Natural durability of some common Indian timbers and marine plywood against biodeterioration in Kochi waters (India)
1992 - IRG/WP 92-4177
Panels of thirty-eight timber species and marine plywood were tested in Kochi harbour (South-west India) for periods ranging from 3 to 21 months, so as to evaluate their natural resistance against marine borers. Results indicate that all the timber species studied are non-durable, 6 of them having undergone more than 50% internal destruction within 3 months; 14 species in 6 months, 13 species and ...
L N Santhakumaran, M V Rao


Biodegradation of acetylated southern pine and aspen composition boards
1994 - IRG/WP 94-40020
This objective of this study was to investigate the influence of the acetylation treated wood fiber, Phenol-formaldehyde resin content level, two wood fiber species, three fungi species on the dimensional stability and decay resistence of high density composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species...
P Chow, T Harp, R Meimban, J A Youngquist, R M Powell


Bending properties of treated western hemlock plywood
1996 - IRG/WP 96-40064
This study investigated the mechanical properties of western hemlock plywood after treatment with waterborne preservatives and redrying. Unlike previously reported results for southern pine plywood, western hemlock plywood was more sensitive to redrying temperature than to preservative treatment. Generally, western hemlock plywood was affected by temperature and other variables. Losses in mechanic...
H M Barnes, A Khouadja, D E Lyon


A Soil Bed Test of the Effect of CCA Penetration on the Performance of Hem-fir Plywood
2004 - IRG/WP 04-30332
An accelerated decay test was set up to compare the performance of CCA-treated Western hemlock/amabilis fir plywood treated to meet the preserved wood foundation (PWF) retention standard with various patterns of preservative penetration. Short lengths of treated plywood and comparable untreated material were installed in a soil bed. After eleven years of exposure, the CCA treatments were all sou...
P I Morris, J K Ingram


The evaluation of the occurrence of soft rot in creosoted wooden poles
1988 - IRG/WP 1368
The occurrence of soft rot decay in creosoted wooden poles for overhead power lines was investigated by collection of field samples, their subsequent microscopic examination and statistical analysis of the data collected. Examination of samples collected from 296 poles revealed that approximately 15% of the pole population studied (Eastern Electricity Board) showed the presence of soft rot decay. ...
A Wylde, D J Dickinson


Bending creep test of plywoods under long term exposure to fungal attack
1981 - IRG/WP 2163
Bending creep test and decay test were coupled in order to evaluate the durability of structural plywoods and preservative efficacy. Experimental blocks, 5.0 x 1.2 cm² section x 35.0 cm length, were impregnated with distilled water and inoculated with mycelial fragments of test fungus. Polyethylene bags stretched with metal frame were used as decay chambers. The chambers containing inoculated blo...
M Takahashi


Health and safety aspects of the use of wood preservatives in Sweden
1977 - IRG/WP 396
The Act on products Hazardous to Health and to the Environment (Swedish Code of Statutes SFS 1973:329) came into force on 1st July 1973. The Act cancelled and superseded the Poison Act, the Pesticides Act and the PCB Act from 1962, 1962 and 1971 respectively. Regulations for the implementation of the Act are contained in the Ordinance on Products Hazardous to Health and to the Environment (SFS 197...
B Henningsson


Treatment of wood-based panel products with volatile borate
1990 - IRG/WP 3616
The paper presents recent developments in the use of volatile borate esters for the preservative treatment of wood based board materials. Several advances on previous reports are discussed. In laboratory studies, treatment times of approximately ten minutes at 20°C on boards at equilibrium moisture content provided full penetration and retentions of 1% wt/wt boric acid. Biological tests have been...
P Turner, R J Murphy, D J Dickinson


Durability of plywood made from soft- and hardwoods assessed according to ENV 12038 after artificial and natural ageing
2000 - IRG/WP 00-20191
Plywood was prepared from Norway Spruce and pure heartwood of Douglas Fir, Scots Pine, European Oak, False Acacia and Macoré using a phenol-formaldehyde glue. The panels of 38 mm in thickness were pre-conditioned according to the following procedures: a) 12 weeks storage at 20°C/65% rh, b) 2 weeks artificial weathering (with rain and UV-radiation at changing temperatures), and c) a natural weath...
H Leithoff, R-D Peek


Serviceability modeling-Predicting and extending the useful service life of FRT-plywood roof sheathing
2000 - IRG/WP 00-20210
One of the most, if not the most, efficient methods of extending our existing forest resource is to prolong the service life of wood currently in-service by using those existing structures to meet our future needs (Hamilton and Winandy 1998). It is currently estimated that over 7 x 109 m3 (3 trillion bd. ft) of wood is currently in service within the United States of America (PATH 1999). Research ...
J E Winandy


Worldwide in-ground stake test of acetylated composite boards
1997 - IRG/WP 97-40088
Acetylated wood composite stakes are being tested in ground contact (graveyard test) in seven fields around the world. Three types of acetylated wood composites were prepared: spruce fiberboard in Sweden, aspen fiberboard in Madison and rubber wood particle board in Indonesia. Two levels of acetylation were used, a high level of ~20% acetyl content and a low level of 10% acetyl content. Control bo...
R M Rowell, B S Dawson, Y S Hadi, D D Nicholas, T Nilsson, D V Plackett, R Simonson, M Westin


The foreign exchange situation and fate of wood preservation in Nigeria
1989 - IRG/WP 3558
Up to about 15 years ago, wood utilization industry in Nigeria gave no serious thoughts to wood preservation. After this period however, as a result of escalated local demand for sawn timber, logs with wider sapwood and mainly of secondary tree species requiring protection of the sawn timber became dominant in the local timber scene. Preservatives both for protection in and out of ground contacts ...
M A Odeyinde, S C Ifebueme


Effect of alkaline phenolic resin adhesive on the stability of preservatives incorporated into the glue-line of plywood
1991 - IRG/WP 3650
Stability of preservatives was determined by gaschromatographic analysis when they were applied to glue-line treatment of plywoods. Among organophosphorous insecticides, emulsified forms of chlorpyrifos, dichlofention and diazinon were more stable than others. Fenitrothion, pyridafenthion and phoxim were not practically acceptable as emulsifieable forms due to the relatively low recovery rates aft...
S Fushiki, Y Katuzawa


Evaluation of the european standard ENV 12038 for durability testing of plywood
2001 - IRG/WP 01-20237
The latest improved version of the standard ENV 12038 drafted as document N44 by CEN Technical Committee 38 (WG 7 - WG 23) is used to evaluate the effect of wood composition and structure on plywood durability. The method described is based on the agar-block test of the EN 113 standard used for the determination of the efficacy of wood preservatives and the assessment of the natural durability of ...
J Van Acker, M Stevens, E De Clercq


Treatment of poplar plywood with solvent and water-borne preservatives
1989 - IRG/WP 3538
Poplar as a light hardwood is appropriate for plywood production. Owing to its low natural durability it is generally recommended to preserve it in all conditions where risks of fungal attack may be present. A research project has been carried out on preservative treatments of plywood commodities. Parameters studied were various treatment cycles, three types of plywood, and a number of solvent and...
J Van Acker, M Stevens


Effect of vapour boron treatment on mechanical properties of wood based board materials
1992 - IRG/WP 92-3727
The mechanical properties of Medium density fibre board, Chipboard and Oriented strand board were investigated after treatment to two retention levels of boric acid applied as a vapour phase system. A range of mechanical properties were investigated. The vapour boron treatment does not have any significant effect on most of the mechanical properties of the boards. The exception is a reduction in i...
R Hashim, D J Dickinson, R J Murphy, J Dinwoodie


Test methods for wood preservatives against Lyctus: (1) Testing of treated veneer. (2) Testing of glue-line treated plywood. (Laboratory methods)
1977 - IRG/WP 293
Powder-post beetles destroy large quantities of veneer and plywood. Two test procedures are described which can be used to support application-oriented research into veneer and plywood preservatives. These procedures simulate practical conditions on a laboratory scale. Their characteristic feature is that wood species of special susceptibility are used for the tests; the susceptibility of the spec...
S Cymorek


The effect of alternative pre-conditioning procedures on the durability of wood based board materials to decay fungi
1997 - IRG/WP 97-20105
In the biological testing of wood based board materials it has been shown that exposure of boards in a closed vessel system may lead to inaccurate results due to the build up of volatile substances that inhibit the test fungi. It is thought that this is a transitory effect of freshly manufactured boards. In the European standard for testing fungal durability of board materials which is currently u...
S F Curling, R J Murphy, J K Carey


An attempt to grow dry rot fungus Serpula lacrymans on mortar substrate in non-sterile conditions
1989 - IRG/WP 1385
According to many experts, Serpula lacrymans is probably the most dangerous wood destroying fungus in houses. Investigations of KOCH, A.P. (2) showed that incidence of this fungus in percent was around 20% when the frequency of some other standard fungi was far below (Coriolus versicolor: 0.2% for example). The work presented here is a part of a program carried out at CTFT for assessing the resist...
L N Trong


Preservation of wood-based panels against fungi and insects and and testing its efficiency
1976 - IRG/WP 270
Wood-based panel products which are made of susceptible wood species may be destroyed by fungi under wet conditions and by termites. The glues do not provide sufficient protection unless very high concentrations are applied. Particle boards and fibre boards are not susceptible to beetle infestation, although some species may attack plywood. Various types of preservatives provide sufficient protect...
G Becker, M Gersonde


Serial techniques for producing fire-retardant wood products
1997 - IRG/WP 97-30127
A series of techniques including fire-retarders denoted by WFR-1, WFR-2. WFR and their applications in producing fire-retardant wood (WFR wood), fire-retardant plywood (WFR plywood), fire-retardant particleboard (WFR particleboard) and fire-retardant MDF (WFR MDF) were investigated The fire retarders were low toxic, decay resistant and less leachable. The treated wood and WFR panels were of excell...
Zhu Jia Qi, Liu Yan Ji, Gao Chao Ying


Comparison of two laboratory methods for screening potential anti-sapstain chemicals
1993 - IRG/WP 93-10036
Two methods were used to screen a number of potential anti-sapstain chemicals in the laboratory. In one method miniature boards of freshly felled Scots pine sapwood were dip treated with the candidate chemical, sprayed with a suspension of stainers or moulds and incubated for five weeks. In the other method antibiotic assay discs were treated with precise quantities of chemical, plated out on malt...
S M Gray, D J Dickinson


Fire retardant treated wood and plywood: A comparative study Part III. Combustion properties of treated wood and plywood
2002 - IRG/WP 02-40236
The fire retardant treated and untreated plywood and alder wood samples were prepared with the aim to investigate the effects of the way of treatment on the combustion properties. Alder wood was used for the preparation of plywood. Boric acid and borax were used as fire retardant. The plywood samples were impregnated by using three different methods; first group samples were impregnated by soaki...
S Çolak, A Temiz, Ü C Yildiz, G Çolakoglu


Effect of species composition of preservative-treated Douglas fir plywood on its decay resistance
1978 - IRG/WP 2114
Plywood is now commonly used for constructional purposes in environmental situations where decay by wood-destroying fungi can be a considerable risk. However there seems to be a lack of understanding of the relative durability of plywood, both untreated and when treated with wood preservatives. Part of the reason for this situation has been the difficulty of carrying out laboratory decay tests on ...
R S Smith, P Balcaen


The efficacy of preservatives into the glue-line of plywood
1993 - IRG/WP 93-30002
This research is anti-termite/decay preservatives mixed with resin to produce the plywood. Thereafter, anti-decay/termite plywood were produced by the ordinary methods. To produce suitable plywood in the utilization and certified performance, the preservatives should be 0.3 to 0.4 kg/m³ of Chlorpyrifos; 0.88 and 1.10 kg/m³ of mix preservatives of Chlorpyrifos + IF-1000. Laboratories decay test (...
S Fushiki, T Saito, Y Katuzawa, Y Imamura, S Yusuf, B Subiyanto