IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 129 documents. Displaying 25 entries per page.


Soil-bed decay resistance evaluation of strandboards treated with preservative at different points of the manufacture process after 18 months exposure
2002 - IRG/WP 02-40230
Strandboards were treated with a copper-boron water-based preservative at different points of manufacture process namely, green strand diffusion, vacuum, spray application in the resin blender and post manufacture heat and cold quench. Preservative was applied to achieve five different retentions (0, 1.5, 3, 6, 12 kg m-3). The modulus of rupture and modulus of elasticity were assessed before expo...
G J Goroyias, M D C Hale


Temperature and pressure inside wood during creosote impregnation
1991 - IRG/WP 3649
Creosote gives the best protection against decay for sleepers and poles. However, it has a major drawback - bleeding. Modified impregnation processes to reduce bleeding have been tried. For developing such processes it is important to know the actual temperature and pressure inside the wood. This paper describes measurement of temperature and pressure inside wood during creosote impregnation. The ...
Ö Bergman


The effect of rate of pressure application on preservative uptake along and across the grain of fir (Abies bornmulleriana Mattf.) at different ramp and constant pressure times
2004 - IRG/WP 04-20292
This study was particularly design to determine the preservative uptake at different ramp (rate of increase in pressure) and constant pressure times on longitudinal, tangential and radial penetrations of fir (Abies bornmulleriana Mattf.) which grown indigeneously in Turkey. The samples of 2 cm cubes of kiln-dried wood (nominated to 12% moisture content) were treated at different ramp times varied ...
I Usta


The improvement of wood durability by retification process
1993 - IRG/WP 93-40015
A material with new properties is obtained by retification process. It consists of a light pyrolysis of wood which becomes more stable and especially more resistant to fungal attack with few decrease of mechanical properties. Tests were carried out on three susceptible wood species (Poplar, Spruce, Fir) that are used in construction and are difficult to treat with wood preservatives. Retified wood...
D Dirol, R Guyonnet


Wood kiln drying. Simple process of material treament or soft method of preservation? (Le séchage arificiel du bois. Simple opération de traitement du metériau ou méthode douce de préservation?)
1993 - IRG/WP 93-50001-14
Among the processes enabling to extend wood durability, kiln drying can be considered as a treatment and soft preservation method. Dry woods are naturally durable provided they are not subject to important retaking of the moisture. Drying thanks to the application of temperatures from 50 to120°C enable to execute a thermic treatment which kills grubs and mushrooms to ensure a sterilization that c...
F More-Chevalier


Controlled envelope treatments of Pinus sapwood, achieved by modifications to impregnation process and carrier solvents
2003 - IRG/WP 03-40258
Specimens of slash pine or radiata pine were treated to a target retention of 0.02% m/m permethrin with conventional light organic solvent fluids or with oil-modified fluids (Tanalith® T). Best achievable envelopes from LOSP fluids were poorly controlled, penetrating not only the target outer 0-5 mm zone (mean 0.019%, RSD 28%), but also breaking through into the 5-10 mm zone (mean 0.013%, RSD 37%...
M J Kennedy, P R S Cobham


Preservative treatment of rubber wood (Hevea brasiliensis) to increase its service life
2005 - IRG/WP 05-40320
Rubber wood (Hevea brasiliensis) possess excellent properties for interior designing, wood working and furniture making. But it is very much susceptible to sap stain and mould fungi which decreases the service life. For profitable uses , it is necessary to increase the service life of rubber wood. To protect the rubber wood from wood degrading agents, the sawn timber were treated with Borax – b...
K Akhter


Practical experiments with Boracol 10 Rh used as a fungicide in the repair process after attack by the dry rot fungus (Serpula lacrymans)
1987 - IRG/WP 3458
The test is carried out in an old house in Nyhavn, Copenhagen. The roof and the walls close to were heavily attacked by dry rot fungus (Serpula lacrymans) because damage to the zinc covering the frontspice were letting in water to the wood and wall construction. An attack by the dry rot fungus is more complicated to repair compared with other wood destroying fungi because beside the damage on wood...
J Bech-Andersen


Step-wise pressure process for reducing surface roughness in Japanese cedar timber
2003 - IRG/WP 03-40256
Sixteen dried sawn-timber (10.5 x 10.5 x 360 cm) were cut into half. The half of them was treated by step-wise pressure process with 2.5 MPa maximum, and the other half was treated by conventional pressure process with 2.5 MPa maximum. Average DDAC preservative absorption was 461 kg/m3 in the former and 525 kg/m3 in the later. Surface roughness was expressed as the profile element height of collap...
K Yamamoto, M Nozoki


Service Life Prediction of Wood Claddings by in-situ Measurement of Wood Moisture Content
2004 - IRG/WP 04-20304
The Danish Technological Institute is in co-operation with industry partners running a project aiming at predicting the service life of different wood protecting systems. The project focuses on examining the moisture reducing effect of different wood claddings and the ability to maintain the appearance of the surfaces, when the wood is used in service class 3. A façade construction is exposed t...
B Lindegaard, N Morsing


Gaseous boron treatments of wood and wood products
1992 - IRG/WP 92-3691
Treatment of wood and wood products by gaseous organoborates has now been under study for about 5 years. This technique has potential for boron treatment of a wide range of substrates from solid wood through to wood composite materials such as particleboard or wet and dry formed fibreboards. The vapour treatment technique is proving to be very flexible in that it can be adapted to integrate into a...
A J Bergervoet, R Burton, K Nasheri, D R Page, P Vinden


Development process of a new anti-sapstain formulation and its present status with the relevant problems
2001 - IRG/WP 01-30257
An anti-sapstain formulation, which contains 2-(thiocyanomethylthio)benzothiazol (TCMTB) and methylene-bis-thiocyanate (MBT) as active ingredients, was developed by a technical agreement with Buckman Laboratories (Memphis, TN, USA) as an alternative to chlorinated phenols for the Japanese market. The formulation was commercialized as BAM 12 years ago. As anti-sapstain treatment is commonly conduct...
K Nobashi, Y Nomura, K Tsunoda


Estimation of the impregnation degree of pine wood by the distribution analysis of active ions concentration in the cross-section
1999 - IRG/WP 99-20174
Samples in the form of pine wood rollers of diversified moisture content of ca. 50, 28 and 12% were impregnated with a water solution of the mixture type CCB with the use of the full-cell process. Moisture content was determined in individual layers from the girth to the pith. In the same way the concentrations of copper and chromium ions with the use of the spectrophotometric method and recalcula...
K Lutomski, B Mazela


The multi-phase pressure (MPP) process. One-stage CCA treatment and accelerated fixation process - The process as a new concept in preservative treatment
1997 - IRG/WP 97-40078
The background to current commercial CCA treatment schedules used in New Zealand and fixation processing is reviewed. The limitations of these conventional practices with respect to treated product quality and CCA solution handling issues are defined. A novel, patented treatment schedule has been developed using a combination of hydraulic and pneumatic pressure phases and hot (~ 75°C) CCA solutio...
K Nasheri, A J Pendlebury, J A Drysdale, H Pearson, M E Hedley


Effect of treatment process on performance of copper-chrome-arsenate. Part 1: Fungus cellar tests
1995 - IRG/WP 95-40045
Pinus radiata sapwood stakes 20 x 20 x 400 mm³ were treated with CCA Type C using a range of concentrations and three treatment processes; Bethell, Lowry and Rueping. Preservative retention was determined by chemical analysis of treated material. Following fixation, fungus cellar stakelets, 5 x 10 x 180 mm³ were cut from treated material and after leaching were exposed in unsterile soil beds in ...
M E Hedley, J Anderson, J B Foster, B E Patterson


Comparison of the anti-fungal efficacy of Cobra with drill perforation on oscillating pressure treated spruce transmission poles -Laboratory test
1988 - IRG/WP 3469
A laboratory method for measuring the depth of penetration of the fungicidal concentrations effective against basidiomycetes (brown rot) was developed. The tests on CCB oscillating pressure treated spruce transmission poles have shown that the depth of salt penetration can be increased by about 10 mm by a drill perforation before the impregnation. An even better penetration is reached, however, if...
E Graf, B Zgraggen


Microwave modification of Yellow Stringybark (Eucalyptus Muelleriana) posts for impregnation with Copper-Chrom-Arsenic (CCA) preservatives
2000 - IRG/WP 00-40185
Yellow Stringybark posts with diameters ranging from 60-100 mm were microwave conditioned using a 60 kW microwave (MW) generator. A substantial improvement in heartwood penetration of preservatives and relaxation of growth stresses was indicated such that there was no split formation following drying of the posts. High preservative absorption of copper-chrome-arsenic (CCA) was achieved ranging fro...
G Torgovnikov, P Vinden


Exterior wood stains
1979 - IRG/WP 3136
The use of semi-transparent exterior wood stains has grown remarkably since their development during the 1960s. This can be partly attributed to their offering a break with tradition at a time when it was being recognised that changes in the quality of timber and how it was used demanded different methods of exterior wood finishing. Information is already available on the characteristics and uses ...
E R Miller


Termite durability of sugi (Cryptomeria japonica) heartwood kiln-dried under high-temperature process in relation to wood extractives
2005 - IRG/WP 05-10547
Termite durability of sugi heartwood samples kiln-dried under a high-temperature process were evaluated by using Reticulitermes speratus (Kolbe) as a test termite sp. The n-hexane extractives of these samples were analysed by a GC technique. The less termite durability was shown on the wood samples dried under the high-temperature process, in comparison with that of the air-dried samples. No GC-p...
S Shibutani, E Obataya, K Hanata, S Doi


Microdistribution of water-borne preservatives in blue gum treated by full-cell process
1990 - IRG/WP 3617
The present work deals with the study of the microdistribution of copper, chrome and arsenic elements in Eucalyptus globulus Labill. sapwood, treated with a CCA water-borne preservative by full-cell process, with the help of scanning electron microscopy together with energy dispersion X-ray analysis technique. The work shows that the retention of CCA elements is high in vessels and vasicentric par...
D De Sousa Castro Reimão, J M Palacios


Multiple-Phase Pressure (MPP) Process: One-stage CCA treatment and accelerated fixation process. 4. MPP compared with other processes for achieving acceptable treatment of radiata pine heartwood
1998 - IRG/WP 98-40115
Although radiata pine sapwood is very amenable to preservative treatment, it is often difficult to achieve the required standard for heartwood treatment. A preliminary investigation showed that to achieve the NZ Timber Preservation Council minimum penetration requirements for radiata pine heartwood using the Multiple-Phase Pressure (MPP) Process, a hydraulic pressure of at least 1250 kPa for 20 m...
K Nasheri, J A Drysdale, G Durbin, M E Hedley


Gaseous preservative treatment of wood
1990 - IRG/WP 3631
A recent development in processing wood with a gaseous preservative means that dry, treated wood can be produced in under 30 hours with the benefits of product diversification, faster stock turnover and the ability to respond to short term demand. About 400,000 m³ of wood are treated each year in New Zealand with boron salts to protect from borer infestation. Traditionally this treatment is effec...
R Burton, A J Bergervoet, K Nasheri, P Vinden, D R Page


Environmental characterisation of retification process by-products (liquid and gaseous wastes)
2005 - IRG/WP 05-50224-10
In order to reduce environmental risks during the service life of the treated wood and to find new alternative developments on the durability of wood, some research and technology development have been made on thermal treatment. The retification process is one of these processes. The retification process induces chemical modification of the lignin and cellulosic components and modifies the intrins...
G Labat, E Bucket, S Legay, C Yriex, P Marchal, E Raphalen, M Vernois, R Guyonnet, H Besset, E Fredon), G Vilarem, L Rigal, C Raynaud


Wood preservatives treatment of black spruce
1997 - IRG/WP 97-40092
A representative sample of black spruce logs from Central Newfoundland was harvested and processed to dressed 2"x4" lumber. Over 400 pieces of lumber were then incised and treated with ACQ preservative in a semi-industrial retort. 9 charges of 20 samples were used to determine treating parameters and 11 charges of 20 pieces were treated using the optimized process. This material was inspected by a...
A R Zahora, J P Hösli


Detoxification of salt impregnated wood by organic acids in a pulping process
1993 - IRG/WP 93-50012
The paper descibes a novel method to detoxify pine wood (Pinus silvestris L.) treated with CCB-, CCF- CC-, and Cu-HDO-type salt preservatives. In the process of biological detoxification organic acids produced by strains of Antrodia vaillantii and other brown rot fungi are used for the dissolution of the previously fixed inorganic compounds. These findings are the basis for applying an acid pulpin...
I Stephan, H H Nimz, R D Peek


Previous Page | Next Page