Your search resulted in 48 documents. Displaying 25 entries per page.


Progress report on co-operative research project on L-joint testing
1983 - IRG/WP 2192
A F Bravery, D J Dickinson, M Fougerousse


Co-operative research project on L-joint testing. Sampling after 8 months exposure
1983 - IRG/WP 2208
It was anticipated in Document No IRG/WP/2192 that exposure of L-joints by the European co-operators would take place on 1 April 1983. Where L-joints were exposed at this time, sampling after 8 months exposure is due on 1 December 1983. The present document draws attention to relevant previous documents which describe the sampling methods to be adopted. It also provides Tables for recording the re...
J K Carey, A F Bravery


Co-operative research project on L-joint testing. Progress report to March 1988
1988 - IRG/WP 2315
Further sets of data received from CTFT (France), BAM (Germany) and PRL (UK) after 46-48 months exposure and STU (Sweden) after 22 months exposure are presented and discussed in conjunction with data reported previously. Colonisation and attack of the L-joints has progressed with increasing exposure period. The new data are generally in agreement with those presented previously and the major diffe...
J K Carey, A F Bravery


Climate indices at work: Above ground decay L-joint tests (EN 330 and AWPA E9) at two sites 12000 km apart and with Scheffer climate indices of 60-65 and 300-330
1996 - IRG/WP 96-20095
Matched sets of Scots pine sapwood (Pinus sylvestris) L-joints were exposed above ground at two field sites for approximately five years. One site, at Garston, Watford, UK has a climate index between 60 and 65 while the other, close to Hilo, HI, USA has an index between 300 and 330. The joints were treated with a range of organic solvent treatments applied either by three minute dip immersion or b...
A F Preston, K J Archer, D M Roberts, J K Carey, A F Bravery


Co-operative research project on L-joint testing. Progress report to May 1989
1989 - IRG/WP 2338
Further sets of data received from STU (Sweden) after 36 months exposure and Sipad-IRC (Yugoslavia) after 45 months exposure are presented and discussed in conjunction with data reported previously. The new data are generally in agreement with those presented previously and the major difference between institutes continues to be one of rate of colonisation rather than any relative difference in pe...
J K Carey, A F Bravery


Status of the Working Group on Preservation of Wood in the Marine Environment - Questionnaire results
1977 - IRG/WP 434
At the joint meeting of the IRG and COIPM dealing with preservation of wood in the marine environment, it was suggested that a Marine Group should be formally recognised within IRG. It was agreed that a questionnaire (Document No: IRG/WP/424) should be circulated to determine the views of the membership on the future status of this group. The results of this questionnaire are presented....
R A Eaton


Natural durability of European wood species for exterior use above ground
2003 - IRG/WP 03-10499
The main interest in using more timber for exterior constructions is to protect the environment, where wood is considered an environmentally friendly material. However, chemicals for wood protection are getting more and more restricted, consequently, the focus on the natural durability of wood is increased. Good, well-documented data on the durability of wood species in ground contact exist, which...
B Lindegaard, N Morsing


Co-operative research project on L-joint testing. Progress report to March 1984
1984 - IRG/WP 2211
Each participant was intended to expose L-joints in the main trial on 1 April 1983 and the first sampling, after 8 months exposure, was to be undertaken on 1 December 1983. Some participants have had to vary this schedule. Results are presented from CTFT (France) and PRL (United Kingdom). These show a greater effectiveness by the double vacuum treatments compared with the 1 minute dip treatments. ...
J K Carey, A F Bravery


L-joint trials: Part 2: The relationship between colonisation by decay fungi and long-term performance
2002 - IRG/WP 02-20251
Many of the L-joint trials conducted at BRE were assessed during the early stages to establish the rate of colonisation by fungi, principally basidiomycetes. At that time, a system of assessment incorporating colonisation studies was proposed for inclusion within the European Standard EN 330 but was rejected for the final version of the standard. The long-term trials associated with the colonisa...
J K Carey


L-joint trials: Part 3: Relative performance of a range of preservative products
2002 - IRG/WP 02-30292
Long-term trials using the L-joints described in BS EN 330 and AWPA Standard E9-97 have been in progress at BRE since 1982. This paper records the current assessments of decay of L-joints in trials started between 1982 and 1994 with treatments applied to both Scots pine sapwood (Pinus sylvestris) and spruce (Picea sp.). Data are provided on a range of active ingredients including TnBTO, PCP, a...
J K Carey


L-joint trials: Part 1: Observations on the process of colonisation and decay
2002 - IRG/WP 02-20250
The first trials using the small L-joint, later adopted for use in BS EN 330 and AWPA Standard E9-97 were exposed at BRE in 1975 but all were assessed destructively during the early stages of exposure. The longest running trial which included replicates for long-term exposure will have been exposed for 20 years in July 2002. This paper provides an overview of the results of testing during that p...
J K Carey


Above-Ground Durability Estimation in Australia. Results after 16 years exposure
2005 - IRG/WP 05-20314
A program of research was established in 1987 to examine the above-ground durability of a selection of timbers that are commercially significant in Australia. Test samples were assembled in an L-Joint design and placed on exposure racks in a format to replicate joinery that is exposed to the weather above ground. Both painted and unpainted material has been exposed. Test samples have been evaluat...
L P Francis, J Norton


Moisture content development in lap-joints of different wood species in outside exposure trials
1998 - IRG/WP 98-20143
Lap-joint trails (following European Standard EN 12037) were set up with 11 different softwood and hardwood species. Half of the number of the lap-joint specimens were coated with an alkyd coating. The moisture development has been followed during a 19 months period. In this paper, the out comes of different moisture contents evaluations are presented. The results show, that the moisture content o...
H Militz, M Broertjes, C J Bloom


Aboveground Microbial Decay Test of Biocide Treated and Untreated Wood Exposed to Danish and Humid Tropical Climates
2004 - IRG/WP 04-20306
A co-operative study was initiated to compare the aboveground field decay test of untreated and preservative-treated timbers under Nordic (Danish) and a representative humid tropical (Malaysian) environment according to CEN standard method. Matched specimens of untreated and both preservative-impregnated and surface-treated wood were simultaneously exposed at The Danish Technological Institute (DT...
A H H Wong, N Morsing, K H Henriksen, S Ujang


Interim balance after 20 months of lap-joint exposure
1999 - IRG/WP 99-20164
The application of natural resins and integrated resin systems to improve the performance of Pinus sylvestris was assessed in a lap-joint test according to DIN V ENV 12037 (1996). Lap-joints of Pinus sapwood were exposed at the test field in Hamburg (Germany) in May 1997. The treated lap-joints were assessed with regard to the performance of the resin treatments out of ground. The exposure of lap-...
M Sailer, A O Rapp, R-D Peek, A J Nurmi, E P J Beckers


Co-operative research project on L-joint testing. Sampling after 18 months exposure
1984 - IRG/WP 2233
In September 1983, Document No: IRG/WP/2208 was distributed giving guidance on sampling after 8 months exposure (due 1 December 1983 for those L-joints exposed on schedule on 1 April 1983), and including tables on which to record the test results. No major problems have been notified to Princes Risborough Laboratory concerning the sampling method. It is therefore proposed that the next sampling, a...
J K Carey, A F Bravery


Co-operative research project on L-joint testing. Progress report to March 1986
1986 - IRG/WP 2272
Further sets of data received from CTFT (France) after 18 months exposure, BAM (Germany) after 18 months exposure, STU (Sweden) after 9.5 months exposure and TI (Denmark) after 12 and 17.5 months exposure are presented and discussed in conjunction with data previously reported. The new data are generally in agreement with those presented previously and indicate the major difference between the co-...
J K Carey, A F Bravery


Co-operative research project on L-joint testing. Progress report to March 1985
1985 - IRG/WP 2236
It was originally intended that each participant would expose L-joints in the main trial on 1 April 1983 with the first sampling at 8 months (1 December 1983) and the second sampling at 18 months (1 October 1984). In the event, some participants have had to vary this schedule. Results after the first sampling have been received from CTFT (8 months), BAM (12 months) and Sipad-IRC (8 months) and aft...
J K Carey, A F Bravery


The accelerated L-joint test method for determination of the out of ground natural durability
1998 - IRG/WP 98-20146
The accelerated L-joint test incorporates a moistening device and uses a close end water trap in an open joint connection with a laminated tenon member consisting of the perishable reference wood species scots pine sapwood and beech. After one year of exposure it is possible to show a distinct identification of natural durability classes 4 and 5 against the more durable wood species. Both weight ...
J Van Acker, C Brauwers, M Stevens


Standard and accelerated testing of boron-additive wood protection systems
2005 - IRG/WP 05-30381
The main objective of this research was to determine the effectiveness of boron-additive protection systems for above ground applications by means of field testing. The two field test procedures used are based on the L-joint test described in the European standard EN 330. For the first set up the boron treated timber was coated in accordance with the standard EN 330 system. The second set up is ba...
A Mohareb, J Van Acker, M Stevens


A new concept for the evaluation of wood durability for out of ground contact using accelerated L-joint testing
1997 - IRG/WP 97-20123
Since the wood preservation sector is developing in favour of defining exactly the utilization of wood products and preservation techniques as a function of the envisaged hazard class, more in particular the hazard classes 3 and 4 (EN 350) there is obviously a need for a test method evaluating natural durability for out of ground contact applications. Based on the L-joint test as described in the ...
J Van Acker, M Stevens


Co-operative research project on L-joint testing. Sampling after 4 years exposure
1987 - IRG/WP 2274
In September 1983, Document No: IRG/WP/2208 was distributed giving guidance on sampling after 8 months exposure and including tables on which to record the test results. Similarly in September 1984, Document No: IRG/WP/2233 was distributed concerning sampling after 18 months exposure. No major problems have been notified to Princes Risborough Laboratory concerning the sampling method. It is theref...
J K Carey, A F Bravery


The status of the Working group on Preservation of Wood in the Marine Environment
1977 - IRG/WP 424
At the last joint meeting of IRG/COIPM members in May 1976 at Wildhaus, Switzerland, a proposal was made that the existing 'Marine Group' should become a formal part of IRG. At present, members of the Wood Group of the COIPM (Comite International Permanent pour la Recherche sur la Preservation des Materiaux en Milieu Marin), and members of IRG who are interested in wood preservat...
R A Eaton


A field study on the suitability of the European lap-joint test
2001 - IRG/WP 01-20239
Within the framework of the European SM&T Research Project "Co-normative research on field tests for wood preservatives out of ground contact in conjunction with methods for preconditioning test specimens prior to test" (FACT) one aim was to establish the suitability of the European lap-joint test (as it is described in ENV 12037:1996) to assess wood preservatives in the field in EHC 3. Scots ...
M Grinda, Ö Bergman, H-V Borck, D Dickinson, P Esser, R Gründlinger, H Leithoff, S Molnar, L Paajanen, N Pfabigan, E D Suttie, F Thomassin, T Nilsson, J Van Acker, M Van Der Zee, A Voss


The use of lap-joints in natural durability testing: moisture content development during 36 months outside exposure trials
2000 - IRG/WP 00-20217
Lap-joint trials (following European Standard ENV 12037) were set up with 11 different softwood and hardwood species. The main aim was to evaluate the suitability of this test standard (developed for testing wood preservative effectiveness) for natural durability testing. The moisture development has been followed during a 36 months period. In this paper, the outcomes of different moisture content...
H Militz, C J Bloom