Applications of the shower test. Part A: Results from CCA type C treated wood: influence of fixation process
1993 - IRG/WP 93-50009
This report outlines the results of shower tests conducted on CCA type C treated wood. The results indicate the inherent good fixation of CCA type C, as judged by the leaching limits within the Environmental Regulations. The shower test has proven to be a useful quality control and research test. It determines reasonably accurately the leaching under simulated conditions and, admittedly from a lim...
W J Homan, H Militz, D A Lewis


Effect of test site, preservative and wood species on decay type Glenbervie pastoral and radiata pine forest sites
2000 - IRG/WP 00-30248
Pinus radiata stakes were treated with 0.8, 1.2, 1.8, 2.7 and 4.1 kg/m3 of CCA and Fagus sylvatica with 2.7, 4.1 and 6.1 kg/m3 of CCA. Both wood species were also treated with equivalent retentions of a copper plus triazole preservative (CT) (0.89, 1.3, 2 and 3 kg/m3 of copper for pine & 2.5 and 4 for beech) and chlorothalonil plus chlorpyriphos in oil (CC) (1.4, 2.1, 3.2 and 4.8 kg/m3 of chlo...
R N Wakeling


Preservative treatment of two bamboo species Borak (Bambusa balcooa Roxb) and Talla (Bambusa tulda Roxb) by Boucherie method
2003 - IRG/WP 03-40262
Bamboo is widely used as a construction material in rural and urban areas of Bangladesh. It is perishable in nature and highly susceptible to the attack of borer, termites and fungi. As a result, bamboo products do not last long. This short life of bamboo is increasing demand thereby increasing pressure on our homestead and natural reserve of bamboo. For this reason, it is needed to make the bambo...
M N Islam, A S M A Huda, A K Saha, S M Mithue


Effect of soil type and moisture content on soft rot testin
1986 - IRG/WP 2270
Several soils of different types were tested at a range of moisture contents for their suitability for use in a soil burial soft rot test. Their effectiveness was assessed by weight loss in CCA treated and untreated beech and birch outerwood. A horticultural loam (John Innes No. 2) was the most appropriare soil in terms of amount of weight loss caused, tolerance to changes in soil moisture content...
S M Gray


Laboratory studies of CCA-C-leaching: influence of wood and soil properties on extent of arsenic and copper depletion
2002 - IRG/WP 02-50186
The extent which a wood preservative leaches is important for efficacy studies and environmental concerns. However, little information exists on the effect soil properties have on leaching. This study investigated leaching of stakelets which had been cut from five different southern yellow pine (SYP) sapwood boards then treated with CCA-C to a target retention of 6.4 kgm-3 (0.4 pcf). All stakel...
D Crawford, R F Fox, D P Kamden, S T Lebow, D D Nicholas, D Pettry, T Schultz, L Sites, R J Ziobro


Decay and termite resistance of wood treated with boron-containing quaternary ammonia compound, didecyl dimethyl ammonium tetrafluoroborate (DBF) incorporated with acryl-silicon type resin
2004 - IRG/WP 04-30334
This study evaluates the decay and termite resistance of surface-treated wood with didecyl dimethyl ammonium tetrafluoroborate (DBF) incorporated with acryl-silicon type resin emulsion. DBF is a quaternary ammonia compound and contains boric tetrafluoride (BF4-) as a counter ion in its chemical structure. In the study, DBF was incorporated with an acryl-silicon type resin to increase water-resista...
S N Kartal, W J Hwang, K Shinoda, Y Imamura


Dimensional stability and decay resistance of wood upon modification with some new type chemical reactants
1994 - IRG/WP 94-40028
Solid wood of home grown species can be upgraded by chemical modification with environmentally acceptable chemicals. The best kwown example of modification reaction is acetylation with acetic anhydride. A continued search for reactive chemicals other than acetic anhydride is ongoing, aiming at the improvement of technical properties of wood. This contribution deals with the results of a screening ...
P Goethals, M Stevens


Effect of substrate type and moisture requirements in relation to colony initiation in two carpenter ant species
1999 - IRG/WP 99-10320
Conditions necessary for optimal colony initiation or the rate of initial colony expansion by early brood in the carpenter ant species Camponotus modoc and C. vicinus on various substrates conditioned to different moisture contents were studied. Camponotus modoc and Camponotus vicinus queens were placed in Douglas-fir, western red cedar and Styrofoam® blocks conditioned in sealed chambers at 70% ...
M E Mankowski, J J Morrell


Estimation of the impregnation degree of pine wood by the distribution analysis of active ions concentration in the cross-section
1999 - IRG/WP 99-20174
Samples in the form of pine wood rollers of diversified moisture content of ca. 50, 28 and 12% were impregnated with a water solution of the mixture type CCB with the use of the full-cell process. Moisture content was determined in individual layers from the girth to the pith. In the same way the concentrations of copper and chromium ions with the use of the spectrophotometric method and recalcula...
K Lutomski, B Mazela


Evaluation of the efficiency of industrial kiln type CCA fixation chambers
1996 - IRG/WP 96-40063
Six commercial CCA treating plants in Canada were assessed for the fixation efficiency of their hot air fixation chambers. The wood temperature was measured with thermocouples over the fixation period at different locations in the chamber and at the end of the fixation cycle, the degree of chromium fixation was determined by a boring leaching procedure. There was a great variation in the effective...
A Taylor, P A Cooper


CCFZ, a new type of water-borne wood preservative for vacuum pressure impregnation
1991 - IRG/WP 3643
By combination of CCF-Salt types with zinchexafluorosilicate a remarkable improvement of efficacy is achieved. In the same time the ecotoxicoligical data become more save. As well as the efficacy against wood-destroying organisms (Basidiomycetes, Soft rot and Long horn beetle) the basic data to evaluate the ecotoxicological behaviour of a CCFZ-Salt are described and compared with the properties of...
W Metzner, D Seepe, H-W Wegen


Variable chlordane residues in soil surrounding houses in Louisiana
1989 - IRG/WP 1404
Eight soil samples from each of 30 houses in greater New Orleans, Louisiana were collected in October, 1986 and analyzed for chlordane residues (ppm). All houses had reportedly been treated in the late 1960's or early 1970's. Chlordane occurred in all samples, and the overall mean (+ SEM) was 870.6 + 96.5 ppm. Residue levels were unaffected by construction type (slab, crawl, craw...
J P La Fage, K S Delaplane


Method of embedding and staining of wood after biological testing to support the identification of decay type
1998 - IRG/WP 98-20131
A method for preparing wood for microscopic analysis after decay testing is described, with special regard to a novel fast simultaneous staining, which helps to identify different types of decay. The novel staining process is explained as well as the embedding of heavily decayed samples in polyethylene glycol (PEG) and picking up of sections by transparent adhesive tape. Special feature of the int...
A O Rapp


The influence of carrier fluid type on the efficacy of a wood preservative against cavity forming soft rot
2000 - IRG/WP 00-30244
Propiconazole was applied to Scots pine sapwood (Pinus sylvestris) and beech (Fagus sylvatica) using three different carrier systems selected on their varying ability to swell timber. The effects of microdistribution on the activity of cavity forming soft rot fungi were examined to determine the practical benefits of using swelling and non-swelling carriers with this active ingredient. Efficacy of...
P A Hodges


A new type of biocide suitable for use in different fields of wood preservation
1993 - IRG/WP 93-30014
A new type of polymeric biocides was developed containing quaternary ammonium and boron ester groups as active structure elements, to overcome the disadvantages of AAC's in wood preservation use and to utilise their good performance due to a broad efficacy against fungi on the other hand. The new biocides called polymeric betains have been tested in laboratory and field tests and especial...
V Barth, H Härtner


The relationship between preservative type and surface degrade in Pinus radiata
1980 - IRG/WP 3158
Samples of Pinus radiata D. Don were impregnated with one of two preservative types, a copper chrome arsenic salt and a light organic solvent preservative. The panels were exposed to the weather for 4-5 years at a site near Sydney, Australia. Macroscopic and microscopic examinations showed different rates and patterns of weathering between the samples treated with each preservative and an untreate...
R S Johnstone, R K Bamber


The development of soft rot decay in bamboo fibres
1992 - IRG/WP 92-1572
The development of decay by soft rot fungus Chaetomium globosum was investigated in young and mature culms of bamboo Phyllostachys virideglaucescens. Soft rot decay was influenced both quantitatively and qualitatively by the differing levels of lignification in the material. Weight loss was significantly greater in the younger culm compared with the older, more heavily lignified culm. The distribu...
O Sulaiman, R J Murphy


A Novel Type of Multiple Cavity Attack in Wood Cell Walls of Heat-treated Timber Exposed in Seawater – Preliminary Observations
2004 - IRG/WP 04-10523
Samples of untreated and heat-treated Norway spruce and Douglas fir were submerged in Langstone Harbour, Portsmouth for 4 years at a depth of ca. 0.3 metres. The heat-treated samples had been prepared using the Plato process. Samples were initially assessed for the severity of marine borer damage and were then examined microscopically for evidence of microbial decay. Longitudinal and transverse wo...
R A Eaton, C Björdal, T Nilsson


Fixation of chromated wood preservatives through technical drying
1990 - IRG/WP 3623
Twin samples of sawn timber of Pinus sylvestris and Picea sp. were treated with copper-chromate-containing wood preservatives and subsequently kiln resp. air dried. After drying, the distribution of preservative and rate of fixation were determined. Drying of freshly treated wood in a condenser type kiln at temperatures of 60°C and 80°C and in a vacuum type kiln at 55°C with a pressure of about...
R-D Peek, H Klipp


CCA type C depletion of Southern yellow pine utility poles
1995 - IRG/WP 95-50049
Depletion and redistribution of preservative components were evaluated on five CCA-C treated poles in service for over six years in Conley, Georgia. A statistical approach was taken in which retentions below ground were compared to retentions above ground due to a lack of initial data on individual poles. It was hypothesized that the below ground retentions should be lower than the corresponding a...
P D Osborne, R F Fox


Shockwaves in wood preservation
2005 - IRG/WP 05-40308
Shockwaves are strong perturbations in aerodynamics that propagate at supersonic speeds independent of the wave amplitude. Physically the occurrence of shockwave is always characterized in a fluid flow by instantaneous changes in pressure, velocity and temperature. In this paper we describe a new wood preservative injection system that has been developed utilizing the non-linear pressure spike beh...
G Jagadeesh, R Lal, G Ravikumar, K S Rao


Bamboo: A Material Rediscovered
2006 - IRG/WP 06-10577
Bamboo has resurfaced as a valuable raw material as an inexpensive substitute for wood and a variety of value added products for engineered composites. Being a fast growing material available in the tropics, its real value was not realized until recently. Property evaluation studies and efforts to develop processing methods were initiated in the bamboo growing countries in the nineteenth century....
S Kumar


Micromorphological Characteristics of Degradation in Bamboo Attacked by White Rot Fungus Lentinus edodes
2006 - IRG/WP 06-10575
In comparison with micromorphological works for wood decay, little known is about the decay pattern of bamboos by wood decay fungi. The present work was undertaken to understand the general degradation pattern of bamboo and the influence of polylaminate layers in bamboo fiber walls on the restriction of fungal decay. The weight loss of bamboo species Phyllostachys puberscens against the white rot ...
Chang Hyun Cho, Kwang Ho Lee, Yoon Soo Kim


Micromorphology of Bamboo Fibers Degraded by Brown-Rot Fungus Gloeophyllum trabeum
2006 - IRG/WP 06-10576
The decay pattern of bamboo by brown-rot fungus was examined. In addition, the influence of polylaminate structures in bamboo fibers on the restriction of fungal decay was also investigated. The weight loss of bamboo Phyllostachys puberscens by the brown-rot fungus Gloeophyllum trabeum after 16 week incubation was about 25%. Parenchyma cells were severely degraded. Microscopical studies showed tha...
Kwang Ho Lee, Chang Hyun Cho, Yoon Soo Kim


Is Field Test Data from 20 x 20mm Stakes Reliable? Effects of Decay Hazard, Decay Type and Preservative Depletion Hazard
2006 - IRG/WP 06-20327
Effects of decay hazard, decay type and preservative depletion hazard on the performance of variously preservative treated 20 x 20 x 500 mm Radiata pine and Fagus sylvatica test stakes across 13 field test sites in New Zealand and Queensland Australia were determined. Radiata pine treated with an ammoniacal copper quaternary preservative (ACQ) (1.56% m/m a.i.) and copper chrome arsenate (CCA) (...
R Wakeling


Previous Page | Next Page