Your search resulted in 61 documents. Displaying 25 entries per page.


Testing of alkylammonium compounds
1981 - IRG/WP 2152
Following laboratory soil block tests which showed that Bardac 20 possessed a fungicidal threshold similar to that of chromated copper arsenate, treated ponderosa pine sapwood stakes were installed in a field test site near Vancouver, Canada. Two years after installation all the stakes show signs of fungal degradation. Seven stakes have been removed from the test due to total loss of strength afte...
J N R Ruddick


Effects of various preservative treatments on the mechanical and physical properties of plywood
1993 - IRG/WP 93-40007
The technical properties of plywood are related to both the intrinsic characteristics of its composing wood species and the quality and performance of the glue bond which acts as an interface between veneer sheets. Consequently mechanical and physical testing and glue bond strength analysis offer an appropriate means for studying the effect of preservative treatments on the overall quality of plyw...
J Van Acker, M Stevens


The 1999-2000 annual report for the IRG - Wood Preservation in Egypt
2000 - IRG/WP 00-40188
The wood destroying insects in Egypt are belonging to several families of Coleoptera, Lepidoptera and Isoptera. Imported woods are treated by The Agricultural Quarantine or the authorized companies. The materials used for protection as pre-treatment are the same of the treatment. They are Bromide methyl, copper or fluoride salts, organo-phosphorus compounds, pyrethroides, creosote or creosodial. A...
S I M Moein


Effectiveness and synergistic effects between copper and polymer betaine
1996 - IRG/WP 96-30097
Different formulations of "Copper Amine" and Polymer Betaine were studied. During laboratory tests a synergism between both active ingredients against soft rot and dry rot has been found. The efficacy against soft rot according to the "BAM method" and the European Standard ENV 807 depends only on the amount of copper. Long term tests in a fungus cellar for determining the relative protective effec...
H Härtner, V Barth


The influence of previous anti-blue-stain preservative treatments on the fixation of CC in spruce
1997 - IRG/WP 97-30134
Freshly cut and kiln dried spruce boards were treated with 4 different anti-blue stain preservatives (ABP). After a period of 10 days allowing the samples to dry and fixate, the samples were treated with CC (chromium, copper formulation) using a vacuum pressure cycle. After impregnation the wood was steam fixed. A submersion leaching test showed differences in the leachable quantity of copper and ...
M Van der Zee, W J Homan


Absorption of inorganic salts solutions. Retentions of inorganic salts. Fire retardants
1990 - IRG/WP 3625
The study aims evaluated the impregnation capacity using fire retardants on woods with differents densities. At the same time, impregnation with several fire retardant salts were carried out in order to obtain their absortion and retention in wood....
A Garcia, J Navarro


Contribution of wood components on the absorption of copper amine
2000 - IRG/WP 00-30216
The contribution of wood components on the absorption of copper amine was investigated. Holocellulose, lignin and xylan absorbed significant amount of copper. The amount of copper absorbed by cellulose was almost negligible. The removal of extractive also decreased the amount of copper absorption. This study clearly indicates the importance of lignin, hemicellulose in the absorption of copper amin...
D P Kamdem, Jun Zhang


The preliminary evaluation of selected sulfonium salts for use in wood preservation
1984 - IRG/WP 3278
Five sulfonium compounds, including two sulfonium methosulfates, one sulfonium bromide and two amphoteric sulfonium propanesulfonates, were prepared in crude form and subjected to various biocidal screening tests. A rapid screening test in which treated Pinus radiata pulp pellets were exposed to one of three wood-decaying fungi growing on malt agar revealed that dodecyl dimethyl sulfonium methosul...
D V Plackett


Antifungal properties of new quaternary ammonium and imidazolium salts against wood decay, staining and mould fungi
2004 - IRG/WP 04-30347
The biological activity of twenty-four potential wood preservatives – imidazolium and quaternary ammonium salts with a modified anion structure was determined employing screening agar-plate and agar-block methods. Experiments were carried out on Scots pine (Pinus sylvestris L.) wood. The aim of the performed studies was to investigate the effect of structure modification of IC and QAC with organ...
J Zabielska-Matejuk, W Wieczorek


The use of plastic meshes in soft rot monoculture testing
1990 - IRG/WP 2353
Plastic meshes were introduced between the wood blocks and agar medium in a miniaturised soft rot monoculture test in order to minimise transfer of the preservative from the wood and mineral salts from the agar. Although several different sizes and types of mesh were used and the blocks were wetted up to an appropriate moisture content for soft rot attack the amount of decay was substantially redu...
S M Gray


Summaries of two Russian papers received from Professor Dr. D.A. Belenkov and V.A. Seletskaya of the Ural Forest Engineering Institute, Sibirsky Trakt, 37, Sverdlovsk, USSR, on the toxicity to Coniophora cerebella of salts of hydrofluoric acid and some fluoroborates
1977 - IRG/WP 298
1) Evaluation of the toxicity of some salts of hydrofluoric acid against the house cellar fungus (Coniophora cerebella Schroet) Data are presented on the method of probability evaluation of the toxicity of the fluorides of sodium, ammonium, potassium, zinc and iron. On the retention of fluorine in wood all salts, except iron, possess practically equal toxicity at the standard level of the probability of the protection of the wood - 0.95 . There is good agreement between the analytically and graphically determined dose level. Evidence is given for dose variabitility, probabilities of wood protection at 0.5 and 0.95, the curve of efficacy - activity and the construction of the empirical probit graph. 2) Investigation of the toxicity of some borofluorides towards the house cellar fungus Probability evaluation of the toxicity of borofluorides against the cellar fungus, and probit analysis evidence show that toxicity decreases in the sequence sodium borofluoride, copper borofluoride, tributyltin borofluoride. The effectiveness of protection method is able to evaluate the amount of fluorine and boron required in the wood.
C Grant


Effectiveness of copper/chromium salts as wood preservatives against Limnoria tripunctata Menzies in laboratory tests
1977 - IRG/WP 431
During the last joint meeting of IRG and COIPM a co-operative programme of tests with copper/chromium salts as wood preservatives against marine borers was discussed and agreed. In this connection the results of a laboratory test in the BAM with Limnoria tripunctata Menzies will be of interest. But as the respective paper is written in German (H. Kühne; G. Becker: Laboratoriumsversuche über die ...
H Kühne


Evaluation of the corrosivity of the treated wood - Laboratory vs field test methodologies
2000 - IRG/WP 00-20211
The corrosivity of treated wood to fasteners has been evaluated using laboratory test procedures, including AWPA Standard E12-94. The standard method was modified in order to allow detailed study of commercial metal fasteners in terms of sample types, installation configuration and exposure conditions. Parallel field tests were also performed. The experimental results generated from these tests su...
L Jin, A F Preston


Fungicidal efficacy of some dimethyldithiocarbamates, dymethylaminopropionitrile and some salts of S-substituted thioglycolic acid
1998 - IRG/WP 98-30180
Screening for fungicidal activity against Trametes versicolor and Coniophora puteana of the following compounds was performed: sodium N,N-dimethyldithiocarbamate, dimethylalkylammonium (C12-C14) N,N-dimethyldithiocarbamate, benzyldimethylalkylammonium (C12-C14) N,N-dimethyldithiocarbamate, N,N-dimethylaminopropionitrile and ammonium, copper and zinc salts of N,N-dimethyldithiocarbamoylacetic acid....
M Petric, F Pohleven, M Humar, U Kolman


Preservative-efficacy of boric acid-triethanol amine solution against wood-decay fungi
1994 - IRG/WP 94-30050
Laboratory preservative-efficacy tests were conducted using boric acid-triethanol amine (BTEA) solution in accordance with the JIS A 9201 (1991) test method excluding the standard weathering process. Sapwood specimens of Picea jezoensis or Fagus crenata to achieve nominal retentions of 0.40-41.2 kg/m³ of boric acid were exposed to Tyromyces palustris, Coriolus versicolor, Serpula lacrymans or Cha...
S Doi, M Mori, Y Mineki


Pentachlorophenol, its salts and esters; UK review of its uses in wood preservation and surface biocides
1995 - IRG/WP 95-50040-27
The review on pentachlorophenol was undertaken by the Health and Safety Executive on behalf of the independent Advisory Committee on Pesticides in response to the 9th Amendment to the Marketing and Use Directive. The high toxicity to man and the environment was noted and the associated risks were assessed. The Cornmittee concluded that the potential carcinogenicity was probably via a non-genotoxic...
M Fitzpatrick, C Mackie


Adsorption of ACQ and CuMEA Wood Preservatives in Red pine
2005 - IRG/WP 05-30374
The rates of stabilization or fixation of ACQ subcomponents (CuO, DDAC and MEA) in red pine (Pinus resinosa) were compared for different solution concentrations (0.75%, 1.5%, 2.25% and 3% ACQ-D) and post treatment conditioning temperatures. Preservative solutions were impregnated into red pine sapwood by a full-cell treatment. Copper and MEA adsorptions from copper monoethanolamine solutions witho...
C Tascioglu, P A Cooper, Y T Ung


Evaluating the potential of amine chemicals for use as wood protecting agents. Part 1: Investigation of cation components of quaternary ammonium compounds
1994 - IRG/WP 94-30049
Quaternary ammonium compounds (quats) have shown a great potential as more environmentally acceptable wood preservatives. In order to identify chemicals possessing the wood protecting potential, an evaluation was carried out of a range of commercially available 'quats', using a modified soil block test. Ponderosa pine sapwood blocks were treated with selected 'quat&a...
Hang Tang, J N R Ruddick


Tests with ammoniacal copper and alkyl ammonium compounds as wood preservatives
1984 - IRG/WP 3299
Formulations based on copper and alkyl ammonium compounds in ammonia solution have been tested in a fungus cellar on Pinus radiata and Fagus sylvatica. This type of products gives promising results as wood preservatives, especially on hardwood and are safe to destroy by e.g. combustion. The best results were achieved with a dialkyl ammonium compound, Cu/octyldecyl dimethyl ammonium chloride (NH3)....
C-E Sundman


Marine trials with water-borne salts and organotin compound
1986 - IRG/WP 4128
Pinus sylvestris blocks treated with water-borne salts (CCA, CCB, CCF) and organotin compounds (TBTO, TBTCl) were submerged in the sea at Follonica station. The results obtained after 12 years of immersion are presented. The samples treated with CCA, CCB and CCF at the lowest concentration (2%) were destroyed after 7-9 years and the samples treated with CCB and CCF at the highest concentrations (4...
A Gambetta, E Orlandi


The relationship between the electrical resistance and fixation of water-borne CCA salts and pressure-treated wood
1991 - IRG/WP 3657
Two investigations at 22°C and 30°C have been carried out. The electrical resistance in the treated wood and chemical analyses of the remaining amount of unfixed copper, chromium and arsenic were investigated. Samples impregnated with water were used as references. To hold the samples moist during the investigation, each sample was wrapped in a polyethylene plastic foil immediately after impregn...
F G Evans, B Nossen


Influence of carboxylic acids on LEACHING of copper amine based preservatives
2005 - IRG/WP 05-30365
The importance of chromium free preservatives is increasing. Leaching of copper from wood preserved with such solutions is still higher compared to leaching from wood impregnated with copper chromium ones. In order to decrease leaching, different carboxylic acids (octanoic, 2-etilheksanoic, decanoic) were added to copper/amine/boron aqueous solutions. Experiment of leaching of copper from Norway s...
M Humar, P Kalan, F Pohleven


Disproportionate absorption of different constituents of CCA salts
1988 - IRG/WP 3484
Results of preliminary experiments carried out to study selective absorption of different constituents of CCA salts and sludge formation in commercial treatment, using Terminalia myriocarpa and Pinus kesia timbers, are reported in this paper. The objective of these experiments is to evolve simple and practical methods to prevent/minimise sludge formation and differential absorption of the constitu...
V R Sonti, S Sonti, B Chatterjee


Determination of the amine to copper ratio remaining in wood after leaching
2002 - IRG/WP 02-30285
The effectiveness of the protection and the environmental impact of the treated wood are two of the most important aspects that need to be understood for all preservatives. Both are particularly influenced by the loss of biocidal components from treated wood. For amine copper preservatives, copper fixation determines the leaching resistance of the copper and amine compounds formed in wood. Previou...
N Lucas, J N R Ruddick


Weathering of copper-amine treated wood
2000 - IRG/WP 00-40155
Copper ethanolamine (Cu-EA) treated southern pine (SP) were artificially weathered with a QUV Weathering Tester. The weathering regime was composed of a continuous UV-light irradiation for 2 hours followed by a water spray for 18 minutes for a total time of 1200 hours. The changes on the surface of the weathered samples were characterized by Fourier transform infrared spectroscopy (FTIR) analysis,...