibrium moisture content of pine sapwood (25.1%) approach...
C Grant, J G Savory
Performance of above ground decay test units treated with a substituted isothiazolone
1989 - IRG/WP 3503
RH 287, a substituted isothiazolone, was evaluated for efficacy against decay fungi in an above ground test in Mississippi. After 45 months of exposure, all test units that were pressure treated with this biocide at levels of 0.026 pcf and higher have no deterioration. In addition, the test units that were dip-treated with a solution concentration of 0.5% also have no deterioration. Compared to pe...
D D Nicholas, J A Wilson, D E Greenley
Effects of hard water, sea water and humic acid on the release of CCA components from treated wood
2005 - IRG/WP 05-50228
Leaching medium is an important factor affecting release of preservative components from treated wood because physical and chemical characteristics of medium increase or decrease the solubility of fixed preservative components. This study evaluated the leaching properties of copper, chromium and arsenic elements from chromated copper arsenate (CCA)-treated wood specimens subjected to laboratory le...
S N Kartal, W J Hwang, Y Imamura
The resistance of wood coated with different water-borne paints against colonisation by decay fungi
1996 - IRG/WP 96-10165
The susceptibility of wood painted with model paints of known composition to decay fungi was tested without previous weathering. Included in the study were five alkyd emulsion paints and five acrylic paints; one linseed oil paint and two solvent-borne alkyd paints. It was found that several components influenced the susceptibility of these paints. The results of the present study indicate that the...
J Bjurman
Effects of the delay in the beginning of treatment on absorption and distribution of water-soluble salts in posts treated by sap-replacement method
1992 - IRG/WP 92-3719
One of the most important matters in green wood treatments, such as sap-replacement method, is knowing the longest time available for beginning treatment without losing efficacy. In this paper, the influence of this factor on absorptions and distribution of the preservative into the wood is analized. Tree start-up times were first chosen: 3-6 hours, 48 h and 120 h after being cut down. The treatme...
M V Baonza Merino
A questionnaire survey to establish the perceptions of UK specifiers concerning the key material attributes of timer for use in marine and fresh water engineering
2004 - IRG/WP 04-10519
Engineers have a key role in making informed decisions on the type of materials to be used in the schemes they design and construct. Currently, in England and Wales, it is believed that some £500m per year is invested in flood and coastal defence engineering. There is a lack of centralised data in the UK holding information on timber for usage in fluvial and, particularly coastal engineering. A...
J R Williams, G S Sawyer, S M Cragg, J Simm
A field evaluation of chromated fluoride as a remedial treatment for creosoted wooden distribution poles
1989 - IRG/WP 3556
A commercial chromated fluoride formulation was applied by injection process to previously inoculated creosoted wooden distribution pole sections at a field site in Scotland and appraisal of the efficacy of the formulation against Lentinus lepideus was undertaken at two month and fifteen month intervals. Preliminary results suggest a rapid elimination of organisms from colonised areas. The usage o...
B King, A Bruce
New method to find out the volatile organic compounds (VOC) of wooden material
2000 - IRG/WP 00-20189
Volatile organic compounds (VOC) of pine, spruce and larch wood were studied using a new technique developed at VTT Chemical Technology. 50 mg of crushed wood material was placed into glass tubes. The tubes were closed with a glass wool, which is pressed with a tube cap. Wood samples were analysed with a gas chromatograph after thermal desorption using four different temperatures (50°C, 100°C, 1...
H Viitanen, K Villberg, K Saarela
Social and economocal impact of an extension of service life resulting of an adequate preventive treatment. Application to wooden components used in urban areas with a high density of population
1993 - IRG/WP 93-50001-15
Le document évalue les problèmes rencontrés en zone urbaine pour le sauvetage des constructions: coordination de la lutte, délimination des chantieres et des périmètres d'investigation, nuisances causées par les interventions, risques pour la santé, risques pour l'environnement. Coûts. Comparaison socio-économique du traitement préventif et des interventions à posteri...
A T De Lelis, G A C Lopez
Some Experiences with Stake Tests at BAM Test Fields and in the BAM Fungus Cellar
Part 1: Comparison of Results of Visual Assessments and Determinations of Static Moduli of Elasticity (MOE)
2005 - IRG/WP 05-20319
With examples of routine in-ground stake tests differences are shown in the performance of wood preservatives at the BAM test fields Lehre and Horstwalde and in the BAM fungus cellar. Signs of attack of micro-organisms were assessed visually according to EN 252. Periodical determinations of static moduli of elasticity (MOE) revealed the influence of the attack on the elastic properties of the wood...
M Grinda, S Göller