IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1012 documents. Displaying 25 entries per page.


Preservative effect of cellulose insulation material against some mould fungi and brown rot fungus Coniophora puteana in pine sapwood
1991 - IRG/WP 1484
The influence of mineral wool and loose-fill cellulose wool on biodeterioration of pine sapwood was studied. The test fungi were mould fungi Aspergillus versicolor, Cladosporium sphaerospermum, Penicillium sp. and Aureobasidium pullullans and brown rot fungus Coniophora puteana. Cellulose wool inhibited the growth of mould fungi on the face of wood contacted with insulation material at RH of 97 an...
H Viitanen


The suitability of high pressure sap-displacement for the retention of UK grown spruce and pine
1990 - IRG/WP 3595
The concentration and radial distribution of copper, chrome, arsenic (CCA), and the moisture content and depth of radial checking in UK grown, field exposed spruce and pine poles treated by high pressure sap-displacement are examined. The concentration of CCA elements in samples obtained from increment cores is similar in Norway spruce, Scots pine and Corsican pine but is significantly lower in Si...
P D Evans, S D Hainey, A Bruce, G M Smith, B King


The effect of primary blue-staining fungi on the strength properties of Scots pine sapwood
2004 - IRG/WP 04-10515
The fungi action may have influence on wood properties especially Basidiomycotina fungi causing wood decay. The investigation of influence of fungi causing mainly wood discoloration and disfigurement on wood properties is still in development process. There were determined the differences between the bending strength, the compression along the grains and impact strength of control and blue stained...
A Fojutowski


Field and greenhouse testing of window joinery of pine and spruce treated with LOSP
1991 - IRG/WP 3658
Norwegian window frame components of full size were double vacuum-treated with TBTN and TBTO, and connected as 'L-joints' and subsequently coated with stains. The corner sections were exposed (out of ground contact) both in field (temperated coastal climate, Taastrup, Denmark) and in a greenhouse (Uppsala, Sweden). The window frame L-joints of spruce (Picea abies Karst.) - treate...
F G Evans, B Henningsson, E Borsholt


Models of the critical time of humidity and temperature conditions for the development of mould fungi in pine and spruce sapwood
1995 - IRG/WP 95-20066
Regression models of the time factor for the growth of mould fungi in pine and spruce sapwood are studied. The first group of models are based on the results of exposures of mould fungi in static humidity and temperature conditions indicating the time for the start of mould growth in wood. The second group of models are based on the exposures of mould fungi in fluctuating or alternating humidity a...
H Viitanen


Micromorphology of Schizophyllum commune attack in pine (Pinus sylvestris) wood
1983 - IRG/WP 1184
The decay pattern caused by Schizophyllum commune in pine latewood tracheids was studied using both light and transmission electron microscopy. The attack began as isolated concentric slits within the S2 layer with extensive lamellation and separation of individual wall layers observed in subsequent stages of decay. The slits resulting from attack appeared to be formed in thin, regular concentric ...
T Nilsson, G F Daniel


Leachability of didecyldimethylammonium chloride (a quaternary ammonium compound) from four wood species
1982 - IRG/WP 3204
Sapwood blocks prepared from red pine, ponderosa pine, southern yellow pine and hem-fir (a commercial mixture of western hemlock and amabilis fir) were treated with didecyldimethylammonium chloride, (an alkylammonium compound, AAC). After oven drying the blocks were vacuum impregnated with distilled water and subjected to a static leach cycle for 48 hours. The leachate was analyzed and the amount ...
J N R Ruddick, A R H Sam


Screening of the efficacy of tall oils against wood decaying fungi
2004 - IRG/WP 04-30354
Tall oil is a by-product in pulping of resinous wood by the sulphate process. Tall oil contains a complex mixture of wood extractives. Some of these extractives act as natural protection against wood decaying fungi while other serve as nutrition for the fungi. This report describes a screening of the efficacy of four refined tall oils with different chemical composition on wood decaying fungi. ...
G Alfredsen, P O Flæte, A Temiz, M Eikenes, H Militz


Effect of humidity fluctuations on mould growth on pine wood
1989 - IRG/WP 1412
Most studies on mould development on wood material have been made at constant moisture conditions during the experimental period. As a consequence of such studies, a maximum permittable humidity level to avoid mould problems in wood constructions has been recommended. In the practical situation, the constructions are seldom subject to constant humidity or temperature. In the present paper, we repo...
J Bjurman


Mould growth at lumber surfaces of pine after kiln and air drying
1994 - IRG/WP 94-40033
Distribution of water soluble substances in green wood and later redistribution during drying is of importance for the colonisation of wood by microorganisms. According to literature the availability of nitrogenous materials is probably a major limiting factor to the microbial colonisation of wood. King et al. (1974) and Oxley et al. (1976) have shown correlation between surface nutrient concentra...
N Terziev, J Bjurman, J B Boutelje


Natural durability of larch heartwood against decay
1997 - IRG/WP 97-10201
Larch heartwood has been promoted in Sweden and in other European countries as an alternative to preservative treated timber. It has even beeen stated that larch heartwood is more durable than preservative treated timber. This paper presents a compilation of facts from scientific reports on the durability of larch heartwood. Some recent data from this department are also reported. All data suggest...
T Nilsson


Differentiation of Scots pine heartwood and sapwood by near infrared spectroscopy
2003 - IRG/WP 03-10459
In Scandinavia Scots pine heartwood has, in recent years, gained popularity as material for external structures exposed to moderate risk of decay. As non-durable sapwood surrounds the heartwood in pine trunks it is of crucial importance to separate this wood from the heartwood during log processing into heartwood products. Heartwood and sapwood can be differentiated by visual evaluation of colour ...
P O Flæte, E Ystrøm Haartveit


Effect of Pseudomonas cepacia on the activity of a mixture of wood staining fungi on ponderosa pine sapwood
1995 - IRG/WP 95-10107
There are major incentives for limiting the degree of fungal discoloration which occurs during wood processing. Most lumber producers apply prophylactic fungicides which limit microbial growth, but increasing restrictions on the use of these chemicals have encouraged the search for alternative stain prevention strategies. Among the possible strategies for stain prevention is biological control. Wh...
J J Morrell, R K Velicheti


Study of modulus of rupture, circumference taper, sapwood thickness and CCA treatment of Norwegian origin Pinus sylvestris poles
1994 - IRG/WP 94-20054
Nondestructive strength testing with Pilodyn (6J) of Norwegian Pinus sylvestris poles revealed effective modulus of rupture (MOR) of 54.39 N/mm² at wet conditions after CCA-C treatment and circumference measurement revealed circumference taper of 0.021 m/n. Sapwood thickness or penetration of CCA-C study revealed that 77% poles were with sapwood thickness equivalent to 39.6% of radius of poles an...
A K Lahiry, S Begum, G N M Ilias, M A B Fakir, R U Hafiz


Studies and experiences of occurrence and development of soft rot in salt-treated poles of pine (Pinus sylvestris) installed in Swedish transmission lines in the years 1940-1945
1977 - IRG/WP 277
The present work describes the result of microscopic examinations of some 2,000 borings extracted from 20 to 23-year-old salt-treated poles (Scots pine) from the southern and central parts of Sweden. The purpose was to map out the occurrence of soft rot in Sweden and its influence on the mechanical strength of the poles as well as to contribute to the development of new and more satisfactory metho...
H Friis-Hansen


The development of blue stain in service in sapwood of European softwood species
1997 - IRG/WP 97-10236
The utilisation of softwood species for window joinery applications is gaining importance in countries frequently using tropical hardwood species up to now. Since wood preservation is not always part of the total concept of window frames manufactured from sapwood containing wood elements it is essential to know the impact of durability on the performance. Moisture content control is a major tool i...
J Van Acker, R Klaassen, H Militz, M Stevens


Biological control of internal decay in Scots pine poles: A seven year experiment
1992 - IRG/WP 92-1529
The interactions between key fungi were monitored, by non-destructive and destructive sampling methods, during the course of an experiment on the effectiveness of Scytalidium sp. and Trichoderma spp. for eliminating established infections of Lentinus lepideus (Fr. ex Fr.) Fr. in creosoted Pinus sylvestris poles. Although extensively isolated at the beginning and end of the experiment, Trichoderma ...
P I Morris, D J Dickinson, B Calver


An analysis of the effects of some factors on the natural durability of pine (Pinus sylvestris L.) and spruce (Picea abies Karst.)
1986 - IRG/WP 1279
The effects of some factors on the natural resistance of pine and spruce sapwood against fungal decay and against attack of house-longhorn beetle larvae have been studied in laboratory tests and the results are evaluated by analysis of variance and regression analysis. Following conclusions were reached: Wood from summer-felled trees did not have a lower inherent natural durability against fungal ...
J B Boutelje, T Nilsson, S Rasmussen


Le pin: Matériau à contact alimentaire [Pine wood as a material for food contact]
1995 - IRG/WP 95-50040-01
Monoterpenes emitted to air from woods of pine (Pinus nigra, Pinus laricio, Pinus pinaster and Pinus sylvestris) were determined on the one hand by static analysis and by other hand by sampling on the Tenax adsorbent, followed by analysis using thermal desorption, both being combined with gas chromatography coupled with mass spectrometric detection. The major monoterpenes were alpha-pinene and 3-c...
A Waymel, M Lamour, G Labat


The natural durability of wood in different use classes - PART II
2006 - IRG/WP 06-10598
The natural durability of important European wood species has been tested on 3970 speci¬mens in field trials. The wood was exposed at five test sites in Germany with different climates, at each site in European use class 4 and 3 (with and without soil contact). Within European use class 3 three different expositions were tested: vertical with sheltered end grain, vertical unsheltered and horizont...
A O Rapp, U Augusta, K Brandt


Moisture correction for ultrasonic MOE measurements above fibre saturation point in Scots pine sapwood
2006 - IRG/WP 06-20333
There is a high correlation between methods for dynamic modulus of elasticity (MOEdyn) and static modulus of elasticity (MOEstat). MOEdyn methods have been found sensitive to detect early stages of decay and may be seen as an option for non-destructive wood durability testing. As the MOEstat measurements do not change after reaching the fibre saturation point, the uncorrected MOEdyn data from ultr...
E Larnøy, G Alfredsen, H Militz


Validity of above ground testing according to ENV 12037
2008 - IRG/WP 08-20379
The standard ENV 12037 for testing of treated and untreated wood (lap-joint) exposed above ground was issued in 1996 by The European Committee for Standardization. A draft for the development of the standard was presented by CEN-TC 38/WG 25/DOC N 076 in 2002. For a test to become valid the median rating of decay for untreated control replicates (Scots pine sapwood) must be equal or greater than ...
Ö Bergman, U Råberg, N Terziev


Variations of Furfuryl alcohol and Wolmanit CX-8 treatability of pine sapwood within and between trees
2008 - IRG/WP 08-40421
The variations on the ratio of filling (RoF) were investigated on Norwegian grown Scots pine (Pinus sylvestris). The samples were taken from 10 different stands in south-east Norway, and treated with furfuryl alcohol and a copper-containing wood preservative. Both within tree variations, between tree variations and variations between stands were investigated for significant differences. Factors li...
E Larnøy, S Lande, G I Vestøl


Testing of decay resistance of sapwood and heartwood of thermally modified Scots pine and Norway spruce
2010 - IRG/WP 10-40523
Thermal modification at elevated temperatures changes the chemical, biological and physical properties of wood. One of the main targets of thermal modification is to increase the biological durability and decay resistance of wood. Although the effects of thermal modification on wood have been widely studied, the significance of sapwood and heartwood on the resistance of thermally modified wood has...
H Viitanen, S Metsä-Kortelainen


Basidiomycete colonization of Scots pine sapwood quantified by qPCR and TGA
2011 - IRG/WP 11-10750
Scots pine (Pinus sylvestris L.) is an important softwood species in Northern Europe and is frequently used as material for various wood protection systems. In Europe, EN 113 is the standard basidiomycete laboratory durability test method, using mass loss as evaluation criteria. In this paper quantitative real-time PCR (qPCR) and thermogravimetric analysis (TGA) was used to characterize coloniza...
G Alfredsen, S Bollmus, T K Bader, K Hofstetter


Previous Page | Next Page