IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 159 documents. Displaying 25 entries per page.


The use of modulus of rupture and modulus of elasticity in natural durability testing
1997 - IRG/WP 97-20117
Losses in weight, losses in bending strength and changes in elastic behaviour were assessed in a fungus cellar test with beech wood stakes (Fagus sylvatica). Results were gained after 8, 12, 16 and 20 weeks resp . The outcomes show, that the non-durable species beech is very rapidly attacked by fungi and loses up to 60% of its initial bending strength even within the first 8 weeks. Earlier researc...
L Machek, H Militz, W Gard


Improvement of wood decay resistance by tannin impregnation
1991 - IRG/WP 2380
The fungical effect of tannins is appraised after exposure of treated woods samples to wood rotting fungi. A screening-test is carried out with several solutions containing extracts of two kinds of tannins; a condensed tannin derived from Quebracho heartwood (Schinopsis sp.) and a hydrolyzable one extracted from chestnut heartwood (Castanea sativa Mill). If a fungicidal action was indeed found it ...
D Dirol, A Scalbert


Accelerated decay tests to investigate postulated effects of tannins on CCA efficacy in wood
1988 - IRG/WP 3497
Five groups of blocks (10 x 10 x 5 mm³) viz., Pinus patula, Pinus patula impregnated to 4% (w/w) tannin; Eucalyptus grandis, Eucalyptus grandis with natural tannins extracted; and extracted Eucalyptus grandis with tannins returned as above; were prepared. Blocks from each group were then treated to 0, 5, 10 and 15 kg/m³ CCA and challenged in four 15-week decay tests, viz., soil burial, and expos...
U L Scherer, A A W Baecker


Chemical evaluation of borate treated pine sapwood attacked by the subterranean termite Coptotermes acinaciformis
1993 - IRG/WP 93-20003
Sapwood of hoop (Araucaria cunninghamii Ait. ex D. Don) and slash (Pinus elliottii Englem.) pines were treated by Vacuum Pressure Impregnation (VPI) to provide test specimens. The concentration of boron was defined by chemical analyses of the timber, in the zone of primary attack by the termite being bioassayed. A common method of definition of preservative retention, weight uptake of preservative...
A R Moffat, B C Peters


The critical moisture and temperature conditions for the growth of some mould fungi and the brown rot fungus Coniophora puteana on wood
1988 - IRG/WP 1369
The growth of some mould fungi on pine and spruce sapwood was studied in 40 different constant moisture and temperature conditions. The temperature range was between +10 and +40°C and the relative humidities varied from 76 to 100% relative humidity (RH). The incubation time was 12 weeks. The mixed mould inoculation used included typical fungi growing on wood: Aspergillus versicolor, Cladosporium ...
H Viitanen, L Paajanen


Hygroscopicity of decayed wood - Implications for weight loss determinations
1996 - IRG/WP 96-20085
Hygroscopicity changes were observed in red maple blocks subjected to brown rot, white rot and soft rot. Brown rot reduced hygroscopicity, soft rot increased hygroscopicity, and white rot showed only a very slight increase in hygroscopicity. The effect of these changes on weight loss tests is a slight overestimation of weight loss for brown rot and a slight underestimation for soft rot and white r...
S E Anagnost, W B Smith


Soft rot decay in acetylated wood. Chemical and anatomical changes in decayed wood
2002 - IRG/WP 02-40231
Acetylated Beech (Fagus sylvatica) and Scots Pine (Pinus sylvestris) wood were studied in soil beds under laboratory conditions for longer periods. High mass losses and dynamic MOE losses were measured in non-acetylated wood and at lower weight percent gains (WPG). Rapid losses of lignin, holocellulose and ?-cellulose occurred in non-acetylated beech wood and no losses were detected at the highest...
B Mohebby, H Militz


Effect of cyclic change of temperature on fungal growth and mass loss
1994 - IRG/WP 94-10065
For estimating the effect of cycling change of temparature on fungal growth, four Japanese species, sugi (Cryptomeria japonica), hinoki (Chamaecyparis obtusa), akamatsu (Pinus densiflora) and buna (Fagus crenata), four fungal species, Tyromyces palustris, Gloeophyllum trabeum, Coriolus versicolor, Pycnoporus coccineus, and five temperature conditions, 10, 20, 27, 35°C and cyclic temperature (20°...
K Suzuki, K Okada


The effect of extent and location of decay on strength loss in constructional timber
1994 - IRG/WP 94-30039
Radiata pine heartwood billets, 50 x 100 x 1000 mm³ were end-sealed and treated with copper-chrome-arsenate preservative (NZ Type I) to a range of retentions and penetration patterns. Cross-sections, 10 mm thick, were cut from the centre of each billet and used for determination of preservative distribution, for preservative analysis and for decay tests. The decay test consisted of laying samples...
M E Hedley, H Bier


Accelerated decay tests on DNBP-treated Pinus patula and Eucalyptus grandis
1987 - IRG/WP 3441
Blocks (10 x 10 x 5 mm³) of Pinus patula and Eucalyptus grandis were impregnated to 0, 1.5, 3.0 and 4.5 kg/m³ 2-sec-butyl, 4, 6 dinitrophenol (DNBP). They were monitored microscopically and for weight losses over 16 weeks against monocultures of Coriolus versicolor and Coniophora puteana. Treated ministakes (10 x 10 x 100 mm³) and blocks in soil contact were similarly monitored to determine wei...
L D Abraham, A A W Baecker


Assessment of wood decay in small-scale unsterile soil-bed tests
1997 - IRG/WP 97-20111
This study is concerned with the investigation of wood decay in small-scale unsterile soil-bed tests. Tests were performed with untreated heartwood samples from five hardwood species of different natural durability classes ranging from highly perishable to very resistant. Our results confirmed the critical role of soil moisture content on wood decay. The highest decay rates were observed at moistu...
L Machek, A M Derksen, R Sierra-Alvarez


Steam/hold/APM boron treatment - Treatability trials with green gauged radiata pine
1987 - IRG/WP 3439
Freshly sawn 100 x 50 mm radiata pine was green gauged, steam conditioned and preservative treated with a mixture of borax and boric acid using a modified Alternating Pressure Method (APM) treatment schedule. A 12 hour holding period between steam conditioning and treatment resulted in the necessary moisture loss and moisture re-distribution to facilitate treatment to NZ Timber Preservation Author...
P Vinden


Natural progression of decay in unrestrained, Southern pine sapwood exposed above ground
1995 - IRG/WP 95-20060
In this study, the natural progression of decay is being monitored in 2.4-m (8-ft) lengths of dimension lumber. The 2.4-m lengths are supported without restraint in a horizontal plane approximately 0.75 m above ground in a partially shaded field plot in southern Mississippi. The lumber is 100% sapwood. Prior to installation in the field, each piece was planed to exactly 38 by 89 mm² (1.5 by 3.5 i...
R C De Groot, R J Ross, W Nelson


Application of a novel strength evaluation technique during screening of wood preservatives
1986 - IRG/WP 2262
The effectiveness of CCA and ACA in treated aspen mini stakes tested using a novel bag procedure, with unsterile soil fortified with Chaetomium globosum and Ceratocystis albida, is reported. Good agreement between toxic limits determined using the standard weight loss procedure, and those determined by the strength technique were found, with some indication that the strength loss method is more se...
J N R Ruddick


Evaluation of wood durability by laboratory test - A new equation to predict wood durability
2001 - IRG/WP 01-20230
To estimate the wood durability in a short term, periodical weight determination was carried out in a laboratory test. This test provided the results comparable to those of the field test and the fungus cellar test, but it required much more jobs in comparison to the usual accelerated laboratory test. To save the time and jobbing for this method, a new equation was devised from simple two assumpti...
I Momohara, K Yamamoto


A technique for the rapid assessment of wood surface degradation during weathering
1987 - IRG/WP 2281
Radiate pine (Pinus radiata D. Don) sapwood samples taken from four trees were converted into thin strips 100 x 10 x 0.085 (85 µm) mm³, (longitudinal x radial x tangential) in size and exposed in preweighed hatches to the weather inclined at 45° facing equatorially for 10, 20, 40, 60, 80 and 100 days. Significant (P < 0.001) weight losses occurred with time over the exposure period. Differen...
P D Evans, D Abbott, S Thein


IUFRO rating system compares favourably to weight loss for soil-bed testing
1990 - IRG/WP 2343
The soil-bed/small stake test is commonly used for rapidly evaluating the performance of new, more environmentally acceptable, preservatives. In a 1.5 year experiment with three copper-based waterborne preservatives, visual evaluation and probing using the IUFRO performance rating scale (0-4) gave very similar toxic thresholds to those derived from measurement of weight loss at the end of the expe...
P I Morris


Soluble nutrient influences on toxicity and permanence of CCA preservatives in wood
1980 - IRG/WP 3144
The influence of soluble carbohydrate and nitrogenous components concentrated at evaporative surfaces of wood on the toxicity and permanence of CCA preservatives has been examined using soil-burial techniques. Nutrient concentrations in lime (Tilia vulgaris Hayne) have been shown to be associated with reduction of toxic limits of preservatives to an extent in which a 100% increase in preservative ...
B King, G M Smith, A Bruce


Treatment of poplar plywood with solvent and water-borne preservatives
1989 - IRG/WP 3538
Poplar as a light hardwood is appropriate for plywood production. Owing to its low natural durability it is generally recommended to preserve it in all conditions where risks of fungal attack may be present. A research project has been carried out on preservative treatments of plywood commodities. Parameters studied were various treatment cycles, three types of plywood, and a number of solvent and...
J Van Acker, M Stevens


Laboratory testing of wood natural durability - In soil-bed assays
1998 - IRG/WP 98-20141
Laboratory methods for assessing wood decay resistance are being investigated in the framework of an ongoing European research project. This paper summarizes the main results obtained for soil-bed tests based on the European prestandard ENV 807-Test 2. The data suggest that this testing methodology is suitable for evaluating the natural durability of timber species in soil-contact under conditions...
R Sierra-Alvarez, I Le Bayon, J K Carey, I Stephan, J Van Acker, M Grinda, G Kleist, H Militz, R-D Peek


Rapid loss of lignin at wood surfaces during natural weathering
1992 - IRG/WP 92-2390
Thin veneers of radiata pine (Pinus radiata D. Don) were exposed to natural weathering over a period of 30 days. Incident UV radiation was monitored at the test site. FTIR internal reflectance spectroscopy was used to study the chemical changes taking place at the veneer surface during weathering. Spectra obtained show that after only 3 days exposure there was substantial delignification at veneer...
P D Evans, K J Schmalzl, A J Michell


Laboratory tests on the natural durability of timber methods and problems
1984 - IRG/WP 2217
In literature a large variety of test methods is mentioned to examine the natural resistance of timber against fungal attack. This concerns the kind of sampling as well as the test procedure, the test fungi, the duration of test, and the classification of the resistance according to the test results. These variations, however, are of great influence on the test result. Long term exposure will lead...
H Willeitner


The comparative resistance to fungi of the wood munika (Pinus heldreichii Christ.), fir (Abies alba Mill.) and spruce (Picea excelsa Poir.) compared with Pinus sylvestris L. and some physical and mechanical characteristics of munika
1981 - IRG/WP 1129
The munika (Pinus heldreichii Christ.) is situated primarily in the Balkans, and partially in the south of the Apenine peninsula. As an endemic species, with a very little annual increment, it has not been used enough as a timber for mechanical conversion up till now, although the oldest trees can grow to 27 m in height, with a diameter at breast height of about 60 cm. According to data of many Ba...
M Petrovic, M Miric


A dynamic approach to assess the modulus of elasticity in wood decay testing
1998 - IRG/WP 98-20139
In this study, the changes in elastic behaviour and mass losses of different hardwood and softwood species exposed to decay in a laboratory soil tests were assessed. Wood decay was monitored using different assessment methods, namely: mass loss and changes in elastic behaviours (MOE) determination. Elastic changes were determined by static and dynamic methods, for the latter, acoustic technique wa...
L Machek, H Militz, R Sierra-Alvarez


Observations on the destruction of fishing craft in India by marine wood-borers with special reference to the West Coast
1981 - IRG/WP 468
The paper highlights the economic importance of the destruction of fishing craft in India by marine wood-destroying agencies. The annual loss involved is to the extent of over 94 million rupees. Thirty-nine spectes and one variety of woodborer have so far been recorded from India, of which Bankia campanellata, Bankia carinata, Bankia rochi, Dicyathifer manni, Lyrodus pedicellatus, Teredo clappi, T...
L N Santhakumaran, J C Jain


Previous Page | Next Page