IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 228 documents. Displaying 25 entries per page.


Effects of timber surface properties and dipping conditions on uptake of antisapstain actives from two aqueous suspensions, and ultimate effects on efficacy against mould and staining organisms
1995 - IRG/WP 95-30073
Green-off-saw rough sawn Pinus elliottii (slash pine) boards were dipped in aqueous suspensions of two antisapstain formulations, and the resultant surface retentions of active ingredients MTC (methylene bisthiocyanate), CTL (chlorothalonil) or TCMTB (2(thiocyanomethylthio)benzothiazole) were monitored by chemical analysis. Surface retentions increased with suspension concentration and surface rou...
M J Kennedy, T L Woods


Performance results of wood treated with CCA-PEG
1986 - IRG/WP 3363
The addition of polyethylene glycol (PEG) to the CCA system has been shown to reduce the surface hardness of poles and ease spur penetration during climbing. This paper addresses the results of tests dealing with preservative retention and penetration, permanence of CCA and PEG, strength, drying rate, and checking characteristics....
W P Trumble, E E Messina


Surface retentions of PCP, TCMTB and MTC obtained during a field trial of antisapstain formulations
1993 - IRG/WP 93-20002
Formulations containing NaPCP or TCMTB and MTC were included as reference products in a recent field trial of antisapstain formulations in Queensland. Retentions of these actives on the surface of treated sawn Pinus elliottii were monitored by ultrasonic solvent extraction of excised samples and analytical determination by high performance liquid chromatography. Distribution of actives with depth ...
D E Ferlazzo, M D Needham, M J Kennedy


Field trial with poles of Scots pine treated with six different creosotes
1996 - IRG/WP 96-30115
In the middle of the 50's field trials with creosote-treated poles were started in France, Germany and Sweden. The trials were initiated by WEI (Western-European Institute for Wood Preservation). Six different creosotes were used and 40 poles per creosote were installed at each test field. Results after 39 years of exposure in Simlangsdalen, Sweden are reported. Poles treated with a heavy...
Ö Bergman


JWPA method for testing effectiveness of surface coatings with preservatives against decay fungi
1981 - IRG/WP 2164
In 1979 JWPA established a new method for testing effectiveness of surface coatings in accordance with practical use of preservative-treated lumber. Comparing the new testing method with JIS A 9302, a few new trials - size of wood specimen, weathering procedure, and decay-test procedure - are incorporated....
K Tsunoda


Dimensional stability and decay resistance of hot-melt self-bonded particleboard by surface benzylated pine chips
1991 - IRG/WP 3652
Akamatsu (Pinus densiflora Sieb. et Zucc: Japanese red pine) particles were pretreated with 40% NaOH solution and benzylated with benzyl chloride, and the surface of particle was converted into meltable materials. Hot-melt self bonded particleboard having smooth and high glossiness surface was prepared by hot pressing at 150°C and 1.96 MPa without using any conventional adhesives. Dimensional sta...
M Kiguchi, K Yamamoto


Blue stain in service on wood surface coatings. Part 3: The nutritional capability of Aureobasidium pullulans compared to other fungi commonly isolated from wood surface coatings
1993 - IRG/WP 93-10035
The nutritional capability of Aureobasidium pullulans was previously examined, using agar plate tests, with regard to nutrient sources that are potentially available in fresh and weathered wood (Sharpe and Dickinson, 1992). This study compared these findings with the nutritional capability of four other fungi (Alternaria sp., Cladosporium cladosporoides, Stemphylium sp. and Trichoderma sp.) common...
P R Sharpe, D J Dickinson


A proposal for an international wood preservation standard
1994 - IRG/WP 94-20031
Two factors are driving the need for an international wood preservation standard. First, the global need to use our natural resources more wisely and second, the movement towards free trade exemplified by the General Agreement on Tariffs and Trade. The International Research Group on Wood Preservation is the ideal organisation to undertake the task of developing such a standard. This paper is inte...
P I Morris


Leaching of the new boron based biocide from coated wood
2001 - IRG/WP 01-30267
We investigated leachability of the new boron based biocide - a complex of an amine and boric acid - from vacuum impregnated spruce wood samples. It was determined by the standard ENV 1250-2 procedure that the new biocide is susceptible to leaching so from the water borne as well as from the ethanol borne boron containing preservative treated wood. Leaching may be retarded by application of surfac...
M Petric, M Pavlic, F Cadez


A case study on quality control on telephone poles as a cost saving tool in Tanzania
1987 - IRG/WP 3418
A sample of 28 CCA treated Eucalyptus poles from a lot of 2,000 poles awaiting delivery to the field, was studied to reveal the quality of treatment. Results showed a product of very poor quality. Average figures for penetration and retention were 8.4 mm and 2.2 kg/m³; these results are 66% and 91% below the required standards, respectively. Consequences of such results are estimated to amount to...
K K Murira


Light organic solvent preservative treatment schedules for New Zealand-grown radiata pine
1986 - IRG/WP 3379
The influence of pressure differential and treatment time on preservative uptake and distribution in radiata pine heartwood and sapwood is investigated. Treatment schedules are defined which minimise solvent usage but ensure complete sapwood penetration and optimise heartwood penetration....
P Vinden


Problem of the treatment of dried sawn spruce building timbers with water-borne preservatives. Interim reports for discussion at the 4th Annual Meeting in West Berlin on 27 October 1972
1972 - IRG/WP 311
One of the most difficult technical problems facing the preservation industry is how to improve the treatment of refractory species of timber such as spruce. Its resistance to penetration, even under pressure' precludes its use for more hazardous service situations, and even in less severe conditions a higher level of treatment would be desirable. The importance of this subject led us to ...
W Liese, J W W Morgan, T Hof, R O Ullevålseter


Effects in vivo of various tensides (surface-active agents) on Reticulitermes santonensis De Feyteaud
2001 - IRG/WP 01-10417
The results of studies of surface active agents (tensides, surfactants) on the feeding behavior and mortality of Reticulitermes santonensis De Feyteaud are described. The effects of these agents on the nature and relative populations of eight gut-inhabiting symbionts are also examined. Among the various tensides tested, bee's poison was the most effective in causing rapid termite death. A...
W Unger


Blue stain in service on wood surface coatings. Part 2: The ability of Aureobasidium pullulans to penetrate wood surface coatings
1992 - IRG/WP 92-1557
The ability of Aureobasidium pullulans to penetrate seven different wood surface coatings was examined. Eight isolates of Aureobasidium pullulans were used. Following penetration, light microscopy was used to examine the effect of the fungus upon the coating, and growth at the wood-film interface. The fungus showed different growth capabilities with different types of surface coatings. Some isolat...
P R Sharpe, D J Dickinson


Rational weight per weight (w/w) qualifying retention from a pole bank in Bangladesh
2000 - IRG/WP 00-40187
Weight per weight (w/w) vs weight per volume (w/v) retention study revealed that the w/w % retention is found to be appropriate and uniform for all timber species in respect of its real effectiveness. The pole species having density below 512 kg/m3 (32pcf.) showing w/v retention below 20kg/m3 (1.25pcf.) have equal w/w retention of 4%. The apparently reduced w/v retention of low density poles will ...
A K Lahiry


Treatment behaviour of fresh and inservice catamaran logs
2001 - IRG/WP 01-30255
Catamaran is a conventional fishing craft fabricated by lashing 4 - 6 shaped logs of soft timber together. Over 73,000 of these craft fabricated out of 165,000 m3 of wood are in use along the vast east coast of India. Each craft lasts for 5-7 years. Over 15,000 m3 of timber is required annually for repairs and replacements of the craft. Such huge demand exerts enormous pressure on the resources. I...
V Kuppusamy, M V Rao, M Balaji, K S Rao


Creosoted radiata pine by non-pressure methods
1988 - IRG/WP 3486
Posts of Pinus radiata have been impregnated with creosote by immersion for 1, 3, and 7 days, and by hot-and-cold open tank with hot bath temperatures at 40°C and 60°C. On the basis of the retention rates obtained, suitable procedures are described for wood elements that are going to be in ground contact, and an analysis is made of the way in which the variables tested affect the results....
M V Baonza Merino, C De Arana Moncada


Performance of surface-treated hardwoods and softwoods out of ground contact
1990 - IRG/WP 3592
A number of fungicides were tested as brush treatments for protection of southern pine, Douglas-fir, maple, and red oak against decay above ground. Cross-brace and L-joint test units were treated just before assembly and exposed from 3-10 years. Untreated Douglas-fir cross-brace units were not decayed at either the Mississippi or Madison, WI, site. Untreated red oak cross-brace units were not deca...
T L Highley


Marine borers as wood degraders in Bangladesh and their protection
1996 - IRG/WP 96-10186
Field study on timber piles used in Bangladeshi brackish waters revealed that untreated and pentachlorophenol treated piles drastically degraded by the attack of molluscs and pholads (marine borers). Adequately CCA-C impregnated (30 kg/m³ or 6% W/W dry oxide retention) timber piles can protect the attack of molluscs. It is very difficult to protect pholads which can invade naturally very durable ...
A K Lahiry


How best to specify retentions of preservative treatments: kg/m3 or % (m/m)
1998 - IRG/WP 98-20151
When specifying treatments according to the European Standard EN 351-1, retentions in the analytical zone are based on the amount of product found to be effective in biological tests; this is expressed in terms of the retention of the product per unit volume (kg/m3) for penetrating treatments and per unit area (g/m2) for superficial treatments. However, to check whether the retentions have been ac...
J K Carey


Light organic solvent preservative treatment of glue-laminated radiata pine
1986 - IRG/WP 3380
The high permeability of radiata pine (Pinus radiata D. Don) is associated with ray-tissue and in particular the cross-field pits linking ray-tissue to tracheids. This pathway is absent in the tangential grain direction, leading to poor preservative penetration when treatment is restricted to the radial face - for example, timber fabricated into glue-laminated beams....
P Vinden


Soft rot and bacterial decay in preservative treated eucalypt power transmission poles
1982 - IRG/WP 1155
Bacterial type decay was observed in CCA and PCP treated eucalypt power transmission poles. Detailed observations made with the SEM revealed bacterial colonisation and decay, especially in fibres. Plug samples taken from poles throughout Queensland were examined for preservative retention and presence of soft-rot decay. The severity of decay was different according to location, retention and speci...
L E Leightley


The influence of previous anti-blue-stain preservative treatments on the fixation of CC in spruce
1997 - IRG/WP 97-30134
Freshly cut and kiln dried spruce boards were treated with 4 different anti-blue stain preservatives (ABP). After a period of 10 days allowing the samples to dry and fixate, the samples were treated with CC (chromium, copper formulation) using a vacuum pressure cycle. After impregnation the wood was steam fixed. A submersion leaching test showed differences in the leachable quantity of copper and ...
M Van der Zee, W J Homan


Surface Barriers for Protection of Culture and Heritage Wooden Objects from Insect Attack
2004 - IRG/WP 04-40286
Anoxic treatment is an environment friendly procedure for eradication of wood boring insects in wooden objects of cultural and historical heritage. However, after the anoxic treatment, wooden antiques remain susceptible to further insect attacks. Possible protection against insects could be provided by the so-called post-repression protective barriers. Potential coating materials for such barriers...
M Petric, M Pavlic, B Kricej, M Humar, F Pohleven


Evaluation of the leach resistance and preservative efficacy of novel biocides as surface treatments applied by brush to spruce (Picea abies)
1998 - IRG/WP 98-30170
The comparative leach resistance and preservative efficacy of a number of alternative organic preservatives (available from Zeneca Specialties) and selected commercially available biocides as surface coatings to wood in Hazard Class 3 have been assessed. Two concentrations of test preservatives were applied by brush to Spruce (Picea abies), including formulation and untreated controls. A leaching ...
I M Tierney, A Bruce, D C R Sinclair, T Yeates


Next Page