IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 325 documents. Displaying 25 entries per page.


Method for determining the critical moisture level for mould growth on building materials
2013 - IRG/WP 13-20530
The natural conditions of relative humidity (RH) and temperature (T) in different parts of a building is rarely constant over time. Instead, RH and T often vary cyclically and may pose a risk of mould growth as these conditions are the two key environmental parameters that controls mould growth. Consideration to both humidity and temperature conditions and the susceptibility to mould in a material...
A Ekstrand-Tobin, P Johansson, G Bok


Critical moisture levels and mould resistance of five different wood treatments
2013 - IRG/WP 13-30632
Mould resistance of five different treatments were tested using two methods, a recently developed method for the determination of critical moisture levels of building materials (RHcrit), and ASTM D3273-94. The critical moisture level method exposed samples at 22 °C and 98, 92, 86 and 82% relative humidity (RH) for 12 weeks. ASTM D3273-94 was performed at 29 °C and about 95% RH. Treatments c...
G Bok, P Johansson, A Ekstrand Tobin, S Bardage


The critical moisture and temperature conditions for the growth of some mould fungi and the brown rot fungus Coniophora puteana on wood
1988 - IRG/WP 1369
The growth of some mould fungi on pine and spruce sapwood was studied in 40 different constant moisture and temperature conditions. The temperature range was between +10 and +40°C and the relative humidities varied from 76 to 100% relative humidity (RH). The incubation time was 12 weeks. The mixed mould inoculation used included typical fungi growing on wood: Aspergillus versicolor, Cladosporium ...
H Viitanen, L Paajanen


In-service performance of wood depends upon the critical in-situ conditions. Case studies.
2008 - IRG/WP 08-20382
Wood is a unique building material, but is by nature designed to deteriorate. A detailed understanding of the factors and interactions involved are important when working with service life prediction of wooden components in buildings. Wood may experience exponential fungal degradation caused by variation in the climatic factors within a small limited area and by minor imperfection in the wooden ...
L Ross Gobakken, J Mattsson, G Alfredsen


Theoretic discussion on the way and driving forces of moisture migration in wood during vacuum drying
2011 - IRG/WP 10-40538
Most of parameters in conventional drying cannot explain a lot of phenomena appeared in vacuum condition, so it is necessary to further explore the moisture migration way and driving forces in wood under vacuum condition. For the water movement channel in wood is very narrow, the characteristic of heat and mass transfer in wood is similar to that in microscale. This article applies theory of liqui...
Zhengbin He, Xueli Yao, Liqiong Chen, Songlin Yi


Critical parameters on moisture dynamics in relation to time of wetness as factor in service life prediction
2014 - IRG/WP 14-20555
The concept of natural durability or enhanced durability based on the presence of active ingredients having an impact on both fungi and insects is not the only parameter steering the material resistance. Complementary resistance to getting wet (wetting ability) and consequently the ease of drying afterwards will lead to a parameter related to the time a piece of wood will remain under such wet con...
J Van Acker, I De Windt, W Li, J Van den Bulcke


Moisture content levels and decay of hemlock
1986 - IRG/WP 1287
As a model of decay conditions of wooden members in wooden houses, a decay test was set up in which samples of western hemlock (Tsuga heterophylla) under 4 moisture levels were examined. Each week the samples were weighed and if the weights indicated that their moisture contents were lower than the expected levels, distilled water was added. Every 8 weeks 3 samples from each condition were oven dr...
K Suzuki


How to Document the Performance of Super-Critical Treated Wood in above Ground Situations?
2005 - IRG/WP 05-20316
The paper presents practical experiences from the preparation of a new preservative treated wood product for introduction to the market. The product in question is Superwood™, which is treated with organic biocides using CO2 in a supercritical state as a solvent. The question is how to evaluate the performance of a new product such as Superwood™ in order to get an acceptance on the market a...
N Morsing, A H H Wong, F Imsgard, O Henriksen


Developments in the protection of wood and wood-based products
1980 - IRG/WP 340
Technology is playing an increasingly important role in the field of wood protection. This current review highlights how modern techniques have provided greater insight into the biological and physical processes affecting the durability of wood and wood-based products. Emphasis is also given to developments in preservative testing methodology and to the encouraging changes towards both the correct...
J M Baker


Proposed methodology for the assessment of safety indexes
1990 - IRG/WP 3562
Safety Indexes (SI)s are developped on the same concept as Efficacy Indexes (EI)s: EIs are retentions of wood preservatives (percentages of the critical values "efficacy") which are presumed efficient for a given biological class of risk. In the same way, SIs are retentions of wood preservatives (percentages of the critical values "safety") which are taken as acceptable for human health and the ge...
G Ozanne


New technique to analyze impregnation processes
1988 - IRG/WP 2304
Equipment has been developed to measure liquid flow in wood during impregnation processes. Basic principles of flow measurements using directly heated negative temperature coefficient thermistors, and some characteristics of the hardware developed are presented in this paper....
J P Hösli


Soil virulence tests using Scots pine sapwood
1973 - IRG/WP 222
Following the tests reported in Document No: IRG/WP/210, in which soils from different laboratories were investigated for virulence, supplementary tests have been carried out using Scots pine sapwood and an extended incubation period....
J K Carey, J G Savory


Co-operative research project on L-joint testing. Sampling after 8 months exposure
1983 - IRG/WP 2208
It was anticipated in Document No IRG/WP/2192 that exposure of L-joints by the European co-operators would take place on 1 April 1983. Where L-joints were exposed at this time, sampling after 8 months exposure is due on 1 December 1983. The present document draws attention to relevant previous documents which describe the sampling methods to be adopted. It also provides Tables for recording the re...
J K Carey, A F Bravery


Influence of moisture content of rubber wood on the growth of Botryodiplodia theobromae
1993 - IRG/WP 93-10029
Botryodiplodia theobromae is the main fungus causing sapstain on rubber wood (Hevea brasiliensis). The entry and establishment of the stain fungus is nighly influenced by the moisture content of the wood. To determine the optimum moisture content of wood required for maximum growth of Botryodiplodia theobromae wood blocks at different moisture contents were inoculated with the test fungus and incu...
E J M Florence, R Gnanaharan, J K Sharma


Successive collections of Basidiospores from wood decay fungi (in vitro) show variation in germination levels on common media
1978 - IRG/WP 191
In the course of various preliminary experiments in which spore germination levels of 6 decay fungi on malt and water agar were recorded as controls, it was noted that one could not reliably obtain an expected level of spore germination for any particular fungus. Inconsistent 'control' spore germination levels of a fungus greatly complicates large scale experiments in which compa...
E L Schmidt, D W French


Comparison of the agar-block and soil-block methods used for evaluation of fungitoxic value of QAC and CCA wood preservatives
1994 - IRG/WP 94-20039
The modyfied agar-block and soil-block methods were used for comparing the fungitoxic value of QAC and CCA type preservatives against Coniophora puteana and Coniophora olivacea The mass loss and moisture contents of wood were analysed....
J Wazny, L J Cookson


Collaborative soft rot tests: Programme and test method
1973 - IRG/WP 229
J G Savory, J K Carey


Observations on the failure of anti-sapstain treated timber under non-drying conditions
1990 - IRG/WP 1437
A range of bacteria and yeasts were isolated from antisapstain treated timber and fresh sawdust. Solution samples containing 100 ppm of TCMTB in a nutrient medium were inoculated with these organisms and incubated at 25°C for 5 days. The levels of TCMTB remaining in solution were determined by HPLC analysis after this time. Results indicated high losses of active ingredient for a range of organis...
G R Williams


Wood preservation in France. "Bois plus" chain of quality. Description of the scheme early 1989
1989 - IRG/WP 3519
1989 - description of the French "CTB-BOIS PLUS" homologation scheme
G Ozanne


Co-operative research project on L-joint testing. Progress report to March 1988
1988 - IRG/WP 2315
Further sets of data received from CTFT (France), BAM (Germany) and PRL (UK) after 46-48 months exposure and STU (Sweden) after 22 months exposure are presented and discussed in conjunction with data reported previously. Colonisation and attack of the L-joints has progressed with increasing exposure period. The new data are generally in agreement with those presented previously and the major diffe...
J K Carey, A F Bravery


Collaborative soft rot tests: Interim report on PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1972 - IRG/WP 211
Preservative: Tanalith CT.106 - Results obtained with beech are given in the table and indicate a toxic limit of 16.7-19.2 kg/m³ - The initial soil moisture content was adjusted to 27.8% (the water holding capacity). Noticeable drying out has occurred in some of the test bottles....
J G Savory


A critical review of the AWPA standard method (M12-72) for laboratory evaluation to determine resistance to subterranean termites
1986 - IRG/WP 1298
The American Wood Preservers' Association standard (M12-72) for evaluation of candidate wood preservatives against subterranean termites is reviewed and suggestions for revision are made. The most serious flaws in the current test procedure involve a failure to recognize inter- and intraspecific variation and a lack of quantification of test results....
J P La Fage, M Jones


A standardised procedure for the treatment of timber with test chemicals
1986 - IRG/WP 2257
A procedure is described which allows the standardisation of sample handling and data manipulation during trials invastigating the treatability of timber with test chemicals. The use of computer software allows the data to be handled efficiently....
J Norton, A Zosars, L E Leightley


Diffusion of fused borate rods in top ends of poles
1989 - IRG/WP 3518
Diffusion tests of fused borate rods were carried out on extremities of sapwood poles in service. Rods were set in drills under the cone with or without addition of liquid Boracol 40. After one year of weathering, a good diffusion in the slice under the cone and even below the slice and in the cone itself was observed in Scots pine and spruce poles. The rods were still intacts and constitute, in f...
D Dirol, J P Guder


Analysing the characteristic role of moisture content for drying and fluid flow in Sitka spruce. - Part 1: The drying process of sapwood and heartwood of two different thickness of Sitka spruce using a kiln. - Part 2: Effects of moisture content on longitudinal permeability of Sitka spruce in vertical variation of the tree
2000 - IRG/WP 00-40173
The characteristic role of the moisture content in Sitka spruce (Picea sitchensis (Bong.) Carr.) that grown in the United Kingdom was examined by this study on the basis of (1) the reduction of moisture content in two different thickness of sapwood and heartwood by kiln drying process, and (2) the effects of moisture content to the longitudinal void volume filled of tanalith-C by the full-cell pro...
I Usta