Your search resulted in 1235 documents. Displaying 25 entries per page.


A six-year ground proximity trial of TRU-CORE treatments at Innisfail, Queensland
2023 - IRG/WP 23-30775
This article describes an H3 (above ground outdoor) ground proximity field trial that compares the performance against decay fungi of TRU-CORE (also known as the Buffered Amine Oxide Enhancement System) Copper Quat (CQ) with CCA and commodity Alkaline Copper Quat (commodity-CQ) treatments, all in Pinus radiata. The retentions achieved reflected commercial practice, where higher mean retentions are...
L Cookson


Above Ground Proximity Decay Field Trial of Modified ACQ-A, Wolman® CA-B and Wolman® CA-C in Taiwan
2023 - IRG/WP 23-30793
An above ground proximity decay field trial was established at Chiayi county, Taiwan in July 2016. The purpose of this study was to generate local field performance data for Taiwan for Slash Pine treated with Wolman® CA-B, Wolman® CA-C and a modified ACQ-A product at AWPA UC3B actives retention. After 6 years of field trial, the efficacy of the wood preservative in preventing decay fungi and ter...
J-Y Gan


Wood above ground project – Results and future plans
2024 - IRG/WP 24-11041
In 2000, the Danish Technological Institute (DTI) initiated an extensive study to investigate the natural durability of wood. The study involved exposing wood in various orientations to assess its performance. A total of 35 wood material types were exposed at DTI test site in Taastrup, Denmark. Moisture content (MC) was measured through weighing for the initial five years, decay was assessed follo...
A W Christof, R Digaitis, P Fynholm, J Stenbaek, N Morsing, B Lindegaard


Potential of heartwood extracts as wood preservatives combined with linseed oil in 8-year above-ground and in-ground field trials
2024 - IRG/WP 24-20719
The current study assessed the efficacy of heartwood extracts from Tectona grandis, Dalbergia sissoo, Cedrus deodara, and Pinus roxburghii, combined with linseed oil, as protectants for two non-durable wood species against termites and decay fungi. Stakes measuring 45.7 × 1.9 × 1.9 cm and blocks measuring 12.5 × 3.75 × 2.5 cm of the sapwood of southern pine (Pinus sp.) and cottonwood (Populus ...
M E Mankowski, G T Kirker, B Hassan


Evaluation of the water exclusion ability and inherent bioactivity of heartwood against decay in Japanese and European wood species via above-ground exposure and water absorption tests
2024 - IRG/WP 24-40998
The natural durability of wood has been thought to mainly depend on bioactive extractives and the water exclusion ability. To clarify the contribution of each factor to wood durability, above-ground exposure tests were conducted on Japanese and European wood species. A double-layer test was carried out using heartwood specimens of four wood species, i.e., Japanese cedar, Japanese cypress, Scots pi...
T Osawa, R Noda, K Yamamoto


Modelling the service life of wood in ground contact – Verification of remotely sensed soil data from the reanalysis dataset ERA5-Land using in-situ measurements at a test site of utility poles in Eastern Norway
2024 - IRG/WP 24-41003
This study compared soil moisture and temperature estimates from the 5th European reanalysis (ERA5-Land) dataset with in-situ measurements to assess the accuracy and applicability of ERA5-Land data for modelling the service life of wood in ground contact. The ERA5-Land soil temperature estimates showed a moderate correlation with the in-situ temperature measurements (Spearman’s ρ of 0.73) and a...
U Hundhausen, P B van Niekerk, B Marais


Changes in decay risk of wood in ground contact over Europe, from analysis of historic climate conditions
2024 - IRG/WP 24-41008
Changing climate conditions will affect global temperature and precipitation patterns, shifting some geographical areas into states that are more suitable for fungal wood decay. Climate normals, which are taken over a 30-year period, capture vast spatial and temporal variations in these conditions and comparing these can show changes over time. Importantly, being able to identify locations that ha...
P B van Niekerk, B N Marais, G Alfredsen, C Brischke


Progress report on co-operative research project on L-joint testing
1983 - IRG/WP 2192
A F Bravery, D J Dickinson, M Fougerousse


Confocal laser scanning microscopy of a novel decay in preservative treated radiata pine in wet acidic soils
1997 - IRG/WP 97-10215
Light microscopy of radiata pine (Pinus radiata D. Don) field test stakes (20x20x500mm3) exposed in wet acidic (pH 3-4) soil for 12 - 24 months showed predominance of an unusual type of decay characte-rised by tunnelling attack of wood cell walls. After two years decay was moderate to severe in wood treated to ground contact CCA specifications and also equivalent retentions of creosote, and a numb...
R N Wakeling, Ying Xiao, A P Singh


Effect of acetylation on decay resistance of wood against brown-rot, white-rot and soft-rot fungi
1989 - IRG/WP 3540
Effect of acetylation on decay resistance of wood was investigated using wood blocks of Cryptomeria japonica, Pinus densiflora, Albizia falcata and Fagus crenata. Blocks were treated with uncatalyzed acetic anhydride for different lengths of time and exposed to Tyromyces palustris, Serpula lacrymans, Coriolus versicolor and unsterilized soil. The action of OH-radical on acetylated wood was also ex...
M Takahashi, Y Imamura, M Tanahashi


Field trial with poles of Scots pine treated with six different creosotes
1996 - IRG/WP 96-30115
In the middle of the 50's field trials with creosote-treated poles were started in France, Germany and Sweden. The trials were initiated by WEI (Western-European Institute for Wood Preservation). Six different creosotes were used and 40 poles per creosote were installed at each test field. Results after 39 years of exposure in Simlangsdalen, Sweden are reported. Poles treated with a heavy...
Ö Bergman


Proposed method for out-of-ground contact trials of exterior joinery protection systems
1981 - IRG/WP 2157
Methods for testing the efficacy of preservative treatments for exterior joinery are described using the format of a European Standard. Commercially used treatments applied to jointed test units (L-joints) which are then protected by conventional finishes are exposed to normal outdoor hazards out of ground contact. Assessment is made a) by determining eventual failure through decay and b) by destr...
J K Carey, D F Purslow, J G Savory


Questionnaire - Fungal decay types
1985 - IRG/WP 1265
T Nilsson


JWPA method for testing effectiveness of surface coatings with preservatives against decay fungi
1981 - IRG/WP 2164
In 1979 JWPA established a new method for testing effectiveness of surface coatings in accordance with practical use of preservative-treated lumber. Comparing the new testing method with JIS A 9302, a few new trials - size of wood specimen, weathering procedure, and decay-test procedure - are incorporated....
K Tsunoda


Wood preservatives: Field tests out of ground contact. Brief survey of principles and methodology
1976 - IRG/WP 269
This paper contains the following spots: 1.: The general need for field tests. 2.: Interests and limits of field tests in ground contact. 3.: Various methods in use for out-of-ground contact field tests. 4.: Fungal cellar tests are they an alternative to above-ground decay exposure tests? 5.: Conclusions....
M Fougerousse


Nondestructive Evaluation of Oriented Strand Board Exposed to Decay Fungi
2002 - IRG/WP 02-20243
Stress wave nondestructive evaluation (NDE) technologies are being used in our laboratory to evaluate the performance properties of engineered wood. These techniques have proven useful in the inspection of timber structures to locate internal voids and decayed or deteriorated areas in large timbers. But no information exists concerning NDE and important properties of wood composites exposed to dec...
B Illman, V W Yang, R J Ross, W J Nelson


Moisture content levels and decay of hemlock
1986 - IRG/WP 1287
As a model of decay conditions of wooden members in wooden houses, a decay test was set up in which samples of western hemlock (Tsuga heterophylla) under 4 moisture levels were examined. Each week the samples were weighed and if the weights indicated that their moisture contents were lower than the expected levels, distilled water was added. Every 8 weeks 3 samples from each condition were oven dr...
K Suzuki


Dimensional stability and decay resistance of hot-melt self-bonded particleboard by surface benzylated pine chips
1991 - IRG/WP 3652
Akamatsu (Pinus densiflora Sieb. et Zucc: Japanese red pine) particles were pretreated with 40% NaOH solution and benzylated with benzyl chloride, and the surface of particle was converted into meltable materials. Hot-melt self bonded particleboard having smooth and high glossiness surface was prepared by hot pressing at 150°C and 1.96 MPa without using any conventional adhesives. Dimensional sta...
M Kiguchi, K Yamamoto


Utilization of curcumin for detection of presence of boron in wood
1982 - IRG/WP 3191
It has been shown that curcumin is not a reliable reagent for detecting boron in wood that has been attacked by fungi...
M-L Edlund


Co-operative studies on determining toxic values against wood-destroying Basidiomycetes: Progress report to May 1989
1989 - IRG/WP 2339
This document reports progress on the co-operative study between nine laboratories set up following the proposals contained in Document IRG/WP/2316. Results have been received from two laboratories. Toxic values data have been established successfully using the test fungus Coniophora puteana but problems have been encountered with the other test fungi....
A F Bravery, J K Carey


Effects of acetylation on the dimensional stability and decay resistance of kenaf (Hibiscus cannabinus L.) fiberboard
1996 - IRG/WP 96-40059
The objective of this study was to investigate the influence of the acetylation treated kenaf fiber, Phenol formaldehyde resin content level, and three fungi species on the dimensional stability and decay resistance of high density non wood composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species were also ...
P Chow, T Harp, R Meimban, J A Youngquist, R M Rowell


The dry rot fungus Serpula lacrymans. Examples of attack and remedial treatment
1988 - IRG/WP 1347
The film deals with several aspects of dry rot attack and eradication in buildings. The detailed biology and morphological charasteristics of the fungus are portrayed. The various forms of mycelial growth, the role of the strands in the nourishment and spread of the fungus, as well as the many types of fruitbody formation are outlined. Environmental and nutritional requirements of the fungus as we...
G Buchwald, B M Hegarty, W Metzner, R Pospischil, H Siegmund, P Grabow


Physical properties of ß-1,4-Xylanase produced by Postia (=Poria) placenta: Implications for the control of brown rot
1987 - IRG/WP 1318
The degradation of hemicelluloses is an early event in wood decay by brown-rot fungi. An understanding of the physical properties of hemicellulases may suggest target mechanisms for the development of new control agents. Endo-b-1,4-xylanase was partially purified by column chromatography from wood decayed by Postia (= Poria) placenta. The enzyme was extremely resistant to denaturing conditions; no...
J A Micales, F Green III, C A Clausen, T L Highley


The decay resistance of chemically modified aspen composites to the white rot fungus Coriolus versicolor (L.) Quelet
1998 - IRG/WP 98-40122
Chemical modification of Aspen wood (Populus tremula L.) in the form of solid wood, veneers and sawdust was undertaken by a two step procedure consisting of esterification with maleic anhydride (MA) and subsequent oligoesterification with MA and glycidyl methacrylate (GMA) or allyl glycidyl ether (AGE). Modified wood was thermoplastic and was thermally formed by hot-pressing to produce veneer or s...
M C Timar, A J Pitman, M D Mihai


Monographic cards for wood-destroying fungi. [Fiches monographiques pour les champignons lignivores]
1970 - IRG/WP I 5B
C Jacquiot