Your search resulted in 1824 documents. Displaying 25 entries per page.
Five-year evaluation of a field trial of Eucalyptus grandis poles treated with zinc and boron
2017 - IRG/WP 17-30721
…the first treatment by simple ascent and diffusion of the preservative, at the same time as it was sought to impregnate the heartwood. The second preservative was applied by pressure and non-pressure methods, and the effectiveness and retention achieved were compared. This paper presents the results of treatments…
C Ibáñez, A Camargo, C Mantero, M Rabinovich
The durability of manufactured structural building materials
2016 - IRG/WP 16-40718
The projected market potential for Engineered Wood Products such as CLT (cross laminated timber) is very positive however, potential prolonged rain leakage or moisture exposure during construction and in-service could pose considerable concern for its durabili…
T Singh, D Page
Properties of Wood Plastic Composites Made of Recycled HDPE and Remediated Wood Flour from CCA/CCB Treated Wood Removed from Service
2016 - IRG/WP 16-40747
Chromated copper arsenate (CCA) and copper, chromium and boron (CCB) have been widely used in pressure treated wood as a heavy duty preservative to protect wood against insects and fungi for more than 60 years. Although many attempts have been done to solve th…
E D Gezer, S Akbaş, M Tufan, A Temiz
Above ground field testing: results of experiments in Brazil after one year
2015 - IRG/WP 15-30660
…be to bring these tests to locations that are conducive to biodeterioration, like tropical climates. Tropical sites provide higher temperature and humidity, which are excellent environmental conditions for wood biodegradation. Adaptations of four internationally-recognized standards were used to evaluate the…
M F Natale, J M Vidal
The effect of preservative treatment on mechanical strength and structural integrity of wood
2015 - IRG/WP 15-30667
The use of wood for demanding construction applications is increasing in Europe. Wooden constructions are frequently designed of susceptible conifer wood, which is endangered by wood decay fungi in wet applications. Therefore in many cases treating wood with p…
M Humar, D Kržišnik, C Brischke
The development of accelerated test systems to evaluate the durability of framing timber
2014 - IRG /WP 14-20547
Various accelerated decay resistance trials including small simulated wall units, samples exposed in enclosed tanks and ‘I’ samples in stacks have been explored and used to test the durability of treated and untreated radiata pine framing at Scion since 20…
T Singh, D Page, J van der Waals
Environmental aspects of wood preservation
1987 - IRG/WP 3406
The preservation industry employs a wide range of chemicals and processes to provide timber commodities capable of resisting biodeterioration and degradation. The public often perceives the chemicals as health hazards and treatment plants as potential threats…
H Greaves
Mold Control for Treated Lumber in Block-Stack Storage Conditions
2012 - IRG/WP 12-30588
The mold development and control for freshly treated and block-stacked wood have been evaluated using a green house mold testing method. The results for the mold resistance of several commonly used water boron preservative treatment systems, such as ACQ, Copp…
L Jin, P Walcheski, A Preston
Sample Origin Influencing the Leachability of Wood Preservatives
2011 - IRG/WP 11-20474
The aim of this study is to see if the raw material influences fixation and leachability of wood preservatives. Moving towards more eco-friendly and –concious society, the wood industries must adjust itself to new rules and regulations. Greener solutions in…
K Kängsepp. E Larnøy, P Meier
A Method for Studying Boron Redistribution and Leaching in Timber Framing
2011 - IRG/WP 11-20476
In typical New Zealand timber framed house construction, the timber framing has a vapour permeable building wrap applied to the exterior and a cladding applied over 20 mm battens. An interior lining usually of gypsum plasterboard is then fixed once the timber…
J A Drysdale, N Marston, M E Hedley
Fixed Borates Anyone?
2011 - IRG/WP 11-30563
The quest for a borate based preservative system that resists leaching or is “fixed” has long been a research goal. Boron fixation has been attempted with numerous strategies but there have been problems associated with past methods. This paper discusses…
C R McIntyre, M A Lake
Tannin resin-boron for outdoor wood protection and fire retardancy
2011 - IRG/WP 11-30567
Boron in the form of boric acid is well known for its efficacy against wood destroying organisms, as well as for its high leachability from treated wood when in outside exposure. Moreover, due to the European directive 2008/58/EC, boric acid is only authorized…
M-F Thévenon, G Tondi, N Leménager, S Wieland, A Pizzi
Protective Levels of Borates in timber Foundation Piles 5 – 18 Years after In-situ Remedial Treatment in Areas with Wet Clay Ground Conditions. The Jerbor and Eurobor Protocol, Part 1.
2011 - IRG/WP 11-30571
Timber has been used as foundation piles and grillages for decades or even centuries. Since the late 1970s a method for investigate, analyze and treat building timber foundations in soft clay grounds against decay fungus with a biocide have been developed and…
M Theorin, K-M Bandh
The case for using borates in termite control in tropical Australia
2011 - IRG/WP 11-30573
A brief historical overview of boron based wood preservatives efficacy against subterranean termite management worldwide, and in Australia, is presented. The boron based compounds to be used in H2 hazard conditions, may be applied as a surface treatment by dip…
B M Ahmed (Shiday), J R J French
Assessment of Boracol 200RH (FrameSaver) as a remedial treatment to control decay in pre-decayed model timber frame units
2010 - IRG/WP 10-30529
Model timber frame units constructed from untreated radiata pine were pre-wetted to approximately 40% moisture content and inoculated with Coniophora puteana and Oligoporus placenta. Units were transferred to a controlled environment room maintained at 25°C a…
Mick Hedley, Dave Page, Jackie van der Waals
Sorption properties of wood impregnated with aqueous solution of boric acid and montan wax emulsion
2010 - IRG/WP 10-40492
Non-biocidal techniques for wood protection become more and more important, nowadays. One of the possible treatments is use of water repellents. In the present research influence of, one of the possible water repellent, the montan wax emulsion, on the moisturi…
B Lesar, M Humar
Preservative Treatment of simul (Bombax ceiba) Veneers with Hot and Cold Water Solution of borax-boric acid by Soaking Process
2010 - IRG/WP 10-40528
Veneers of simul (Bombax ceiba) were treated with different concentrations of water- borne preservatives borax-boric acid (BB) by soaking process for different time periods. In the case of hot water treatment, it was found that the average retention of preserv…
K Akhter, Md Abul Hashem, S Akhter
Comparison of laboratory and semi-field tests for the estimation of leaching rates from treated wood
2010 - IRG/WP 10-50274
The authorization of wood preservative formulations in the European Union according to the Biocidal Products Directive (BPD) includes the assessment of environmental risks by the emission of active ingredients. This risk assessment includes scenarios for prese…
N Morsing, M Klamer, B Seidel, J Wittenzellner, M Maier, J Habicht
Accelerated H3 above-ground decay trials in Australia
2009 - IRG/WP 09-20411
An above-ground H3 fungal field trial was installed at five sites (3 in Australia, 2 in New Zealand), with the aim of finding a method that would shorten the time required for evaluating new preservatives and protection systems. One-quarter of the H3 preservat…
L J Cookson, J Carr
Resistance to decay fungi of ammonium borate oleate treated wood
2009 - IRG/WP 09-30505
Ammonium borate oleate molecule (ABO) produced from reaction between boric acid, ammonia and oleic acid was tested as wood preservative treatment against brown and white rot fungi according to European standards. This compound was prepared according to a previ…
F Lyon, M-F Thevenon, A Pizzi, J Gril
Modification of Wood by a Water-Repellent Compound Used in the Textile Industry: Boron Release and Termite Resistance
2009 - IRG/WP 09-40447
In the study, wood specimens were treated with disodium octoborate tetrahydrate (DOT) and a commercial water and oil repellent compound, FORGUARD M®, a weak cationic emulsion containing dipropylene glycol monomethylether, water and solids in its formulation a…
S N Kartal, E Terzi, B Erilkun, Y Imamura
Effects of concentration and temperature of CCA and CCB on wood strength of Turkish fir (Abies bornmulleriana Mattf.)
2009 - IRG/WP 09-40450
The purpose of this study was to present evidence for the effects of concentration and temperature of solutions of water-borne preservatives (chromated copper arsenate, CCA and chromated copper boron, CCB) on the static bending properties (modulus of elasticit…
I Usta, M Hale
Influence of Polyvinyl acetate emulsion (PVA) on boron leaching and fungicidal properties
2008 - IRG/WP 08-30451
Boron compounds are very effective fungicides, but unfortunately they leach from wood. In order to improve boron fixation, boric acid, borax were combined with polyvinyl acetate emulsion (PVA). For comparison copper salts were included into this research as we…
M Humar, B Lesar, P Kralj
Effects of CCB on wood strength of Eastern spruce (Picea orientalis L.)
2008 - IRG/WP 08-40416
The effects of CCB (chromate copper boron) on the static bending properties of Eastern spruce (Picea orientalis L.) based on MOE (modulus of elasticity) and MOR (modulus of rupture) were evaluated after full-cell vacuum/pressure treatment using a 3.0 % concent…
I Usta, M Hale
Wood decay fungi from New Zealand ‘leaky’ buildings: PCR identification and laboratory decay tests of wood preservative-treated Pinus radiata (Part 1)
2007 - IRG/WP 07-10620
Fungi colonising Pinus radiata D. Don framing timber of ‘leaky’ New Zealand buildings were isolated to produce pure cultures. Mycelia from these cultures on agar media were collected to extract DNA. To identify the fungi to the species level, polymerase ch…
D Stahlhut, R L Farrell, R Wakeling, M Hedley