Your search resulted in 324 documents. Displaying 25 entries per page.


Probing red maple pit membrane pore size at FSP and OD using polystyrene macromolecules
2001 - IRG/WP 01-40217
A modified solute exclusion technique was used to pressure impregnate a polystyrene molecular weight (MW) series dissolved in styrene into red maple samples at approximately the fiber saturation point (FSP) and oven dry (OD). Radial penetration was less than tangential and FSP less than OD. There was a marked penetration change with MW in the tangential direction, although there appeared to be a ...
A Omidvar, M H Schneider, A R P Van Heiningen


The growth and behaviour of Australian isolates of dry rot fungi, mainly Serpula lacrymans (Schum. ex Fr.) S.F. Gray. A comparision with the world literature
1983 - IRG/WP 1190
In Australia Serpula lacrymans occupies a rather unique environment, being restricted to growth within basal regions of buildings containing masonry. Its rate of timber attack in these situations appears to be far faster than that experienced in other parts of the world. Therefore the question arises as to how Australian isolates (particularly 16508 which has become a "standard" test fungus for so...
J D Thornton, O Collett


Determination of the water sorption properties and preliminary results from field tests above ground of thermally modified material from industrial scale processes
2004 - IRG/WP 04-40279
In this study the differences in moisture behavior and durability above ground of heat treated wood originating from different European industrial heat treatment plants by means of the water sorption properties as well as field tests were examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood (Premium wood)/ Finland and Menz Holz/ Germany, where Oil-...
C R Welzbacher; A O Rapp


Preliminary modelling of methylisothiocyanate movement through Douglas fir transmission poles
1988 - IRG/WP 3466
Methylisothiocyanate is a volatile solid that is the active ingredient of several registered and experimental wood fumigants. Information on the sorption and diffusion of this chemical in Douglas-fir heartwood and sapwood was used to develop a two-dimensional model of fumigant movement within a single horizontal cross-section of a transmission pole. The model indicated that dry wood (14% MC) stron...
A R Zahora, P E Humphrey, J J Morrell


Remedial treatments of glulam = diffusion of active ingredients through glue lines from solid wood diffusable preservatives
1996 - IRG/WP 96-30117
Diffusable preservatives are very suitable for use in remedial treatments of laminated beams in which too high moisture content involves the development of wood destroying fungi. The diffusion of active ingredients (boric acid, disodium octoborate, bifluoride) is well observed in solid wood but in a composite wood, the glue lines may appear not only as a barrier for the diffusion but also, may be ...
D Dirol, S Mouras


Risk of pulmonary damage as a result of an evaporation of ca. 50 ppb = 42 mg HF, evaporated from wood treated by difluorides
1987 - IRG/WP 3401
In this review of the literature the effects of fluorides and fluorine on man are described, especially the low level effects of inhaled HF on human beings. The term "fluoride" is used as a general term everywhere, where exact differentiation between ionic and moluecular forms or between gaseous and particulate forms is uncertain or unnecessary. The term covers all combined forms of the element, r...
H F M Nijman


Preservative effect of cellulose insulation material against some mould fungi and brown rot fungus Coniophora puteana in pine sapwood
1991 - IRG/WP 1484
The influence of mineral wool and loose-fill cellulose wool on biodeterioration of pine sapwood was studied. The test fungi were mould fungi Aspergillus versicolor, Cladosporium sphaerospermum, Penicillium sp. and Aureobasidium pullullans and brown rot fungus Coniophora puteana. Cellulose wool inhibited the growth of mould fungi on the face of wood contacted with insulation material at RH of 97 an...
H Viitanen


Soil bed studies of the dimensional stability of composite products
1999 - IRG/WP 99-40134
The influence of boron and isocyanate resin on the dimensional stability of high moisture resistant particleboard was assessed after burial in a soil bed for one month. The samples were treated with two levels of a boron compound and coated in isocyanate resin. The samples were randomly placed in a fungal cellar in soils of two different water holding capacities. Weight differences and dimensional...
K M Filcock, P Vinden


Some Experiences with Stake Tests at BAM Test Fields and in the BAM Fungus Cellar Part 2: Comparison of Static and Dynamic Moduli of Elasticity (MOE)
2005 - IRG/WP 05-20320
In routine in-ground stake tests of wood preservatives at the BAM test field Horstwalde and in the BAM fungus cellar periodical determinations of both static moduli of elasticity (MOE) on the basis of bending tests and dynamic MOE on the basis of the vibration method were performed as a possible method for the assessment of fungal attack. As expected from other publications, the absolute values of...
M Grinda, S Göller


Limiting Conditions for Decay in Wood Systems
2002 - IRG/WP 02-10421
Hygrothermal models can predict temperature and moisture conditions in wall components subjected to real weather data, but specific data and a fundamental understanding of how temperature and wood moisture content dictate the progression of decay under these conditions is required for modellers to predict consequences of decay on building performance. It is well understood that wood will decay abo...
P I Morris, J E Winandy


Steam/hold/APM boron treatment - Treatability trials with green gauged radiata pine
1987 - IRG/WP 3439
Freshly sawn 100 x 50 mm radiata pine was green gauged, steam conditioned and preservative treated with a mixture of borax and boric acid using a modified Alternating Pressure Method (APM) treatment schedule. A 12 hour holding period between steam conditioning and treatment resulted in the necessary moisture loss and moisture re-distribution to facilitate treatment to NZ Timber Preservation Author...
P Vinden


The effect of wood preservatives on the relation between the electric resistance and moisture content in scots pine (Pinus sylvestris L.) sapwood
1998 - IRG/WP 98-20142
The effect of two types wood preservatives (TBTO and CuHDO) on moisture content measurements with an electric resistance meter in pine sapwood is assessed. High and low concentration impregnated pine sapwood is climatized at different relative humidities. Once climatized the samples are weighed and the moisture content is measured with an electric resistance meter by fixed stainless steel, isolate...
B W Holleboom, W J Homan


The natural durability assessments of secondary timber species - field trials
1998 - IRG/WP 98-10297
Secondary or 'alternative' hardwood timber species can replace traditional hardwoods and contribute significantly to satisfying the overall demand for hardwoods in the UK timber market. A selection of these 'alternative' hardwoods is currently being tested at BRE-WTC for natural durability both in ground contact (to EN252) at two field sites, and out of ground c...
E D Suttie, R J Orsler


Dip-diffusion of dressed timber - Effect of drying
1990 - IRG/WP 3603
The effect of drying on BFCA dip-diffused, dressed, freshly sawn timber was determined by the depth of penetration of boron achieved on two test timber species, White Cheesewood (Alstonia scholaris) and Light Hopea (Hopea papuana). The results obtained showed that the light density White cheesewood was completely penetrated even after 3 days drying while Light Hopea, treated immediately achieved 5...
H C Konabe


Fungi causing sap stain in wood
1980 - IRG/WP 199
The present paper is a revised edition of former Document No: IRG/WP/125. It contains some additions and an explanation of terminology, as was suggested at a previous meeting of the Group. The paper is a compilation based mainly on available literature. Some of my own unpublished results have been added together with other unpublished data which have been received from the Bundesanstalt für Mater...
A Käärik


Influence of CCA and TnBTO on wood decay, under different oxygen levels and various initial moisture content
2001 - IRG/WP 01-10415
Fagus sylvatica (beech) and Pinus sylvestris (Scots pine) were impregnated by TnBTO (tributyl-tin oxide) and CCA (chromated copper arsenate). In wood blocks two levels of moisture content (50% and 100% of saturation point) were used. Three levels of oxygen concentrations (10, 21, and 50%) were chosen. Treated and untreated wood were exposed to three fungi (C. versicolor a white rot, C. puteana, a ...
S M Kazemi, R J Murphy, D J Dickinson


A novel guide for the determination of the physical properties of wood including kiln drying and full-cell preservative treatment
2004 - IRG/WP 04-20298
An ideal flow chart for the sequential experimental determination of a range of physical properties relevant to wood drying and subsequent preservation was designed as a novel guide to assist wood scientists. In this manner, data assembly and experimental processing are shown. This was designed according to experience and published literature. Aspects emphasised in this review were the physical p...
I Usta, M D C Hale


Field test design for service life prediction of wooden components
2005 - IRG/WP 05-20308
Wood is predominantly degraded by organisms. Thus, compared to other building materials, service life of wooden material is influenced by many more factors, which are divided into direct and indirect factors. Climate, geographical position, and construction criteria count to the indirect decay factors. Besides material inherent properties (natural durability, wood preservatives), wood temperature...
A O Rapp, C Brischke


Long term experiments for assessing the diffusion of boric acid and diluorides from local preservative pills in spruce and pine
1996 - IRG/WP 96-40065
For the experimental assessment of the diffusion of boric acid and difluorides over a three year period 2 tests were set up. In a test with large spruce blocks (150 x 150 x 300 mm³) 3 different pill types were exposed to 3 different climates: climate room (20°C, 65% r.h.), wet room (20°C, 95% r.h.), and to outside exposure. In a test with open L-joints without paint, with an alkyd paint and wit...
W J Homan, H Militz


Borate diffusion in wood from rods and liquid product. Application to laminated beams
1988 - IRG/WP 3482
In the aim to use borate preservatives (fused rods and boracol) in fields of building construction other than external joineries, tests of diffusion of borate rods and secondary boracol, were carried out on different species of woods exposed to different moisture conditions. Tests were also applied on laminated beams very often subjected to high moisture contents and thus decay of rot fungi. Diffu...
D Dirol


On the laboratory use of X-rays in timber decay evaluations
1981 - IRG/WP 2144
The paper reports the results of laboratory experiments on the X-raying of some Pinus radiata sapwood blocks infected with Serpula lacrymans to determine the effect of density and moisture content on the absorption of X-rays by wood. It is concluded that with increasing moisture content there is a very marked increase in time required to pass a constant quantity of X-rays through a test block and ...
J D Thornton, J W Creffield, O Collett


Moisture content development in lap-joints of different wood species in outside exposure trials
1998 - IRG/WP 98-20143
Lap-joint trails (following European Standard EN 12037) were set up with 11 different softwood and hardwood species. Half of the number of the lap-joint specimens were coated with an alkyd coating. The moisture development has been followed during a 19 months period. In this paper, the out comes of different moisture contents evaluations are presented. The results show, that the moisture content o...
H Militz, M Broertjes, C J Bloom


Preservative treatment of green timber by diffusion
1984 - IRG/WP 3291
The preservative treatment of green timber by diffusion is reviewed together with criteria which influence the economics of the process. New process options are described which should overcome some of the technical and economic disadvantages of double diffusion. These include the use of coagulating agents which increase the viscosity of the preservative solution and facilitate treatment by momenta...
P Vinden


The relationship between the electrical resistance and fixation of water-borne CCA salts and pressure-treated wood
1991 - IRG/WP 3657
Two investigations at 22°C and 30°C have been carried out. The electrical resistance in the treated wood and chemical analyses of the remaining amount of unfixed copper, chromium and arsenic were investigated. Samples impregnated with water were used as references. To hold the samples moist during the investigation, each sample was wrapped in a polyethylene plastic foil immediately after impregn...
F G Evans, B Nossen


The effect of chemical treatment on the moisture distribution of Pinus radiata D.Don subjected to wick action
1999 - IRG/WP 99-40135
Radiata pine sapwood stakes were treated with a range of chemicals, including an ammoniacal copper quaternary ammonium compound (ACQ), a copper-chrome and arsenic (CCA) solution and a CCA-oil treatment, potassium linoleate copper linoleate, a paraffin wax and a proprietary alkyd resin. The effect of these treatments on the extent of water absorption and moisture movement through the stakes was inv...
J Hann, P Vinden