Your search resulted in 3520 documents. Displaying 25 entries per page.
Hibernation or spring awakening? – The research on wood durability and protection in marine environment
2018 - IRG/WP 18-10929
Wooden structures in marine applications are exposed to severe degradation conditions caused by mechanical loads and wood degrading organisms. The present paper presents the use of wood in marine environments in Europe from a wood protection perspective and gives an overview over relevant research topics. It compiles the most relevant literature with an emphasis on new wood protection methods and ...
A Treu, K Zimmer, C Brischke, E Larnøy, L R Gobakken, F Aloui, S M Cragg, P-O Flæte, M Humar, M Westin
Superior kempas hardwood protection with two proprietary microemulsion termiticdes based on permethrin and cyermethrin against Coptotermes termite attack under H2 an H3 weathered conditions found in buildings
2018 - IRG/WP 18-10931
SARPECO® and AXIL® solutions are water-based wood preservatives approved for dipping treatment providing 25 years of termite protection for solid wood and wood-based products in Europe and for more than 10 years in Indonesia. SARPECO® and AXIL® solutions are patented formulations based on concentrated microemulsions (ME) diluted with water as a dipping treatment but also for vacuum pressure tr...
D Messaudi, A H H Wong, C A D Tawi, N Bourguiba, O Fahy
Liquefied wood polyols: a bio-based preservative for protection of wood from fungal decay
2018 - IRG/WP 18-30725
The liquefaction of wood is one of promising approaches in utilization of woody waste which is generated during primary and secondary processing of wood and liquefied wood having various application including bio-based preservatives. The biological degradation of wood due to fungi is the major problem encountered in indoor and outdoor utilization of wood. In this study, woody waste recovered from ...
A Kumar, G Vijaylakshmi, S Singh Chauhan
Effects of wood protecting biofinish and linseed oil on fire behaviour and leachability of the fire retardant
2018 - IRG/WP 18-30728
A wood protecting biofinish is based on a protective and decorative fungal-based coating and a linseed oil impregnation (called Xyhlo biofinish). This biofinish enables the long-term use of wood in outdoor applications without using toxic chemicals.
The fire resistant properties of materials used in buildings are very important. Since Xyhlo biofinish is relatively new, only little information is ...
S Rensink, E J van Niewenhuijzen, M F Sailer
Multiscale modification on water resistance and dimensional stability of Populus cathayana by alkali lignin combined with heat treatment
2018 - IRG/WP 18-40826
The aim of this study was to enhance the water resistance and dimensional stability of fast growing wood by alkali lignin combined with heat treatment. Poplar (Populus cathayana) samples were first impregnated with alkali lignin solution and then subjected to heat treatment at 140, 160, and 180°C respectively for 2h. Properties of leachability, moisture adsorption and water absorption, contact an...
H Zhou, J Li, E Ma
Recent findings clarifying the mechanism of brown-rot decay protection in acetylated wood
2018 - IRG/WP 18-40827
This paper summarizes the findings obtained during my PhD research over the past three years. The results provide insights which help to understand the enhanced brown-rot decay resistance of acetylated wood with particular emphasis on the role of water. The protection acetylation provides is derived from moisture exclusion within the acetylated cell wall, but the exact mechanism by which water is ...
G Beck
A Synergistically Stabilized Oil-in-Water Paraffin Pickering Emulsion Used in Wood Treatment
2018 - IRG/WP 18-40840
Pickering emulsions (emulsions stabilized by solid particles) are attractive as they have strong similarities with traditional surfactant-stabilized emulsions. In this study, an oil-in-water (O/W) paraffin Pickering emulsion system with satisfying stability and small droplet size distribution was developed by hydrophilic silica particles and traditional surfactants as mixed emulsifiers. The drople...
J Jiang, J Cao
Improvement of short rotation teak wood properties through thermal modification
2018 - IRG/WP 18-40842
Teak (Tectona grandis L.f) is one of the most popular tropical timber species. Nowadays, the source of long rotation teak is limited in the availability. Many wood processing industries use short rotation teak, which has lower quality especially in durability and dimensional stability. Heat treatment is an eco-friendly method improving dimensional stability and durability of wood. The objectives o...
L A Pratiwi, I W Darmawan, B George, A Merlin, C Gérardin, S Dumarçay, T Priadi, P Gérardin
Polyesterification of wood using sorbitol and citric acid under aqueous conditions
2018 - IRG/WP 18-40851
The aim of this research is to determine if the polyesterification of sorbitol and citric acid in wood has a future potential as a wood modification process. Pine wood was impregnated with an aqueous solution containing citric acid and sorbitol and was thereafter cured at 103, or 140°C for 18 hours. The dimensional stability and leaching resistance were studied for both modification temperatures....
E Larnøy, A Karaca, L R Gobakken, C A S Hill
Enhancing knowledge transfer in the wood protection sector
2018 - IRG/WP 18-50338
In order to meet the needs for the developing bio-based economy, maintaining and expanding the market potential for wood raw materials and wood products in indoor and outdoor construction uses remains a key activity for industries in the biotechnological and forestry sector respectively. A major restraint in this respect is the drastically deviating views and expectations on quality and performanc...
C Brischke, G Alfredsen, S Bollmus, M Humar, D Jones, L Meyer-Veltrup, L Nunes
Chemical defense of trees and wood natural durability: from protection to valorization
2019 - IRG/WP 19-10943
Natural durability of wood is defined as “the inherent resistance of wood against various wood-destroying organisms” (European standard EN 350-1). This property is due in particular to heartwood extractives. However, the wood natural durability is included in a wider defense system, and other organs such as bark and roots also host protective compounds. Studying the mechanisms on which global ...
E Houel, D Stien, N Amusant
Protecting Sustainable Wood Infrastructure ̶ Improving the Performance of Poles, Piles, Ties & Timbers with Dual Treatments
2019 - IRG/WP 19-30735
Wood is by far the best structural material in terms of environmental impact, as shown by a number of LCA studies. This environmental impact superiority can be improved if the longevity of the commodity is extended. The main durability concern in large cross-section treated materials is the susceptibility of the heartwood to decay, as it is not typically treatable using traditional methods. This ...
J Lloyd, A Taylor, C Brischke, N Irby, M Manning
Biosourced hybrid phenolic resins as coatings for the protection of wood and wood composites
2019 - IRG/WP 19-30745
Biosourced phenolic resins, based on the phenol-formaldheyde (PF) type, were prepared for their application as coating for wood and wood composites protection, especially against fire. The resins were synthesized by combining an organic polymeric matrix with another inorganic phase. The organic phase was prepared substituting phenol by natural phenolic compounds such as lignin and tannins. The ino...
P L de Hoyos-Martínez, R Herrera, J Labid, F Charrier El Bouhtoury
Wood Protection Through Diffusion: Dimensional Stabilisation with Amine Oxides
2019 - IRG/WP 19-30747
Wood is a phenomenal construction material. In addition to its great physical properties and its beautiful appearance, it possesses many environmental-friendly virtues like the sequestration of carbon dioxide. It is however subject to dimension changes when submitted to fluctuating moistures levels, which can lead to warps, cracks and the peeling of paints. Many water repellents can slow down the ...
S Pepin, P Blanchet, V Landry
The use of bicine and tricine as possible Maillard reagents in a combined thermal/chemical modification of beech
2019 - IRG/WP 19-40852
The effects of thermal modification have been well established, particularly in terms of reductions in mechanical performance. In recent years, there has been an increase in studies related to the Maillard reaction. More commonly associated with food chemistry, it involves the reaction of amines and reducing sugars during cooking procedures. This paper has attempted to combine the use of amines an...
D Jones, C-M Popescu, D Krzisnik, M Hocevar, M Humar, M-C Popescu
Antifouling wood matrix with natural water transfer and micro reaction channels for water treatment
2019 - IRG/WP 19-40853
Wood with abundant nutrition transport channels could be considered as a kind of natural water purifier due to quick and effective passages for separation. Nevertheless, microporosity as main porous structure of initial wood are not enough to effectively separate small molecular, such as organic dye pollutants. Meanwhile, like most filters the fouling resulting in blocking and poor water flux will...
G Liu, D Xu, S Chang, J Hu, Xianjun Li5, Y Liu
Using X-ray scattering to elucidate the mechanisms behind the moisture and fungal decay resistance of epoxybutene modified wood
2019 - IRG/WP 19-40854
Chemical modification of the hydroxyl groups of wood can improve the properties of wood by providing moisture and biological resistance, as well as dimensional stability. Southern pine solid wood was chemically modified to various weight percentage gains (WPG) with epoxybutene (EpB, 8%-38% WPG). After modification, specimens were extracted with a toluene: ethanol (2:1) solution for 2 hours or wate...
R E Ibach, N Plaza
Development of beech wood thermo-chemical modification treatments based on different vinylic derivatives of glycerol and polyglycerol
2019 - IRG/WP 19-40855
In this study, a combination between chemical and thermal wood modification has been investigated. Seven types of a low concentration of 10% aqueous additive solution of vinylicglycerol [glycerol-maleic anhydride (Gly-MA), glycidyl methacrylate (GM), and Glycerol methacrylate-maleic anhydride (GM/MA(2eq))], vinylicpolyglycerol [polyglycerol-maleic anhydride (PG-MA), polyglycerol methacrylate (PGM...
M Mubarok, S Dumarcay, H Militz, K Candelier, M-F Thevenon, P Gerardin
Suggestive remarks for designing of experimental samples and trial devices to treat wood by pre-vacuumed immersion method
2019 - IRG/WP 19-40862
This study was conducted to test the impregnability of wood material according to the pre-vacuumed immersion process and to reveal the usability of cylindrical (plug) samples in impregnation experiments in addition to the cuboid or cubic samples. In this context, cuboids were prepared 30 mm in length, 20 mm in width and 20 mm in thickness, whereas plugs were prepared radially and longitudinally wi...
I Usta
Improvement of wood decay and termite durability resulting from combined treatments based on borax/phenol-formaldehyde impregnation followed by thermal modification
2019 - IRG/WP 19-40871
This study determined the factors influencing the boron content after leaching of pine blocks impregnated with aqueous solution of phenol-formaldehyde (PF) resin with or without borax and subjected to heat treatment by response surface methodology. An experimental design permits to analyze the effects of heat treatment temperature (150, 185 and 220°C), curing time (5, 12, 5 and 20 hours), resin c...
S Salman, M-F Thevenon, A Petrissans, S Dumarcay, P Gerardin
Protecting wood exterior infrastructures above ground in Spain. The importance of protection by design in the performance
2019 - IRG/WP 19-40874
Across Spain is very common to find wood exterior infrastructures build mainly in sawn and glue-laminated wood. Most of these exterior wood infrastructures use softwood wood species such as: fir, spruce, larch and pine. In Spain exterior wood infrastructures, became more and more popular since nineties, when sawn and glue-laminated wood were utilized for building exterior wood infrastructures in o...
D Lorenzo, M Touza, J Fernandez-Golfín, A Lozano, J Benito, M T Troya, L Robertson
The impact of additional interior layers to the moisture dry-out and mould growth risk of CLT walls
2019 - IRG/WP 19-40876
The objective of this study was intended to determine the maximum allowable initial moisture content for CLT walls having both exterior and interior thermal insulation. A laboratory test was conducted, for which four test walls with two different insulation solutions and two different initial moisture contents were built. Based on the test results a simulation model was configured and simulations ...
V Kukk, J Kers, T Kalamees
Engineered wood constructions in Brazil: the challenge of protection against biodeterioration for market growth
2019 - IRG/WP 19-40878
This paper presents some thoughts about Brazilian wood constructions market regarding to biodeterioration and protection against biodeterioration, especially termites. Despite of being a forestry country, there is no tradition in wood engineered buildings and some prejudice must be overcome.
New companies are interested in this market and as a continental country, different problems regarding of...
L F T di Romagnano, S Brazolin, G A da Silva, G A C Lopez
Wood veneer with high flexible decorated with nanoparticles for highly efficient water treatment
2019 - IRG/WP 19-50347
Natural wood is mainly comprised of numerous long, partially aligned channels (lumens) as well as nanochannels. Wood with these quick and effective passages is suitable for a membrane/separation material. However, a suitable thickness range of wood along its growth direction is essential to effectively separate small molecular, and the wood membrane is too thick to clean easily. In this paper, woo...
S Chang, D Xu, G Liu, J Hu, X Li, Y Liu
Wood protection techniques and natural weathering: their effect on aesthetics and preference of people
2019 - IRG/WP 19-50351
Current research successfully contributes to improving wood protection techniques. However, the vast majority of research on preventing degradation of wood ignores a critical aspect of making successful products and processes – user selection of materials, which may largely depend on the aesthetical qualities. Wood treatments change the tactile and visual properties of wood substantially and the...
D Lipovac, M D Burnard, A Sandak, J Sandak