Effect of kerfing on performance of Douglas-fir utility poles in the Pacific Northwest
1990 - IRG/WP 3604
Preservative treatment produces an external layer of protection in Douglas-fir poles, but the development of deep checks as the wood dries after treatment can permit entry by fungi and insects. A variety of remedial treatments can arrest this decay; however, it is far more efficient to prevent checking. Kerfing represents one potential method for limiting the development of deep checks. In previou...
J J Morrell


A comparison between different accelerated test methods for the determination of the natural durability of wood
1996 - IRG/WP 96-20099
According to the European standard EN 350-1 the natural durability of wood is defined as: "the inherent resistance of wood to attack by wood destroying organisms". This standard also describes how, for certain hazard classes, the durability is determined. The two methods described in this standard are the kolleflask method (EN 113) and the field-stake-test method (EN 252). The EN 113 test gives re...
H Militz, S G L Michon, J E Polman, M Stevens


Performance of preservative-treated timber against biodeterioration in Indian waters
1984 - IRG/WP 4106
Results on the investigation on the durability of panels of 32 timber species, pressure-treated with various preservatives and exposed along the Indian coast for varying periods upto a maximum of 15 years, are summarised. Panels of even non-durable timber gave excellent results against biodeterioration after treatment. Their life was comparable to that of treated durable timber. The preservative t...
L N Santhakumaran, J C Jain, M C Tewari


Non-destructive stress wave measurement of decay and termite attack in experimental wood units
1986 - IRG/WP 2256
The purpose of this study was to determine if stress wave analysis could be used to monitor the degradation of wood specimens exposed to the brown-rot decay fungi (Gloeophyllum trabeum) and of wood specimens subjected to attack by subterranean termites. One hundred fifty 3/4 by 3/4 by 12 in. Southern pine specimens were used for exposure to brown-rot decay fungi and two hundred twenty-five 3/4 by ...
R F Pellerin, R C De Groot, G R Esenther


Evaluating the potential of amine chemicals for use as wood protecting agents. Part 1: Investigation of cation components of quaternary ammonium compounds
1994 - IRG/WP 94-30049
Quaternary ammonium compounds (quats) have shown a great potential as more environmentally acceptable wood preservatives. In order to identify chemicals possessing the wood protecting potential, an evaluation was carried out of a range of commercially available 'quats', using a modified soil block test. Ponderosa pine sapwood blocks were treated with selected 'quat&a...
Hang Tang, J N R Ruddick


Decay resistance of densified ammonia-plasticized stems of oil palm (Elaeis guineensis)
1991 - IRG/WP 3673
When wafers of oil palm stems (Elaeis guineensis) were plasticized with 28% aqueous ammonia and immediately compressed mechanically, the treated material, gained 73% in basic density (average basic density, 0.695 g/cm³), and was highly resistant to decay by wood rot basidiomycetes. Compared with the control specimens (density, 0.403 g/cm³), resistance to decay of the densified specimens by Corio...
A H H Wong, M P Koh


Dimensional lumber model demonstrates the sensitivity of the particle capture immunoassay in early detection of brown-rot fungi
1995 - IRG/WP 95-20058
A dimensional lumber model was designed to test the sensitivity of the particle capture immunoassay (PCI) compared to traditional methods of culturing and microscopic examination for detection of brown-rot fungi. Southern yellow pine 2 x 4's (5.1x10.2 cm²), and 86.4 cm in length, were inoculated on one end with the brown-rot fungus, Postia placenta, and tested over the full length of the...
C A Clausen, L Ferge


Severe decay damages of bridges made of ekki (Lophira alata) wood known as a durable species
2000 - IRG/WP 00-10383
Bridges made of ekki (azobe, bongossi, Lophira alata Banks et Gaertn.) timbers were severely decayed only 10 years after the construction possibly caused from no maintenance for the periods. The reason of no maintenance is due to the misunderstandings on wood durability against wood-decaying fungi. Some civil-engineers and architectures understand "durable species" means "absolutely decay-durable ...
S Doi, T Sasaki, Y Iijima


Evaluation of the european standard ENV 12038 for durability testing of plywood
2001 - IRG/WP 01-20237
The latest improved version of the standard ENV 12038 drafted as document N44 by CEN Technical Committee 38 (WG 7 - WG 23) is used to evaluate the effect of wood composition and structure on plywood durability. The method described is based on the agar-block test of the EN 113 standard used for the determination of the efficacy of wood preservatives and the assessment of the natural durability of ...
J Van Acker, M Stevens, E De Clercq


The WOODCARE project: Development of detection methods for Death watch beetle larvae and fungal decay
1999 - IRG/WP 99-20172
Woodcare was a European project coordinated by English Heritage. The aim of the research was to develop more targeted and more environmentally friendly treatment methods for Death watch beetle infections in Oak constructions of historical buildings. TNO has developed two new methods for fast and reliable detection of Death watch beetle larvae and related fungal decay in Oak. The problem with Death...
P Esser, P Van Staalduinen, A C Tas


Durability of surface coating systems. Mycologg - an accelerated mycological test.
2004 - IRG/WP 04-20301
Field testing and natural aging/degradation of test sample, e.g. coated wooden surfaces is a slow process. Accelerated tests focus on mechanical properties, water uptake or sometimes stain fungi. Artificially weathered coated panels are not easily compared with naturally aged panels, and show the importance of involving the biological component among the degrading facors. It is a need for acce...
L Ross Gobakken, J Mattsson, B Jacobsen, F G Evans


Laboratory evaluation of termite resistance of five lesser-known Malaysian hardwoods used for roof and ceiling construction
2001 - IRG/WP 01-10398
The general laboratory procedure of AWPA E1-97 was used to evaluate the termite resistance of 5 lesser- known species (LKT) of Malaysian hardwoods: Kekatong (Cynometra sp.), Kelat (Eugenia spp.), Mempening (Lithocarpus spp.), Perah (Elateriospermum tapos) and Pauh Kijang (Irvingia malayana) against the subterranean termite Coptotermes curvignathus over 28 days. Kempas (Koompassia malaccensis) and ...
A A H Wong, Kee Suan Cheok, J K Grace


Treatment of poplar plywood with solvent and water-borne preservatives
1989 - IRG/WP 3538
Poplar as a light hardwood is appropriate for plywood production. Owing to its low natural durability it is generally recommended to preserve it in all conditions where risks of fungal attack may be present. A research project has been carried out on preservative treatments of plywood commodities. Parameters studied were various treatment cycles, three types of plywood, and a number of solvent and...
J Van Acker, M Stevens


Disodium octaborate tetrahydrate, alone and in conjunction with a selected isolate of Trichoderma viride, reduces decay of fresh felled pine independent of the effect of weathering
1994 - IRG/WP 94-10054
Unpeeled billets of Corsican pine were treated with the following: 5% aqueous disodium octaborate tetrahydrate (DOT) solution; 5% DOT solution with an isolate of Trichoderma viride with a low susceptibility to borate; the Trichoderma viride isolate alone. Half of the billets in each treatment group were also placed in large-diameter plastic pipes to protect the billets from the weather. All three ...
M W Schoeman, D J Dickinson, J F Webber


Kiln drying of poles as a means of solving the problems of pre-treatment decay in poles
1985 - IRG/WP 1263
The concept that pre-treatment decay can cause wide variation in the treatability of wood and especially wood poles has caused much discussion and debate in wood preservation circles. Yet it seem only logical that if decay has effected the strength characteristics of the wood and caused a differential moisture content in the wood the treatment of the end product will be highly variable and the lon...
J A Taylor


Occurrence of termite species on decaying heartwood specimens exposed 18 to 23 years at an Australian site
1998 - IRG/WP 98-10270
The occurrence of species of subterranean termites on hardwood and softwood specimens (including preservative-treated), exposed in-ground at a semi-arid site at Walpeup (north-western Victoria), 18 to 23 years after installation, is reported. This paper presents maps of the cumulative occurrence on specimens, after six annual inspections, of the following species: Coptotermes acinaciformis, Hetero...
J W Creffield, J-D Thornton, G C Johnson


Above-Ground Durability Estimation in Australia. Results after 16 years exposure
2005 - IRG/WP 05-20314
A program of research was established in 1987 to examine the above-ground durability of a selection of timbers that are commercially significant in Australia. Test samples were assembled in an L-Joint design and placed on exposure racks in a format to replicate joinery that is exposed to the weather above ground. Both painted and unpainted material has been exposed. Test samples have been evaluat...
L P Francis, J Norton


Tolerance of Wood Decay Fungi to Commercial Copper Based Wood Preservatives
2002 - IRG/WP 02-30291
Due to the use of copper based preservatives like CCB or CCA for more than a century, copper tolerant fungi have appeared in some European countries in recent times. It is therefore important to find out whether this phenomenon is specific for only classical copper ingredients, or generally for all copper based formulation. Thus, we tested the tolerance of three commercial copper based pres...
F Pohleven, M Humar, S A Amartey, J Benedik


Decay resistance of Platanus acerifolia wood against White Rot Fungi (Coriolus versicolor)
2002 - IRG/WP 02-10431
Degradation of the lignocellulose complex in wood varies on the microorganism causing decay and chemical composition of wood. The weight loss of Platanus acerifolia wood after decay by white rot fungus (Coriolus versicolor) for period 16 weeks were evaluated according to European standard EN 113 and beech wood as a control. The samples were collected in October 2000 from Nantes, France. The aim of...
M Irmouli, O Duchelier, N Ayadi, B Charrier


On the laboratory use of X-rays in timber decay evaluations
1981 - IRG/WP 2144
The paper reports the results of laboratory experiments on the X-raying of some Pinus radiata sapwood blocks infected with Serpula lacrymans to determine the effect of density and moisture content on the absorption of X-rays by wood. It is concluded that with increasing moisture content there is a very marked increase in time required to pass a constant quantity of X-rays through a test block and ...
J D Thornton, J W Creffield, O Collett


The wood-attacking insects in wooden houses of an old open air museum in southern Finland
1989 - IRG/WP 1409
Harmful insects of wood in a open-air museum were investigated in 1985-1988 by order of the National Board of Antiquities and Historical Monuments of Finland in nine old log houses. Many thousands of insects and altogether 1073 anobiids (Coleoptera, Anobidae) were obtained by window and light traps. The most common Anobiidae-species were Hadrobregmus confusus (Kraatz) 60.3%, Hadrobregmus pertinax ...
H Viitanen, M Pulkkinen


The long road to understanding brown-rot decay. A view from the ditch
1995 - IRG/WP 95-10101
Interest in understanding how brown-rot fungi decay wood has received increasing interest in recent years because of a need to identify novel targets that can be inhibited for the next generation of antifungal wood preservatives. Brown-rot fungi are unique in that they can degrade holocellulose (cellulose and hemicellulose) in wood without first removing the lignin. Furthermore, they degrade holoc...
F Green III, T L Highley


Assessment of the Inhibition of wood decay fungi by volatile organic compounds identified from Trichoderma spp.
1999 - IRG/WP 99-10302
Previous research identified five volatile organic compounds produced by Trichoderma spp. that may be inhibitory to wood decay fungi. The effects of four of these volatile organic compounds, 2-propanone, 2-methyl-1-butanol, heptanal and octanal were tested over a range of concentrations against four selected wood decay fungi. The fungi were incubated in malt extract broth under appropriate conditi...
S N Humphris, R E Wheatley, A Bruce, C Payne


Moisture content development in lap-joints of different wood species in outside exposure trials
1998 - IRG/WP 98-20143
Lap-joint trails (following European Standard EN 12037) were set up with 11 different softwood and hardwood species. Half of the number of the lap-joint specimens were coated with an alkyd coating. The moisture development has been followed during a 19 months period. In this paper, the out comes of different moisture contents evaluations are presented. The results show, that the moisture content o...
H Militz, M Broertjes, C J Bloom


Bestimmung der pilzwidrigen Wirksamkeit von Holzschutzmitteln gegen Moderfäule-Erreger
1977 - IRG/WP 2125
Ziel der vorliegenden Arbeit war der Vergleich der in verschiedenen Ländern zur Bestimmung der pilzwidrigen Wirksamkeit von Holzschutzmitteln gegen Moderfäule-Erreger angewandten Methoden. Als Vergleichsmaterial dienten drei normierte Methoden: die britische (42), skandinavische (45) und die in der DDR angewendete (47) sowie wichtige, von verschiedenen Fachleuten ausgeführte Arbeiten experiment...