Quantification of wood decay effects by HPLC analysis
1992 - IRG/WP 92-1576
The present work quantified the effects of the white rot basidiomycetes Coriolus versicolor and Phanaerochaete chrysosporium, and also those of the brown rot fungi Coniophora puteana and Lentinus lepideus, on Pinus patula and Eucalyptus grandis. Wood colonisation was quantified by Kjeldahl nitrogen determinations converted to biomass assays, and degradation was quantified by weight losses produced...
V Singh, M Tarin, G D Shelver, A A W Baecker


The colonisation pattern of anaerobic fungi in wood
1989 - IRG/WP 1403
Timber foundations may be degraded in service in anaerobic conditions. The present work was conducted to investigate whether anaerobic fungi could colonise wood, using rumen fungi as test microorganisms. Strictly anaerobic fungi were isolated and purified from cow dung and goat and sheep rumen fluids respectively. Colonisation of Eucalyptus grandis and Pinus patula by these fungi and Neocallimasti...
A H Wiederhold, M Morrison, A A W Baecker


Field Liners™ prevent creosote migration from transmission poles to soil during service
1996 - IRG/WP 96-40067
A full scale trial utilised 150 12m Eucalyptus grandis transmission poles treated with standard retentions of creosote according to SABS Method 457. One hundred poles had Field Liners™ applied while 50 did not. The 150 poles were used to complete an electricity transmission line in Southern KwaZulu-Natal. After 18 months service, incremental cores were taken from 15 cm below the ground lines of ...
M R Behr, G D Shelver, A A W Baecker


A novel solvent penetration assessment technique for wood preservativation treatments using waterborne systems
1990 - IRG/WP 2346
Solvent and hence solute (a.i.) penetration during any wood preservation treatment cycle and the flow pathways taken by the solvent in the wood are crucial elements in determining the adequacy of any treatment. Inadequate solvent penetration into specimens or an inappropriate tissue throughflow pattern during impregnation will markedly affect the distribution pattern achieved by many non-diffusibl...
A J Pendlebury, J Coetzee, E Sorfa, A Botha


Influence of felling time on the natural durability of norway spruce (Picea abies (L.) Karst.)
1998 - IRG/WP 98-10250
Natural durability was tested in a laboratory test according to EN 113. The test fungi were Coniophora puteana and Poria placenta. Additionally, the test method was modified by using water agar instead of malt agar, so that wood was the only nutrient source for the fungi. In a third attempt the samples were inoculated with Trichoderma harzianum before testing. The trees were felled on the 22.7.97...
M Hirmke, K Messner, J Fellner, A Teischinger, R Wimmer


The use of spruce for transmission poles
1973 - IRG/WP 326
A series of preservative treatments with creosote using Lowry and Rueping schedules was undertaken. From these treatments the most suitable impregnation conditions for water stored Sitka spruce (Picea sitchensis) and Norway spruce (Picea abies) transmission poles were determined. Preservative distribution and permeability values for poles of both species were used to decide the optimum season and ...
J A Dunleavy, D J Balfe, J P Prendergast


Studies on the permeability of Norway spruce (Picea abies)
1987 - IRG/WP 2295
It is well known that the bordered pits play a dominating role for liquid transport in softwoods. The mechanism behind pit aspiration during drying or heartwood formation seems to be well understood. The reason why the fixation of the membrane (torus) to the pit opening remains almost irreversible is, however, still unclear. A technique has been developed combining so-called "solvent exchange dryi...
I Johansson, K Nordman-Edberg


The comparative resistance to fungi of the wood munika (Pinus heldreichii Christ.), fir (Abies alba Mill.) and spruce (Picea excelsa Poir.) compared with Pinus sylvestris L. and some physical and mechanical characteristics of munika
1981 - IRG/WP 1129
The munika (Pinus heldreichii Christ.) is situated primarily in the Balkans, and partially in the south of the Apenine peninsula. As an endemic species, with a very little annual increment, it has not been used enough as a timber for mechanical conversion up till now, although the oldest trees can grow to 27 m in height, with a diameter at breast height of about 60 cm. According to data of many Ba...
M Petrovic, M Miric


Field and greenhouse testing of window joinery of pine and spruce treated with LOSP
1991 - IRG/WP 3658
Norwegian window frame components of full size were double vacuum-treated with TBTN and TBTO, and connected as 'L-joints' and subsequently coated with stains. The corner sections were exposed (out of ground contact) both in field (temperated coastal climate, Taastrup, Denmark) and in a greenhouse (Uppsala, Sweden). The window frame L-joints of spruce (Picea abies Karst.) - treate...
F G Evans, B Henningsson, E Borsholt


The effect of pretreatments on the impregnation of air-dried sawn Belgian spruce
1988 - IRG/WP 3490
In general the impregnation of airdried spruce results in a variable treatment and limited penetration. This is the result of pit aspiration that occurs during drying of the spruce sapwood and heartwood. Spruce timber is becoming of greater importance in Belgium and hence research for better treatment of this vulnerable wood species is needed. Squared airdried timber of different dimensions were e...
J Van Acker, M Stevens


Leachability of didecyldimethylammonium chloride (a quaternary ammonium compound) from four wood species
1982 - IRG/WP 3204
Sapwood blocks prepared from red pine, ponderosa pine, southern yellow pine and hem-fir (a commercial mixture of western hemlock and amabilis fir) were treated with didecyldimethylammonium chloride, (an alkylammonium compound, AAC). After oven drying the blocks were vacuum impregnated with distilled water and subjected to a static leach cycle for 48 hours. The leachate was analyzed and the amount ...
J N R Ruddick, A R H Sam


The effect of water storage on the cell-structure of Sitka spruce (Picea sitchensis) with reference to its permeability and preservation
1970 - IRG/WP III 3A
Commercial treatment trials with full sized transmission poles have shown that water storage considerably improves the permeability of Sitka and Norway spruce. These results were confirmed by laboratory measurements which showed that in the sapwood of ponded Sitka spruce there is a vast improvement in permeability in all three grain directions. Heartwood permeability does not seem to be affected t...
J A Dunleavy, A J McQuire


Field evaluation of CCA movement in sap-displaced copper chrome arsenic treated softwood poles
1989 - IRG/WP 3539
Commercial sap-displaced UK grown Scots and Corsican pine, and Sitka and Norway spruce poles were exposed in a field site at Dundee, Scotland and radial distribution profiles of CCA monitored prior to implantation and after subsequent field exposure. Results show that groundline levels of all preservative elements were higher after 1 and 2 years field exposure compared with those recorded prior to...
S D Hainey, G M Smith, A Bruce, P D Evans, B King, H J Staines


Investigation of the suitability of silver fir (Abies alba Mill.) for thermal modification
2004 - IRG/WP 04-40275
In this study the suitability of silver fir (Abies alba Mill.) was examined for thermal modification. Comparative experimental investigations were performed with silver fir and Norway spruce (Picea abies Karst.) after thermal treatments. Besides properties, which characterize the quality of heat treatments, like dimensional stability and resistance against fungal attack, strength properties of the...
C Brischke, A O Rapp


The effect of rate of pressure application on preservative uptake along and across the grain of fir (Abies bornmulleriana Mattf.) at different ramp and constant pressure times
2004 - IRG/WP 04-20292
This study was particularly design to determine the preservative uptake at different ramp (rate of increase in pressure) and constant pressure times on longitudinal, tangential and radial penetrations of fir (Abies bornmulleriana Mattf.) which grown indigeneously in Turkey. The samples of 2 cm cubes of kiln-dried wood (nominated to 12% moisture content) were treated at different ramp times varied ...
I Usta


The improvement of wood durability by retification process
1993 - IRG/WP 93-40015
A material with new properties is obtained by retification process. It consists of a light pyrolysis of wood which becomes more stable and especially more resistant to fungal attack with few decrease of mechanical properties. Tests were carried out on three susceptible wood species (Poplar, Spruce, Fir) that are used in construction and are difficult to treat with wood preservatives. Retified wood...
D Dirol, R Guyonnet


Preservative treatment of wood by diffusion processes - Simulation of commercial treatment processes
1988 - IRG/WP 3498
Spruce (Picea abies), Scots pine (Pinus sylvestris) and birch (Betula pendula) were preservative treated by diffusion with mixtures of copper sulphate and arsenic pentoxide. The preservative was fixed after a suitable diffusion storage period by soaking in ammonia solution. A high standard of treatment could be achieved in spruce sapwood. This was attributed to its low wood density, and high wood ...
P Vinden


Persistance of active ingredients in treated wood
1993 - IRG/WP 93-50001-20
Disposing of chemically protected waste wood implies the distinction between surface and pressure treatment. Considering that barked round-wood merely contains, after 7 months open storage, less than 30 g per ton of bark or 25 mg per ton of sapwood, depending on the type of insecticide, the bark or sapwood shavings may be incinerated normally, according to less severe legal prescriptions than for ...
E Graf, P Manser, S Rezzonico, B Zgraggen


Investigations of the treatability of various commercially significant Turkish timbers
1976 - IRG/WP 370 E
Timbers which naturally deteriorate quickly can only be used commercially when their life is increased by the use of chemical treatments. The treatment of the timber can only be planned on a regular basis when the treatability of the wood is known. The purpose of the experiments was therefore to determine to what extent the various types of wood could be sufficiently impregnated. The question of t...
R Ilhan


Evaluation of teak sawdayst Tectona grandis L Fil as a potential source to obtain a natural wood preservative in Colombia
2004 - IRG/WP 04-30356
Plantation Teak (Tectona grandis L. Fil) has been tested as a possible source of natural wood preservatives due to the known excellent durability of old-growth teak wood. Field tests (ground proximity termite and above ground simulated decking exposures) were established in Colombia in April 2003 at two different test sites with different climates (Tropical Dry and Rain forest). Teak heartwood ex...
A Castillo, Y Cabrera, A F Preston, R Morris


Färbeverfahren zur Unterscheidung von Holzzonen mit unterschiedlichem Absorptionsvermögen, insbesondere bei Fichtenholz (Picea abies Karst.). [Staining method for distinguishing zones of wood with different absorption behaviour, particularly in spruce (Picea abies Karst.)]
1980 - IRG/WP 3163
A simple regressive staining method for crosscut wood surfaces is described. Phloroglucinol-hydrochloric acid serves as stain; flowing water and a solution of sodium carbonate are used for development and fixation of a picture showing the differences of absorption. Hydrophobic zones and, contrary to this, zones with a high water content can also be shown. Comparing green spruce wood before and dur...
S Cymorek


Sawn timber of fir (Abies alba Mill.) - Treatability and usability for the Hazard Classes 3 and 4
1999 - IRG/WP 99-40147
Within a national research project, tests on the treatability on sawn timber of fir (Abies alba Mill.) in oscillation pressure, vacuum pressure and double-vacuum processes have been worked out with 95 trunks taken from 3 different altitude levels (up to a height of 590 metres, 600 to 990 metres and over 1000 metres) and from 4 different regions of Switzerland. As the treatability of round wood can...
E Graf, T Bör


Influence of surface coating on the leachability of boric acid and bifluorides from spruce wood
1995 - IRG/WP 95-50050
In the Netherlands, window joinery made from non-durable timber species (spruce) are widely protected with preservative rods. These rods contain non-fixing wood preservatives (e.g. bifluorides or boric acid). This reseach was performed to show the possible influence of a coating system to hinder the leaching of the active ingredients. The results of the leaching tests show, that bifluorides and ev...
W J Homan, H Militz


Soft-rot in Tabebuia sp. wood used in water cooling tower: identification and degradation capacity of the fungi
1998 - IRG/WP 98-10253
Tabebuia sp. (ipe), a native Brazilian wood, is considered of high natural resistance to decaying fungi, and has been used in harsh environments, as cooling towers. Fifty-one fungi, belonging to mitosporic fungi group (Fungi Imperfecti), were isolated from deteriorated Tabebuia sp. wood samples, collected from the mist eliminator and packing of a cooling tower in operation for about 23 years. The ...
S Brazolin, M Tomazello, I H Schoenlein-Crusius


Marine wood-borer test with preservatives on the coasts of Turkey
1995 - IRG/WP 95-10091
Marine wood-borer tests were carried out on the coasts of Turkey (Marmara, Mediterranean Sea and Black Sea). Sapwood blocks of 8 x 15 x 30 cm³ in size from Scots pine, Bornmüller's fir oriental beech and sessile oak were used. The test blocks were treated with CCB-salts by full cell process and coal tar creosote by empty cell process. The test blocks were installed on exposure sites bef...
A Bobat