Using DNA probes to characterize the metabolic pathway of pigment production in several wood-staining fungi
1996 - IRG/WP 96-10146
During shipment and storage, lumber is susceptible to sapstain, a wood discoloration caused by fungi. Currently kiln drying and chemical applications are used to control sapstain. However, the chemicals used to protect wood have a broad range of action, and so can affect other organisms. In addition, in Canada most of these chemicals are under temporary registration. Thus there is a need to develo...
R Eagen, S Riecken, J Kronstad, C Breuil


The influence of the natural extractives of opepe (Nauclea diderrichii) and African padauk (Pterocarpus soyauxii) timbers on their durability
1996 - IRG/WP 96-30098
Many timbers contain chemical extractives that undoubtedly play a key role in the timber's natural durability. Opepe (Nauclea diderrichii) and padauk (Pterocarpus sp.) are both very durable timbers (class 1), yet they are described as being moderately permeable. This suggests the presence of biocidal chemicals within these timbers, rather than simple blocking agents. Initial trials on the...
E D Suttie, R J Orsler


Dimension of lysimeters and the evaluation of the migration of wood preservative components in soil
1996 - IRG/WP 96-50065
In the past, investigations concerning the migration behaviour of wood preservatives were made to a minor extent and no uniform methods of test exist. The migration behaviour of CFB was determined using 5 lysimeters of different dimension. The results of the migration and distribution of the anions in the soil showed considerable differences between both ions. Approximately the whole quantity of c...
E Melcher, R-D Peek


Distinguishing isolates of Aureobasidium on the basis of their ability to utilise lignin breakdown products as a sole carbon source
1996 - IRG/WP 96-10151
Wild isolates of Aureobasidium were obtained by dilution plating from a ca 20 year old painted pine window frame. Four isolates were obtained from the paint/wood interface region and four isolated from regions deep in the wood. The isolates were then used to inoculate liquid cultures containing ferulic acid, a lignin breakdown product, present as the sole carbon source. Ability of the isolates to ...
M W Schoeman, D J Dickinson


Fixation of copper-chrome-arsenic treated timber: A comparison of leaching methodologies
1996 - IRG/WP 96-50075
Five packs of kiln dried radiata pine heartwood were treated with copper-chrome-arsenic preservative treated, utilising a modified Bethell treatment schedule. Two methods of determining the level of preservative fixation were compared. These included the diphenylcarbazide method and simulated rainfall testing. The fixation levels were generally higher for tests involving simulated rain leaching. F...
S Walley, P R S Cobham, P Vinden


Hygroscopicity of decayed wood - Implications for weight loss determinations
1996 - IRG/WP 96-20085
Hygroscopicity changes were observed in red maple blocks subjected to brown rot, white rot and soft rot. Brown rot reduced hygroscopicity, soft rot increased hygroscopicity, and white rot showed only a very slight increase in hygroscopicity. The effect of these changes on weight loss tests is a slight overestimation of weight loss for brown rot and a slight underestimation for soft rot and white r...
S E Anagnost, W B Smith


Remedial treatments of glulam = diffusion of active ingredients through glue lines from solid wood diffusable preservatives
1996 - IRG/WP 96-30117
Diffusable preservatives are very suitable for use in remedial treatments of laminated beams in which too high moisture content involves the development of wood destroying fungi. The diffusion of active ingredients (boric acid, disodium octoborate, bifluoride) is well observed in solid wood but in a composite wood, the glue lines may appear not only as a barrier for the diffusion but also, may be ...
D Dirol, S Mouras


Fenton's reagent as a modification tool in brown-rot decay
1996 - IRG/WP 96-10155
A biomimetic approach was used to clarify the role and importance of the Fenton-type reaction in the carbohydrate degradation by brown-rot fungi. Spruce sawdust and microcrystalline cellulose were modified in the H2O2/Fe(II) treatment. The degree of hydrolysis of the pretreated spruce sawdust was clearly increased with the complete cellulase (Econase), purified endoglucanase from Trichoderma reese...
M Rättö, A-C Ritschkoff, J Buchert, L Viikari


How predictive are laboratory experiments for assessing the effects of chitin synthesis inhibitors (CSI) on field colonies of terrnites? - A comparison of laboratory and field data from Australian mound-building species of termit
1996 - IRG/WP 96-10143
A singular advantage of using mound building species of termite is their directly accessible nest. This allows evaluation of control methods by accurate assessment of the effects at the colony level. The mound building species Coptotermes acinaciformis (Froggatt) and Nasutitermes exitiosus (Hill) were used to test the CSI, hexaflumuron, in laboratory and field trials. Laboratory results showed tha...
M Lenz, P V Gleeson, L R Miller, H M Abbey


Options for termite management using the insect pathogenic fungus Metarhizium anisopliae
1996 - IRG/WP 96-10142
The insect pathogenic hyphomycete fungus Metarhizium anisopliae (Metschnikoff) Sorokin is promising as a biological insecticide for many species of subterranean termites. In Australia, a survey of termite mounds and feeding sites using a selective medium showed that this fungus is widespread but rarely causes mortality of termites under natural conditions. One isolate, codenamed FI610, has been se...
R J Milner, J A Staples, M Lenz


Protection of wood blocks treated with Trichoderma isolates selected on the basis of preliminary agar screening studies
1996 - IRG/WP 96-10154
Previously reported results of agar interaction screening studies for biocontrol agents of wood decay basidiomycetes showed two Trichoderma viride isolates, killed 16 of 19 target fungi (Tucker and Bruce, 1995). Testing of these isolates in wood was required to assess their performance at preventing decay of wood blocks. Standard testing of chemical wood preservatives is used to determine the toxi...
E J B Tucker, A Bruce, H J Staines


Risk assessment of energetic valorization of treated wood - wooden recycling
1996 - IRG/WP 96-50072
The most useful method for the valorization of wood wastes and wooden wastes is energetic valorization. In France the percentage of wood treated by antisaptain products is around 30%. Currently with the growing regulation, there is a need for cleaner methods and technology to allow sustainable valorization. The preservatives concerned are common organochlorine compounds (NaPCP) less used nowadays ...
G Deroubaix, P Marchal, G Labat


Destaining wood sapstains caused by Ceratocystis coerulescens
1996 - IRG/WP 96-10159
Fungal sapstain does not reduce the strength of wood, but it does discolor the wood, detracting from its appearance and decreasing the value of wood and wood products. The purpose of this investigation was to assess whether wood sapstain caused by Ceratocystis coerulescens could be destained and existing growth eradicated. The hydroxyl radicals generation under optimized conditions destained the s...
S C Croan


Fungitoxic effect of the quaternary ammonium compounds preservatives against Basidiomycetes by using agar-plate and agar-block methods
1996 - IRG/WP 96-30118
Results of investigations on the fungitoxic value of three versions of wood preservatives based on the quaternary ammonium compounds (lauryldimethylbenzylammonium chloride, lauryldimethyl-benzylammonium bromide and alkylbenzyldimethylammonium chloride) and borates in relation to the wood destroying fungi have been presented. The agar-plate (screening) and agar-block method were applied. A wide ran...
J Wazny, P Rudniewski


Resistance of wood inorganic material composites against decay fungi and subterranean termites
1996 - IRG/WP 96-40062
Double diffusion process was applied to the treatment of small sound sapwood specimens [20(T) x 20(R) x 10(L) mm³] of Cryptomeria japonica D. Don. The specimens were consecutively dipped in the two kinds of acqueous solutions to form water insoluble deposits within the wood after an expected reaction between the solutes. Following the comparison of deposits formed and treating conditions (tempera...
K Tsunoda, T Yoshimura, M Takahashi, S Hirao, H Usui


Optimun storage period for the boron diffusion treatment of rubber wood
1996 - IRG/WP 96-30121
The study determined the maximum thickness of rubber wood that can be diffusion treated and the effect of diffusion storage period on the distribution of chemicals in treated wood of various thicknesses. Wood of thickness up to 50 mm can be easily diffusion treated with 10% boric acid equivalent (BAE) solution to adequate loading of chemicals. The optimum diffusion storage period to get uniform an...
T K Dhamodaran, R Gnanaharan


Field Liners™ prevent creosote migration from transmission poles to soil during service
1996 - IRG/WP 96-40067
A full scale trial utilised 150 12m Eucalyptus grandis transmission poles treated with standard retentions of creosote according to SABS Method 457. One hundred poles had Field Liners™ applied while 50 did not. The 150 poles were used to complete an electricity transmission line in Southern KwaZulu-Natal. After 18 months service, incremental cores were taken from 15 cm below the ground lines of ...
M R Behr, G D Shelver, A A W Baecker


A comparison between different accelerated test methods for the determination of the natural durability of wood
1996 - IRG/WP 96-20099
According to the European standard EN 350-1 the natural durability of wood is defined as: "the inherent resistance of wood to attack by wood destroying organisms". This standard also describes how, for certain hazard classes, the durability is determined. The two methods described in this standard are the kolleflask method (EN 113) and the field-stake-test method (EN 252). The EN 113 test gives re...
H Militz, S G L Michon, J E Polman, M Stevens


Long term experiments for assessing the diffusion of boric acid and diluorides from local preservative pills in spruce and pine
1996 - IRG/WP 96-40065
For the experimental assessment of the diffusion of boric acid and difluorides over a three year period 2 tests were set up. In a test with large spruce blocks (150 x 150 x 300 mm³) 3 different pill types were exposed to 3 different climates: climate room (20°C, 65% r.h.), wet room (20°C, 95% r.h.), and to outside exposure. In a test with open L-joints without paint, with an alkyd paint and wit...
W J Homan, H Militz


Detection of brown-rot antigens in southern pine
1996 - IRG/WP 96-20090
Brown rot fungal antigens were detected by particle capture immunoassay (PCI) in southern pine 2 x 4's beyond visible or culturable hyphal growth. Further analysis of test samples revealed changes along the 2 x 4's that could be grouped into zones. Zone 1, the point of inoculation through 6 cm, showed low pH, measurable oxalic acid, high moisture, and high protein. Zone 2, throug...
C A Clausen


Is laboratory testing of decay resistance questionable as a single criterion for natural durability?
1996 - IRG/WP 96-20096
In a laboratory test set up over 20 hardwood species were evaluated according to the European Standard EN 350-1 including Basidiomycete and soft rot testing. Half of the species used were of a known natural durability. The Basidiomycete testing was carried out using Coriolus versicolor, Gloeophyllum trabeum and Coniophora puteana in a malt agar test similar to EN 113. From this test it was not pos...
J Van Acker, M Stevens, T Van Cauwenberghe, T Seynaeve


A shower test protocol for measuring antisapstain wash-off from small individual log billets
1996 - IRG/WP 96-50069
According to New Zealand Timber Industry Federation statistics New Zealand exported 4,835,000 m³ of logs in 1994 and it is estimated that c. 20% were anti-sapstain treated. Loss of preservative from logs as a result of rain impact after application is of considerable concern both with respect to potential loss of efficacy and environmental contamination. Whilst Environment Canada have a proposed ...
A J Pendlebury, H Pearson


Evaluation of a utility pole inspection procedure
1996 - IRG/WP 96-20084
Methods were developed and are currently being utilized to appraise residual strength of utility poles based on visual assessment of increment cores. Strength tests, mycological descriptions and anatomical analyses were performed on eight utility poles taken out of service and one new (never in service) pole. Samples were obtained from increment cores removed from 6 levels in the pole: 2 feet, gro...
S E Anagnost, C J K Wang


Comparative study of the degradative ability of autochthonous and standardized strains of wood decay fungi
1996 - IRG/WP 96-10178
This study is intended to assess the biomass, the extracellular protein production, and the carbohydrate degradating ability of three standarized (Chaetomium globosum, Trametes versicolor and Gloeophyllum trabeum) and six autochthonous wood decay fungi strains, with unknown degradating effects. The carbohydrate sources used were those that are usually found in wood cells (glucose, galactose, manos...
F Llinares, D Muñoz-Mingarro, J E Garcia de los Rios, M T De Troya, M Yuste, F Rubio, F Alvarez, P Jiménez, C Rodríguez-Borrajo, A M Navarrete


The role of contact chemoreception in location of wood by the marine borer Limnoria (Isopoda)
1996 - IRG/WP 96-10157
This paper investigates the ability of Limnoria (Isopoda: Limnoriidae) to determine chemical differences in wood substrates, while in contact with the substrates. Test substrates were chosen on the basis of previous arguments concerning the chemical state of wood prior to Limnoria attack: microbial, ergosterol, metabolite, humic, extract and control (autoclaved) veneers were used as experimental s...
S M Henderson, S M Cragg