Rates of emission from CCA-treated wood in the marine environment: measurement, modelling and requirements for further research
2001 - IRG/WP 01-50166-12
Accurate estimates of rates of emission of leachate from preservative treated wood are crucial for realistic predictions of the environmental impact of its use in maritime construction. Estimates are available for some commonly used preservatives, but these vary widely. Though variable, these measurements suggest that emission generally decreases exponentially with time. Part of the variation is d...
S M Cragg, C J Brown, R A Albuquerque, R A Eaton


Test procedure to determine the effect of timber substrate on the effectiveness of different preservatives in sea-wate
1975 - IRG/WP 414
R A Eaton


Wood-destroying insects found in the Eastern Black Sea sub-region of Turkey
1982 - IRG/WP 1153
The Eastern Black Sea subregion has important forest resources. The settlement areas are scattered at the countryside. That's why a good deal of wood and timber is used in the construction of buildings without sufficient protective measures in the rural areas. In the forests and rural buildings 52 wood-destroying insect species have been specified 35 of which are new in this subregion and...
O A Sekendiz


Procedure for a collaborative study of leaching from CCA-treated timber in the sea
1988 - IRG/WP 4143
As a follow-up to the collaborative IRG/COIPM marine trial of CCA and CCB preservatives, a further trial is proposed with the objective of measuring the degree of leaching of CCA components from three timber species at marine sites in Malaysia and the U.K.. Details of the planned procedure are given....
S M Cragg, J E Barnacle, J D Bultman, R A Eaton, B R Johnson, L E Leightley, K D Singh


Changed susceptibility of the chemically and thermally degraded spruce wood to its attack by the dry rot fungus Serpula lacrymans
1999 - IRG/WP 99-10322
In buildings, some intentional or unintended situations can occur at which some wood products are exposed to aggressive chemicals and also to higher temperatures. Occasional activity of fungi on such pre-attacked wood products can be either higher or lower. This paper deals with changes in the susceptibility of spruce wood (Picea abies L. Karst.) to attack by the dry rot fungus Serpula lacrymans, ...
L Reinprecht


Conditions for basidiospore production in the brown rot fungus Gloeophyllum separium in axenic culture
1984 - IRG/WP 1232
Attempts to control and optimize the production of hymenial structures and basidiospore production in Gloeophyllum sepiarium in axenic culture resulted in the proposal of the following conditions as being suitable. The dikaryotic mycelia originally isolated from basidiocarps could consistently be induced to produce hymenial structures and pure basidiospore collects if illuminated by near ultraviol...
J Bjurman


Development of novel techniques for evaluating the feeding rate of Limnoria lignorum with specific reference to temperature influences
1999 - IRG/WP 99-10325
The faecal pellet production of Limnoria lignorum placed into repli-dish chambers containing seawater and a small chip of untreated Corsican pine (Pinus nigra) was observed. The repli-dishes were kept at a range of constant temperatures between 10 and 25°C and the number of faecal pellets produced by each of the animals was monitored. It was found that faecal pellet length generally increased wit...
A Praël, S M Cragg, R A Eaton


Natural Resistance of timbers to marine borer attack. COIPM/IRG CO-OPERATION. Final report concerning panels exposed in the sea at Sekondi, Ghana
1979 - IRG/WP 449
The test was carried out according to Document COIPM/72.044, Revised procedure for the testing of naturally durable timbers against marine borers. The panels of the three species remaining in the test at the end of 1978 were removed and assessed visually. An average rating was given to the panels of each species....
F F K Ampong


Microbial biofouling of 10-40% naphthalene in creosote treated and untreated wooden pilings in the marine environment
1978 - IRG/WP 442
R R Colwell, P L Fish, D A Webb, A J Emery


Evaluation of polystyrene as a protective of wood in sea-water
1986 - IRG/WP 4129
A test is described on the biological protection of wood by treatment with polystyrene. The results, obtained in marine trials, after 18 months, show that the treatment with polystyrene is not all that effective in preventing the attack of marine borers....
A Gambetta


Marine borers and marine wood protection - Some answers and some outstanding questions - A comment
1990 - IRG/WP 4163
A brief description of the nature of hazards encountered in different parts of the marine environment is given. An attempt is then made to assess what were the essential findings of selected areas of research in the marine wood protection field and what still needs to be done. That is, if we are to more adequately understand what we are attempting to do in this field of study!...
J E Barnacle


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water: Final report
1987 - IRG/WP 4133
Three timbers chosen as reference species were treated with 3, 6 and 10% solutions of CCA and CCB preservatives and exposed for up to 93 months at 8 tropical and temperate marine sites. Eleven local species treated in the same way were exposed at 4 of the 8 sites. There was no apparent difference in performance between CCA and CCB treated specimens. The severest test site was Panama Canal but mari...
R A Eaton


Supercooling points of Anobium punctatum, the common furniture beetle
1995 - IRG/WP 95-10120
Ice formation within the body of larvae of the common furniture beetle Anobium punctatum causes death of the larvae. Freezing can therefore be used as a means of eradication of the larvae in infested wood. To optimize the freezing process, knowledge of the temperatures sufficient to kill the larvae is essential. Ice formation is initiated by temperatures equaling the so-called supercooling point, ...
T E Hallas, K Bohn Hansen


A fixation model, based on the temperature dependence of CCA-C fixation
2000 - IRG/WP 00-40163
A model was prepared for the fixation of 1% CCA-C in red pine that allows the prediction of extent of fixation based on the temperature history of the treated wood following pressure treatment. The reaction kinetics of the rapid initial reaction and the slower main reaction were characterized using the Van t'Hoff equation. The initial reaction could be represented by a 10th order chemical...
P A Cooper, K M F Kazi, Jianbin Chen, Y T Ung


Examination of timbers from the Mary Rose in storage
1988 - IRG/WP 4149
Timbers from the Tudor ship, Mary Rose, have been examined for the presence of fungal fruiting structures. Wood specimens were also examined for the presence of microbial decay patterns using light and scanning electron microscopy. Structural timbers were surveyed using the Pilodyn for an overall picture of the extent of decay. Mary Rose timbers were predominantly inhabited by marine fungi. Fourte...
R Mouzouras


Virulence testing of cultures of different origins of the test fungus Coriolus versicolor strain CTB 863 A
1986 - IRG/WP 2267
The virulence of cultures of different origins of Coriolus versicolor CTB 863 A - a strain which is mentioned in EN 113 - was tested. Standard blocks of beech wood were used at temperatures of 20-22°C and 26-28°C and particleboard was tested at 26-28°C. The decay capacity of the different inoculations varied widely, as could be expected it was greatest at the higher temperature level....
W Kerner


A preliminary report on lignicolous marine fungi in the Java Sea, Indonesia
1982 - IRG/WP 488
This report is part of a study on the natural durability of Indonesian timbers against marine borers conducted in Pari Island waters, Java Sea (Suhirman and Eaton, 1981), and contains preliminary information which has not yet been published....
Suhirman, R A Eaton


Laboratory fumigations to determine the minimum temperature for methyl bromide eradication of the oak wilt fungus in red oak
1983 - IRG/WP 3243
Laboratory chamber fumigations of naturally-infected ret oak log sections exterminatet the oak wilt fungus in sapwood at temperatures down to 0°C. Only low, sporadic fungus survival was observed when log sections were gassed with methyl bromide at -5°C and aired for 4 da. at 0°C. Lower temperature treatments were not effective even if gas levels or exposure times were increased by 50%....
E L Schmidt


The variation in electrical resistance in the CCA-treated wood during the fixation
1989 - IRG/WP 3554
The curve commonly used in Scandinavia for describing the fixation period at different temperatures for CCA-impregnated wood is based on investigation by Dahlgren on the pH-variations in a mixture of sawdust and preservative solution. As far as we know there is no such investigation on solid wood. We have therefore measured the electrical resistance in CCA-treated solid wood to see if this will di...
F G Evans, B Nossen


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic conditions. Part 2: Semi-industrial investigation
1995 - IRG/WP 95-50040-13
In continuation of previous leaching research on the quantification and modelling of metal elements released from CCA treated timber, a series of experiments has been carried out dealing with the influence of temperature and pH of the relative aquatic environment. The leaching method used is the Dutch prestandard for building materials, a long term static leaching test simulating practical bank-sh...
G M F Van Eetvelde, W J Homan, H Militz, M Stevens


Emission of trimethyl borate and methanol from radiata pine (Pinus radiata D. Don)
1995 - IRG/WP 95-30088
Sawn and kiln dried radiata pine conditioned to 3, 6, and 12% moisture content was treated with trimethyl borate (TMB). The treated wood samples were placed in mini-desiccators maintained at 20 or 40°C. The air space within the mini-desiccator was analysed for TMB and methanol. An initial period of emission of TMB and methanol was observed. This was followed by a period of gradual dissipation of ...
F J Romero, P Vinden, J A Drysdale


Thermotolerant mould growth in dehumidifier kilns in New Zealand
1996 - IRG/WP 96-10169
Growth of Aspergillus fumigatus and Paecilomyces variottii is common on wood dried in dehumidifier kilns that operate within a temperature range of 35-55°C. Aspergillus fumigatus causes an unacceptable blue / grey discolouration of the woods surface and prolonged exposure to spores during handling of mouldy wood can cause health problems amongst timber workers. A survey of dehumidifier kiln opera...
R N Wakeling, J G Van der Waals


The isolation of actinomycetes from wood in ground contact and the sea
1980 - IRG/WP 1110
M S Cavalcante, R A Eaton


Biodegradation of creosote/naphthalene-treated wood in the marine environment
1977 - IRG/WP 428
The present study was undertaken to determine the biodegradability of marine grade creosote and selected components, including naphtalene, and to determine the effectiveness of (up to 40%) creosote in protecting wood from microbial attack. Also, the impact(s) of creosote and naphtalene-enriched creosote on the microbial ecology os estuarine environments was examined....
P A Seesman, R R Colwell, A Zachary, A J Emery


Development of a method for testing wood preservatives with soft rot fungi
1975 - IRG/WP 250
Although the first publications on experimental soft rot attack date back 20 years ago, so far no test method for evaluating the efficacy of wood preservatives against soft rot attack (Ascomycetes and Fungi Imperfecti) has been generally accepted. The reasons are diverse and the shortcomings and the disadvantages of the methods described are well known and have repeatedly been discussed. The soil ...
M Gersonde, W Kerner-Gang