Short term preconditioning of preservative-treated wood in soil contact in relation to performance in field trials
2000 - IRG/WP 00-20185
The effect of pre-exposure to primary colonising micro-organisms on preservative-treated wood, prior to a basidiomycete decay test, was determined by preconditioning in two soil types. Scots pine EN 113 blocks treated with 3 model systems (a triazole, a copper quaternary compound and a copper boron triazole) were leached according to EN 84 and subjected to 6 weeks and 8 weeks burial in either John...
S Molnar, D J Dickinson


The effect of storage or simulated internal use on the durability of wood based panels to decay fungi
1997 - IRG/WP 97-20106
Wood based panels such as particleboard and medium density fibreboard are experiencing a steady increase in use, in areas from structural to decorative applications. Understanding the "natural" durability of these panel products against basidiomycete fungal decay is therefore of great importance. Various methods have been proposed or are under development to test the durability/susceptibility of v...
S F Curling, R J Murphy, J K Carey


Questionnaire for Volume 2 of the basidiomycete monographs
1985 - IRG/WP 1254
12 monographs of wood destroying basidiomycetes were published in volume 1. Volume 2 includes the following 17 basidiomycetes: Antrodia serialis, Chondrostereum purpureum, Climacocystic borealis, Fomitopsis pinicola, Hyphoderma tenue, Lentinus degener, Lentinus squarrulosus, Paxillus panuoides, Phellinus contiguus, Poria xantha, Pycnoporus sanguineus, Rigidoporus vitreus, Serpula himantoides, Sistotrema brinkmannii, Stereum sanguinolentum, Trametes corrugata
T Nilsson


Report on the status of collaborative experiments within the Sub-group on Basidiomycete tests
1983 - IRG/WP 2194
This report summarises the results of co-operative work carried out within the Sub-Group on Basidiomycete tests up to December 1982. The principle findings are recorded in the Conclusions Section. Work intended between IRG-13 in Turkey and IRG-14 in Australia is cited under Future Programme. An Annex provides a response sheet for existing and new participants to notify their contributions....
A F Bravery


An experimental method to simulate incipient decay of wood by basidiomycete fungi
2000 - IRG/WP 00-20200
At very early stages of decay of wood by basidiomycete fungi, strength loss can be measured from wood before any measurable weight loss. Therefore, strength loss is a more efficient measure of incipient decay than weight loss. However, common standard decay tests (e.g. EN 113 or ASTM D2017) use weight loss as the measure of decay. A method was developed that allowed progressive removal of samples ...
S F Curling, J E Winandy, C A Clausen


Effect of light and ventilation condition on the rate of wood decay by the brown rot basidiomycete, Tyromyces palustris
1991 - IRG/WP 1517
Effect of light and the ventilation conditions of incubation jars on the wood decay by Tyromyces palustris (Berk. et Curt.) Murr. FFPRI 0507 was investigated. Under no irradiation of light, the ventilation conditions gave extensive effect on mass loss of the test pieces when the culturing was performed with culture medium designated in Japanese Industrial Standard (JIS) A 9302 (Medium A; glucose 4...
T Suzuki, M Higaki


The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh


Effects of the specimen position on fungal colonisation and wood decay by en 113 test fungi
1998 - IRG/WP 98-20136
For testing wood preservatives according to EN 113 it is common practice to plant the test blocks on neutral supports in order to prevent (1) a diffusion of chemicals into the agar medium and (2) an excessive moistening of the specimens. The procedure was employed in EN 350-1 for testing the natural durability of solid wood. It turned out to be of problematic nature because of the individual requ...
G Kleist, M-T Lenz, R-D Peek


Evidence for Basidiomycete Tunnelling in Pinus radiata and Fagus sylvatica
2006 - IRG/WP 06-10587
Decay micromorphology was studied systematically for diversely preservative treated Pinus radiata and Fagus sylvatica 20 x 20 x 500 mm stakes across 13 in-ground field test sites, during a 6.5 year exposure. Sites were selected to maximise occurrence of a diverse range of decay types. Presence of clamp connections in close associated with tunnelling coupled with macroscopic features similar to whi...
R Wakeling


Isolation and characterization of hydroxyl-radical-producing glycopeptide genes from the white-rot basidiomycete Phanerochaete chrysosporium
2006 - IRG/WP 06-10588
During wood decay, the white-rot basidiomycete Phanerochaete chrysosporium secretes low-molecular-weight glycopeptides that catalyze a redox reaction between O2 and electron donors to produce hydroxyl radical. This reaction accounts for most of the hydroxyl radical produced in wood-degrading cultures of P. chrysosporium. In combination with phenol oxidases, hydroxyl radical is believed to play a r...
H Tanaka, G Yoshida, Y Baba, K Matsumura, S Itakura, A Enoki


The involvement of hydroxyl-radical-producing glycoprotein from the white-rot basidiomycete Ceriporiopsis subvermispora in wood decay
2009 - IRG/WP 09-10688
White-rot decay can be divided into two subtypes. One type involves the simultaneous degradation of all wood components through the formation of erosion troughs with a progressive thinning of wood cell walls. This type of decay is consistent with a model in which several polymer-degrading enzymes act on the exposed surfaces of the wood cell walls, producing progressive erosion from the lumen to th...
H Tanaka, Y Inoue, T Morikawa, S Itakura, A Enoki


Structural changes, basidiomycete richness, enzyme activity and proteomic profiling of decay resistant and non-resistant woods over 18 months in soil contact
2010 - IRG/WP 10-10733
Wood decay fungi damage wood by production of enzymes that attack the structural components. The objective of this study was to better understand which suite of decay genes and proteins are expressed during biodeterioration of three different wood types in forest soil over time. Variation in decay genes and proteins were determined for pine (non-resistant), cedar (naturally durable), and ACQ-treat...
Youngmin Kang, S Diehl, L Prewitt, D Nicholas


Diversity of wood decay fungi isolated from ground-contact wood stakes in Korea
2019 - IRG/WP 19-10952
This study was conducted to investigate wood decay fungi from 5 different ground-contact wood stakes in Korea. A total of 73 basidiomycetes were isolated and identified into 20 genera and 22 species by using molecular method. Among all fungi, only 6 species were brown-rot fungi and the others were white-rot fungi. Pinus densiflora and Quercus variabilis showed high fungal diversity and isolation f...
S-M Yoon, M-J Kim, W-J Hwang, Y-S Choi, D-W Son


How personality traits influence the perception of fungal decay in a wooden cladding – A survey in three Modelling wood moisture content in outdoor conditions from measured data
2024 - IRG/WP 24-41002
This study examined perceptions of fungal decay damage on wooden cladding across Norway, Sweden, and Germany. The majority of respondents across all countries did not find the fungal decay damage in question acceptable, with the least acceptance in Norway. This could be due to Norway having the highest frequency of wooden residential buildings and the most experience with maintaining wooden claddi...
G W Gustavsen, G Alfredsen, P B van Niekerk, J Niklewski, C Brischke


Confocal laser scanning microscopy of a novel decay in preservative treated radiata pine in wet acidic soils
1997 - IRG/WP 97-10215
Light microscopy of radiata pine (Pinus radiata D. Don) field test stakes (20x20x500mm3) exposed in wet acidic (pH 3-4) soil for 12 - 24 months showed predominance of an unusual type of decay characte-rised by tunnelling attack of wood cell walls. After two years decay was moderate to severe in wood treated to ground contact CCA specifications and also equivalent retentions of creosote, and a numb...
R N Wakeling, Ying Xiao, A P Singh


Effect of acetylation on decay resistance of wood against brown-rot, white-rot and soft-rot fungi
1989 - IRG/WP 3540
Effect of acetylation on decay resistance of wood was investigated using wood blocks of Cryptomeria japonica, Pinus densiflora, Albizia falcata and Fagus crenata. Blocks were treated with uncatalyzed acetic anhydride for different lengths of time and exposed to Tyromyces palustris, Serpula lacrymans, Coriolus versicolor and unsterilized soil. The action of OH-radical on acetylated wood was also ex...
M Takahashi, Y Imamura, M Tanahashi


Field trial with poles of Scots pine treated with six different creosotes
1996 - IRG/WP 96-30115
In the middle of the 50's field trials with creosote-treated poles were started in France, Germany and Sweden. The trials were initiated by WEI (Western-European Institute for Wood Preservation). Six different creosotes were used and 40 poles per creosote were installed at each test field. Results after 39 years of exposure in Simlangsdalen, Sweden are reported. Poles treated with a heavy...
Ö Bergman


Questionnaire - Fungal decay types
1985 - IRG/WP 1265
T Nilsson


JWPA method for testing effectiveness of surface coatings with preservatives against decay fungi
1981 - IRG/WP 2164
In 1979 JWPA established a new method for testing effectiveness of surface coatings in accordance with practical use of preservative-treated lumber. Comparing the new testing method with JIS A 9302, a few new trials - size of wood specimen, weathering procedure, and decay-test procedure - are incorporated....
K Tsunoda


Utilization of curcumin for detection of presence of boron in wood
1982 - IRG/WP 3191
It has been shown that curcumin is not a reliable reagent for detecting boron in wood that has been attacked by fungi...
M-L Edlund


Co-operative studies on determining toxic values against wood-destroying Basidiomycetes: Progress report to May 1989
1989 - IRG/WP 2339
This document reports progress on the co-operative study between nine laboratories set up following the proposals contained in Document IRG/WP/2316. Results have been received from two laboratories. Toxic values data have been established successfully using the test fungus Coniophora puteana but problems have been encountered with the other test fungi....
A F Bravery, J K Carey


Monographic cards for wood-destroying fungi. [Fiches monographiques pour les champignons lignivores]
1970 - IRG/WP I 5B
C Jacquiot


On Donkioporia expansa (Desm.) Kotl. & Pouzar
1986 - IRG/WP 1285
Donkioporia expansa is found more often in houses than realised until now. Virulence tests according to EN 113 show not only an attack of oak, but also of other hardwoods and even soft-woods....
G Buchwald


Nondestructive Evaluation of Oriented Strand Board Exposed to Decay Fungi
2002 - IRG/WP 02-20243
Stress wave nondestructive evaluation (NDE) technologies are being used in our laboratory to evaluate the performance properties of engineered wood. These techniques have proven useful in the inspection of timber structures to locate internal voids and decayed or deteriorated areas in large timbers. But no information exists concerning NDE and important properties of wood composites exposed to dec...
B Illman, V W Yang, R J Ross, W J Nelson


Moisture content levels and decay of hemlock
1986 - IRG/WP 1287
As a model of decay conditions of wooden members in wooden houses, a decay test was set up in which samples of western hemlock (Tsuga heterophylla) under 4 moisture levels were examined. Each week the samples were weighed and if the weights indicated that their moisture contents were lower than the expected levels, distilled water was added. Every 8 weeks 3 samples from each condition were oven dr...
K Suzuki


Next Page