Your search resulted in 784 documents. Displaying 25 entries per page.


Experimental test site to prevent maritime pine logs from bluestaining: water-spraying and water-immersion methods
2003 - IRG/WP 03-10497
Following a storm which led to windfall wood, a research project was launched to develop preservation methods with a low environmental impact for maritime pine logs. These preservation methods are intended to be suitable for large-scale storage areas of maritime pine. In addition the aim was to maintain wood quality during long term storage. An experimental field test with 1 900 m3 of maritime pin...
I Le Bayon, H Callot, D Reuling, C Brunet, P Castéra


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...
C R Welzbacher, C Brischke, A O Rapp


Fire Safety of Wood Floor Assembly: Model and Full-scale Test
2007 - IRG/WP 07-20375
The present paper describes the model for the prediction of fire safety of wood floor assemblies. The model includes heat transfer model for the calculation of the flow of heat in floor assembly and structural model for the analysis of the mechanical performance of wood joists. The floor assemblies considered in this paper are constructed with nominal 2x10 (38x241mm) wood joists lined by Type X ...
H Takeda


Evaluation and identification of extractives from Iranian walnut (Juglans regia L.) by GC/MS technique for protection of non-decay resistant species
2008 - IRG/WP 08-10670
The use of walnut extractives is interest as environment friendly wood preservatives in the wood preservation industry. In this study, organic solvents were used to remove extractives from Iranian walnut heartwood samples. The solvent was removed by rotoevaporation, and Identification of chemical compounds in the Walnut extractives was done by using GC/MS technique. The toxicity of various extract...
S K H Hashemi, D Parsapajouh, H Khademi Eslam


Mechanical strength of wood from the Vasa shipwreck
2008 - IRG/WP 08-20381
Samples from three ancient ship wrecks (Vasa, Elefanten, and Gröne Jägaren) and recent oak samples as reference were examined with regard to mechanical strength using the high-energy multiple impact (HEMI) - test method, which delivers the resistance to impact milling (RIM) of a material. Adoption and optimisation of the test method for the particular sample size of the wooden drilling cores was...
A O Rapp, C Brischke, C R Welzbacher, T Nilsson, C Björdal


Changes in mechanical and chemical properties of wood exposed outdoors
2014 - IRG/WP 14-20550
The aim of this study was to investigate differences in certain mechanical and chemical properties of three different wood species (common beach (Fagus sylvatica), Norway spruce (Picea abies), and copper-ethanolamine (CuE) impregnated Norway spruce (Picea abies)) that were exposed in use class 3 (CEN, 2006) for periods between 4 and 30 months. The results show, that changes in the investigated me...
N Thaler, C Brischke, D Žlindra, V Vek, M Humar


Using Commercial Water Repellent Chemicals on Wood Protection
2014 - IRG/WP 14-30656
Lately, researchers have been looking for process and products that use environmental friendly technologies in wood protection. These sorts of innovations on wood protection should be carried out for wood evaluated at outdoor conditions. Using water repelling chemicals is one of those innovations which improve wood durability and dimensional stability by decreasing content of moisture. In this ...
G Köse, A Temiz, S Demirel, O E Özkan


The effect of preservative treatment on mechanical strength and structural integrity of wood
2015 - IRG/WP 15-30667
The use of wood for demanding construction applications is increasing in Europe. Wooden constructions are frequently designed of susceptible conifer wood, which is endangered by wood decay fungi in wet applications. Therefore in many cases treating wood with preservatives is unavoidable to ensure the desired service life. However, chemical treatment of wood can result in changes of its mechanical ...
M Humar, D Kržišnik, C Brischke


Some comments on durability testing of WPC according to EN 15534-1
2015 - IRG/WP 15-40695
The standard EN 15534-1 (2014) gives advice for broad characterization of WPC materials and products. It contains instructions for test procedures concerning different properties e.g. mechanical properties, thermal properties, as well as durability. In this paper some WPC materials from the market were tested for their resistance against brown rot. Furthermore, the water uptake and bending prope...
S Bollmus, A Gellerich, H Militz


Estimation of wood degradation determined by visual inspection, mechanical testing and DNA characterisation – report after 3 years of exposure
2016 - IRG/WP 16-30700
The influence of two separate treatments, thermal modification and alkaline copper quaternary (ACQ, Silvanolin©) treatment, on fungal decay, visual disfigurement, deterioration in mechanical properties and fungal community structure was assessed on Norway spruce (Picea abies) and compared with the performance of two naturally more resistant tree species native to North America: Douglas fir (Pseud...
N Thaler, T Martinović, M Bajc, D Finžgar, H Kraigher, A Sinha, J J Morrell, M Humar


Impact of fungal decay on the bending properties of wood
2020 - IRG/WP 20-20671
Wood used outdoors is generally prone to fungal degradation, and its impact on the structural integrity of wood is an immanent factor for service life planning with timber. Wood decayed to very small mass losses can suffer from a significant reduction in mechanical strength and elastic properties. Hence, the latter are preferred indicators to detect decay in wood durability studies. Numerous previ...
S Bollmus, P B van Niekerk, C Brischke


Mechanical and biological durability properties against soft-rot and subterranean termite in the field (grave-yard test) of beech wood impregnated with different derivatives of glycerol or polyglycerol and maleic anhydride followed by thermal modification in an opened or in a closed system
2021 - IRG/WP 21-40917
This paper presents mechanical and biological durability properties in soil beg test (soft-rot test) and field test (grave-yard test) against subterranean termite of the wood modified with an aqueous vinylic derivative of glycerol/polyglycerol or maleic anhydride cured in an opened or in a closed system. Wood modification was performed through impregnation of European beech (Fagus sylvatica) with ...
M Mubarok, H Militz, S Dumarcay, I W Darmawan, Y S Hadi, P Gerardin


Programme section 2, Test methodology and assessment
1997 - IRG/WP 97-20126
IRG Secretariat


Progress report on co-operative research project on L-joint testing
1983 - IRG/WP 2192
A F Bravery, D J Dickinson, M Fougerousse


A comparison of soft rot, white rot and brown rot in CCA, CCP, CCF, CCB, TCMTB and benzalkonium chloride treated Pinus radiata IUFRO stakes, after 9-15 years exposure at five test sites in New Zealand
1991 - IRG/WP 1485
The aim of this study was to determine if decay type varies significantly between five field trial test sites of different soil type, aspect and climate in 9-15 year old, replicate CCA, CCF, CCP. CCB, TCMTB and AAC treated IUFRO stakes. A visual on-site assessment of decay type on every test stake was made and observations confirmed by microscopical examination. Regression analyses were used to de...
R N Wakeling


Wood preservatives: Field tests out of ground contact. Brief survey of principles and methodology
1976 - IRG/WP 269
This paper contains the following spots: 1.: The general need for field tests. 2.: Interests and limits of field tests in ground contact. 3.: Various methods in use for out-of-ground contact field tests. 4.: Fungal cellar tests are they an alternative to above-ground decay exposure tests? 5.: Conclusions....
M Fougerousse


Collaborative soft rot tests. Names and addresses of collaborators
1973 - IRG/WP 231
IRG Secretariat


A suggested method to test the toxicity of wood preservatives towards the house longhorn beetle
1977 - IRG/WP 275
This method was developed in the Institute for Wood Technology in Sarajevo, Yugoslavia and is used to get quick information on the toxicity of wood preservatives against house longhorn beetle (Hylotrupes bajulus). The method can be used for superficially treated or deeply impregnated wood blocks, and by using small or normal size test material it can be used as a laboratory or field test, and also...
N Vidovic


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 2: Report of treatment and installation in Australia
1978 - IRG/WP 440
The purpose of this test and the procedures to be followed have been fully set out in documents distributed by the International Research Group on Wood Preservation and numbered IRG/WP/414 and IRG/WP/420. The prescriptions set out in these two documents have been closely followed....
J Beesley


Field test evaluation of preservatives and treatment methods for fence posts
1985 - IRG/WP 3347
This work presents the field test results after fifteen years exposure of Eucalyptus saligna fence posts treated with six different preservatives and five treatment methods. All the combinations with oil-borne preservatives presented the best results and among the waterborne preservatives, the fence posts treated by immersion method were with the lowest performance in the field test....
G A C Lopez, E S Lepage


A rapid field bioassay technique with subterranean termites
1983 - IRG/WP 1188
Details are summarised of a field procedure which is designed to ensure continuous exposure to a replenishing termite biomass. After pre-baiting to determine the presence and identification of a termite hazard, test specimens (35 x 35 x 250 mm³) are installed vertically in the ground adjacent to and in contact with bait specimens of the same dimensions and interconnected by susceptible feeder str...
C D Howick, J W Creffield


Utilization of curcumin for detection of presence of boron in wood
1982 - IRG/WP 3191
It has been shown that curcumin is not a reliable reagent for detecting boron in wood that has been attacked by fungi...
M-L Edlund


Performance of treated fence posts after 6 years in five test plots in the State of Sao Paulo - Brazil
1976 - IRG/WP 376
Fence posts treated with creosote, pentachlorophenol and creosote/ pentachlorophenol mixtures showed good performance after 6 years of exposure in five test plots located in the State of Sao Paulo - Brazil. Good results were also achieved with copper sulphate/sodium arsenate and copper sulphate/potassium dichromate mixtures. Fungi and termites were the main destroying agents found attacking the po...
M S Cavalcante


How to Document the Performance of Super-Critical Treated Wood in above Ground Situations?
2005 - IRG/WP 05-20316
The paper presents practical experiences from the preparation of a new preservative treated wood product for introduction to the market. The product in question is Superwood™, which is treated with organic biocides using CO2 in a supercritical state as a solvent. The question is how to evaluate the performance of a new product such as Superwood™ in order to get an acceptance on the market a...
N Morsing, A H H Wong, F Imsgard, O Henriksen


Influence of different fixation and ageing procedures on the leaching behaviour of copper from selected wood preservatives in laboratory trials
2003 - IRG/WP 03-20264
The paper focuses on the role of different parameters, such as fixation, sample size, wood species, and leaching in internationally standardized ageing procedures for wood preservatives from Europe, Japan and the United States. The leaching protocols used were EN 84, JIS K 1571 and AWPA E11 protocols. The wood species were Scots pine, Sugi and Southern Yellow Pine respectively. Three types of com...