IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 300 documents. Displaying 25 entries per page.


Determination of the water sorption properties and preliminary results from field tests above ground of thermally modified material from industrial scale processes
2004 - IRG/WP 04-40279
In this study the differences in moisture behavior and durability above ground of heat treated wood originating from different European industrial heat treatment plants by means of the water sorption properties as well as field tests were examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood (Premium wood)/ Finland and Menz Holz/ Germany, where Oil-...
C R Welzbacher; A O Rapp


Wood plastic composites from modified wood; Part 1 - Conceptual idea, mechanical and physical properties
2006 - IRG/WP 06-40338
Wood plastic composites, WPCs, are rapidly taking shares from preservative treated wood on the decking market. However, the long term performance of the WPC products in this application is uncertain. Therefore, in an attempt to increase the long term performance and durability, the substitution of the unmodified wood component with modified wood has been studied in the work presented in this paper...
P Larsson Brelid, B K Segerholm, M Westin, M E P Wålinder


Moisture adsorption isotherms of wood studies using a dynamic vapour sorption apparatus
2009 - IRG/WP 09-20398
Five types of wood including two Malaysian hardwoods acacia mangium (Acacia mangium) and sesenduk (Endospermum malaccense), two temperate softwoods, Sitka spruce (Picea sitchensis), radiata pine (Pinus radiata) and Accoya (commercially modified wood) were studied to determine their moisture sorption behaviour using a Dynamic Vapour Sorption (DVS) apparatus. The isotherm plot for each species teste...
J Zaihan, C A S Hill, S Curling


The effect of chemical changes on the wood-moisture relationships in thermally-modified wood
2009 - IRG/WP 09-40473
Small specimens of three wood species were thermally modified following twenty schedules in the 190-245°C temperature range for treatment times between 0.3 and 16 h. Five wood-moisture relations were subsequently determined, namely: anti-swelling efficiency (ASE), movement, hygroscopicity (adsorption and desorption), transversal swelling (radial and tangential directions), and equilibrium moistur...
M M González-Peña, M D C Hale


Sorption properties of wood impregnated with aqueous solution of boric acid and montan wax emulsion
2010 - IRG/WP 10-40492
Non-biocidal techniques for wood protection become more and more important, nowadays. One of the possible treatments is use of water repellents. In the present research influence of, one of the possible water repellent, the montan wax emulsion, on the moisturizing and the sorption characteristic of impregnated wood was investigated. To achieve a better protection against wood decay fungi, montan w...
B Lesar, M Humar


Improving our understanding of moisture and other durability-related properties of wood in building envelope performance prediction
2011 - IRG/WP 11-20468
Building science has become an increasingly important field in recent years with rapid changes in construction methods, building materials and consumer expectations. The field has also been brought to prominence by a few large-scale premature building envelope failures in a few regions across the world. Considerable effort has been put into developing hygrothermal models to simulate heat, air, vap...
Jieying Wang, P Morris


Climatic impacts on the moisture performance of wooden decking and facades
2013 - IRG/WP 13-20518
In outdoor usage wood is exposed to a variety of influences, which reduce its durability against biological deterioration and wetting. Besides many other factors the service life of wooden facades and cladding is dominated by occurring moisture loads on the one hand and their capability to withstand moisture on the other hand. Hence, climatic factors have a direct impact on the material climate an...
T Bornemann, C Brischke, G Alfredsen


The sorption behaviour of wood
2017 - IRG/WP 17-20605
The use of dynamic vapour sorption to determine the sorption properties of wood has become an increasingly popular technique. The method has many advantages when compared with many other gravimetric methods. However, it is necessary to set an equilibrium condition in order to obtain data for an isotherm in a reasonable amount of time. An important recent finding has been that multiple sorption cyc...
C Hill


Studying amount, location and state of water in modified wood at moisture levels relevant for fungal degradation
2020 - IRG/WP 20-40889
Water is an essential parameter for fungal degradation of wood, but degradation primarily occurs at high moisture levels at water potential in the range of -4 to -0.1 MPa, which corresponds to 97-99.9% relative humidity. At these moisture levels, water is present in the wood structure both in and outside of cell walls. The majority of previous studies on the interaction between wood and water for ...
M Fredriksson, E Engelund Thybring, Ramunas Digaitis


Significance of the thermal design and the sorption isotherm shape in hygroscopic wood moisture dynamics and service life
2022 - IRG/WP 22-20682
Moisture dynamics are considered important for predicting the service performance of wood in exterior applications. Above a critical moisture content, water acts a softener on the structural polymer matrix of the wood cell wall, enabling the necessary diffusion of molecular species involved in the fungal degradation mechanism of wood. Water may enter solid wood in either liquid form or in vapor fo...
W Willems


Moisture sorption behaviour of poplar and thermally modified poplar using dynamic vapour sorption (DVS)
2022 - IRG/WP 22-40947
The moisture sorption behaviour of wood has a critical impact on service life. In Europe, softwood is mostly used to manufacture engineered wood products such as cross-laminated timber (CLT) or glue-laminated timber (GLT or glulam). Yet fast-growing and widespread tree species such as hybrid poplar with or without modification, have potential to meet the increasing demand. This study shows the moi...
X Jiang, J Van den Bulcke, L De Boever, M Minsart, A Mignon, J Van Acker


Moisture content levels and decay of hemlock
1986 - IRG/WP 1287
As a model of decay conditions of wooden members in wooden houses, a decay test was set up in which samples of western hemlock (Tsuga heterophylla) under 4 moisture levels were examined. Each week the samples were weighed and if the weights indicated that their moisture contents were lower than the expected levels, distilled water was added. Every 8 weeks 3 samples from each condition were oven dr...
K Suzuki


Developments in the protection of wood and wood-based products
1980 - IRG/WP 340
Technology is playing an increasingly important role in the field of wood protection. This current review highlights how modern techniques have provided greater insight into the biological and physical processes affecting the durability of wood and wood-based products. Emphasis is also given to developments in preservative testing methodology and to the encouraging changes towards both the correct...
J M Baker


New technique to analyze impregnation processes
1988 - IRG/WP 2304
Equipment has been developed to measure liquid flow in wood during impregnation processes. Basic principles of flow measurements using directly heated negative temperature coefficient thermistors, and some characteristics of the hardware developed are presented in this paper....
J P Hösli


Influence of moisture content of rubber wood on the growth of Botryodiplodia theobromae
1993 - IRG/WP 93-10029
Botryodiplodia theobromae is the main fungus causing sapstain on rubber wood (Hevea brasiliensis). The entry and establishment of the stain fungus is nighly influenced by the moisture content of the wood. To determine the optimum moisture content of wood required for maximum growth of Botryodiplodia theobromae wood blocks at different moisture contents were inoculated with the test fungus and incu...
E J M Florence, R Gnanaharan, J K Sharma


Soil virulence tests using Scots pine sapwood
1973 - IRG/WP 222
Following the tests reported in Document No: IRG/WP/210, in which soils from different laboratories were investigated for virulence, supplementary tests have been carried out using Scots pine sapwood and an extended incubation period....
J K Carey, J G Savory


Co-operative research project on L-joint testing. Sampling after 8 months exposure
1983 - IRG/WP 2208
It was anticipated in Document No IRG/WP/2192 that exposure of L-joints by the European co-operators would take place on 1 April 1983. Where L-joints were exposed at this time, sampling after 8 months exposure is due on 1 December 1983. The present document draws attention to relevant previous documents which describe the sampling methods to be adopted. It also provides Tables for recording the re...
J K Carey, A F Bravery


Comparison of the agar-block and soil-block methods used for evaluation of fungitoxic value of QAC and CCA wood preservatives
1994 - IRG/WP 94-20039
The modyfied agar-block and soil-block methods were used for comparing the fungitoxic value of QAC and CCA type preservatives against Coniophora puteana and Coniophora olivacea The mass loss and moisture contents of wood were analysed....
J Wazny, L J Cookson


Collaborative soft rot tests: Programme and test method
1973 - IRG/WP 229
J G Savory, J K Carey


Collaborative soft rot tests: Interim report on PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1972 - IRG/WP 211
Preservative: Tanalith CT.106 - Results obtained with beech are given in the table and indicate a toxic limit of 16.7-19.2 kg/m³ - The initial soil moisture content was adjusted to 27.8% (the water holding capacity). Noticeable drying out has occurred in some of the test bottles....
J G Savory


A standardised procedure for the treatment of timber with test chemicals
1986 - IRG/WP 2257
A procedure is described which allows the standardisation of sample handling and data manipulation during trials invastigating the treatability of timber with test chemicals. The use of computer software allows the data to be handled efficiently....
J Norton, A Zosars, L E Leightley


Observations on the failure of anti-sapstain treated timber under non-drying conditions
1990 - IRG/WP 1437
A range of bacteria and yeasts were isolated from antisapstain treated timber and fresh sawdust. Solution samples containing 100 ppm of TCMTB in a nutrient medium were inoculated with these organisms and incubated at 25°C for 5 days. The levels of TCMTB remaining in solution were determined by HPLC analysis after this time. Results indicated high losses of active ingredient for a range of organis...
G R Williams


Co-operative research project on L-joint testing. Progress report to March 1988
1988 - IRG/WP 2315
Further sets of data received from CTFT (France), BAM (Germany) and PRL (UK) after 46-48 months exposure and STU (Sweden) after 22 months exposure are presented and discussed in conjunction with data reported previously. Colonisation and attack of the L-joints has progressed with increasing exposure period. The new data are generally in agreement with those presented previously and the major diffe...
J K Carey, A F Bravery


Diffusion of fused borate rods in top ends of poles
1989 - IRG/WP 3518
Diffusion tests of fused borate rods were carried out on extremities of sapwood poles in service. Rods were set in drills under the cone with or without addition of liquid Boracol 40. After one year of weathering, a good diffusion in the slice under the cone and even below the slice and in the cone itself was observed in Scots pine and spruce poles. The rods were still intacts and constitute, in f...
D Dirol, J P Guder


Analysing the characteristic role of moisture content for drying and fluid flow in Sitka spruce. - Part 1: The drying process of sapwood and heartwood of two different thickness of Sitka spruce using a kiln. - Part 2: Effects of moisture content on longitudinal permeability of Sitka spruce in vertical variation of the tree
2000 - IRG/WP 00-40173
The characteristic role of the moisture content in Sitka spruce (Picea sitchensis (Bong.) Carr.) that grown in the United Kingdom was examined by this study on the basis of (1) the reduction of moisture content in two different thickness of sapwood and heartwood by kiln drying process, and (2) the effects of moisture content to the longitudinal void volume filled of tanalith-C by the full-cell pro...
I Usta


Next Page