Evaluation of exposure conditions for wooden facades and decking
2009 - IRG/WP 09-20408
During their functional life, building components are exposed to moisture and other environment stress conditions in numerous ways. This is a fact that should be taken into account during manufacture, product development, designing and work execution of building components. For wood material, moisture stress and biological factors like mould and decay fungi are often critical in cladding and decki...
H Viitanen, T Toratti, R Peuhkuri, T Ojanen, L Makkonen


Modelling of onset of mould growth for wood exposed to varying climate conditions
2009 - IRG/WP 09-20414
A performance-based service life design format based on climatic exposure on one hand and “resistance” of wood against mould growth on the other hand, is presented in this paper. A limit state for onset of mould growth is defined as the occurrence of traces of mould observed by microscopy. A dose-response model is proposed by which onset of mould growth can be predicted for an arbitrary climat...
S Thelandersson, T Isaksson, A Ekstrand-Tobin, P Johansson


Modelling hyphal growth of the bio-incising fungus Physisporinus vitreus
2010 - IRG/WP 10-10710
The white-rot fungus Physisporinus vitreus preferentially degrades the pit membranes of bordered pits in tracheids and subsequently enhances wood permeability. Thus, P. vitreus can be used to improve the uptake of wood preservatives and environmentally-benign wood modification substances. This process can be used to enhance the use and sustainability of native conifer wood species by the wood indu...
M Fuhr, C Stührk, F W M R Schwarze, M Schubert, H J Herrmann


Qualitative - Quantitative Analysis of Wood-Inhabiting Fungi in External Wooden Structures of the Latvian Cultural Heritage
2010 - IRG/WP 10-10728
The frequency and diversity of wood inhabiting fungi in the exterior wood were established in the Araishi lake fortress, the Lielvarde wooden castle, the Latvian Ethnographic Open-Air Museum, Riga, and twelve wooden heritage objects in the Eastern part of Latvia (Latgale). The inspected wooden structures of the external woodwork included windows, stairs, walls, floorings, roofs, fences, and benche...
I Irbe, M Karadelev, B Andersons


Structural changes, basidiomycete richness, enzyme activity and proteomic profiling of decay resistant and non-resistant woods over 18 months in soil contact
2010 - IRG/WP 10-10733
Wood decay fungi damage wood by production of enzymes that attack the structural components. The objective of this study was to better understand which suite of decay genes and proteins are expressed during biodeterioration of three different wood types in forest soil over time. Variation in decay genes and proteins were determined for pine (non-resistant), cedar (naturally durable), and ACQ-treat...
Youngmin Kang, S Diehl, L Prewitt, D Nicholas


Finite Element Modelling of the Checking of Wood Exposed to Accelerated Weathering
2010 - IRG/WP 10-20459
The surface checking that develops when wood is exposed to the weather reduces the visual appeal of treated wood products and can reduce the effectiveness of preservative treatments. There is strong interest in developing solutions to this problem and also a growing realization that such solutions may evolve from a deeper understanding of the mechanisms responsible for surface checking. In this pa...
S G Ribarits, P D Evans


Decay hazard mapping for Europe
2011 - IRG/WP 11-20463
In this study, two different dose-response models for above-ground decay as well as a model transferring macro climate data to wood climate data are presented. The models base on data from field trials, which had been conducted at 28 European test sites, and were used to calculate the relative risk for decay caused by climate variability in Europe. The two dose-response models give coherent result...
C Brischke, E Frühwald Hansson, D Kavurmaci, S Thelandersson


Service life prediction of wooden components - Part 3: Approaching a comprehensive test methodology
2011 - IRG/WP 11-20464
This paper is the third in a series on 'service life prediction' of wooden components and should be considered as a discussion paper. The authors tried to analyze the topic with a look from a distance and comment sometimes with a smile on the current controversial discussion about SLP issues. Nevertheless, the viewpoints of different groups, such as natural scientists, engineers, approva...
C Brischke, C R Welzbacher, L Meyer, T Bornemann, P Larsson Brelid, A Pilgård, E Frühwald-Hansson, M Westin, A O Rapp, S Thelandersson, J Jermer


Aesthetic service life of coated and uncoated wooden cladding - influencing factors and modelling
2011 - IRG/WP 11-20470
Mould growth on exterior coated cladding façades is an undesirable element and will often shorten the aesthetical service life. Mould growth on painted surfaces is influenced by type and concentration of film fungicides, the paint formulation and the wood substrate itself, and wooden cladding may experience exponential fungal deterioration caused by variation in the climatic factors, often within...
L Ross Gobakken, O A Høibø


Cell wall properties of softwood deteriorated by fungi: combined chemical analyses, FT-IR spectroscopy, nanoindentation and micromechanical modelling
2013 - IRG/WP 13-20527
Mechanical properties of wood are determined by its inherent hierarchical microstructure, starting at the nanometer scale, where the elementary components cellulose, hemicelluloses, and lignin build up the wood cell wall material. Fungi cause degradation and decomposition of these components and, thus, alter the mechanical properties of wood. The aim of this study is to gain new insight into these...
L Wagner, T K Bader, K de Borst, T Ters, K Fackler


Modelling the risk for mould growth on timber stored outdoors protected from rain
2013 - IRG/WP 13-20529
A mould resistance design (MRD) model was used to calculate the maximum duration of storage of timber outdoors under cover (protected from rain) before the onset of mould growth on the surface of wood. The prediction model is based on laboratory tests performed in constant and cyclic climates and were also confirmed against exposure tests in attics and crawl spaces. The prediction model presented ...
E Frühwald Hansson, S Bardage, S Thelandersson


Nondestructive Detection of Biodeterioration in Indonesian Traditional Wooden Construction of “Joglo”
2014 - IRG/WP 14-10834
To decide the repairing and reinforcement method for wooden constructions, it is necessary to get the enough and precise information on the status of the construction beforehand, especially the distribution and the degree of the biodeterioration, such as decay or insect attack (e.g. termite attack). In this study, damage of biodeterioration to teak wood used in Indonesian traditional wooden const...
Y Yanase, T Mori, T Yoshimura, Y P Prihatmaji, J Sulistyo, S Doi


The development of accelerated test systems to evaluate the durability of framing timber
2014 - IRG /WP 14-20547
Various accelerated decay resistance trials including small simulated wall units, samples exposed in enclosed tanks and ‘I’ samples in stacks have been explored and used to test the durability of treated and untreated radiata pine framing at Scion since 2001. These testing methods have been established to determine the effectiveness of commercial formulations in preventing decay in framing sub...
T Singh, D Page, J van der Waals


On-site remediation treatments for framing timber in leaky buildings
2014 - IRG/WP 14-20549
Weathertightness failures in New Zealand buildings due to the combined effects of cladding choices, design and construction faults and the use of untreated framing timber has led to the so called ‘leaky building syndrome’. The latest estimated cost of the leaky building crisis in New Zealand is about NZ$11 billion. This research was conducted to provide a better understanding of the option...
T Singh, D Page, A Bennett


Coconut shell pyrolytic oil as wood protectant against biodeterioration
2014 - IRG/WP 14-30648
Extensive research on various plant and microbial extracts has been conducted as an alternative to using synthetic or inorganic chemicals for wood protection. Development of effective and low environmental impact products and technologies for wood protection is imperative. In the present study, the efficacy of coconut shell pyrolytic oil as a wood protectant is analysed in terms of its antifungal,...
K S Shiny, O K Remadevi


Acceptance levels of surface disfigurement - tolerance to defects of coated wood
2015 - IRG/WP 15-20564
Service life planning (PSL) has become an important issue in performance based building and substantial progress has been made in recent years. The role of predicting the aesthetical service life of wooden building components has been underestimated for quite long time but is recently attracting more and more notice. It is influenced by numerous factors such as discoloration, fading, flaking, crac...
C Brischke, P Kaudewitz


Remedial treatment of difficult to access timber in buildings
2015 - IRG/WP 15-40691
The quest to understand remedial treatment for timber framing begun following the ‘leaky building crisis’ in New Zealand which came to prominence in 2000. Several in-situ remedial treatment products are used in New Zealand. However, effectiveness of these treatments is still unclear particularly in situations where not all faces of the timber can be assessed. This research was conducted to det...
T Singh, I Simpson, D Page


Global survey on durability variation – on the effect of the reference species
2016 - IRG/WP 16-20573
Climate change due to anthropogenic emissions is the largest environmental challenge of our time. Forest-based value chains play an important role in reducing the accumulation of CO2 in the atmosphere. Maximizing the use of wood to tackle climate change requires improved understanding of the service life of timber products. This information can best be obtained from field testing and while there i...
R Stirling, G Alfredsen, C Brischke, I De Windt, L P Francis, E Frühwald Hansson, M Humar, J Jermer, M Klamer, M Kutnik, P Laks, I Le Bayon, S Metsä-Kortelainen, L Meyer-Veltrup, P I Morris, J Norton, T Singh, J Van Acker, J Van den Bulcke, T M Venås, H Viitanen, A H H Wong


Modelling the performance of bio-based building materials
2016 - IRG/WP 16-20582
The ‘bio-based economy’ represents a growing area of development globally and covers a wide range of building materials including wood and wood-based products. A ‘bio-based’ material is intentionally made from substances derived from living (or once-living) organisms. In this context it means that the materials and products are made from renewable resources, with the criteria that a renewa...
C Brischke


Wood biodeterioration monitoring using molecular fluorescence
2016 - IRG/WP 16-20589
Wood is an extremely complex and heterogeneous biological material, susceptible to biodeterioration by wood-destroying organisms. This process can be evaluated by natural resistance tests or non-destructive techniques, such as molecular fluorescence. The fluorescence of wood can be attributed to the presence of fluorophores groups or extractives, as a characteristic of some species. This study aim...
E Meneses Oliveira, A Florian da Costa, J W Batista Brag


Studying fungal growth using automated image analysis and computer simulations
2016 - IRG/WP 16-20590
Wooden materials are prone to fungal attack resulting in damage and economic losses. Therefore many efforts have been made to understand the degradation of wood and to avoid the adverse effect of fungi. Even though the extent of degradation of a material is inversely proportional to the extension of the fungi attacking it, most researchers focus mainly on the former, leaving the study of the latte...
G Vidal-Diez de Ulzurrun, J M Baetens, J Van den Bulcke, B De Baets


Evaluation of advanced tannin-boron preservative in unsterile soil-bed tests
2016 - IRG/WP 16-30693
In Europe, boron compounds are facing restrictions, and due to their natural solubility into water, the only way to keep using them for wood protection is to fix them into the wood, at very low level (Obanda et al. 2008). In the meantime, the idea of protecting wood with natural preservatives has been back into favour (Lotz and Hollaway 1988, Nakayama et al. 2001, Singh and Singh 2012). Tannin a ...
Jinbo Hu, Yiqiang Wu, Shanshan Chang, Guangming Yuan, G Tondi, M-F Thévenon


Hygrothermal performance of ventilated wooden cladding
2016 - IRG/WP 16-40733
The risk for an attack of wooden claddings by decay and discolouring fungi strongly depends on the moisture and temperature conditions in the building envelope. The design of the cladding has a major influence on its hygrothermal performance. In the present study, different wooden ventilated cladding designs were investigated at a test house in Mid-Norway for four years. The objective was to incre...
K Nore, U Hundhausen


Monitoring of wood biodeterioration by infrared spectroscopy
2017 - IRG/WP 17-20607
The susceptibility of wood to deterioration by rotting fungi is intrinsically related to its chemical composition and the environmental conditions at its place of use, and if not detected in time, can cause enormous financial losses. The process of wood biodeterioration by decay fungi can be evaluated through laboratory accelerated test, in specific field tests, or through non-destructive techniqu...
E Meneses Oliveira, A Florian da Costa, J W Batista Braga


Modelling of moisture content in timber bridge details
2017 - IRG/WP 17-20613
The design of details is an important aspect in durability design of timber bridges. Details are often considered the weakest points in bridges due to their tendency to trap and accumulate moisture and thus facilitate decay. When designing maintenance plans and inspection intervals, it is important to know how design choices will come to influence the service life. Moreover, service life and wood ...
J Niklewski, C Brischke, E Frühwald Hansson, L Meyer-Veltrup