IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 28 documents. Displaying 25 entries per page.


A study of poplar LVL durability improvement:
1999 - IRG/WP 99-40148
The aim of this study was to optimise the durability of LVL panels by adding boron during the gluing process. Poplar veneers (2,6 mm thickness ) were selected by ISORY a French company . Two types of glue were tested : Phenol resorcine and Melamine Urea Formaldehyde. Each of them was mixed with various concentrations of borax (for the first one) and Boric acid(for the second one). Mechanical prope...
B Charrier, V Bridaux, N Fauroux, F Charrier


Volatile borates in the treatment of wood and wood based panel products against subterranean termites
1995 - IRG/WP 95-30094
Blocks of pine solid wood, oriented strand board and plywood were treated with trimethyl borate by vapour treatment. It was meant to obtain either a full impregnation of the specimens or a shell treatment of the outer three millimetres. The efficacy of the treatments against subterranean termites (Reticulitermes lucifugus) was evaluated using an European Standard method....
L Nunes, D J Dickinson, R J Murphy


Biodegradation of acetylated southern pine and aspen composition boards
1994 - IRG/WP 94-40020
This objective of this study was to investigate the influence of the acetylation treated wood fiber, Phenol-formaldehyde resin content level, two wood fiber species, three fungi species on the dimensional stability and decay resistence of high density composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species...
P Chow, T Harp, R Meimban, J A Youngquist, R M Powell


Treatment of wood-based panel products with volatile borate
1990 - IRG/WP 3616
The paper presents recent developments in the use of volatile borate esters for the preservative treatment of wood based board materials. Several advances on previous reports are discussed. In laboratory studies, treatment times of approximately ten minutes at 20°C on boards at equilibrium moisture content provided full penetration and retentions of 1% wt/wt boric acid. Biological tests have been...
P Turner, R J Murphy, D J Dickinson


Biocide Treatments for Wood Composites - A Review
2006 - IRG/WP 06-40323
This paper reviews the biocidal treatment of wood composites. Included are in-process and post-process treatments. Various biocides are covered as are methods of application. Novel treatments and technologies are also presented....
J W Kirkpatrick, H M Barnes


The mathematical study of test plot data
1987 - IRG/WP 2282
It has long been desirable to have a mathematical expression, which, by the insertion of statistically derived constants, would describe the behavior of test specimens in service. The philosophy of such expressions is briefly discussed, and the history of the concept is outlined. The modern approach to the problem dates from the graphical presentation of dosage-response and deterioration curves by...
W H Hartford


Wood-based composites exposed to fungal degradation: Laboratory results
2001 - IRG/WP 01-40215
Oriented strandboard (OSB) and laminated veneer lumber (LVL) are widely used as residential construction materials. The durability of OSB and LVL against biological degradation has not been studied comprehensively. The objective of this research was to investigate the durability of OSB and LVL when exposed to wood decay fungi. Fourteen brown-rot and eight white-rot wood decay fungi were screened f...
V W Yang, B Illman, L A Ferge, R J Ross


Termite Field Tests of Various Timber Species Treated with permethrin using supercritical carbon dioxide
2005 - IRG/WP 05-10560
Termite field tests were conducted on permethrin-treated Eucalyptus obliqua heartwood, Pinus radiata sapwood and P. radiata LVL. The permethrin was impregnated using either supercritical carbon dioxide (scCO2) or light organic solvent preservative (LOSP) systems. Comparative permethrin retentions were most accurately achieved in P. radiata sapwood, where no difference between impregnation systems ...
A Qader, L J Cookson, J W Creffield, D Scown


Evaluating the resistance of wood-based panel products to fungal attack
1995 - IRG/WP 95-20071
At present there is considerable disagreement among national research institutes within Europe and panel product manufacturers on the most appropriate method of testing and indeed the need for specific biological durability testing. This paper seeks to place before a broader international audience, the issues related to development of a European standard for evaluating the resistance to fungal dec...
R G Lea, R W Berry


Resistance of acrylic paints on wood against growth of the rot fungus Dacrymyces stillatus
1990 - IRG/WP 2345
In the last few years the presence of the rot fungus Dacrymyces stillatus has been repeatedly confirmed in external wood panels, particularly from wood painted with water based paints. A laboratory method for testing of the fungal resistance of paint films on wood has been developed.This method has been used to test the efficacy of the fungicides Parmetol DF 18 and Parmetol HF 25 against attack by...
J Bjurman


Permatek IM 30 as a termiticide treatment for veneer-based wood products
2003 - IRG/WP 03-30325
Permatek IM 30 is a termiticide designed for incorporation into wood products during manufacture. Whereas existing approved products in Australia are based predominantly on synthetic pyrethroids carried in solvents, Permatek IM 30 is based on imidacloprid, a neonicotinoid insecticide. The formulation has very low mammalian toxicity, is free of VOCs, and has been successfully tested as a glueline ...
J Doyle, K Webb, W R Rae, A F Siraa, J Malcolm-Black


Diagnostics methods and routes proposalsto define selective sorting of demolition wood wastes
2001 - IRG/WP 01-50177
Wood wastes are more and more often used in different wood waste valorisation industries (panels, wood energy, cement factories, ...). These industries are in progress to include in their processes, wood wastes coming from demolition wood. A state of the art and an analysis have been made to propose : (1) diagnostics methods to carry out a classification of wood wastes on demolition sites and in t...
G Labat, E Bucket, C Fréret, G Deroubaix


Biological Protection of Composite Panel from Moulds and Decay
2007 - IRG/WP 07-10612
Composite panels, such as oriented strand board (OSB), are widely used in house construction in North America. These structural panels are normally made of non-durable wood species and are susceptible to moulds and decay when exposed to wet conditions. Building envelope failures due to moulds, decay or poor construction practices can negatively impact the image of wood. To ensure durability of com...
Dian-Qing Yang, Xiang-Ming Wang, Hui Wan


Progress in Fire-Retardant Research on Wood and Wood-Based Composites: a China Perspective
2009 - IRG/WP 09-40476
The fire retardant research on wood and wood-based composites, which was carried out in China in the past two decades, was reviewed with 55 references. While many kinds of fire retardants for wood and wood-based composites have been studied, the mainstream is still the compound or the mixture containing phosphorus, nitrogen and boron elements, which can be used in the form of water solution in th...
Wang Qingwen, Wang Fengqiang, Hu Yunchu, Li Jian


Evaluation of formulation type on the efficacy of bifenthrin as a glueline termiticide for veneer based wood products
2010 - IRG/WP 10-40486
Field trials were carried out in Australia on Coptotermes acinaciformis to evaluate the efficacy of various bifenthrin formulations. One trial tested plywood made by Zelam at their research facility in New Zealand and compared three emulsifiable concentrate formulations (EC), a suspension concentrate (SC) and an encapsulated formulation (CS). A second trial compared laminated veneer lumber (LVL)...
P Lobb, A Siraa


The utilization of sand dusts of MDF panel as filler in wood plastic composites
2010 - IRG/WP 10-40500
Waste management is getting important in the world. Most of wood based panel industries are interested in utilization of wood residues such as saw dust, sand dust and wood flour in other applications. The objective of this study is to investigate the usability of sand dust of MDF in wood plastic composites. HDPE and PP based composites with 30 % sand dusts loading were compounded in the single sc...
A D Cavdar, H Kalaycioglu, F Mengeloglu, K Karakus, H Yel


Biological properties of Pinus radiata veneers modified with hexamethoxymethyl melamine
2011 - IRG/WP 11-40552
An investigation of the effects on decay and termite resistance of a wood modification process involving prepolymers of hexamethoxymethyl melamine (HMMM) was conducted using LVL as a model engineered wood product. Dry Pinus radiata veneers were vacuum-impregnated with a wood modification formulation containing a mixture (P-H:S-H) of two separate prepolymerisation reactions containing polyvinyl al...
A Siraa, S Millward, C Molloy


Thiacloprid as a glueline termiticide for veneer based wood products
2012 - IRG/WP 12-30592
Thiacloprid is an insecticide commonly used in the agricultural industry. No evidence of its commercial use in wood has been discovered by the authors. Results are reported for veneer based wood products treated with thiacloprid via the glueline. Thiacloprid was tested against Coptotermes acinaciformis following the brick assembly technique as described in the Australasian Wood Preservation Com...
K Day, A Siraa, P Lobb


Glueline fungicides in veneer based engineered wood products - results from laboratory work for the H1.2 hazard class in New Zealand
2012 - IRG/WP 12-30593
The use of glueline insecticides in plywood and laminated veneer lumber is commonplace in several countries. However, few glueline fungicides are registered for commercial use with previous work suggesting that achieving control of decay from the glueline is very challenging. This paper summarises two tests completed on Pinus radiata plywood with a new glueline fungicide comprising the active in...
A Siraa, K Day, P Lobb


Wood-leather panels – A biological, fire retardant building material
2012 - IRG/WP 12-40615
The poor flame retardant properties of wood-based products are among the severest obstacles, hindering its use in the commercial building sector. Recently, some attempts to improve the fire properties, relying on inflammable salts or reactive halogen compounds, have been presented, although they either cause problems with machining or embody harmful compounds (halogen derivates). In this paper, ...
S Wieland, U Stöckl, T Grünewald, S Ostrowski, A Petutschnigg


Study on Fire Resistance of Lightweight Panels Made of Honeycomb and Polyurethane Cores
2013 - IRG/WP 13-40645
In response to the increasing demand of lightweight and durable materials in furniture manufacture, potential of different skin types and cores were investigated to make proper lightweight panel. Fire resistance of panels made of different skins and cores were studied to elucidate the board’s behavior exposed to fire. Skins were MDF (3, 6 and 8 mm), particle board, plywood (3 and 5 layers) and c...
A Talaei, M Ghofrani, S Pishan


Comparison of untreated plywood and untreated LVL in a field trial against Coptotermes acinaciformis and in laboratory trials against Tyromyces palustris and Coniophora puteana
2014 - IRG/WP 14-40671
In Australasia, efficacy data obtained on plywood is generally acceptable for laminated veneer lumber (LVL) and vice versa. This is particularly the case with glueline treatment approvals. The rationale is that the two wood products have predominately the same basic structure with the key difference being orientation of the veneer. LVL typically has all veneers in parallel while plywood typical...
A Siraa, K Day, S Millward, P Lobb


Minimum standards for habitability in emergency housing
2015 - IRG/WP 15-50312
In this study we evaluated the properties of a prefabricated HOUSING prototype based on a 64mm thick "Structural Insulated Panel" (SIP; hereinafter SIP64), built by two OSB panels bonded with a two component polyurethane adhesive to a high density expanded polystyrene core. This panel was manufactured as a main element for walls in the construction of emergency housing. The thermal insulation of t...
R Garay, F Pfenniger, W Figueroa


Durability of Thermally Modified Engineered Wood Products
2016 - IRG/WP 16-40745
In this study, rated plywood, oriented strand board (OSB), laminated strand lumber (LSL), and laminated veneer lumber (LVL) were thermally modified as a post-treatment at 140 °C, 150 °C, 160 °C, 170 °C, and 180 °C using a closed, pressurized treatment method. Eastern larch OSB manufactured from heartwood and sapwood was also thermally modified as a post-treatment at 160 °C and 180°C. All ...
H M Barnes, M D Aro, A Rowlen


Glueline fungicides in veneer based engineered wood products – updated results from laboratory work for the H1.2 hazard class in New Zealand
2018 - IRG/WP 18-30726
Results from New Zealand H1.2 ‘bin’ trials containing plywood glueline treated with triadimefon and cyproconazole were reported in 2012 (IRG/WP 12-30593). One of these trials has continued to the present day (2108) and updated results of this trial are reported. The triadimefon and cyproconazole glueline treatment continues to compare with, or outperform, the reference preservative used, bei...
A Siraa, K Day, B Kibby


Next Page