IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 373 documents. Displaying 25 entries per page.


Laboratory test of blue stain control by chemicals
2007 - IRG/WP 07-30430
8 chemicals and some mixtures against Botryodiplodia theobromae Pat., Fusarium verticillioides(Sacc.)Nirenberg, Trichoderma harzianum Rifai, Trichoderma viride Pers., and Penicillium purpurogenum Stoll were conducted in laboratory by inhibition zone in the paper. The results were shown that: CBZ and benomyl as well as copper oxine alone are much high efficacy for inhibiting most of the 5 fungi tha...
Zhijuan Wang, Zehui Jiang, Mingliang Jiang, Chungen Piao


Mold resistance of heat-treated wood
2007 - IRG/WP 07-40358
The resistance of heat-treated sugi sapwood against three mold fungi was evaluated. Wood specimens were first subjected to heat treatments at 180 and 220ºC for 2 and 4 hours. Mold growth on the surface of the specimens was measured 1, 2, 4 and 6 weeks after the inoculation with the fungi in laboratory conditions. Laboratory decay tests were performed using two brown and white-rot fungi along with...
S N Kartal


The effects of chemical modification on the biological properties of alder and spruce particleboards
2007 - IRG/WP 07-40363
This study is evaluated by measuring the weight loss, and the ability of white and brown-rot fungi to attack unmodified and modified particleboards manufactured using spruce (Picea orientalis (L.) Link.) and alder (Alnus glutinosa) chips. The chips were reacted with acetic, succinic, maleic and phthalic anhydride at constant temperature for 3 hours then, hot pressed at 150 °C by using phenol for...
Ü C Yildiz, E Dizman, S Yildiz, A Temiz, M Aslan, E D Gezer


Detection of Anti-Fungal Sapwood Extractives in Non-Durable Scots Pine (Pinus sylvestris), Rubberwood (Hevea brasiliensis) and Jelutong (Dyera costulata)
2007 - IRG/WP 07-10634
A general laboratory bioassay method of Woodward and Pearce (1985) was adopted to detect anti-fungal activity of sapwood or heartwood extractives of 5 Malaysian hardwoods [dark red meranti heartwood (Shorea spp.), red balau heartwood (Shorea spp.), kulim heartwood (Scorodocarpus borneensis), jelutong sapwood (Dyera costulata) and rubberwood sapwood (Hevea brasiliensis), including the temperate Pin...
A H H Wong, R B Pearce


Anatomical, physical and chemical changes of Bamboo (Phyllostachys puberscence ) during weathering processes
2008 - IRG/WP 08-10650
Bamboo (Phyllostachys puberscence) culms with 1, 2, 3 year old were exposed to natural weathering condition in Gwangju, Korea for 12 months. Changes in color, surface topography, strength and chemical properties were investigated using various microscopic and instrumental techniques. After one year’s weathering, the color of bamboo became lighter but strengths of bamboo did not change significan...
Jong Sik Kim, Kwang Ho Lee, Mi Young Cha, Yoon Soo Kim


Whole-of-house protection from subterranean termite attack and damage after four years of field exposure
2008 - IRG/WP 08-10665
This study reports the condition of the whole-of-house termite protection test in tropical Australia after four years. The study was designed to provide maximum protection to whole-of-house timbers in a natural situation posing the highest hazard from subterranean termite populations. The houses were constructed either on concrete slabs or suspended floors using untreated and treated timber fram...
B M Ahmed (Shiday), J R J French, S R Przewloka, P Vinden, J Hann, C Y Adam


Chemical Analysis in Production Quality Control at Wood Treatment Plants
2008 - IRG/WP 08-20396
Analysis methods for quality control analysis in wood treatment plants have evolved with the changes in treatment preservative chemistries and analytical instrument technology. The basic hydrometer specific gravity measurements used for solution strength and classic wet chemistry methods for wood have given way to instrumental techniques such as X-ray fluorescence, automatic titrator, and HPLC. No...
P Walcheski, L Jin


Vacuum drying of European oakwood: Color, chemistry and anti-oxidant potency of wood. Improving appearance in forest value added products
2008 - IRG/WP 08-40432
In hardwoods used for decorative and appearance purposes, wood colour is one of the most important factors of wood quality; in addition colour is related with durability and biological decay of wood. Wood discolouration during drying is mainly affected by heat, light, physiological reactions, combinations of reactions, biochemical and chemical reactions, and micro-organisms attack. In freshly fell...
S Sandoval, W Jomaa, F Marc, J-R Puiggali


Chemical modification of Scots Pine Sawdust by mixed anhydrides
2008 - IRG/WP 08-40439
By making react mixtures containing acetic-fatty anhydrides on Scots pine sawdust (SPS) without any solvent or catalyst; we synthesized mixed acetic-fatty esters of SPS. Such mixtures were synthesized by reaction between a carboxylic acid and acetic anhydride. These mixtures were obtained after reaction of acetic anhydride and a fatty acid that yields at equilibrium a mixture of five compounds: ac...
J Peydecastaing, E Borredon, S El Kasmi


Effect of different ASAs (alkenyl succinic anhydrides) on the treatment of biological protection of wood in use class 4
2008 - IRG/WP 08-40440
The alkenyl suscinic anhydrides (ASAs) used in this work are adducts resulting from the maleinization reaction of fatty acid alkyl esters. Various products with different alkyl groups were synthesized from rapeseed (Brassica napus) oil esters, rich in oleic acid. The liquids obtained showed a viscosity similar to that of vegetable oils and a brown color. When applied into wood, a thermal treatment...
C Vaca-Garcia, O Pignolet


Mechanical and chemical properties of blue stained wood
2009 - IRG/WP 09-10686
Discoloration of wood is frequently caused by blue-staining fungi. In the previous researches there was general opinion that blue-stain fungi do not influence mechanical properties. On the other hand, there were some opposite results reported as well. In order to elucidate this issue, specimens made of Pinus sylvestris sapwood were exposed to two the most frequent and important blue stain fungi Au...
M Humar, V Vek, B Bučar


Discovering anti-fungal agents in New Zealand native plants for use in wood protection
2009 - IRG/WP 09-10692
Extracts from Hinau (Elaeocarpus dentatus) leaves were tested in the laboratory for antifungal activity. In addition, the anatomical structure of the leaf was also examined by a combination of light and scanning electron microscopy. Chemical characterisation of the extracts and investigation into potential use of its components for wood protection is underway. A combination of light microscopy (...
C Rickard, T Singh, A Singh, R Newman


Use of biological and low toxicity products against subterranean termites
2009 - IRG/WP 09-20410
The climatology of Mediterranean countries is favourable to the development of termites that cause important damage to wood structures in both furniture and buildings. Until a few years ago the treatment for this type of insect was based on the impregnation of the wood with chemical products. The use of these chemicals is now being restricted in Europe since the publication and harmonization of n...
M T Troya, M J Prieto, F Rubio


Evaluation of Water Repellency of Treated Wood Using Several Alternative Methods
2009 - IRG/WP 09-20419
In this study, the results of water repellency testing using a digital swellometer method for water-borne organic-preservative systems with water repellent additives are reported. The findings suggest that the traditional method of using matched untreated controls as a reference developed from historic solvent-based treatments for determination anti-swelling efficacy (ASE) may underestimate the a...
L Jin, A F Preston


Synthesis of a rosin amide and its resistance to wood decay fungi
2009 - IRG/WP 09-30517
Rosin was reacted with diethyltriamine (DETA) after being modified by acryl acid with the weight ratio of 4.5:1 and a rosin amide (RA) derivative was produced at the conditions as follows: modified rosin and DETA mole ratio of 1:3.5, dimethylbenzene as water carrying agent, reaction temperature of 160-180°C, and reaction time of 8h. The chemical structure of the product as RA was identified by F...
Shuangyue Li, Shujun Li, Jing Wang


Modification of Wood by a Water-Repellent Compound Used in the Textile Industry: Boron Release and Termite Resistance
2009 - IRG/WP 09-40447
In the study, wood specimens were treated with disodium octoborate tetrahydrate (DOT) and a commercial water and oil repellent compound, FORGUARD M®, a weak cationic emulsion containing dipropylene glycol monomethylether, water and solids in its formulation and used in the textile industry. There were two different processes for preservative treatments: double and single treatments. The leaching ...
S N Kartal, E Terzi, B Erilkun, Y Imamura


Wettability and bonding strength of wood thermally-treated with different combinations of soy oil and chemical additives
2009 - IRG/WP 09-40454
Thermal treatment is a method which has gained wider acceptability as an alternative to the chemical treatment in wood preservation. In order to maximize the benefits of this technique several options have been adopted including the use of soy oil in transferring the heat to the wood. Available information on thermal treatment in general and the oil method in particular show that there are still n...
L Awoyemi, P A Cooper, T Ung


Investigation of chemical changes in acetylated beech wood during weathering
2009 - IRG/WP 09-40460
In this study Beech wood (Fagus orientalis) acetylated and has been subjected to a variety of artificial weathering conditions (water only, light only, water and light together)in difference times (0,50,150 and 300 h), then wood surface analyzed using Fourier Transform Infrared spectroscopy (FTIR).Results shown that weathering process affected the functional groups on the wood surface. Light and w...
M Akhtari, M Arefkhani


The effect of chemical changes on the wood-moisture relationships in thermally-modified wood
2009 - IRG/WP 09-40473
Small specimens of three wood species were thermally modified following twenty schedules in the 190-245°C temperature range for treatment times between 0.3 and 16 h. Five wood-moisture relations were subsequently determined, namely: anti-swelling efficiency (ASE), movement, hygroscopicity (adsorption and desorption), transversal swelling (radial and tangential directions), and equilibrium moistur...
M M González-Peña, M D C Hale


Chemical mediated depolymerization of cotton cellulose for the understanding of non-enzymatic fungal decay
2010 - IRG/WP 10-10731
Small, low molecular weight non-enzymatic compounds have been linked to the early stages of brown rot decay as the enzymes involved with holocellulose degradation are found to be too large to penetrate the S3 layer of intact wood cells. The most pronounced of these which were analyzed in this study are hydrogen peroxide, iron, and oxalic. The compounds related to the Fenton reaction: the combinati...
A C Steenkjær Hastrup, B Jensen, F Green III


Chemical protection of historic timber structures: Results and future needs
2010 - IRG/WP 10-40487
The paper concentrates on the analysis of the effectiveness of chemical protection for timber structures in the Russian State Museums “Kizhi” (Karelia) and “Vitoslavlitsy” (Novgorod). The condition of historic timber was tested at the monuments treated with PCP, borax, potassium carbonate, boric acid, Pinotex chemicals in the 1970-80. Long-term analysis revealed that in many cases the...
M Kisternaya, V Kozlov


Study on the thickness swelling of mould-resistant chemical treated bamboo strand woven outdoor flooring
2010 - IRG/WP 10-40489
To prevent bamboo strand woven flooring from mould, several preservatives were chosen to treat bamboo strand before dipping into adhesives and pressing. The thickness swelling and mould resistant effect of the finished board were studied. Results showed that different preservatives had different influences on the thickness swelling of BSWF, and in order to reduce the thickness swelling of the fini...
Fangli Sun, Binfu Bao, Shenyuan Fu, Anliang Chen


Chapter 7 - Treatment processes of bamboo
2010 - IRG/WP 07-10635-07
For adequate penetration and retention of preservatives in woody bamboos at green, dry, solid and sliced conditions different possible and applied treatment processes have been described along with their classifications. The treated bamboo can be used as building materials; the sufficient treatability ensures its long-term best utilization at ground contact and indoor. All the processes descr...
A K Lahiry


Multilayer hot-press drying and chemical modifying of poplar wood with urea-formaldehyde prepolymer
2011 - IRG/WP 10-40539
The objective of this study was to determine the technology of chemical modifying and multilayer hot-press drying on poplar wood. The chemicals were impregnated into cell lumen space by pulse-dipping machine to improve the dimension stability and mechanical property of timber. The timbers were compressed and dried by the multilayer hot-press drying to increase the density of timber. Results indica...
Guofeng Wu, Yifei Jiang, Sheng Yao, Junwen


Comparative investigations between thermal and microwave assisted digestion as a novel tool for the chemical analysis of inorganic wood preservative components
2011 - IRG/WP 11-20461
The correct chemical impregnation of wood requires an internal as well as external quality control of the treated wood. The active is located in a solid matrix, therefore it is often difficult to analyse such material since most analytical procedures are based on liquid systems. Because of this quite a number of methods – like extraction or thermal digestion - were developed in order to transfer...
H Ahl, J Fromm, E Melcher


Previous Page | Next Page