Laboratory evaluation of borate formulations as wood preservatves to control the subterranean termite coptotermes acinaciformis (isoptera: Rhinotermitidae) in Australia
2001 - IRG/WP 01-30266
The termiticidal efficacy of Borocol (sodium octaborate tetrahydrate), boric acid, bore-ester-7 and tri- methyl borate was evaluated in laboratory bioassays against Coptotermes acinaciformis (Froggatt). Seasoned sapwood blocks of Pinus radiata D. Don, and Eucalyptus regnans (F. Muell) were impregnated with the various borate compounds. There were marked differences in mass loss and mortality rate ...
B M Ahmed, J R J French, P Vinden


A collaborative test to determine the efficacy of polyurethane coatings on wood samples in the marine environment. 2nd Interim Report
1990 - IRG/WP 4161
The results of a collaborative international test to evaluate the performance of elastomeric polyurethane coatings of wooden test samples exposed in seawater at 13 sites around the world are reported. The samples have been exposed at sites with known infestations by molluscan and/or crustacean wood borers. Performance data for up to 4 years exposure at some sites is presented providing information...
R A Eaton


Fixation and leaching of selected Malaysian tropical hardwood after treated with CCA
2001 - IRG/WP 01-40207
The objective of this study is to investigate the fixation and leaching properties of selected Malaysian tropical hardwood (sentang wood (sapwood and heartwood) and rubberwood) after being treated with copper chrome arsenate (CCA) type-C preservative. The samples were treated with retention level of 0.5%, 2.0% and 5.0%. The samples were leached and the leachate were analyzed by AAS and the amount ...
R Hashim, O Sulaiman, Tan Siew Ching, K Yamamoto


Evidence for wood cell wall degradation by the blue stain fungus Botryodiplodia theobromae Pat
1994 - IRG/WP 94-10077
Botryodiplodia theobromae Pat., a world wide ubiquitous polyfagus sapstain fungus, was found able to destroy the cell walls of birch fibres (Betula verrucosa Ehrh.) but not Caribbean (Pinus caribaea var. hondurensis Barr. and Golf.) and Scots pine (Pinus sylvestris L.) tracheids. The fungus caused characteristic erosion of fibre cell walls similar to soft rot type 2; destruction of the S1 - S2 int...
O Encinas, G F Daniel


Low-toxicity DNBP wood preservatives
1987 - IRG/WP 3408
Low and very low toxicity single compound preservatives of both excellent insecticidal and fungicidal activity for interior, extrior and ground-contact applications are presented. These are ester derivatives of alkyl dinitrophenols, in particular of 2-sec-butyl-4,6-dinitrophenol (DNBP) and 2-sec-octyl-4,6-dinitrophenol. These esters, of much lower toxicity than DNBP impart to the treated timber co...
A Pizzi, W E Conradie, A Jansen, R Vosloo


Co-operative work on the performance of treated timber in ground contact
1975 - IRG/WP 344
At the 6th meeting of The International Research Group on Wood Preservation in Vienna, it was decided to approach all interested parties in order to: collate available information, set up collaborative work and to stimulate research on the performance of treated timber, especially hardwoods, in ground contact. In recent years, considerable concern has been expressed about the performance of preser...
D J Dickinson, J F Levy


Some data on the activity of alternative fungicides for wood preservation
1985 - IRG/WP 3333
Data from laboratory tests against basidiomycete fungi are presented for 9 alternative fungicides in organic solvent formulations and also in water for one product. Results are compared with data for reference preservatives, tributyltin oxide, copper and zinc naphthenates and pentachlorophenol. Of special interest is the apparently better than additive effect of mixing tributyltin naphthenate and ...
A F Bravery, J K Carey


An inclination incising technique for the preservative treatment of refractory timbers
1991 - IRG/WP 3664
An inclination incising technique for preservative treatment of refractory timbers was examined by changing cutting angle to the longitudinal direction of test specimen and by using different types of knife edge. Incised wood were impregnated locally into incisions with CCA solution by the specified local pressure process. Width and length of penetration areas of CCA solution were measured on long...
Y Nakamura, K Nishimoto


A comparison of inductively coupled plasma spectroscopy and neutron activity analysis for the determination of concentrations in wood
1993 - IRG/WP 93-10048
As wood decays the ionic composition changes, with increases often being seen in the concentrations of Ca, Mg, Fe, Mn and sometimes K. The concentration of eight cations in red spruce sapwood and heartwood samples was determined independently by inductively coupled plasma spectroscopy (ICP) and by neutron activation analysis (NAA) as part of an effort to standardize our analytical procedures and c...
J Jellison, J Connolly, K C Smith, W T Shortle


Volatile losses of wood preservatives
1973 - IRG/WP 236
The purpose of the work we have undertaken so far has been to try to quantify the volatile losses which occur in treated timber, and to examine some of the factors which influence these losses. The preservative compound chosen for the initial part of the programme was the contact insecticide g-BHC. This was attractive for several reasons, not the least of which was that specific and sensitive anal...
J W W Morgan, D F Purslow


Performance of non-incised CCA-treated hem-fir decking
1993 - IRG/WP 93-40004
The question of what preservative penetration will provide an acceptable service life for treated wood in residential above-ground applications is topical in North American standards committees. Non-incised CCA-treated nominal 2 x 4 inch² hem-fir decking with penetrations close to the proposed CSA O80 2 decking standard of 80% over 5 mm, has remained without decay after 10 years exposure in south...
P I Morris, J N R Ruddick


Tanalith T - a new preservative system for protecting house frames in Australia from termite attack.
2003 - IRG/WP 03-30306
The sawn timber industry in Australia has expressed a desire for a new low cost termite treatment. The treatment needs to be on-line in the dry mill, minimising material handling costs and with a very fast processing time to meet timber flow through the dry mill. The preservative, Tanalith® T, forms an envelope on both Pinus radiata and Pinus elliotti sawn timber. Field trials conducted in Aus...
P R S Cobham, J Snow


Comparative performance of several ammoniacal copper preservative systems
1997 - IRG/WP 97-30151
The efficacy of several ammoniacal copper-based wood preservative systems was evaluated in this study. The selection of potential co-biocides was based on the results of an agar plate test. Following this, the most promising systems were evaluated in a standard field stake test. Good correlation was found between the agar plate and field stake test results. Of the preservative systems tested, copp...
D D Nicholas, T Schultz


Paper for discussion - Incising of spruce to improve preservative penetration
1973 - IRG/WP 318
Large quantities of whitewood or Norway spruce (Picea abies) are regularly imported into the United Kingdom from continental Europe. In addition, increasing amounts of Sitka spruce (Picea sitchensis) are likely to become available over the next decade from the Forestry Commission. In many ways spruce is a good structural timber, eg it is relatively cheap and easily available, it has adequate stren...
W B Banks


A new method for the study of microbiological decay of wood in a strictly anaerobic environment
1988 - IRG/WP 2319
Recent work has suggested that strictly anaerobic bacteria may play a role in the biodeterioration of wood, particularly in aqueous environments. However, no suitable test methods exist for the investigation of this hypothesis. An aqueous minimal medium in specifically adapted conical flasks was sterilised, gassed using a 5.5% H2; 31.8% C02; 62.7% N2 gas mixture to remove oxygen and transferred to...
G M Rogers, A A W Baecker


Service life of pressure treated deckings of spruce in direct contact with the ground
1988 - IRG/WP 3463
For decking outdoors in Sweden, pressure treated Scots pine (Pinus sylvestris L.) is used, on account of its treatability. The feasibility of using instead the refractory Norway spruce (Picea abies Karst.) is tested in a field trial. The spruce decks were treated together with pine decks with an ordinary Bethell process. As yet, after more than four years of exposure, neither in the battens nor in...
J B Boutelje, T Sebring


Using DNA probes to characterize the metabolic pathway of pigment production in several wood-staining fungi
1996 - IRG/WP 96-10146
During shipment and storage, lumber is susceptible to sapstain, a wood discoloration caused by fungi. Currently kiln drying and chemical applications are used to control sapstain. However, the chemicals used to protect wood have a broad range of action, and so can affect other organisms. In addition, in Canada most of these chemicals are under temporary registration. Thus there is a need to develo...
R Eagen, S Riecken, J Kronstad, C Breuil


In vitro sporulation of selected wood decay fungi
1978 - IRG/WP 190
Basidiospores produced axenically without laborious attention in the laboratory are useful in studies of wood decay initiation. Such spores presumably approach those collected from natural sporophores in size and germinability (Morton, 1964). Production of spores in vitro by inversion of cultures grown on 2% malt extract agar in deep glass dishes (100x80 mm²) has been the preferred method (Morton...
E L Schmidt, D W French


Wood extractives as carbon sources for staining fungi in the sapwood of lodgepole pine and trembling aspen
1995 - IRG/WP 95-10098
Wood discoloration by sapstaining fungi reduces lumber value. In Canada, the most commonly recorded sapstaining fungi belong to the genera Ophiostoma. This work evaluated the effect that Ophiostoma piceae, Ophiostoma ainoae, and Ophiostoma piliferum used the lipids present in the sapwood of lodgepole pine (Pinus contorta Dougl.) and trembling aspen (Populus tremuloides Michx.). Wood lipids, common...
Yong Gao, C Breuil


Further thoughts on standard principles of testing termiticides and/or wood preservatives
1992 - IRG/WP 92-1530
At the last annual meeting in Kyoto, Japan, there was a special session devoted to the standard principles of testing termiticides. There was definitely a perceived need by researchers and industry for some guidelines that spell out basic procedures required for any methodology in testing termiticidal formulations anywhere in the world. In the testing of new potential active ingredients, considera...
J R J French


Moisture requirements and wood degradation of pine and spruce wood by some Basidiomycetes-fungi
1989 - IRG/WP 1406
The minimum moisture requirements for the growth of the brown rot fungi, Coniophora puteana, Gloeophyllum trabeum and Serpula lacrymans were near or above the fibre saturation point of pine and spruce, sap and heartwood, during 160 days incubation according to the standard method EN 113. The moisture of wood for the optimum growth of Coniophora puteana and Serpula lacrymans was about 35-80% and fo...
H Viitanen, A-C Ritschkoff


Treatability problems - Relationships between anatomy, chemical composition and treatability
2001 - IRG/WP 01-40213
This report documents the results of phase 1 and 2 of a 3-phase research program. In phase 1, two hundred and fifty-six (256) Southern pine (pinus spp.) nominal 2 x 6's (38 mm x 140 mm) from a single mill in Georgia (southeastern US) were evaluated for treatability with CCA preservative. After treatment, 128 pieces representing a broad range of treatment characteristics were selected and ...
J E Winandy, F Green III, D Keefe


Wood preservation in Kenya
2000 - IRG/WP 00-40190
Focussing an Wood Preservation in Kenya, the Report discusses and elaborates on Education and Training, Research, Wood deteriorating organisms, Treatment Plants and Processes, Preserving Chemicals, Specifications, Markets, Health and Safety and Environmental issues. Education and Research is limited to one Institution only, other Institutions involved with the properties and utilization of wood ha...
R Venkatasamy


Formation of soft rot cavities in relation to concentric layers in wood fibre walls
1983 - IRG/WP 1185
A large number of timber species attacked by soft rot have been examined using light microscopy. The S2 layers in a large number of the timbers exhibited special structural features in the form of thin concentric layers. Several observations indicate that these layers may be characterised as "weak" zones by being more easily degradable than the surrounding wall layers. The chemical structure of th...
T Nilsson, G F Daniel


Correlation between changes in colour and chemical composition during photo-degradation of wood surfaces
2005 - IRG/WP 05-40301
Changes in colour of wood (yellowing) during photo degradation or weathering reflect chemical changes in wood. Therefore, the relationship between changes in chemical composition and CIELAB colour parameters is very important to characterize photodegradation of lignocellulosic surfaces. In this study, the changes in chemical composition and yellowing due to photo-degradation was studied by expos...
K K Pandey