IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1398 documents. Displaying 25 entries per page.


Natural durability of larch heartwood against decay
1997 - IRG/WP 97-10201
Larch heartwood has been promoted in Sweden and in other European countries as an alternative to preservative treated timber. It has even beeen stated that larch heartwood is more durable than preservative treated timber. This paper presents a compilation of facts from scientific reports on the durability of larch heartwood. Some recent data from this department are also reported. All data suggest...
T Nilsson


New ways of chemical wood preservation
1997 - IRG/WP 97-40087
Synergistic effects pertaining to wood preservation have been investigated by combining different polymerizing agents with modifying chemicals, modifying chemicals with known preservatives and new types of preservative chemicals with each other. One of the investigated methods is the use of impregnating solutions based on furfuryl alcohol (produced from biomass), in which the chemicals polymerizes...
M Westin, T Nilsson, B Ohlsson, R Simonson


Evaluation of the natural durability and ultrasonic method for decay detection of some european hardwood and softwood species
2004 - IRG/WP 04-10537
This paper presents the first part of an investigation on the natural durability of mixed plywood made of durable and non durable plies from the following selected timbers : Cedrus atlantica, Cupressus sempervirens, Castanea sativa, Populus sp. I 214 and Fagus sylvatica. In order to carry out this study, the natural durability of the massive wood used to manufacture the plywood panels was asses...
F Faraji, M-F Thévenon, B Thibaut


Characterization of Poria indoor brown-rot fungi
1995 - IRG/WP 95-10094
The heterogeneous group of "Poria" fungi causing brown rot in buildings and also of wood in ground contact comprises Antrodia vaillantii, Antrodia serialis, Antrodia sinuosa, Antrodia xantha and Tyromyces placenta. These fungi have similar morphological appearance and biology. Their nomenclature has a confusing history and is still not uniform. As a consequence, misinterpretations may occur. SDS p...
O Schmidt


Natural Durability studies and Changes in wood chemistry of some Ghanaian hardwoods during decay by white- and brown-rot fungi
2004 - IRG/WP 04-10542
The natural decay resistance of Esa (Celtis mildbraedii), Wawabima (Sterculia rhinopetela) and Dahoma (Piptadeniastrum africanum) obtained from Ghana was determined according to BS EN 113 (1997). Esa was found not durable to the white-rot, but very durable to the brown-rot; Wawabima was very durable to both white- and brown-rots; and Dahoma was durable to the white-rot, and very durable to the bro...
Zeen Huang, K Maher, S A Amartey


Efficacy of waterborne copper naphthenate as preservative for northern hardwood species
1995 - IRG/WP 95-30091
Northern red oak (Quercus rubra) and red maple (Acer rubrum) cubes pressure treated with waterborne formulation of copper naphthenate were evaluated for resistance to attack by brown fungi Gloeophyllum trabeum (Pers. ex Fr.) Murr. (Madison 617 ATCC 11539) and Poria placenta (Fr.) Cooke (Madison 698, ATCC 11538), white rot fungi Trametes versicolor (L. ex Fr.) Pilat (R-105 from Jeff Morrell), Irpex...
D P Kamdem, R Fair, M H Freeman


Colonization of treated and untreated ponderosa pine exposed in Hilo, Hawaii
1995 - IRG/WP 95-20068
The rate of decay in above ground exposures is largely controlled by rainfall and temperature, factors which can be used to construct a climate index of decay hazard in above ground exposures. Developers of new biocide formulations have utilized this knowledge by establishing test sites in sub-tropical regions such as the Gulf Coast of the United States. More recently, field sites have been locate...
C M Freitag, J J Morrell, K J Archer


Immunolocalization of extracellular metabolites from Poria placenta
1988 - IRG/WP 1361
Polyclonal antisera produced to Poria placenta extracellular metabolites was used in immuno-fluoresence microscopy and immuno-gold TEM studies. In the fluorescence work, labelling of Poria placenta hyphae in wet fixed wood material was observed but not in infected wood which was oven dried prior to sectioning and immunolabelling. TEM studies provided better resolution, with gold labelling detected...
B Goodell, G F Daniel, J Jellison, T Nilsson


Method of embedding and staining of wood after biological testing to support the identification of decay type
1998 - IRG/WP 98-20131
A method for preparing wood for microscopic analysis after decay testing is described, with special regard to a novel fast simultaneous staining, which helps to identify different types of decay. The novel staining process is explained as well as the embedding of heavily decayed samples in polyethylene glycol (PEG) and picking up of sections by transparent adhesive tape. Special feature of the int...
A O Rapp


Occurrence and importance of various types of fungal and bacterial decay in CCA-treated horticultural pine posts in New Zealand
1984 - IRG/WP 1234
A detailed microscopical examination has been carried out on samples taken from CCA-treated pine posts exposed in horticultural soils. The following decay types were observed: white rot, brown rot, soft rot, tunnelling bacteria, cavitation bacteria, and bacterial erosion. The occurrence and importance of the various decay types between different regions, and plots within a specific region, varied ...
T Nilsson


Extracellular osmiophilic particles in connection with brown rot and white rot
1982 - IRG/WP 1157
The way of attack on Pine woodblocks of two brown-rot fungi (Fomitopsis pinicola, Coniophora puteana) differing in their cellulase activities, and one white-rot fungus (Trametes hirsuta) has been investigated by transmission electron microscopy. Even at early stages of decay, osmiophilic particles were found with all the fungi investigated. In the brown-rotted wood, the osmiophilic particles occur...
K Messner, H Stachelberger


Hydrolysis of bordered pits during colonization of conifers by brown-rot fungi
1995 - IRG/WP 95-10103
Brown-rot decay results in rapid reduction in degree of polymerization (DP) of holocellulose with concomitant strength loss (MOR) without removing lignin. Development of new methods of wood protection will require focusing on early events in the sequence of depolymerization. Bordered pit membranes (sapwood) represent a readily available source of non-lignified carbohydrate, ie. pectin and cellulos...
F Green III, J L Tschernitz, T A Kuster, T L Highley


The effect of Tween 80 on the growth, morphology, and enzyme secretion of Postia placenta
1990 - IRG/WP 1456
The nonionic surfactant Tween 80 (polyethylene oxide sorbitan mono-oleate) has been reported to increase enzyme production and/or secretion in bacteria and fungi. Such a procedure could greatly facilitate research into the physiology of wood-decay fungi since quantities of available enzyme are often limiting. The brown-rot fungus Postia placenta was grown in a synthetic medium supplemented with 0,...
J A Micales


Preliminary investigation on the natural durability of Guayule (Parthenium argentatum)-based wood products
2000 - IRG/WP 00-40154
Conventional preservatives used to protect wood from insect and microbial damages are presently of major concern to human health and the environment. Finding alternative and economical preservatives has not been successful. Previous studies have shown that the resinous material extracted from the guayule plant (Parthenium argentatum, Gray) has both insect- and microbial-resistant properties. Unfor...
F S Nakayama, P Chow, D S Bajwa, J A Youngquist, J H Muehl, A M Krzysik


Defining fungal decay types - A proposal for discussion
1985 - IRG/WP 1264
The present definitions of the fungal decay types, white rot, brown rot, and soft rot are somewhat vague. The definitions are based on a mixture of criteria involving morphological and chemical aspects of decay as well as taxonomic affiliation of the responsible fungal species. The present vague definitions have led some fungi being erroneously places in a wrong decay type. Furthermore, some fungi...
T Nilsson


The action of siderophores isolated from Gloeophyllum trabeum on the structure and crystallinity of cellulose compounds
1991 - IRG/WP 1479
Low molecular weight, high affinity iron-binding compounds (siderophores) were isolated from the brown-rot fungus Gloeophyllum trabeum. The compounds were shown to be inducible by iron starvation and could be purified by ultra-filtration, ethyl acetate extraction, column chromatography and preparative HPLC. The isolated compounds were shown by analytical and immunological techniques to be produced...
J Jellison, V Chandhoke, B Goodell, F Fekete, N Hayashi, M Ishihara, K Yamamoto


Pretreatment decay in poles of Pinus sylvestris
1987 - IRG/WP 1329
Storage damage by blue stain and decay in poles before impregnation has been increasingly observed during recent years and there have been reports that salt-impregnated poles today are of lower quality because of incipient decay being increasingly common. The attacks may have started at the time of cutting and then continued during the period of seasoning at the plant, which could be as long as tw...
H Lundström, M-L Edlund


Antagonism of Gliocladium virens against wood decay fungi
1995 - IRG/WP 95-10102
Antagonistic abilities of a commercial biofungicide, Gliocladium virens (GL-21, Grace) were evaluated against three white-rot fungi, Trametes versicolor, Phlebia brevispora, Irpex lacteus, and three brown-rot fungi, Postia placenta, Neolentinus lepideus, Gloeophyllum trabeum. In dual culture of Gliocladium virens and wood decay fungi, Gliocladium virens rapidly overgrow the decay fungi and killed ...
T L Highley, L Ferge


Antagonistic effects of Dacrymyces stillatus against growth of other fungi
1991 - IRG/WP 2363
The antagonistic effects in dual cultures on malt extract agar of 5 wood decay fungi and the antagonistic effects of Dacrymyces stillatus against 1 mould fungus and 1 blue stain fungus were determined. Dacrymyces stillatus was the only fungus which exhibited clear antagonistic effects. The effects of Dacrymyces stillatus against the different test fungi varied however to a great extent. Dacrymyces...
J Bjurman


Antagonism of Scytalidium lignicola against wood decay fungi
1989 - IRG/WP 1392
Antagonistic abilities of Scytalidium lignicola against white- and brown-rot wood decay fungi were evaluated. Scytalidium lignicola did not produce inhibition zones but overgrew the decay fungi on a malt-agar medium and in most cases killed them. Pretreatment of Douglas-fir and Southern pine blocks with Scytalidium lignicola prevented decay. Blocks that were heated or treated with propylene oxide ...
T L Highley


Production of monoclonal antibodies to fungal metabolites
1986 - IRG/WP 1306
The role of fungal extracellular enzymes in wood biodegradation is incompletely understood. Our lab is beginning a project utilizing monoclonal antibodies to characterize extracellular metabolites of the brown rot fungus Poria placenta Fr. (Cooke). Monoclonal antibody technology takes advantage of the ability of antibody secreting spleen cells from immunized mice to fuse in the presence of polyeth...
J Jellison, B Goodell


Effects of heart wood extractives in Dahoma (Piptadeniastrum africanum) on decay resistance to white- and brown-rot fungi
2004 - IRG/WP 04-10536
Dahoma (Piptadeniastrum africanum) is a durable but a lesser utilised tropical hardwood species from Ghana that has the potential of being used as an alternative to Iroko (Milicia excelsa) for many end uses. However, the timber gives off a strong odour especially when wet and during processing. The high durability and the strong odour of the timber could be due to the presence of extractives in th...
Zeen Huang, K Maher, S A Amartey


Bioefficacy of Cunapsol® treated western cedar and southern yellow pine
1996 - IRG/WP 96-30120
Western red cedar and southern yellow pine sapwood were dip treated with a new formulation of waterborne copper naphthenate (Cunapsol®) which complies with VOC regulations. Cunapsol dip treated samples were oven dried at 50°C for 48 hours and then water leached for two weeks. Decay resistance and leachability of preservatives from dip treated specimens were evaluated according to AWPA (American ...
D P Kamdem, M H Freeman, T L Woods


The identification of the carbohydrate degrading enzymes from the crude extract of brown-rot fungus Gloeophyllum trabeum
1991 - IRG/WP 1483
The brown-rot fungus, Gloeophyllum trabeum, produces a pattern of carbohydrate degrading enzymes during the wood decay. In liquid sawdust media the activities of endo-b-1,4-gluganase and endo-b-1,4-xylanase were at the maximum after 5-6 weeks cultivation. The production of enzymes started immediately after inoculation suggesting that the degradation of hemicellulose and easily degradable parts of ...
A-C Ritschkoff, J Buchert, L Viikari


Micromorphology of Bamboo Fibers Degraded by Brown-Rot Fungus Gloeophyllum trabeum
2006 - IRG/WP 06-10576
The decay pattern of bamboo by brown-rot fungus was examined. In addition, the influence of polylaminate structures in bamboo fibers on the restriction of fungal decay was also investigated. The weight loss of bamboo Phyllostachys puberscens by the brown-rot fungus Gloeophyllum trabeum after 16 week incubation was about 25%. Parenchyma cells were severely degraded. Microscopical studies showed tha...
Kwang Ho Lee, Chang Hyun Cho, Yoon Soo Kim


Previous Page | Next Page