Durability by design – a case study of the performance of wooden decks after 9.5 years of natural weathering
2019 - IRG/WP 19-20648
The service life expected for wood decking manufactured with poorly durable wood species, left untreated and exposed to severe environmental conditions such as high humidity and active biological agents, is usually assumed to be short (less than 10 years). The current classification of wood’s natural durability is based on EN standardised tests which do not fully reflect the real end-use conditi...
M Kutnik, M Montibus


Quantifying the effect of microclimatic parameters on the moisture-induced decay risk of wooden structures
2019 - IRG/WP 19-20649
Wood exposed outdoors is prone to fungal degradation. Besides its material-inherent resistance, numerous factors are impacting on its service life with both, climate and design having a major effect. In addition, topography, shading, wind barriers, and other local parameters have an effect on the microclimatic conditions at site and therefore need to be quantified for service life prediction of wo...
L Emmerich, C Brischke


Improvement of analytical methods of wood preservatives and its validation with collaborative testing
2019 - IRG/WP 19-20655
This discussion paper presents on-going collaborative test of analytical methods of wood preservatives according to the standardization process of Japan Agricultural Standard (JAS) by the Ministry of Agriculture, Forestry and Fisheries (MAFF). Food and Agricultural Materials Inspection Center (FAMIC) in close cooperated organization with the MAFF, has wide range of tasks about inspections and anal...
T Miyauchi, K Yamamoto, N Shota, Y Akabori, M Ikeda, J Eisawa, K Kambara, T Osawa, C Igarashi, Y Baba, W Ohmura, M Shimizu, M Samejima


Exploring the use of X-ray micro CT as a tool for the monitoring of moisture production and mass loss during lab-based fungal degradation testing
2019 - IRG/WP 19-20654
Bio-based building materials, such as wood and wood-engineered products, are susceptible to degradation by decay fungi. In-depth knowledge on the intricate material-fungus relationship as well as performance data for many bio-based building materials are still lacking, and especially knowledge on how a material’s structure and moisture properties affect the degradation process is missing. Althou...
L De Ligne, J Van den Bulcke, A De Muynck, J M Baetens, B De Baets, L Van Hoorebeke, J Van Acker


Efficacy of microwave treatments against Pine Wood Nematode
2019 - IRG/WP 19-20658
The pine wood nematode Bursaphelenchus xylophilus (Steiner and Buhrer) Nickle (PWN) is the causal agent of “Pine wilt disease” affecting coniferous forests, and since its detection in 1999 in Portugal, has obliged the European Union to take action to prevent its spread (Decision 2006/133/CE). One of the main measures applied is the International Standard for Phytosanitary Measures ISPM No. 15 ...
L Robertson, M T Troya, F Llinares, J C Cabrero


Durability classification of preservative treated and modified wood
2019 - IRG/WP 19-20659
EN 350 (2016) allows formally to determine durability classes (DC) for wood products and wood-based materials, which was previously only possible for untreated wood in the form of natural durability. In a first study, the University of Goettingen carried out the durability classification of chemically modified (modified with 1,3-dimethylol-4,5-dihydroxyethyleneurea, DMDHEU) and preservative-treate...
S Bollmus, L Bachle, C Brischke, H Militz


Impact of water holding capacity and moisture content of soil substrates on the moisture content of wood in terrestrial microcosms
2019 - IRG/WP 19-20662
Terrestrial microcosms (TMC) are frequently used for testing the durability of wood and wood-based materials as well as the protective effectiveness of wood preservatives. In contrary to experiments in soil ecology sciences, the experimental set-up is usually rather simple. However, for service life prediction of wood exposed in ground, it is of immanent interest to better understand the different...
C Brischke, F L Wegener


Development of accelerated decay test for CLT using a fungus grown on agar medium
2019 - IRG/WP 19-20664
CLT is a large-scale wooden board which consists of several layers of sawn lumber stacked in altering directions. Therefore, a lot of large cross sections appear on all narrow faces of CLT. As water penetrates easily into timber from cross section, wooden material whose cross section is exposed to water in in a usage environment is susceptible to deterioration by organisms. Wood deterioration orga...
T Miyauchi, K Kambara, W Ohmura, T Mori, H Matsunaga, N Hattori


Application of nano metal fluorides against termites
2019 - IRG/WP 19-30733
Recent research has shown that fluorides such as NaF have potential as a wood preservative against termite attack (Pan and Wang, 2015). However, NaF has high leaching susceptibility because of its solubility (40 g/l ) which can reduce its efficacy over long term. Metal fluoride nanoparticles such as MgF2 and CaF2 present a viable alternative to water soluble fluoride-based wood preservatives as th...
S M Usmani, K Klutzny, Y de Laval, R Plarre, D McMahon, I Stephan, T Hübert, E Kemnitz


Use of resin obtained from Italian guayule crops for wood preservation purposes: some preliminary results
2019 - IRG/WP 19-30736
The potential of guayule (Partenium argentatum Gray) as a source of anti-termite, anti-fungal and insect repellent products to be used in wood preservation, has been largely explored in the past. The fact that such products are obtained as byproducts in the process of natural rubber extraction from this plant, thus increasing the profit of the process, together with the ability of this crop to gr...
S Palanti, E Conti, M Russo, F Stefani, C Querci


Relative efficacy of various oxine copper formulations against brown-rot fungi
2019 - IRG/WP 19-30741
This paper investigates the relative resistance of three different oxine copper formulations (oil-borne, water-borne, water-borne with pH-adjustment) as a preservative treatment for wood against brown-rot fungi. Impregnated southern pine sapwood cubes were exposed to R. placenta and G. trabeum cultures in a soil-block test. After eight weeks, the weight losses of the cubes were examined in relatio...
M Petruch, J Lloyd, A Taylor


Alternative fumigants to Methyl Bromide for wood products: Review of the development and preliminary tests of Ethane Dinitrile (EDN) in Canada
2019 - IRG/WP 19-30743
This paper reviews recent developments and updates in the search for alternative fumigants to ozone-depleting methyl bromide, for wood products fumigation. The absence of alternative treatments may result in significant market disruption if further restrictions on methyl bromide are imposed. This paper reviews key challenges and key attributes of an ideal fumigant and also the status of standardis...
A Uzunovic


The development of a suitable fire retardant for Radiata pine and other species
2019 - IRG/WP 19-30744
The use of fire retardant chemicals, with the overarching aim of creating a safer environment is not a new one, however it is generally under-developed and is often afflicted with an image of environmental and health issues and misperceived high costs. There is an ever-increasing need and desire for effective fire retardancy in timbers to inhibit or suppress the combustion process. This is paramou...
B R Derham, M R Fortune


Exemplary aboveground hardwood protection from Coptotermes curvignathus under weathered conditions conferred by proprietary microemulsion-based cypermethrin (SARPECO®) and permethrin (AXIL®) biocides
2019 - IRG/WP 19-30749
SARPECO® (with cypermethrin) and AXIL® (with permethrin) solutions are water-based wood preservatives approved for dipping treatment providing 25 years of termite protection for solid wood and wood-based products in Europe and for more than 10 years in Indonesia. SARPECO® and AXIL® solutions are patented formulations based on concentrated microemulsions (ME) diluted with water as a dipping tre...
D Messaoudi, A H H Wong, C A D Tawi, N Bourguiba, O Fahy


Preservative Treatment of CLT: An Example at Shimojishima Airport
2019 - IRG/WP 19-30748
Cross laminated timber (CLT) is a relatively new construction method that allows multi-storey construction using solid wood instead of concrete or steel. It is a method favoured by progressive architects and recognized for its much lower environmental footprint. Wood is an excellent construction material and is a long-term carbon sink that also performs well in the event of earthquakes and fire....
J Lloyd, N Yamashita, A Taylor


Effect ofNano-Copper Oxide on Decay Resistance of Pistachio Twig-Plastic Composite
2019 - IRG/WP 19-30750
The goal of our study was to investigate the decay resistance of pistachio twig-plastic composite treated with nano-copper oxide against the white rot fungus Trametes versicoloer and the brown rot fungus Coniophora puteana. For this purpose, wood–polypropylene composites (WPCs) containing different loadings of nano-copper oxide, namely 0, 1, 2 and 3 percent (W/W), were made from pistachio (Pista...
M R M Farahani,S Pourabdollah


Suggestive remarks for designing of experimental samples and trial devices to treat wood by pre-vacuumed immersion method
2019 - IRG/WP 19-40862
This study was conducted to test the impregnability of wood material according to the pre-vacuumed immersion process and to reveal the usability of cylindrical (plug) samples in impregnation experiments in addition to the cuboid or cubic samples. In this context, cuboids were prepared 30 mm in length, 20 mm in width and 20 mm in thickness, whereas plugs were prepared radially and longitudinally wi...
I Usta


Color change of timber exposed outdoors - Influence of season exposure test starts
2019 - IRG/WP 19-40865
For the client the material and color of the exterior wall are important, because they affect the impression of the building [1]. However, discoloration of the exterior wall begins as soon as the building is completed, by various factors such as rainfall. We tried to quantitatively evaluate the changes of the exterior wood, and to organize the influences of climate conditions, in order to use the ...
K Usami, H Ishiyama


Gloss and hardness variations as early indicators of wood coating failure during weathering tests
2019 - IRG/WP 19-40866
The objective was to track early changes which ultimately will lead to coating failure when exposed to artificial weathering. Two different coatings (one waterborne acrylic paint and one solventborne alkyd stain) were exposed to artificial weathering for 2016 hours according to EN 927-6. Every 168 hours, samples were removed from the artificial weathering device for assessment (general appearance,...
L Podgorski


Potential Use of the Pigment from Scytalidium cuboideum and Chlorociboria aeruginosa as an UV-light Protection Additive in Oil Finishes
2019 - IRG/WP 19-40868
UV-light degradation of wood is one of the top reasons for consumer replacement of outdoor wooden structures. This type of degradation is seldom mechanical, and is instead often motivated by loss of aesthetics (graying). There are numerous commercial products available on the market that deal with this loss of color, many of which contain added pigments to ‘rejuvenate’ or ‘revitalize’ grey...
S M Vega Gutierrez, D W Stone, R He3, P T Vega Gutierrez, Z M Walsh, S C Robinson


Charring of Norway spruce wood surface – an alternative surface modification technique?
2019 - IRG/WP 19-40870
Charring is an old wood surface treatment technique, mainly performed on wooden façade elements with the aesthetical aims, but also with the purpose of protection. This flame treatment method can be grouped into heat treatment processes. Below the top charred layer of damaged wood there is a layer which is during flame treatment exposed to high temperatures in anoxic or semi-anoxic conditions. Th...
M Petric, M Pavlic, J Zigon


Protecting wood exterior infrastructures above ground in Spain. The importance of protection by design in the performance
2019 - IRG/WP 19-40874
Across Spain is very common to find wood exterior infrastructures build mainly in sawn and glue-laminated wood. Most of these exterior wood infrastructures use softwood wood species such as: fir, spruce, larch and pine. In Spain exterior wood infrastructures, became more and more popular since nineties, when sawn and glue-laminated wood were utilized for building exterior wood infrastructures in o...
D Lorenzo, M Touza, J Fernandez-Golfín, A Lozano, J Benito, M T Troya, L Robertson


The impact of additional interior layers to the moisture dry-out and mould growth risk of CLT walls
2019 - IRG/WP 19-40876
The objective of this study was intended to determine the maximum allowable initial moisture content for CLT walls having both exterior and interior thermal insulation. A laboratory test was conducted, for which four test walls with two different insulation solutions and two different initial moisture contents were built. Based on the test results a simulation model was configured and simulations ...
V Kukk, J Kers, T Kalamees


The anti-weathering mechanism of extractives in thermally modified Scots pine
2019 - IRG/WP 19-40880
Results from the electron spin-resonance spectroscopy (ESR) analysis indicated that thermally modification of wood can inhibit the generation of phenoxyl radicals during UV irradiation and consequently lead to the increase of the color stability of wood. In order to clarify the evolution and role of extractives in thermally modified wood during the process of weathering, the compositions of aceton...
H Shen, J Cao


Effect of pretreatment of wood surfaces with a copper monoethanolamine solution on the natural weathering performance of semitransparent stains
2019 - IRG/WP 19-40881
Semitransparent stains for wood products are favored for outdoor applications in Japan because these finishes do not hide the wood grain. However, the photoprotective effects of wood surfaces are low, therefor there is a need to improve the weathering performance. We examined the natural weathering performance of semitransparent stains on wood pretreated with a copper monoethanolamine solution (Cu...
S Isaji, H Shibui, Y Hirabayashi