IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 134 documents. Displaying 25 entries per page.


A technique for the rapid assessment of wood surface degradation during weathering
1987 - IRG/WP 2281
Radiate pine (Pinus radiata D. Don) sapwood samples taken from four trees were converted into thin strips 100 x 10 x 0.085 (85 µm) mm³, (longitudinal x radial x tangential) in size and exposed in preweighed hatches to the weather inclined at 45° facing equatorially for 10, 20, 40, 60, 80 and 100 days. Significant (P < 0.001) weight losses occurred with time over the exposure period. Differen...
P D Evans, D Abbott, S Thein


The relationship between preservative type and surface degrade in Pinus radiata
1980 - IRG/WP 3158
Samples of Pinus radiata D. Don were impregnated with one of two preservative types, a copper chrome arsenic salt and a light organic solvent preservative. The panels were exposed to the weather for 4-5 years at a site near Sydney, Australia. Macroscopic and microscopic examinations showed different rates and patterns of weathering between the samples treated with each preservative and an untreate...
R S Johnstone, R K Bamber


Surface characteristics of wood treated with various AAC, ACQ and CCA formulations after weathering
1991 - IRG/WP 2369
Wood samples treated with various alkylammonium compounds (AACs) as well as ammoniacal copper quat (ACQ) and chromated copper arsenate (CCA) have been studied in accelerated weathering experiments. Microscopic examination of the surfaces of these samples after exposure in a weatherometer revealed several different changes. Samples treated with didecyldimethyl ammonium chloride (DDAC) show consider...
L Jin, K J Archer, A F Preston


The degradation of wood surfaces by dilute acids
1985 - IRG/WP 3326
Thin radial/longitudinal sections(~100 µ) of Corsican Pine (Pinus nigra) and Lime (Tilia vulgaris), were exposed to Sulphuric, Sulphurous, nitric, acetic, and formic acid at 40°C in the pH range 2-6. After about 3 months exposure to Sulphuric, nitric, acetic and formic acid at pH 2.0 Pine lost some 20-25% of its tensile strength. Losses in tensile strength due to sulphurous acid were greater bei...
P D Evans, W B Banks


JWPA method for testing effectiveness of surface coatings with preservatives against decay fungi
1981 - IRG/WP 2164
In 1979 JWPA established a new method for testing effectiveness of surface coatings in accordance with practical use of preservative-treated lumber. Comparing the new testing method with JIS A 9302, a few new trials - size of wood specimen, weathering procedure, and decay-test procedure - are incorporated....
K Tsunoda


Dimensional stability and decay resistance of hot-melt self-bonded particleboard by surface benzylated pine chips
1991 - IRG/WP 3652
Akamatsu (Pinus densiflora Sieb. et Zucc: Japanese red pine) particles were pretreated with 40% NaOH solution and benzylated with benzyl chloride, and the surface of particle was converted into meltable materials. Hot-melt self bonded particleboard having smooth and high glossiness surface was prepared by hot pressing at 150°C and 1.96 MPa without using any conventional adhesives. Dimensional sta...
M Kiguchi, K Yamamoto


Blue stain in service on wood surface coatings. Part 3: The nutritional capability of Aureobasidium pullulans compared to other fungi commonly isolated from wood surface coatings
1993 - IRG/WP 93-10035
The nutritional capability of Aureobasidium pullulans was previously examined, using agar plate tests, with regard to nutrient sources that are potentially available in fresh and weathered wood (Sharpe and Dickinson, 1992). This study compared these findings with the nutritional capability of four other fungi (Alternaria sp., Cladosporium cladosporoides, Stemphylium sp. and Trichoderma sp.) common...
P R Sharpe, D J Dickinson


Leaching of the new boron based biocide from coated wood
2001 - IRG/WP 01-30267
We investigated leachability of the new boron based biocide - a complex of an amine and boric acid - from vacuum impregnated spruce wood samples. It was determined by the standard ENV 1250-2 procedure that the new biocide is susceptible to leaching so from the water borne as well as from the ethanol borne boron containing preservative treated wood. Leaching may be retarded by application of surfac...
M Petric, M Pavlic, F Cadez


Effects in vivo of various tensides (surface-active agents) on Reticulitermes santonensis De Feyteaud
2001 - IRG/WP 01-10417
The results of studies of surface active agents (tensides, surfactants) on the feeding behavior and mortality of Reticulitermes santonensis De Feyteaud are described. The effects of these agents on the nature and relative populations of eight gut-inhabiting symbionts are also examined. Among the various tensides tested, bee&apos;s poison was the most effective in causing rapid termite death. A...
W Unger


Performance results of wood treated with CCA-PEG
1986 - IRG/WP 3363
The addition of polyethylene glycol (PEG) to the CCA system has been shown to reduce the surface hardness of poles and ease spur penetration during climbing. This paper addresses the results of tests dealing with preservative retention and penetration, permanence of CCA and PEG, strength, drying rate, and checking characteristics....
W P Trumble, E E Messina


Surface coatings for impregnated wood
1992 - IRG/WP 92-3684
The use of proper surface coatings enhances the aesthetic and protective properties of impregnated wood. Good results with especially water-borne coatings have been obtained for class-A impregnated L-joints and claddings in field tests started in 1982....
L Kotama


Protecting wooden structures
1980 - IRG/WP 392
Chromium-containing chemicals that effectively retard weathering of wood improve performance of subsequently applied finishes. Current work is focusing on the performance of wood-derived products (plywood, hardboard, fiberboard, particle board) after surface treatment with inorganic chemicals. The overall objective of the continuing research is to investigate new environmentally safe procedures to...
W C Feist


The influence of formulation on the behaviour of LOSP's during industrial impregnation of spruce
1986 - IRG/WP 3387
Evidence is presented that the comparative behaviour of two LOSP formulations during impregnation treatment of spruce cannot be predicted purely on the basis of their physical characteristics (viscosity, surface tension and contact angle) nor on the extent of their &apos;passive&apos; penetration into pine sapwood....
L D A Saunders, D M Zuvencko


Blue stain in service on wood surface coatings. Part 2: The ability of Aureobasidium pullulans to penetrate wood surface coatings
1992 - IRG/WP 92-1557
The ability of Aureobasidium pullulans to penetrate seven different wood surface coatings was examined. Eight isolates of Aureobasidium pullulans were used. Following penetration, light microscopy was used to examine the effect of the fungus upon the coating, and growth at the wood-film interface. The fungus showed different growth capabilities with different types of surface coatings. Some isolat...
P R Sharpe, D J Dickinson


Performance of surface-treated hardwoods and softwoods out of ground contact
1990 - IRG/WP 3592
A number of fungicides were tested as brush treatments for protection of southern pine, Douglas-fir, maple, and red oak against decay above ground. Cross-brace and L-joint test units were treated just before assembly and exposed from 3-10 years. Untreated Douglas-fir cross-brace units were not decayed at either the Mississippi or Madison, WI, site. Untreated red oak cross-brace units were not deca...
T L Highley


Relationship between stacking, location and antisapstain preservatives on visible degrade of Eucalyptus regnans and Pinus radiata boards
1999 - IRG/WP 99-20162
An antisapstain trial was established at a Eucalyptus hardwood sawmill in Victoria, Australia. The trial incorporated two commercial formulations of antisapstain preservatives, used at four different concentrations on both hardwood (Eucalyptus regnans F. Muell) and softwood (Pinus radiata D. Don) boards. The trial also utilised different stacking methods (block-stacked, sticker-stacked, and block-...
J Snow, P Vinden, S M Read


Effects of the addition of polyethylene glycol to the CCA-C preservative treatment
1985 - IRG/WP 3337
A modification of the CCA-C wood preservative system for utility poles has been investigated to see if spur penetration into the poles is assisted during climbing. Addition of polyethylene glycol to the CCA system has been shown to accomplish this purpose. This paper addresses the effects of the addition of polyethylene glycol to other physical properties germane to utility poles....
W P Trumble, E E Messina


The resistance of wood coated with different solvent-borne paints against colonisation by decay fungi
2009 - IRG/WP 09-40468
This paper examines different solvent-borne paints characteristics and their decay resistance when applied on pine wood surface. It was determined by the standard ENV 839 procedure. The part of samples were subjected to accelerated ageing according to the EN 84 standard. The discussed commercial paint systems were typical stains or penetrating oil-based products, with or without biocides....
B Mazela, P Hochmańska


Effects of timber surface properties and dipping conditions on uptake of antisapstain actives from two aqueous suspensions, and ultimate effects on efficacy against mould and staining organisms
1995 - IRG/WP 95-30073
Green-off-saw rough sawn Pinus elliottii (slash pine) boards were dipped in aqueous suspensions of two antisapstain formulations, and the resultant surface retentions of active ingredients MTC (methylene bisthiocyanate), CTL (chlorothalonil) or TCMTB (2(thiocyanomethylthio)benzothiazole) were monitored by chemical analysis. Surface retentions increased with suspension concentration and surface rou...
M J Kennedy, T L Woods


Surface Barriers for Protection of Culture and Heritage Wooden Objects from Insect Attack
2004 - IRG/WP 04-40286
Anoxic treatment is an environment friendly procedure for eradication of wood boring insects in wooden objects of cultural and historical heritage. However, after the anoxic treatment, wooden antiques remain susceptible to further insect attacks. Possible protection against insects could be provided by the so-called post-repression protective barriers. Potential coating materials for such barriers...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


Evaluation of the leach resistance and preservative efficacy of novel biocides as surface treatments applied by brush to spruce (Picea abies)
1998 - IRG/WP 98-30170
The comparative leach resistance and preservative efficacy of a number of alternative organic preservatives (available from Zeneca Specialties) and selected commercially available biocides as surface coatings to wood in Hazard Class 3 have been assessed. Two concentrations of test preservatives were applied by brush to Spruce (Picea abies), including formulation and untreated controls. A leaching ...
I M Tierney, A Bruce, D C R Sinclair, T Yeates


Factors affecting the sorption of preservative during diffusion treatment of wood
1988 - IRG/WP 3500
The sorption of preservative into wood during soaking in aqueous solution was found to comprise absorption as well as diffusion of solute. Absorption was increased by partially seasoning the wood prior to soaking and was characterised by (a) a very rapid initial rate of uptake and (b) an extended period of slow uptake, the rate of which varied with prior conditioning. It was concluded that some pa...
P Vinden


The effect of service life and preservative treatment on the hardness of wooden poles
1989 - IRG/WP 3537
The surface hardness of utility poles is an important parameter which effects the acceptability of the pole as being safe to climb during line maintenance. The current investigation was designed to evaluate how the surface hardness of preservative treated utility poles is effected by the type of preservative, and the age of the poles. Chromated-copper-arsenate (CCA) treated red pine and jack pine ...
E B Jonsson, E M A Nilsson, J N R Ruddick


Inspection method of surface checking of Sugi posts
2003 - IRG/WP 03-20272
In order to establish the method for evaluating the checking of Sugi posts, checks on exposed posts were examined. Checks on Sugi posts exposed for 18 months were superficially inspected, that is, the length, width, and depth of the checks were measured from the outside with a ruler and 0.1 mm thick feeler gauge. Then, each post was cut into cross sections of the 30 mm width, and the check depth w...
H Kurisaki, H Nakatani, K Mizumoto


Washboard effect: A surface deformation of spruce resulting from vacuum-pressure impregnation with water-borne preservatives
1987 - IRG/WP 3450
The washboard effect has been observed in sawn spruce after both commercial and laboratory based preservative treatments and is of increasing economic importance. The effect is defined as a specific phenomenon at the wood surface. It is distinct from internal collapse in the wood, but it may occur in association with internal collapse damage. Experimental investigations on the causes of washboardi...
H Willeitner, R J Murphy


Next Page