Your search resulted in 220 documents. Displaying 25 entries per page.
Supercritical fluid treatment: Effects on bending strength of white spruce heartwood
1993 - IRG/WP 93-20008
The effects of supercritical carbon dioxide on wood strength were evaluated using white spruce heartwood, a species known to be especially susceptible to collapse during exposure to higher pressures. The effects of pressures of 2000 or 3600 psig and temperatures of 40 or 80°C were evaluated using 30 or 60 minute exposure periods. No significant differences were noted in modulus of rupture or modu...
S M Smith, J J Morrell, E Sahle-Demessie, K L Levien
Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 1: Optimisation of the extraction conditions
2000 - IRG/WP 00-30238
As the first phase of a large project aimed at recovering 'waste' durability components from sawmill residues of Callitris glaucophylla, several solvents and extraction methods were evaluated, initially in the laboratory and then at pilot industrial scale. Extracts were compared by crude total dissolved solids content, by chemical analysis using GC-MS and LC-MS, and by laboratory...
M J Kennedy, Hui Jiang, L M Stephens
The treatment of Douglas fir fence posts: specification and compliance using new European standards
1999 - IRG/WP 99-20178
New European standards for the preservative pre-treatment of timber require the results of the treatment process to be specified and subsequently verified by examination of the treated timber for penetration and retention of the preservative. For penetration, the standards are restrictive in that there are only a limited number of options available to the specifier. Thus for ground contact service...
R J Orsler, H Derbyshire
Field evaluation of the above-ground susceptibility of Pinus heartwood and untreated or treated sapwood to two species of Australian subterranean termites
1996 - IRG/WP 96-10147
Plantation-grown Pinus elliottii, Pinus caribaea and Pinus radiata specimens containing heartwood and untreated or preservative-treated sapwood were exposed above ground to the subterranean termites Coptotermes acinaciformis or Mastotermes darwiniensis near Sydney (NSW), Brisbane and Townsville (Qld), and Darwin (NT), using a variety of exposure techniques. Heartwood of Pinus elliottii and Pinus c...
M J Kennedy, J W Creffield, R H Eldridge, B C Peters
Movement of borates in a range of timber species at various moisture contents
1998 - IRG/WP 98-30181
Borate-based wood preservatives are used in industrial pre-treatment as well as remedial treatment of timbers in situ. In both of these areas, understanding the mobile nature of these compounds is important in optimizing the main benefits of borates. Considerable work has been conducted on movement of borates in dip-diffusion treatment of freshly felled wood, as well as focusing on subsequent diff...
M W Schoeman, J D Lloyd, M J Manning
Tunnelling bacteria
1983 - IRG/WP 1186
The micromorphology of decay in wood caused by a certain group of single-cell bacteria, called tunnelling bacteria (TB), is described. TB are characterised by their tunnelling ability within the secondary cell walls of wood fibres. Pure cultures of TB have not yet been obtained although the typical decay patterns can be reproduced using mixed bacterial cultures. Some indications of lignin degradin...
T Nilsson, G F Daniel
Färbeverfahren zur Unterscheidung von Holzzonen mit unterschiedlichem Absorptionsvermögen, insbesondere bei Fichtenholz (Picea abies Karst.). [Staining method for distinguishing zones of wood with different absorption behaviour, particularly in spruce (Picea abies Karst.)]
1980 - IRG/WP 3163
A simple regressive staining method for crosscut wood surfaces is described. Phloroglucinol-hydrochloric acid serves as stain; flowing water and a solution of sodium carbonate are used for development and fixation of a picture showing the differences of absorption. Hydrophobic zones and, contrary to this, zones with a high water content can also be shown. Comparing green spruce wood before and dur...
S Cymorek
Micromorphology of decay in Keruing heartwood by the basidiomycetes Phellinus contiguus and Dacrymyces stillatus
2002 - IRG/WP 02-10454
This study aimed to characterise the micromorphology of fungal decay in a wooden handrailing in an above ground exposure at the Thames embankment in London. Keruing heartwood (Dipterocarpus spp.) was determined as the construction timber and the two basidiomycetes Phellinus contiguus and Dacrymyces stillatus identified as main decay organisms.
Their decay patterns within Keruing heartwood were...
G Kleist, M Ray, R J Murphy
Effects of Prior Establishment of Trichoderma harzianum on Ophiostoma picea Growth in Freshly Sawn Douglas-fir Sapwood
2003 - IRG/WP 03-10476
Trichoderma harzianum has been shown to be an effective biocontrol agent against a number of wood inhabiting fungi under laboratory conditions, but this fungus has performed poorly in field trials. Understanding the interactions between biocontrol agents and their intended targets in wood may provide important clues for developing improved approaches to biocontrol, potentially reducing our relianc...
Ying Xiao, J J Morrell, L M Ciuffetti
Assessment of untreated Papua New Guinea timbers against subterranean termites. Progress report 2
1993 - IRG/WP 93-10040
Eight species of Papua New Guinea wood including Kwila (Intsia palembanica), Taun (Pometia pinnata), Malas (Homalium foetidum), PNG Walnut (Dracontomelon dao), Calophyllum (Calophyllum sp.), Kamarere (Eucalyptus deglupta), PNG Beech (Nothofagus spp.) and White Cheesewood (Alstonia scholaris) were exposed groun contact for their natural durability against subterranean termites. Inspection after 42 ...
M Rokova, H C Konabe
Fluoride movement through Douglas-fir and hem-fir lumber following dipping in potassium/ammonium bifluoride
1995 - IRG/WP 95-40040
The ability of ammonium and potassium fluoride to diffuse through Douglas-fir and hem-fir lumber was evaluated over a 90 day period. Boards were dipped in a solution containing 10% (by weight) of ammonium and potassium bifluoride, then stored under cover for 90 days. Samples removed 30, 60 and 90 days after treatment indicated that the fluoride was unable to completely penetrate the wood. Penetrat...
J J Morrell, C S Love
Natural durability of larch heartwood against decay
1997 - IRG/WP 97-10201
Larch heartwood has been promoted in Sweden and in other European countries as an alternative to preservative treated timber. It has even beeen stated that larch heartwood is more durable than preservative treated timber. This paper presents a compilation of facts from scientific reports on the durability of larch heartwood. Some recent data from this department are also reported. All data suggest...
T Nilsson
Evaluation of the natural durability and ultrasonic method for decay detection of some european hardwood and softwood species
2004 - IRG/WP 04-10537
This paper presents the first part of an investigation on the natural durability of mixed plywood made of durable and non durable plies from the following selected timbers : Cedrus atlantica, Cupressus sempervirens, Castanea sativa, Populus sp. I 214 and Fagus sylvatica.
In order to carry out this study, the natural durability of the massive wood used to manufacture the plywood panels was asses...
F Faraji, M-F Thévenon, B Thibaut
Variation in natural durability of British grown Douglas fir ((Pseudotsuga menziesii (Mirb.) Franco). Part II. Effect of extractive contents and taxifolin
2002 - IRG/WP 02-10446
The previous paper (Part I: Effect of density and growth rate) described the variation in natural durability of 4 Douglas fir (DF) seed origins (Darrington, J. Landing, Naselle and Hawkinsville) in a pure culture decay test and fungal cellar test. The pure culture tests were performed against two brown rot fungi (Coniophora puteana and Postia placenta). In the fungal cellar test soft rot was the p...
S Akhter, M D C Hale
The performance in the sea of seven experimental piles after sixteen years at Port Douglas, North Queensland
1989 - IRG/WP 4151
After 16 years at Port Douglas, two double-treated Pinus radiata piles were in excellent condition, a CCA-treated Pinus elliottii pile was in good condition other than for a confined streak of teredinid attack, while two CCA-treated and two untreated turpentine piles were moderately to severely attacked by Sphaeroma in the tidal zone. The marine borers collected were Sphaeroma terebrans, Martesia ...
L J Cookson, J E Barnacle, C N McEvoy
Sterilization to limit pretreatment decay: Internal temperature during kiln drying of Douglas-fir poles
2001 - IRG/WP 01-40206
Sterilization to limit pretreatment decay: Internal temperature during kiln drying of Douglas-fir poles. Fungal colonization of poles following peeling has been the subject of considerable concern among electric utilities. While the presence of fungi does not, in itself constitute a risk, the survival of these fungi through the conventional treating processes could allow them to continue to degrad...
J J Morrell, P G Forsyth, K L Levien
Differentiation of Scots pine heartwood and sapwood by near infrared spectroscopy
2003 - IRG/WP 03-10459
In Scandinavia Scots pine heartwood has, in recent years, gained popularity as material for external structures exposed to moderate risk of decay. As non-durable sapwood surrounds the heartwood in pine trunks it is of crucial importance to separate this wood from the heartwood during log processing into heartwood products. Heartwood and sapwood can be differentiated by visual evaluation of colour ...
P O Flæte, E Ystrøm Haartveit
Effects of air-seasoning on fungal colonization and wood strength of Douglas fir poles
1987 - IRG/WP 1315
Air seasoning economically reduces the moisture content of Douglas fir poles before pressure treatment with preservatives. Advanced decay in poles in service has resulted when decay fungi (Basidiomycetes) colonized poles during air-seasoning and survived the treatment process. These problems have led to recommendations to severely limit this practice. To determine the role of these fungi in peeled...
J J Morrell, M E Corden, R D Graham, B L Kropp, P Przybylowicz, S M Smith, C A Sexton
Effect of substrate type and moisture requirements in relation to colony initiation in two carpenter ant species
1999 - IRG/WP 99-10320
Conditions necessary for optimal colony initiation or the rate of initial colony expansion by early brood in the carpenter ant species Camponotus modoc and C. vicinus on various substrates conditioned to different moisture contents were studied. Camponotus modoc and Camponotus vicinus queens were placed in Douglas-fir, western red cedar and Styrofoam® blocks conditioned in sealed chambers at 70% ...
M E Mankowski, J J Morrell
Decay evaluation of the effectiveness of a LOSP envelope treatment in eucalypt and meranti heartwoods for window joinery
1996 - IRG/WP 96-30099
The effectiveness and penetration in heartwood boards of an LOSP formulation containing TBTN was examined by determining decay resistance to the white-rot fungus Perenniporia tephropora. Boards, one metre long, of Eucalyptus regnans, Eucalyptus delegatensis, Eucalyptus obliqua and Eucalyptus sieberi were treated, along with boards of 'light' and 'dark' meranti. ...
L J Cookson, A Trajstman
Effect of species composition of preservative-treated Douglas fir plywood on its decay resistance
1978 - IRG/WP 2114
Plywood is now commonly used for constructional purposes in environmental situations where decay by wood-destroying fungi can be a considerable risk. However there seems to be a lack of understanding of the relative durability of plywood, both untreated and when treated with wood preservatives. Part of the reason for this situation has been the difficulty of carrying out laboratory decay tests on ...
R S Smith, P Balcaen
Effect of post-treatment processing on leachability of ACZA-treated douglas-fir lumber
1998 - IRG/WP 98-50109
The effect of post-treatment procedures that more rapidly precipitate copper, zinc, and arsenic in douglas-fir treated with ammoniacal copper zinc arsenate (ACZA) on subsequent leaching resistance were investigated at two retentions (6.4 and 40 kg/m3). Total leaching was greater from boards treated to the higher retention. At both levels, copper was lost at the highest rate. Post-treatment process...
J J Morrell, C S Love, S Kumar, C M Freitag
Fungal decay resistance of Rubber wood treated with heartwood extract of Rosewood
2005 - IRG/WP 05-30367
Alcoholic extract of Dalbergia latifolia heartwood was studied for its toxicity towards wood decaying fungi. Rubber wood blocks were treated with this extract to three different retention levels (0.1%, 0.2% & 0.5%) and the treated wood blocks were assessed for their resistance towards two white rot and two brown rot fungi. Treated blocks showed improved resistance over the control blocks. At 0...
A K Sethy, H C Nagaveni, S Mohan, K T Chandrashekar
Microwave modification of Yellow Stringybark (Eucalyptus Muelleriana) posts for impregnation with Copper-Chrom-Arsenic (CCA) preservatives
2000 - IRG/WP 00-40185
Yellow Stringybark posts with diameters ranging from 60-100 mm were microwave conditioned using a 60 kW microwave (MW) generator. A substantial improvement in heartwood penetration of preservatives and relaxation of growth stresses was indicated such that there was no split formation following drying of the posts. High preservative absorption of copper-chrome-arsenic (CCA) was achieved ranging fro...
G Torgovnikov, P Vinden
A comparison of the diffusion of boron from two types of solid preservative rods into the heartwood of 3 Eucalypt pole species
2000 - IRG/WP 00-30227
The ability of boron to diffuse from polyborate and boron/fluoride rods through the heartwood of three eucalypt pole species (blackbutt, red ironbark and spotted gum) was examined. The aim was simply to determine the effects of rod type, wood species and time on the longitudinal diffusion of boron in eucalypt heartwood. Rapid diffusion of boron from polyborate or boron/fluoride preservative rods o...
P J Beutel, P D Evans