Field trial with poles of Scots pine treated with six different creosotes
1996 - IRG/WP 96-30115
In the middle of the 50's field trials with creosote-treated poles were started in France, Germany and Sweden. The trials were initiated by WEI (Western-European Institute for Wood Preservation). Six different creosotes were used and 40 poles per creosote were installed at each test field. Results after 39 years of exposure in Simlangsdalen, Sweden are reported. Poles treated with a heavy...
Ö Bergman


Preservative treatment of Eucalyptus saligna fence posts by the double-diffusion method
1982 - IRG/WP 3196
Eucalyptus saligna fence posts treated by the double-diffusion method with two chemical combinations showed average lives of 11.2 years (copper sulphate and potassium dichromate at 10.5 kg/m³ retention)and of 14.3 years (copper sulphate and sodium mono-H arsenate at 7.1 kg/m³ retention), as determined in five test sites in the State of Sao Paulo, Brazil. The exponential model was the best fit wh...
E S Lepage, A R De Freitas


Climate indices at work: Above ground decay L-joint tests (EN 330 and AWPA E9) at two sites 12000 km apart and with Scheffer climate indices of 60-65 and 300-330
1996 - IRG/WP 96-20095
Matched sets of Scots pine sapwood (Pinus sylvestris) L-joints were exposed above ground at two field sites for approximately five years. One site, at Garston, Watford, UK has a climate index between 60 and 65 while the other, close to Hilo, HI, USA has an index between 300 and 330. The joints were treated with a range of organic solvent treatments applied either by three minute dip immersion or b...
A F Preston, K J Archer, D M Roberts, J K Carey, A F Bravery


Performance of treated spruce in Canadian field test sites
1989 - IRG/WP 3506
Spruce material under test in Canadian field test sites is performing better than anticipated. From the comparison of the performance of spruce treated with various preservatives, it appears that penetration may be far more important on durability performance than the preservative itself or the retention of preservatives in the wood. However, there is still insufficient data on the influence of pe...
J P Hösli, E E Doyle


Calculation of preformance index of Bardac 20 (an alkylammonium compound) evaluated in a field stake test
1982 - IRG/WP 3206
Bardac 20 treated stakes have been in test for three years at the Westham Island test site near Vancouver, B.C. The Performance Index for the preservative was calculated and found to be 0.009 which infers that, at the standard retention, Bardac 20 added 0.9 y to the life of the stake. It may be concluded that when tested using a standard field stake test using ponderosa pine (Pinus ponderosa Laws)...
J N R Ruddick


A New Decay Hazard Map for North America Using the Scheffer Index
2008 - IRG/WP 08-10672
Wood decay experts in the USA and Canada use the Scheffer Index for above-ground wood decay potential to decide among design and treatment options to ensure the durability of wood construction. This paper provides an updated North American decay hazard map and includes data on Central America. Index values calculated from recent climate data are higher than published values due to directional or c...
P I Morris, J Wang


Decay Hazard Classifications in China for Exterior Above-Ground Wood
2007 - IRG/WP 07-20357
A decay hazard map for exterior above-ground wood structures is presented based on Scheffer’s Climate Index, with the major purpose of promoting awareness for proper protection of wood structures in different locations in China. A very large area in the South, including southern Yunnan, most of Sichuan Province and Chongqing, and part of Hunan, Hubei, Anhui, Jiangxi, and Zhejiang, as well as all...
J Wang, X Wu, M Jiang, P I Morris


To decay or not to decay: An accelerated field test of the validity of the Scheffer index
2008 - IRG/WP 08-20392
The Scheffer Index was introduced in 1971 to predict the relative decay hazard of untreated wood exposed above-ground. Precipitation and temperature parameters are used in the calculation. A higher Scheffer Index value implies a greater risk of decay. An accelerated 18-month study using seven field sites with Scheffer Indices ranging from 35 to 400 and two wood types (Populus tremuloides and Pi...
G M Larkin, P E Laks


Field testing in Colombia: Three years of evaluations and experiences
2008 - IRG/WP 08-20394
Two field test sites have been established in Colombia for the evaluation of fungal and termite resistance of treated wood. The combination of elevated temperature, high and stable humidity and high rainfall at the two test sites accelerates microbial and insect activity (Scheffer, 1971; Thornton et al, 1994; Freitag et al, 1995). Tests established include above ground termite tests, ground contac...
Y Cabrera, A Preston


Decay hazard mapping for Europe
2011 - IRG/WP 11-20463
In this study, two different dose-response models for above-ground decay as well as a model transferring macro climate data to wood climate data are presented. The models base on data from field trials, which had been conducted at 28 European test sites, and were used to calculate the relative risk for decay caused by climate variability in Europe. The two dose-response models give coherent result...
C Brischke, E Frühwald Hansson, D Kavurmaci, S Thelandersson


Development of decay hazard maps based on decay prediction models
2016 - IRG/WP 16-20588
Durability plays a very central role in timber engineering, especially when working with wood in use class 3 and above where the risk of decay is high. As one of the primary decay influencing factors, the external condition, i.e. the local climate, is often graded by some type of climate index value. Predominately, climate indices are based on a direct relationship between weather data and decay. ...
J Niklewski, E Frühwald Hansson, C Brischke, D Kavurmaci


Can CCA be substituted as reference preservative?
2018 - IRG/WP 18-20641
While field testing of wood protective formulations remains probably the best method to find out the effective preservative concentration, the use of chrome-copper arsenate (CCA) as reference becomes debatable due to environmental and legislative reasons. This emerges from the European standardization bodies who have discussed reference alternatives that can omit the use of CCA. The present debate...
N Terziev, M Jebrane, P Larsson Brelid, N Morsing, P-O Flaete, P Torniainen, J S Kim, G Daniel


Observed and projected changes in the climate based decay hazard of timber in the United Kingdom
2020 - IRG/WP 20-20665
The risk of microbiological attack on wood is determined by both material and climatic factors and indeed the hazard for a component is based on its intrinsic durability and the conditions in which it is used. The use of wood and organic materials in construction is increasing but ultimately all these materials will be susceptible to microbiological attack. The Scheffer Climate index applies clima...
S F Curling, G A Ormondroyd


Modelling decay rates of timber exposed above ground on four different continents
2020 - IRG/WP 20-20670
Durability performance data from an international decking trial were analysed to explore relationships with climate variables, particularly those related to temperature and rainfall. Matched decking samples of slash pine (Pinus elliottii) sapwood and heartwood, spotted gum (Corymbia citriodora), Norway spruce (Picea abies) and Scots pine sapwood (Pinus sylvestris) were exposed to the weather above...
L P Francis, J J Morrell, C Brischke, P B Van Niekerk, J Norton


Confocal laser scanning microscopy of a novel decay in preservative treated radiata pine in wet acidic soils
1997 - IRG/WP 97-10215
Light microscopy of radiata pine (Pinus radiata D. Don) field test stakes (20x20x500mm3) exposed in wet acidic (pH 3-4) soil for 12 - 24 months showed predominance of an unusual type of decay characte-rised by tunnelling attack of wood cell walls. After two years decay was moderate to severe in wood treated to ground contact CCA specifications and also equivalent retentions of creosote, and a numb...
R N Wakeling, Ying Xiao, A P Singh


Effect of acetylation on decay resistance of wood against brown-rot, white-rot and soft-rot fungi
1989 - IRG/WP 3540
Effect of acetylation on decay resistance of wood was investigated using wood blocks of Cryptomeria japonica, Pinus densiflora, Albizia falcata and Fagus crenata. Blocks were treated with uncatalyzed acetic anhydride for different lengths of time and exposed to Tyromyces palustris, Serpula lacrymans, Coriolus versicolor and unsterilized soil. The action of OH-radical on acetylated wood was also ex...
M Takahashi, Y Imamura, M Tanahashi


Questionnaire - Fungal decay types
1985 - IRG/WP 1265
T Nilsson


JWPA method for testing effectiveness of surface coatings with preservatives against decay fungi
1981 - IRG/WP 2164
In 1979 JWPA established a new method for testing effectiveness of surface coatings in accordance with practical use of preservative-treated lumber. Comparing the new testing method with JIS A 9302, a few new trials - size of wood specimen, weathering procedure, and decay-test procedure - are incorporated....
K Tsunoda


Utilization of curcumin for detection of presence of boron in wood
1982 - IRG/WP 3191
It has been shown that curcumin is not a reliable reagent for detecting boron in wood that has been attacked by fungi...
M-L Edlund


Co-operative studies on determining toxic values against wood-destroying Basidiomycetes: Progress report to May 1989
1989 - IRG/WP 2339
This document reports progress on the co-operative study between nine laboratories set up following the proposals contained in Document IRG/WP/2316. Results have been received from two laboratories. Toxic values data have been established successfully using the test fungus Coniophora puteana but problems have been encountered with the other test fungi....
A F Bravery, J K Carey


Monographic cards for wood-destroying fungi. [Fiches monographiques pour les champignons lignivores]
1970 - IRG/WP I 5B
C Jacquiot


On Donkioporia expansa (Desm.) Kotl. & Pouzar
1986 - IRG/WP 1285
Donkioporia expansa is found more often in houses than realised until now. Virulence tests according to EN 113 show not only an attack of oak, but also of other hardwoods and even soft-woods....
G Buchwald


Nondestructive Evaluation of Oriented Strand Board Exposed to Decay Fungi
2002 - IRG/WP 02-20243
Stress wave nondestructive evaluation (NDE) technologies are being used in our laboratory to evaluate the performance properties of engineered wood. These techniques have proven useful in the inspection of timber structures to locate internal voids and decayed or deteriorated areas in large timbers. But no information exists concerning NDE and important properties of wood composites exposed to dec...
B Illman, V W Yang, R J Ross, W J Nelson


Moisture content levels and decay of hemlock
1986 - IRG/WP 1287
As a model of decay conditions of wooden members in wooden houses, a decay test was set up in which samples of western hemlock (Tsuga heterophylla) under 4 moisture levels were examined. Each week the samples were weighed and if the weights indicated that their moisture contents were lower than the expected levels, distilled water was added. Every 8 weeks 3 samples from each condition were oven dr...
K Suzuki


Dimensional stability and decay resistance of hot-melt self-bonded particleboard by surface benzylated pine chips
1991 - IRG/WP 3652
Akamatsu (Pinus densiflora Sieb. et Zucc: Japanese red pine) particles were pretreated with 40% NaOH solution and benzylated with benzyl chloride, and the surface of particle was converted into meltable materials. Hot-melt self bonded particleboard having smooth and high glossiness surface was prepared by hot pressing at 150°C and 1.96 MPa without using any conventional adhesives. Dimensional sta...
M Kiguchi, K Yamamoto