Your search resulted in 661 documents. Displaying 25 entries per page.
Creosote movement from treated wood immersed in fresh water: Initial PAH migration
2003 - IRG/WP 03-50201
Creosote has a long history of successful use as a wood preservative, but polycyclic aromatic hydrocarbons (PAHs) in this preservative have raised environmental concerns, particularly when creosote-treated wood is used in aquatic environments. A number of models have been developed to predict the risk of creosote use in aquatic environments, but one limitation of these models is a lack of data o...
Sung-Mo Kang, J J Morrell, J Simonsen, S T Lebow
Copper based water-borne preservatives: The biological performance of wood treated with various formulations
1987 - IRG/WP 3451
Wood samples treated with the various components of CCA preservative singly and in combination were tested against a soft rot organism, a copper tolerant brown rot organism and in soil burial both unleached and after leaching. The results suggest that, of the elements tested, fixed copper is essential for preventing soft rot attack and fixed arsenic is essential for preventing attack by a copper t...
S M Gray, D J Dickinson
The window joinery test hut
1975 - IRG/WP 257
D F Purslow
Collaborative soft rot tests: Proposed amendments to Document No: IRG/WP/208
1973 - IRG/WP 224
J K Carey, J G Savory
300 years water-logged wood: Treatability with CCA-C
1998 - IRG/WP 98-40103
The treatability of 300 years water-logged and recent wood (Abies bornmülleriana M.) was assessed by dip treatment and vacuum and pressure cycling with CCA-C. Treatment runs were evaluated on the basis of weight gain retention and radial and tangential penetration measurements. The preservative penetration and retention levels in the 300 years water-logged wood were higher than in the recent wood...
S N Kartal, N Yilgör
Leaching tests - A paper for discussion
1973 - IRG/WP 221
J W W Morgan
Protecting wooden structures
1980 - IRG/WP 392
Chromium-containing chemicals that effectively retard weathering of wood improve performance of subsequently applied finishes. Current work is focusing on the performance of wood-derived products (plywood, hardboard, fiberboard, particle board) after surface treatment with inorganic chemicals. The overall objective of the continuing research is to investigate new environmentally safe procedures to...
W C Feist
Examination of timbers from the Mary Rose in storage
1988 - IRG/WP 4149
Timbers from the Tudor ship, Mary Rose, have been examined for the presence of fungal fruiting structures. Wood specimens were also examined for the presence of microbial decay patterns using light and scanning electron microscopy. Structural timbers were surveyed using the Pilodyn for an overall picture of the extent of decay. Mary Rose timbers were predominantly inhabited by marine fungi. Fourte...
R Mouzouras
A comparison between methods for evaluating the water repellency of wood
1989 - IRG/WP 2328
Wood specimens treated with a number of water repellent formulations have been tested for their water repellency according to four laboratory test methods, based on weight increase, swelling and contact angle measurements, in order to assess the degree of agreement between the different methods. Treatments representing formulations with a wide range of water repellent efficiency were tested both i...
R Nussbaum
Practical testing of wood preservatives to prevent weathering damage and infection by micro-organisms on spruce and pine
1989 - IRG/WP 3530
Brush application, is generally used to prevent wooden window frames from decay caused by influence of weathering and fungi. Accordingly 10 boards of pine (Pinus sylvestris) and spruce (Picea abies) were treated with 10 commercially used wood preservatives. The efficiency of fungicides by using chiptest and blue stain test (EN 152), the effectiveness against weathering as well as the course of col...
R Gründlinger, O Janotta, H Melzer, K Messner
The use of chlorothalonil for protection against mold and sapstain fungi. Part 1: Laboratory evaluation
1989 - IRG/WP 3515
Laboratory screening of chlorothalonil alone and in combination with other fungicides was conducted against six mold and sapstain fungi. The most promising treatments appear to be chlorothalonil supplemented with CCA or copper-8-quinolinolate. Field tests have been implemented....
J A Micales, T L Highley, A L Richter
Testing wood in ground contact: An artificial soil
1977 - IRG/WP 280
This document is an interim report on the development of the artificial soil medium. It includes some information on the relationship between soil, wood and water which is of relevance in testing....
E F Baines, D J Dickinson, J F Levy
Checking of sodium pentachlorophenate fixation in wood
1990 - IRG/WP 3620
In order to estimate the volatilization of sodium pentachlorophenate from treated wood, wood samples treated with pentachlorophenate were analysed after various durations of an EN 73 weathering The results giving no clear evidence of volatilization, treated wood samples were put in a test chamber with precise climatic conditions, the air used in the experiment being analysed. The pentachlorophenat...
M Lamour, H Sageot
Spot-tests for TnBTO and AAC preservatives
1984 - IRG/WP 3279
Nineteen indicator systems were examined as potential alternative spot-tests for preservative penetration in TnBTO- (bis-tributyltin oxide) or AAC- (alkyl ammonium compound) treated wood. Results indicated phenylfluorone as an acceptable alternative to pyrocatechol violet for assessment of TnBTO, and cobaltous thiocyanate or a bromocresol green/quinine sulphate mixture as alternatives to bromophen...
D V Plackett
Waterborne silicones as wood preservatives
1995 - IRG/WP 95-30062
For more than thirty years silicones are used as water repellents for masonry. Their excellent properties make them also attractive for non-mineral substrates like wood. Although it was always thought that silicones are not able to perform on wood, a new type of aqueous silicone materials proofed the opposite: Excellent water repellency and astonishing durability were achieved. This paper describe...
R Hager
Assessment of contamination of soil and water at a CCA treatment plant: A demonstration project
1996 - IRG/WP 96-50067
Soil, sludge, dust and water samples were collected at a copper/chromium/arsenic wood preservation plant. Contamination of soil, sludge, dust and surface water with copper, chromium and arsenic was detected. Levels of contamination were sufficiently high to require remediation. Contamination originated from preservative solution dripping from recently treated wood. Migration of contaminants was vi...
P N Durrant, D C R Sinclair, G M Smith
Chemical analysis of TnBTO in lap-joints
1999 - IRG/WP 99-20173
This research was performed as part of the EU project FACT (contract SMT4-CT96-2135) on field tests out of ground contact and ageing methods. The results reported here are part of the work on the experimental lap-joint standard (ENV 12037). TNO investigated the TBTO content of 32 lap-joints by analysing the tin content of 90 samples. The lap-joints were treated with two different TBTO-concentratio...
A Voss, P Esser, W L D Suitela
Differential behaviour of wood rotters at water repellent Rubberwood
2000 - IRG/WP 00-10386
Rubberwood samples treated with different concentration of aqueous solution of chromic acid has induced significant increase in water repellency and attains dimensional stability. Though water repellency and dimensional stability was achieved by treatment, the fungal invasion could not be completely controlled. Differential level of decay of brown and white rot in wood treated with water repellent...
H C Nagaveni, S S Chauhan, K S Rao
Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic conditions. Part 2: Semi-industrial investigation
1995 - IRG/WP 95-50040-13
In continuation of previous leaching research on the quantification and modelling of metal elements released from CCA treated timber, a series of experiments has been carried out dealing with the influence of temperature and pH of the relative aquatic environment. The leaching method used is the Dutch prestandard for building materials, a long term static leaching test simulating practical bank-sh...
G M F Van Eetvelde, W J Homan, H Militz, M Stevens
An interim report on trials with 'Boliden K33' and 'Celcure A' in water of different salinities in the Baltic Sea and in the UK
1974 - IRG/WP 406
It was felt necessary to undertake field trials using large test samples exposed in natural water of different salinity in order to determine preservative leaching and to assess the degree of biological attack....
R A Eaton, D J Dickinson
Some observations on miniaturised soil/block tests
1988 - IRG/WP 2317
Results are presented for miniaturised soil/block tests carried out in 120 ml capacity glass jars. The four test fungi (Coniophora puteana, Coriolus versicolor, Gloeophyllum trabeum and Poria placenta) reacted differently to different moisture regimes established by varying the soil moisture content. Acceptable levels of decay were achieved by the three brown rot fungi with soil at 110% whc; howev...
J K Carey
Effect of double-vacuum and vacuum-pressure impregnation with water-borne preservatives on the dimensional characteristics of spruce
1990 - IRG/WP 3613
Air-dried planed spruce (Picea abies) samples were treated with a water-borne preservative (micro-emulsion) and one oil-borne type both containing azaconazole and deltamethrin. Each set of samples contained equal number of specimens with different growth ring orientation, heartwood content and density. In addition to the preservative retention and the penetration of a.i., the swelling of the sampl...
J Van Acker, M Stevens, G Rustenburg
Life cycle analysis: Assessing environmental impact
1994 - IRG/WP 94-50034
Environmental impact assesment is a major issue that faces every nation today. However, consistently and objectively measuring the environmental impact is difficult. During the past two decades, a process called life cycle analysis was developed that tried to make consistent and objective environmental assessments. The Society of Environmental Toxicology and Chemistry broadened the concept to not ...
S L LeVan
Washboard effect: A surface deformation of spruce resulting from vacuum-pressure impregnation with water-borne preservatives
1987 - IRG/WP 3450
The washboard effect has been observed in sawn spruce after both commercial and laboratory based preservative treatments and is of increasing economic importance. The effect is defined as a specific phenomenon at the wood surface. It is distinct from internal collapse in the wood, but it may occur in association with internal collapse damage. Experimental investigations on the causes of washboardi...
H Willeitner, R J Murphy
Copper based water-borne preservatives: The use of a thin section technique to compare the protection of wood by copper based preservatives against soft-rot and bacterial decay
1987 - IRG/WP 2286
This paper describes the techniques developed and gives examples of results obtained for the performance of copper based wood preservatives against both the bacterial and fungal hazards....
A M Wyles, D J Dickinson