Gaseous boron treatments of wood and wood products
1992 - IRG/WP 92-3691
Treatment of wood and wood products by gaseous organoborates has now been under study for about 5 years. This technique has potential for boron treatment of a wide range of substrates from solid wood through to wood composite materials such as particleboard or wet and dry formed fibreboards. The vapour treatment technique is proving to be very flexible in that it can be adapted to integrate into a...
A J Bergervoet, R Burton, K Nasheri, D R Page, P Vinden


Restrictions on the use of chlorosilanes as potential wood preservatives
1985 - IRG/WP 3345
The biological protection of wood by chemical modification with different types of chlorosilanes has been investigated. The impregnation of wood has been carried out by means of liquid phase and vapor phase treatments using pure silane and silane-solvent systems. The biological efficacy against wood rotting fungi, molds and staining fungi was determined in a number of screening trials, subsequentl...
M Stevens


Treatment of wood with boron esters
1995 - IRG/WP 95-30087
The treatment of wood and wood products with boron esters is reviewed. The physical and chemical characteristics of boron esters affecting the treatability of wood are discussed, in particular thermal decomposition and rates of hydrolysis. The uses and methods applying boron esters as wood preservatives include: (i) Solutions of boron esters for remedial and diffusible treatment of wood; (ii) soli...
J Romero, P Vinden, J A Drysdale


Gaseous preservative treatment of wood
1990 - IRG/WP 3631
A recent development in processing wood with a gaseous preservative means that dry, treated wood can be produced in under 30 hours with the benefits of product diversification, faster stock turnover and the ability to respond to short term demand. About 400,000 m³ of wood are treated each year in New Zealand with boron salts to protect from borer infestation. Traditionally this treatment is effec...
R Burton, A J Bergervoet, K Nasheri, P Vinden, D R Page


Selecting fumigants for treatment of internal decay in wood
1986 - IRG/WP 3370
A number of potential fumigants were screened with respect to their toxicity to decay fungi, (Poria carbonica, and Lentinus lepideus) and their sorption characteristics on Douglas Fir (Pseudotsuga menziesii Mirb. Franco) wood. Wafers of infected wood were exposed to different fumigant concentrations for various times then cultured to determine viability. The lethal concentration X time (ct) factor...
P A Cooper


Redistribution of boric acid in radiata pine during drying after preservative treatment
1993 - IRG/WP 93-40010
Samples of 100 x 50 mm² radiata pine were processed with a variety of options to produce dry, boron-treated wood. Concentrations of boric acid in the central one-ninth and in the whole of the wood cross-sections were determined by chemical analysis and compared. Diffusion treated material was dried by air, conventional kiln (70/60°C), or high temperature kiln (120/70°C). Four different predryin...
A J Bergervoet, D R Page, J A Drysdale


Survey of North American practice in conditioning forest products before preservative treatment
1972 - IRG/WP 308
Seasoning requirements for the wide range of forest products which are treated with preservatives and fire retardants must be capable of dealing with a very complex set of conditions which are summarized under a number of variables including type and hazard of end use, the most effective distribution of preservative, a wide range of cross sectional dimensions, the possibility of seasoning by a ran...
J Rak, T S McKnight


Survey of practical methods for conditioning of forest products before preservative treatment
1971 - IRG/WP 39
The seasoning of forest products is undertaken for a wide range of end uses and is becoming increasingly required for applications and building construction and secondary manufacturing industries. A wide range of applications of new technology and specifically required seasoning schedules is being actively developed for such requirements, but less attention has been given to the means by which woo...
J Rak, T S McKnight


Moisture correction for ultrasonic MOE measurements above fibre saturation point in Scots pine sapwood
2006 - IRG/WP 06-20333
There is a high correlation between methods for dynamic modulus of elasticity (MOEdyn) and static modulus of elasticity (MOEstat). MOEdyn methods have been found sensitive to detect early stages of decay and may be seen as an option for non-destructive wood durability testing. As the MOEstat measurements do not change after reaching the fibre saturation point, the uncorrected MOEdyn data from ultr...
E Larnøy, G Alfredsen, H Militz


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...
C R Welzbacher, C Brischke, A O Rapp


High-energy multiple impact (HEMI)-test – Part 1: A new tool for quality control of thermally modified timber
2006 - IRG/WP 06-20346
Thermal modification processes improve durability and dimensional stability of wood, but the strength properties, especially the dynamic ones, are compromised and need to be considered with respect to industrial quality control. Results from standard dynamic strength testing, such as impact bending tests, suffer from high variability, and therefore require a high number of replicates. To overcome ...
C Brischke, A O Rapp, C R Welzbacher


Wood plastic composites from modified wood; Part 1 - Conceptual idea, mechanical and physical properties
2006 - IRG/WP 06-40338
Wood plastic composites, WPCs, are rapidly taking shares from preservative treated wood on the decking market. However, the long term performance of the WPC products in this application is uncertain. Therefore, in an attempt to increase the long term performance and durability, the substitution of the unmodified wood component with modified wood has been studied in the work presented in this paper...
P Larsson Brelid, B K Segerholm, M Westin, M E P Wålinder


Measurement of wood decay by dynamic MOE in an accelerated soil contact test
2008 - IRG/WP 08-20390
Current laboratory and field testing of preservatives involves various techniques to determine the extent of fungal attack, including visual inspection, mass loss, and static bending and compression strength measurements. The objective of this study was to compare decay measurement by conventional compression strength versus dynamic MOE, employing small wood stakes in an accelerated laboratory so...
Gan Li, D D Nicholas, T P Schultz


Evaluation of variables that influence dynamic MOE in wood decay studies
2009 - IRG/WP 09-20409
The effect of wood moisture content (MC) and outdoor exposure of southern pine lap-joint components on dynamic MOE values was investigated. The use of dynamic MOE as a method of measuring progressive biodeterioration of above ground test samples shows promise, but the accuracy of this method for evaluating test samples subjected to fluctuating environmental conditions has not been reported. The re...
D Nicholas, J Shi, T Schultz


Use of wax emulsions for upgrading of wood properties
2009 - IRG/WP 09-40451
Waxes are used for treatment of wood surfaces for several decades, predominately as surface treatments, because they did not penetrate into the wood. In order to overcome this issue, water emulsions were applied in present experiment. Five water emulsions of various concentration was used namely; two emulsions of montan wax (LGE, MW1), emulsion of polyethylene (WE1), emulsion of ethylene copolymer...
B Lesar, F Pohleven, M Humar


The effect of chemical changes on the wood-moisture relationships in thermally-modified wood
2009 - IRG/WP 09-40473
Small specimens of three wood species were thermally modified following twenty schedules in the 190-245°C temperature range for treatment times between 0.3 and 16 h. Five wood-moisture relations were subsequently determined, namely: anti-swelling efficiency (ASE), movement, hygroscopicity (adsorption and desorption), transversal swelling (radial and tangential directions), and equilibrium moistur...
M M González-Peña, M D C Hale


Sorption properties of wood impregnated with aqueous solution of boric acid and montan wax emulsion
2010 - IRG/WP 10-40492
Non-biocidal techniques for wood protection become more and more important, nowadays. One of the possible treatments is use of water repellents. In the present research influence of, one of the possible water repellent, the montan wax emulsion, on the moisturizing and the sorption characteristic of impregnated wood was investigated. To achieve a better protection against wood decay fungi, montan w...
B Lesar, M Humar


Improving our understanding of moisture and other durability-related properties of wood in building envelope performance prediction
2011 - IRG/WP 11-20468
Building science has become an increasingly important field in recent years with rapid changes in construction methods, building materials and consumer expectations. The field has also been brought to prominence by a few large-scale premature building envelope failures in a few regions across the world. Considerable effort has been put into developing hygrothermal models to simulate heat, air, vap...
Jieying Wang, P Morris


The study of fungicidal values und sorption processes of ionic liquids- potential wood preservatives on soils
2011 - IRG/WP 11-30572
In the paper, the fungicidal activity of new ionic liquids structures, N,N-dimethylalkylamines derivatives, containing a spacer built of 7 or 10 methylene groups with nitrate(V) and tetrafluoroborate anions, didecyldimethylammonium and benzalkonium nitrate(V) were presented. The research was also conducted on the sorption of cations of ammonium ionic liquids on five types of podzolic, humic alluvi...
W Przybylska, J Zabielska-Matejuk, A Stangierska, A Skrzypczak


Thermally modified timber (TMT) for decking applications – determination of relevant surface properties
2011 - IRG/WP 11-40544
In recent years thermally modified timber (TMT) entered various market segments. It is used for facades, horticultural equipment, garden furniture, and also for kitchen and bathroom cabinets. However, flooring turned out to be the most important application for TMT, either as interior parquet or as exterior decking. Besides durability and dimensional stability, which had been the initial target pr...
L Meyer, C Brischke, C R Welzbacher


Effect of an antioxidant on the efficacy of organic wood preservatives in an accelerated soil contact decay test
2012 - IRG/WP 12-30583
In comparison to inorganic wood preservatives, organic biocides in transient carriers are considerably less effective when the treated wood is exposed to soil contact. Various oils are used in some formulations with pentachlorophenol to improve the efficacy. However, use of these oils imparts unacceptable properties to products used in residential applications. Consequently, there is a need to de...
D D Nicholas, J Shi, T P Schultz, L Sites


Changes of fungicidal, mechanical and sorption properties of wood during above ground outdoor exposure
2013 - IRG/WP 13-20513
The aim of this preliminary study was to investigate differences in mechanical, fungicidal, and sorption properties of four different wood species (sweet chestnut (Castanea sativa), common beach (Fagus sylvatica), Norway spruce (Picea abies), and copper-ethanolamine (CuE) impregnated Norway spruce (Picea abies)) that were exposed in the 3rd use class (CEN, 1992) for periods between 4 and 30 months...
N Thaler, M Humar


Climatic impacts on the moisture performance of wooden decking and facades
2013 - IRG/WP 13-20518
In outdoor usage wood is exposed to a variety of influences, which reduce its durability against biological deterioration and wetting. Besides many other factors the service life of wooden facades and cladding is dominated by occurring moisture loads on the one hand and their capability to withstand moisture on the other hand. Hence, climatic factors have a direct impact on the material climate an...
T Bornemann, C Brischke, G Alfredsen


Dynamic mechanical analysis (DMA) of nano cupric oxide (CuO) modified aqueous phenol formaldehyde (PF) resin
2014 - IRG/WP 14-40654
Phenol formaldehyde (PF) resins, modified by nano CuO incorporating alkane surfactant and polyvinyl alcohol (PVA) 17-99, were analyzed by dynamic mechanical analysis (DMA). The mechanical properties of its bonded plywood including tensile strength, modulus of rupture (MOR), modulus of elasticity (MOE) and shear strength under five test conditions were evaluated. Results indicated that the incorpor...
Wei Gao, Guanben Du


Decay resistance of wood-plastic composites reinforced with extracted or delignified wood flour
2014 - IRG/WP 14-40655
The moisture and decay resistance of wood-plastic composites (WPCs) reinforced with extracted or delignified wood flour (WF) was investigated. Three different extractions were preformed: toluene/ethanol (TE), acetone/water (AW), and hot water (HW). Delignification (DL) was performed using a sodium chlorite/acetic acid solution. All WPCs specimens were made with 50% by weight HDPE and WF, first com...
R E Ibach, Yao Chen, N M Stark, M A Tshabalala, Yongming Fan, Jianmin Gao