Basidiosporogenesis by brown-rot basidiomycetes in vitro
1995 - IRG/WP 95-10126
Basidiospores of wood-rotting basidiomycetes are a primary sourse of infection causing wood biodeterioration, especially in wood above ground. Most studies evaluating wood preservatives have used mycelia or basidiospores obtained from wild mushrooms. The objective of this study was to demonstrate in vitro methods that promote carpogenesis and basidiosporogenesis by the brown-rot fungi Antrodia car...
S C Croan


Fungal degradation of wood treated with metal-based preservatives. Part 2: Redox states of chromium
1996 - IRG/WP 96-10164
Concerns have arisen about the leaching of heavy metals from wood treated with metal-based preservatives, such as chromated copper arsenate (CCA). Of particular concern is the toxic redox state of chromium and arsenic in aging and decayed CCA-treated wood. Generally, hexavalent chromium is more toxic than trivalent chromium and trivalent arsenic is more toxic than pentavalent arsenic. The desired ...
B Illman, S Bajt, T L Highley


Factors affecting the sorption of preservative during diffusion treatment of wood
1988 - IRG/WP 3500
The sorption of preservative into wood during soaking in aqueous solution was found to comprise absorption as well as diffusion of solute. Absorption was increased by partially seasoning the wood prior to soaking and was characterised by (a) a very rapid initial rate of uptake and (b) an extended period of slow uptake, the rate of which varied with prior conditioning. It was concluded that some pa...
P Vinden


The permanence of permethrin in wood preservation
1984 - IRG/WP 3288
The permanence of the synthetic pyrethroid permethrin in treated wood has been assessed for double vacuum and immersion treated Scots pine sapwood and whitewood using a 0.5% m/m solution of the insecticide in a hydrocarbon solvent. It is concluded that for all but the outermost 0.5 mm of the treated battens the distribution of the permethrin is relatively permanent. The outermost 0.5 mm appears vu...
R J Orsler, M W S Stone


The effect of service life and preservative treatment on the hardness of wooden poles
1989 - IRG/WP 3537
The surface hardness of utility poles is an important parameter which effects the acceptability of the pole as being safe to climb during line maintenance. The current investigation was designed to evaluate how the surface hardness of preservative treated utility poles is effected by the type of preservative, and the age of the poles. Chromated-copper-arsenate (CCA) treated red pine and jack pine ...
E B Jonsson, E M A Nilsson, J N R Ruddick


Inspection method of surface checking of Sugi posts
2003 - IRG/WP 03-20272
In order to establish the method for evaluating the checking of Sugi posts, checks on exposed posts were examined. Checks on Sugi posts exposed for 18 months were superficially inspected, that is, the length, width, and depth of the checks were measured from the outside with a ruler and 0.1 mm thick feeler gauge. Then, each post was cut into cross sections of the 30 mm width, and the check depth w...
H Kurisaki, H Nakatani, K Mizumoto


Washboard effect: A surface deformation of spruce resulting from vacuum-pressure impregnation with water-borne preservatives
1987 - IRG/WP 3450
The washboard effect has been observed in sawn spruce after both commercial and laboratory based preservative treatments and is of increasing economic importance. The effect is defined as a specific phenomenon at the wood surface. It is distinct from internal collapse in the wood, but it may occur in association with internal collapse damage. Experimental investigations on the causes of washboardi...
H Willeitner, R J Murphy


Laboratory evaluation of organophosphates as termiticides
1985 - IRG/WP 3330
In accordance with Japan Wood Preserving Association Standard 11(1) laboratory evaluations of five organophosphate insecticides and chlordane were conducted. Superficially treated sapwood of Pinus densiflora Sieb. et Zucc. (10 x 10 x 20 mm³) was compulsorily exposed to the attacks of 150 workers and 15 soldiers of Coptotermes formosanus Shiraki for 21 days at 28±2°C in the dark. Percentage weig...
K Tsunoda, K Nishimoto


The use of TCMTB in applications other than sapstain prevention: A review
1990 - IRG/WP 3606
The efficacy of TCMTB against staining fungi and surface moulds has been thoroughly investigated during the last decade. As a result, the chemical is used as an alternative to the chlorinated phenols in various parts of the world for the preservation of freshly sawn timber. Less known are the data obtained against brown rot, white rot and soft rot fungi. The termite repellent and bactericidal prop...
R Van der Eynde


Chromium on the surface of CCA-treated wood
1978 - IRG/WP 386
Chromium in solutions of CCA preservatives is predominantly in the hexavalent state (Cr VI). It is well known that Cr VI is associated with dermatitis and skin ulceration in workers handling chromium containing products and processes. When reduced to the trivalent state, however, chromium is considerably safer. An essential part, therefore, of safety procedures in any chromium - using industry is ...
C R Coggins, P Hiscocks


Role of cell wall structure in soft rot decay of bamboo
1995 - IRG/WP 95-10133
Models of soft rot hyphal penetration of bamboo cell walls are proposed. Soft rot hyphae show an interesting capability of penetrating the bamboo cell wall in different forms; typical longitudinal penetrating hyphae and tangentially orientated penetrating hyphae. The second form of penetration was found to be different from that normally associated with wood cell walls. The differences can be attr...
O Sulaiman, R J Murphy


Work programme of CEN/TC 38 (April 1999) and European publications
1999 - IRG/WP 99-20165
Scope of the CEN/TC38: Standardization of the characteristics of natural or conferred durability of wood and its derived materials against biological agents, including the characteristics of protection products and associated processes to obtain this durability. This applies in particular to: - the identification of hazard classes-, - the test methods (wood preservatives and treated wood and wood ...
R Hüe


The dry rot fungus Serpula lacrymans, its growth and damaging of wood
2004 - IRG/WP 04-10511
The dry rot fungus (Serpula lacrymans) is one of the most dangerous wood rotting fungi, especially in the built environment. In our mycological laboratory more experiments with this fungus have been carried out aimed at:- its growth under stable and variable climatic conditions, - its possibility to attack either natural wood of different species and also modified wood primary pre-treated with ...
L Reinprecht


Preliminary study on relation of wood structure to copper/chrome/arsenic (CCA) distribution in kempas (Koompassia malaccensis)
1995 - IRG/WP 95-40054
Kempas had been treated with copper/chrome/arsenic (CCA) preservative using full cell process. Analysis of preservative distribution at the micro level in relation to wood structure was carried out using scanning electron microscope (SEM) and energy dispersive X-ray (EDXA) analysis. The results showed that CCA elements were detected in all wood tissues at different ratios. Distribution of chemical...
S Ani, S Salamah


Evaluation of chlorpyrifos as an insecticidal component of a wood preservative
1984 - IRG/WP 3301
After two years of laboratory and field testing, chlorpyrifos is showing excellent potential as an insecticidal treatment to wood. In laboratory termite tests, retentions as low as 1-2 parts-per-million or approximately 0.0008 kg/m³ (0.00005 lbs/ft³) are effective against the Coptotermes formosanus. Laboratory leaching tests have shown no significant effect on the concentration of the retained c...
K Rose, J Kozuma, P Sparrow


Relationship between bond strength and surface characteristics of CCA-treated Douglas-fir
1993 - IRG/WP 93-30008
Chromated-copper-arsenate (CCA) treated Douglas-fir was laminated using a commercial phenol-resorcinol resin. CCA treatment enhanced the water repelleney of wood espeeially in the presence of extractives. However, the shear strength of CCA treated wood was 12% lower in dry condition and 38% lower in wet condition after six cycles of vacuum-pressure test than that of untreated wood. Slight removal ...
K Yamamoto, J N R Ruddick


Durability of surface preserved wood particle boards submitted to atmospherical influence
1995 - IRG/WP 95-40039
The worldwide problem of the continuously growing deficit of high quality natural wood material has caused the attempts of many research workers to find effective composites such as wood particle boards (WPBs) for replacing the massive wood for constructive purposes, depending on where the boards are exploited - in the open or under a shed, they are submitted to various climatic factors such as he...
L Valcheva


Resistance of painted wood to mould fungi. Part 2. The effect of wood substrate and acrylate paint systems on mould growth
1997 - IRG/WP 97-10234
Resistance of acrylate paint systems on different types of pine and spruce sapwood to mould fungi was studied. Dipping into the preservative prior to painting, a primer with and without a fungicide (propiconazole + IPBC 0.50 + 0.2%) and a topcoat with and without a fungicide (propiconazole + IPBC 0.25 + 0.12%) were combinations of the treatments studied. The efficacy of the treatment systems varie...
H Viitanen, P Ahola


Evaluation of substituted isothiazolone as a potential new wood preservative
1984 - IRG/WP 3306
Laboratory decay tests were carried out with isothiazolone (4,5-dichloro-2-n-octyl-4-isothiazolone-3-one) treated wood. This compound was found to be extremely effective against three common wood decaying brown-rot fungi, exhibiting toxic threshold values in the range of 0.37 to 0.50 kg/m³. For the white-rot fungus, Coriolus versicolor, the toxic threshold values for treated pine and sweetgum wer...
D D Nicholas, A F Preston, D E Greenley, S V Parikh


Changed permeability and surface properties of hornbeam wood due to its degradation by erosive strain of Phanerochaete chrysosporium
2004 - IRG/WP 04-40290
Specimens of hornbeam wood were submitted to a medium-term degradations by erosive fungus Phanerochaete chrysosporium. Biodegradations of specimens resulted in their apparent structural alterations, changes in permeability and increased intensity of interactions with polar liquids. Modified physical properties of biodegraded wood may significantly influence its penetration with polar media and che...
R Solár, S Kurjatko, L Reinprecht, M Mamon, V Vacek


Natural weathering of wood in a sunny climate effects on surface chemistry and paint adhesion
1997 - IRG/WP 97-20109
Radiata pine veneers and blocks were exposed to natural weathering under Australian summer conditions over a period of 30 days. Infrared spectroscopy revealed that there was perceptible surface delignification after 4 hours exposure, substantial surface delignification after 3 days exposure and almost complete surface delignification after 6 days. Viscometry determinations on holocellulose samples...
P D Evans, P D Thay, K J Schmalzl


Some experiences with attack of microorganisms on wooden constructions supporting foundations of houses and bridges
1997 - IRG/WP 97-10232
Reconstructions of bridges and public buildings or damage of houses during the construction of subway lines in Berlin have led to a number of inspections of wooden foundations, mostly pine or spruce piles, representing service lives of between ca. 70 and 140 years. In all cases bacterial attack was found both in wood submerged in ground water and in surface water. The extent of deterioration diffe...
M Grinda


Surface Barriers for Protection of Culture and Heritage Wooden Objects from Insect Attack
2004 - IRG/WP 04-20286
Anoxic treatment is an environment friendly procedure for eradication of wood boring insects in wooden objects of cultural and historical heritage. However, after the anoxic treatment, wooden antiques remain susceptible to further insect attacks. Possible protection against insects could be provided by the so-called post-repression protective barriers. Potential coating materials for such barriers...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


Wood protection by surface treatment of two borate preservatives, TIM-BOR® and BORA-CARE®, for the formosan subterranean termite and eastern subterrean termite
1993 - IRG/WP 93-10044
TIM-BOR® (disodium octaborate tetrahydrate: DOT, Na2B8O134H2O) and BORA-CARE® (40% DOT in ethylene glycol) are two borate products marketed for treating wood in use by brushing or spraying onto the wood surface. The active ingredients presumably diffuse into wood by the 10-15% existing wood moisture. Few data, however, are available to demonstrate the diffusion rate. Su & Scheffrahn (1991) s...
M Toroko, N-Y Su


Improving the weather resistance of glue-laminated jarrah and karri
1994 - IRG/WP 94-40017
Surface modification and dimensional stabilisation significantly increased the dry and wet shear strength of karri and jarrah lap-shear specimens (laminates) bonded with resorcinol formaldehyde. The combination of surface modification (sanding/sodium hydroxide treatment), and furfurylation produced the highest dry and wet shear strengths. Acetylated laminates had the lowest dry bond strength, but ...
J Balfas, P D Evans