The movement of iron into field test stakes
1987 - IRG/WP 2284
Failed and sacrificial stakes recovered from the Westham Island field test site were examined for their iron content. Varying amounts were recorded, which were greatest in the failed stakes. The possible role of the iron taken up by the below ground portion of the stakes, in accelerating the decay process and/or the preservative leaching is under investigation. The reaction of the iron with the ch...
J N R Ruddick, P I Morris


Modelling of PCP migration in the environment: Feeding the models with laboratory data
1993 - IRG/WP 93-50001-08
In 1989, Hydro-Québec began a study program on pentachlorophenol (PCP) to ensure safe use of the product at all stages. One of the aspects of the study is the creation of a predictive system for evaluating the behavior of PCP and oil migration from wood poles to the environment. This system comprises four mathematical models for predicting PCP and oil migration in and on the surface of the pole, ...
A Besner, P Tétreault, R Gilbert


Système informatisé d'aide à la décision pour la gestion de la migration du pentachlorophénol dans l'environnement
1993 - IRG/WP 93-50001-10
This paper describes a Decision Support System (DSS), concerning pentachlorophenol (PCP) migration in the environment. The principal objectives of the DSS are to assist managers in siting of PCP-treated poles in the Hydro-Québec system and the storage areas and in the treatment of customer complaints. Four mathematical models are incuded in the system: a model simulating migration inside and on t...
G Lefebvre, J-C Tessier


Iron promotes decay capacity of Serpula lacrymans
1993 - IRG/WP 93-10008
The influence of iron and iron compounds on the decay capacity of Serpula lacrymans was studied. Mass losses of pine wood caused by dry rot fungus were increased when FeSO4 was added into the culture medium or when there were iron nails or stone wool on the culture medium. This supports the hypothesis that iron in stone-based building materials is one reason for the increased decay capacity of Ser...
L Paajanen


Migration of active ingredients from treated timber into fresh water
1991 - IRG/WP 3669
Spruce roundwoods and segments were treated with three different wood preservatives. Two of them containing copper and chromium the other one free of chromium. After fixation (3 weeks, 20°C) the specimens were leached by using artifical rain or by shaking the segments for one hour in contact with demineralized water. The water was analysed for the relevant elements of the preservative tested. Lea...
H Klipp, H Willeitner, K Brandt, A Müller-Grimm


Prevention of brown-rot decay by chelators
1992 - IRG/WP 92-1540
In this work the brown-rot decay was shown to be prevented by chelating the endogenous metals existing in wood by using organic or inorganic chelators or iron-binding siderophores. The fungal growth and decaying ability were significantly decreased by the chelating treatments of the solid wood-based culture medium and pine wood pieces, respectively. The transition metals existing in native wood ar...
L Viikari, A-C Ritschkoff


Elimination of alternative explanations for the effect of iron on treated wood
1993 - IRG/WP 93-30006
Amounts of iron which had previously been found in stakes removed from ground contact reduced decay of untreated wood by four brown-rot fungi. This suggested that the effect of iron may be on the preservative. Analysis of the leachates from CCA- and ACA-treated wood blocks first exposed to rusting iron, then to a brown-rot fungus, showed that the increased decay found in the laboratory for wood ex...
P I Morris, J K Ingram, D L Gent


Available iron promotes brown rot of treated wood
1992 - IRG/WP 92-1526
Exposure of treated wood blocks to rusting iron increased the toxic threshold of chromated copper arsenate and ammoniacal copper arsenate to a brown-rot fungus Leucogyrophana sp. This supports the hypothesis that the movement of iron ions into wood contributes to the unexpectedly high decay rate of treated wood at the stake test site at Westham Island BC. To what extent this phenomenon may occur e...
P I Morris


Role of Global Cooperation in Wood Protection for Conserving Forest Resources
2007 - IRG/WP 07-50249
The current uses of treated wood are discussed along with the emerging concerns for continued use of these products. The issues of new chemicals, treatments for wood based composites, migration of chemicals from treated wood, and the disposal of these products at the end of their useful life are all outlined. The potential for the IRG to serve as the focus for research discussion as well as coll...
J J Morrell, G Deroubaix


Non-enzymatic Gloeophyllum trabeum decay mechanisms: Further study
2001 - IRG/WP 01-10395
Information will be presented on the mechanisms involved in, and potential application of, non-enzymatic wood decay by brown rot decay fungi. Specifically, the hypothesized role of low molecular weight phenolate derivatives will be discussed in relation to non-enzymatic degradation of wood. The mechanism of binding of iron by cellulose, and binding and reduction of iron by fungal derivatives and m...
B Goodell, J Jellison


Creosote movement from treated wood immersed in fresh water: Initial PAH migration
2003 - IRG/WP 03-50201
Creosote has a long history of successful use as a wood preservative, but polycyclic aromatic hydrocarbons (PAHs) in this preservative have raised environmental concerns, particularly when creosote-treated wood is used in aquatic environments. A number of models have been developed to predict the risk of creosote use in aquatic environments, but one limitation of these models is a lack of data o...
Sung-Mo Kang, J J Morrell, J Simonsen, S T Lebow


Metal carboxylates for wood pest control
1996 - IRG/WP 96-30109
Metal carboxylates have been used as wood preservatives for more than fifty years. Predominantly salts of naphtenic acids have been commercially applied so far. They have water repellent as well as fungicidal and insecticidal properties. In the last years, metal carboxylates of saturated fatty acids were introduced. Fatty acids with 7-10 carbon atoms already have fungicidal activity by themselves....
F Pohleven, M Petric


Migration of Metals from Douglas-fir Lumber Treated with ACZA or Pentachlorophenol Using Best Management Practices: Preliminary Tests
2005 - IRG/WP 05-50224-4
The potential for migration of preservative components from ammoniacal copper zinc arsenate (ACZA) and pentachlorophenol treated Douglas-fir lumber in non-soil contact exposure was assessed in a simulated rainfall device. Metal levels from ACZA treated wood were elevated for the first 30 minutes of rainfall and then declined sharply. Repeated cycles of rainfall led to declines in initial metal l...
J J Morrell, Hua Chen, J Simonsen


Transmission poles with sub-standard retentions protected by Field Liners outperform standard poles in service
1997 - IRG/WP 97-40095
Eucalyptus cloeziana 12m transmission poles were treated with sub-standard creosote retentions of 80kg/m3 and Field Liners were fitted to the poles before they were placed in service at Umbumbulu, Kwazulu Natal. Poles treated with standard creosote retentions of 130kg/m3 but without Field Liners were also placed in service in the same area. Core samples were taken from both groups of poles after 1...
M R Behr, G D Shelver, A A W Baecker


The effect of low molecular weight chelators on iron chelation and free radical generation as studied by ESR measurement
2000 - IRG/WP 00-10367
The focus of this work was to improve our current knowledge of the non-enzymatic mechanisms involved in brown-rot decay. Electron Spin Resonance (ESR), also known as Electron Paramagnetic Resonance (EPR), is an attractive technique for the identification and study of chemical species containing unpaired electrons (such as radicals and certain transition metal species). ESR spin-trapping techniques...
Yuhui Qian, B Goodell


Wood degradation mechanisms by the brown rot fungus Gloeophyllum trabeum
1997 - IRG/WP 97-10229
A mechanism for the degradation of wood by the brown rot fungus Gloeophyllum trabeum is outlined. The mechanism includes the function of redox-cycling, low molecular weight phenolic derivatives which sequester and reduce iron in acidic environments. The role of oxalate for the sequestration of iron (hydr)oxides and the pH dependent transfer of iron to the G. trabeum phenolic chelators, as well as ...
B Goodell, J Jellison


Iron in stone wool - one reason for the increased growth and decay capacity of Serpula lacrymans
1992 - IRG/WP 92-1537
The chemical compositions of stone wool and glass wool were analysed. There was more iron in the stone wool than in the glass wool. It was found that iron present in stone wool was easily dissolved by oxalic acid that Serpula lacrymans is able to produce. The stone wool promoted the decay of pine wood by Serpula lacrymans. The glass wool had no effect on the decay capacity of Serpula Iacrymans. Th...
L Paajanen, A-C Ritschkoff


Leaching of Arsenic from Mulch Made from Recycled Construction and Demolition Wood
2005 - IRG/WP 05-50232
Mulch made from recycled construction and demolition (C&D) wood has been reported to contain chromated copper arsenate (CCA)-treated wood and potentially release arsenic in the leachate by rainfall. Such recycled wood mulch is commonly masked with iron-oxide colorant, which is known to combine with arsenic. The objective of this study was to evaluate the levels of arsenic leaching from C&...
T Shibata, H M Solo-Gabriele, T G Townsend, B Dubey


Dimension of lysimeters and the evaluation of the migration of wood preservative components in soil
1996 - IRG/WP 96-50065
In the past, investigations concerning the migration behaviour of wood preservatives were made to a minor extent and no uniform methods of test exist. The migration behaviour of CFB was determined using 5 lysimeters of different dimension. The results of the migration and distribution of the anions in the soil showed considerable differences between both ions. Approximately the whole quantity of c...
E Melcher, R-D Peek


Preliminary modelling of methylisothiocyanate movement through Douglas fir transmission poles
1988 - IRG/WP 3466
Methylisothiocyanate is a volatile solid that is the active ingredient of several registered and experimental wood fumigants. Information on the sorption and diffusion of this chemical in Douglas-fir heartwood and sapwood was used to develop a two-dimensional model of fumigant movement within a single horizontal cross-section of a transmission pole. The model indicated that dry wood (14% MC) stron...
A R Zahora, P E Humphrey, J J Morrell


Oxalic acid quantification, oxaloacetase assay and ESI localization of P, C, and Fe from the brown rot fungus Postia placenta
1994 - IRG/WP 94-10063
The mechanism by which brown-rot fungi initiate depolymerization of holocellulose in wood remains unknown. Recently, oxalic acid (OA) has received considerable attention in cellulose breakdown by brown-rot fungi. The OA could serve as a proton donor for hydrolytic or an electron donor for oxidative (Fenton's reaction-H2O2/Fe2+) cleavages of cellulose. The acid may originate via oxaloaceta...
C R Jordan, W V Dashek, T L Highley


Environmental fate of copper-based wood preservatives in different soil substrates - Part 2: Study of the metal sorption and migration potential under simulated rainfall
1998 - IRG/WP 98-50101-21 b
In order to examine the potential environmental impact of spillages of the saltborne wood preservative CCA in treatment plants, four large scale experiments are set-up so as to follow the water transport and ion mobility in various field soils. A plastic container is filled with a sand, silt, clay and potting soil, made up at their respective bulk density and wetted to a given moisture content. U...
G M F Van Eetvelde, R Hartmann, J M Mwangi, H S Öztürk, M Stevens


Field Liners™ prevent creosote migration from transmission poles to soil during service
1996 - IRG/WP 96-40067
A full scale trial utilised 150 12m Eucalyptus grandis transmission poles treated with standard retentions of creosote according to SABS Method 457. One hundred poles had Field Liners™ applied while 50 did not. The 150 poles were used to complete an electricity transmission line in Southern KwaZulu-Natal. After 18 months service, incremental cores were taken from 15 cm below the ground lines of ...
M R Behr, G D Shelver, A A W Baecker


Construction of dhows in Kuwait
1981 - IRG/WP 465
To most people Kuwait means oil and the opulence associated with it, but to the seafarer, Kuwait means Dhows. There are as early references to the Kuwaiti Dhows as the 17th century. The Danish explorer Nebuhr in 1756 described Kuwait as having a work power of 10,000 people and 800 wooden boats involved in fishing, pearl diving, and trade. Dhows might well have been the original carriers of "The Pe...
A S Zainal, M A Ghannoum


A comparison of the migration behaviour in soil of different waterborne wood preservatives and their leachates
1997 - IRG/WP 97-50091
Lysimeter tests were carried out on water-soluble wood preservatives and on wood preservative components leached out of impregnated wood. The purpose of these tests was to determine the extent to which the migration behaviour of environmentally relevant ions in the soil is influenced under comparable conditions. The results clearly show that the groundwater is especially at risk when wood preserva...
E Melcher, R-D Peek